2 resultados para Rap

em Digital Commons - Michigan Tech


Relevância:

10.00% 10.00%

Publicador:

Resumo:

With the increasing importance of conserving natural resources and moving toward sustainable practices, the aging transportation infrastructure can benefit from these ideas by improving their existing recycling practices. When an asphalt pavement needs to be replaced, the existing pavement is removed and ground up. This ground material, known as reclaimed asphalt pavement (RAP), is then added into new asphalt roads. However, since RAP was exposed to years of ultraviolet degradation and environmental weathering, the material has aged and cannot be used as a direct substitute for aggregate and binder in new asphalt pavements. One material that holds potential for restoring the aged asphalt binder to a usable state is waste engine oil. This research aims to study the feasibility of using waste engine oil as a recycling agent to improve the recyclability of pavements containing RAP. Testing was conducted in three phases, asphalt binder testing, advanced asphalt binder testing, and laboratory mixture testing. Asphalt binder testing consisted of dynamic shear rheometer and rotational viscometer testing on both unaged and aged binders containing waste engine oil and reclaimed asphalt binder (RAB). Fourier Transform Infrared Spectroscopy (FTIR) testing was carried out to on the asphalt binders blended with RAB and waste engine oil compare the structural indices indicative of aging. Lastly, sample asphalt samples containing waste engine oil and RAP were subjected to rutting testing and tensile strength ratio testing. These tests lend evidence to support the claim that waste engine oil can be used as a rejuvenating agent to chemically restore asphalt pavements containing RAP. Waste engine oil can reduce the stiffness and improve the low temperature properties of asphalt binders blended with RAB. Waste engine oil can also soften asphalt pavements without having a detrimental effect on the moisture susceptibility.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Traditionally, asphalt mixtures were produced at high temperatures (between 150°C to 180°C) and therefore often referred to as Hot Mix Asphalt (HMA). Recently, a new technology named Warm Mix Asphalt (WMA) was developed in Europe that allows HMA to be produced at a lower temperature. Over years of research efforts, a few WMA technologies were introduced including the foaming method using Aspha-min® and Advera® WMA; organic additives such as Sasobit® and Asphaltan B®; and chemical packages such as Evotherm® and Cecabase RT®. Benefits were found when lower temperatures were used to produce asphalt mixtures, especially when it comes to environmental and energy savings. Even though WMA has shown promising results in energy savings and emission reduction, however, only limited studies and laboratory tests have been conducted to date. The objectives of this project are to 1) develop a mix design framework for WMA by evaluating its mechanical properties; 2) evaluate performance of WMA containing high percentages of recycled asphalt material; and 3) evaluate the moisture sensitivity in WMA. The test results show that most of the WMA has higher fatigue life and TSR which indicated WMA has better fatigue cracking and moisture damage resistant; however, the rutting potential of most of the WMA tested were higher than the control HMA. A recommended WMA mix design framework was developed as well. The WMA design framework was presented in this study to provide contractors, and government agencies successfully design WMA. Mixtures containing high RAP and RAS were studied as well and the overall results show that WMA technology allows the mixture containing high RAP content and RAS to be produced at lower temperature (up to 35°C lower) without significantly affect the performance of asphalt mixture in terms of rutting, fatigue and moisture susceptibility. Lastly, the study also found that by introducing the hydrated lime in the WMA, all mixtures modified by the hydrated lime passed the minimum requirement of 0.80. This indicated that, the moisture susceptibility of the WMA can be improved by adding the hydrated lime.