3 resultados para Fly Ash and Concrete Bricks, Mineralogy, Elemental Analysis, Crushing Strength

em Digital Commons - Michigan Tech


Relevância:

100.00% 100.00%

Publicador:

Resumo:

This dissertation established a standard foam index: the absolute foam index test. This test characterized a wide range of coal fly ash by the absolute volume of air-entraining admixture (AEA) necessary to produce a 15-second metastable foam in a coal fly ash-cement slurry in a specified time. The absolute foam index test was used to characterize fly ash samples having loss on ignition (LOI) values that ranged from 0.17 to 23.3 %wt. The absolute foam index characterized the fly ash samples by absolute volume of AEA, defined as the amount of undiluted AEA solution added to obtain a 15-minute endpoint signified by 15-second metastable foam. Results were compared from several foam index test time trials that used different initial test concentrations to reach termination at selected times. Based on the coefficient of variation (CV), a 15-minute endpoint, with limits of 12 to 18 minutes was chosen. Various initial test concentrations were used to accomplish consistent contact times and concentration gradients for the 15-minute test endpoint for the fly ash samples. A set of four standard concentrations for the absolute foam index test were defined by regression analyses and a procedure simplifying the test process. The set of standard concentrations for the absolute foam index test was determined by analyzing experimental results of 80 tests on coal fly ashes with loss on ignition (LOI) values ranging from 0.39 to 23.3 wt.%. A regression analysis informed selection of four concentrations (2, 6, 10, and 15 vol.% AEA) that are expected to accommodate fly ashes with 0.39 to 23.3 wt.% LOI, depending on the AEA type. Higher concentrations should be used for high-LOI fly ash when necessary. A procedure developed using these standard concentrations is expected to require only 1-3 trials to meet specified endpoint criteria for most fly ashes. The AEA solution concentration that achieved the metastable foam in the foam index test was compared to the AEA equilibrium concentration obtained from the direct adsorption isotherm test with the same fly ash. The results showed that the AEA concentration that satisfied the absolute foam index test was much less than the equilibrium concentration. This indicated that the absolute foam index test was not at or near equilibrium. Rather, it was a dynamic test where the time of the test played an important role in the results. Even though the absolute foam index was not an equilibrium condition, a correlation was made between the absolute foam index and adsorption isotherms. Equilibrium isotherm equations obtained from direct isotherm tests were used to calculate the equilibrium concentrations and capacities of fly ash from 0.17 to 10.5% LOI. The results showed that the calculated fly ash capacity was much less than capacities obtained from isotherm tests that were conducted with higher initial concentrations. This indicated that the absolute foam index was not equilibrium. Rather, the test is dynamic where the time of the test played an important role in the results. Even though the absolute foam index was not an equilibrium condition, a correlation was made between the absolute foam index and adsorption isotherms for fly ash of 0.17 to 10.5% LOI. Several batches of mortars were mixed for the same fly ash type increasing only the AEA concentration (dosage) in each subsequent batch. Mortar air test results for each batch showed for each increase in AEA concentration, air contents increased until a point where the next increase in AEA concentration resulted in no increase in air content. This was maximum air content that could be achieved by the particular mortar system; the system reached its air capacity at the saturation limit. This concentration of AEA was compared to the critical micelle concentration (CMC) for the AEA and the absolute foam index.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Compiler optimizations help to make code run faster at runtime. When the compilation is done before the program is run, compilation time is less of an issue, but how do on-the-fly compilation and optimization impact the overall runtime? If the compiler must compete with the running application for resources, the running application will take more time to complete. This paper investigates the impact of specific compiler optimizations on the overall runtime of an application. A foldover Plackett and Burman design is used to choose compiler optimizations that appear to contribute to shorter overall runtimes. These selected optimizations are compared with the default optimization levels in the Jikes RVM. This method selects optimizations that result in a shorter overall runtime than the default O0, O1, and O2 levels. This shows that careful selection of compiler optimizations can have a significant, positive impact on overall runtime.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The novel approach to carbon capture and storage (CCS) described in this dissertation is a significant departure from the conventional approach to CCS. The novel approach uses a sodium carbonate solution to first capture CO2 from post combustion flue gas streams. The captured CO2 is then reacted with an alkaline industrial waste material, at ambient conditions, to regenerate the carbonate solution and permanently store the CO2 in the form of an added value carbonate mineral. Conventional CCS makes use of a hazardous amine solution for CO2 capture, a costly thermal regeneration stage, and the underground storage of supercritical CO2. The objective of the present dissertation was to examine each individual stage (capture and storage) of the proposed approach to CCS. Study of the capture stage found that a 2% w/w sodium carbonate solution was optimal for CO2 absorption in the present system. The 2% solution yielded the best tradeoff between the CO2 absorption rate and the CO2 absorption capacity of the solutions tested. Examination of CO2 absorption in the presence of flue gas impurities (NOx and SOx) found that carbonate solutions possess a significant advantage over amine solutions, that they could be used for multi-pollutant capture. All the NOx and SOx fed to the carbonate solution was able to be captured. Optimization studies found that it was possible to increase the absorption rate of CO2 into the carbonate solution by adding a surfactant to the solution to chemically alter the gas bubble size. The absorption rate of CO2 was increased by as much as 14%. Three coal combustion fly ash materials were chosen as the alkaline industrial waste materials to study the storage CO2 and regeneration the absorbent. X-ray diffraction analysis on reacted fly ash samples confirmed that the captured CO2 reacts with the fly ash materials to form a carbonate mineral, specifically calcite. Studies found that after a five day reaction time, 75% utilization of the waste material for CO2 storage could be achieved, while regenerating the absorbent. The regenerated absorbent exhibited a nearly identical CO2 absorption capacity and CO2 absorption rate as a fresh Na2CO3 solution.