6 resultados para Hard And Brittle Coating

em Digital Commons - Montana Tech


Relevância:

100.00% 100.00%

Publicador:

Resumo:

It is known that the electrical resistance of annealed metals is usually smaller than that of metals in their cold worked state. The curve showing the relation between electrical resistance and annealing temperature reaches a minimum; continued annealing at higher temperature produces an increase in the electrical resistance. In the case of alloys it has been noted that a second decrease occurs at higher annealing temperature. The following work corroborates the observance of previous investigations. The electrical resistance of cold worked copper, gold, nickel, and iron decreased with annealing and then increased, the minimum being around 300° C. or 400° C. Monel metal showed a minimum resistance followed by an increase which in turn was followed by a second decrease.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Many investigations have shown that the electrical resistance of soft annealed metals is usually smaller than that of metals in their hard, cold worked state. By annealing cold-worked metals, the electrical resistance decreases to a minimum and then increases upon continued annealing at higher temperatures. The work performed in this investigation upon silver, aluminum, copper, nickel, and soft steel corroborates this idea.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Many attempts have been made to improve iron and steel and their alloys by the addition of boron. The re­sults obtained were not encouraging for the reason that the amount of boron used, generally from 0.2 to 2.0 per cent is altogether too high. This percentage of boron ren­ders the product hard and brittle and of late the experiments with boron in this connection have been practically abandoned.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The object of casehardening is to produce articles of steel having a tough or ductile interior and a hard sur­face. Quenching produces a surface somewhat harder than the interior, but in order to obtain a high surface hard­ness, the percentage of alloying elements in the steel must be raised to such an extent that the core or central por­tion becomes hard and brittle also.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The original objective of this project was to determine the effect of varying current intensity and electrode coating composition upon the spatter losses and porosity of arc welds made by alternating current. This subject was suggested by the Welding Research Council of the Engineering Foundation, which is a clearing house for welding research in order to avoid du­plication of work.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The tin alloys of tellurium are extremely hard and have very great tensile strength. It was thought that the reduction of the rate of grain growth of tin with the addition of tellurium accompanied this hardening and strengthening and such way found to be true.