2 resultados para Lv comm
em Bucknell University Digital Commons - Pensilvania - USA
Resumo:
Altered pressure in the developing left ventricle (LV) results in altered morphology and tissue material properties. Mechanical stress and strain may play a role in the regulating process. This study showed that confocal microscopy, three-dimensional reconstruction, and finite element analysis can provide a detailed model of stress and strain in the trabeculated embryonic heart. The method was used to test the hypothesis that end-diastolic strains are normalized after altered loading of the LV during the stages of trabecular compaction and chamber formation. Stage-29 chick LVs subjected to pressure overload and underload at stage 21 were reconstructed with full trabecular morphology from confocal images and analyzed with finite element techniques. Measured material properties and intraventricular pressures were specified in the models. The results show volume-weighted end-diastolic von Mises stress and strain averaging 50–82% higher in the trabecular tissue than in the compact wall. The volume-weighted-average stresses for the entire LV were 115, 64, and 147Pa in control, underloaded, and overloaded models, while strains were 11, 7, and 4%; thus, neither was normalized in a volume-weighted sense. Localized epicardial strains at mid-longitudinal level were similar among the three groups and to strains measured from high-resolution ultrasound images. Sensitivity analysis showed changes in material properties are more significant than changes in geometry in the overloaded strain adaptation, although resulting stress was similar in both types of adaptation. These results emphasize the importance of appropriate metrics and the role of trabecular tissue in evaluating the evolution of stress and strain in relation to pressure-induced adaptation.
Resumo:
There are two main types of bone in the human body, trabecular and cortical bone. Cortical bone is primarily found on the outer surface of most bones in the body while trabecular bone is found in vertebrae and at the end of long bones (Ross 2007). Osteoporosis is a condition that compromises the structural integrity of trabecular bone, greatly reducing the ability of the bone to absorb energy from falls. The current method for diagnosing osteoporosis and predicting fracture risk is measurement of bone mineral density. Limitations of this method include dependence on the bone density measurement device and dependence on type of test and measurement location (Rubin 2005). Each year there are approximately 250,000 hip fractures in the United States due to osteoporosis (Kleerekoper 2006). Currently, the most common method for repairing a hip fracture is a hip fixation surgery. During surgery, a temporary guide wire is inserted to guide the permanent screw into place and then removed. It is believed that directly measuring this screw pullout force may result in a better assessment of bone quality than current indirect measurement techniques (T. Bowen 2008-2010, pers. comm.). The objective of this project is to design a device that can measure the force required to extract this guide wire. It is believed that this would give the surgeon a direct, quantitative measurement of bone quality at the site of the fixation. A first generation device was designed by a Bucknell Biomedical Engineering Senior Design team during the 2008- 2009 Academic Year. The first step of this project was to examine the device, conduct a thorough design analysis, and brainstorm new concepts. The concept selected uses a translational screw to extract the guide wire. The device was fabricated and underwent validation testing to ensure that the device was functional and met the required engineering specifications. Two tests were conducted, one to test the functionality of the device by testing if the device gave repeatable results, and the other to test the sensitivity of the device to misalignment. Guide wires were extracted from 3 materials, low density polyethylene, ultra high molecular weight polyethylene, and polypropylene and the force of extraction was measured. During testing, it was discovered that the spring in the device did not have a high enough spring constant to reach the high forces necessary for extracting the wires without excessive deflection of the spring. The test procedure was modified slightly so the wires were not fully threaded into the material. The testing results indicate that there is significant variation in the screw pullout force, up to 30% of the average value. This significant variation was attributed to problems in the testing and data collection, and a revised set of tests was proposed to better evaluate the performance of the device. The fabricated device is a fully-functioning prototype and further refinements and testing of the device may lead to a 3rd generation version capable of measuring the screw pullout force during hip fixation surgery.