9 resultados para Wear of materials

em BORIS: Bern Open Repository and Information System - Berna - Suiça


Relevância:

100.00% 100.00%

Publicador:

Resumo:

PURPOSE: To investigate the effect of curing rate on softening in ethanol, degree of conversion, and wear of resin composites. METHOD: With a given energy density and for each of two different light-curing units (QTH or LED), the curing rate was reduced by modulating the curing mode. Thus, the irradiation of resin composite specimens (Filtek Z250, Tetric Ceram, Esthet-X) was performed in a continuous curing mode and in a pulse-delay curing mode. Wallace hardness was used to determine the softening of resin composite after storage in ethanol. Degree of conversion was determined by infrared spectroscopy (FTIR). Wear was assessed by a three-body test. Data were submitted to Levene's test, one and three-way ANOVA, and Tukey HSD test (alpha = 0.05). Results: Immersion in ethanol, curing mode, and material all had significant effects on Wallace hardness. After ethanol storage, resin composites exposed to the pulse-delay curing mode were softer than resin composites exposed to continuous cure (P< 0.0001). Tetric Ceram was the softest material followed by Esthet-X and Filtek Z250 (P< 0.001). Only the restorative material had a significant effect on degree of conversion (P< 0.001): Esthet-X had the lowest degree of conversion followed by Filtek Z250 and Tetric Ceram. Curing mode (P= 0.007) and material (P< 0.001) had significant effect on wear. Higher wear resulted from the pulse-delay curing mode when compared to continuous curing, and Filtek Z250 showed the lowest wear followed by Esthet-X and Tetric Ceram.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The wear of telescopic crowns is a common problem often reducing the patient's satisfaction with the denture and resulting in a renewal of the denture. The study aims to compare the wear behavior of conical crowns using electroplated copings (group E ) with standard telescopic crowns with cast female parts (group C).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Wear of attachments leads to a loss of retention and reduces the function of overdentures. This study evaluated the retention force changes of an attachment system for overdentures. The influence of the lubricant and the alloy on wear constancy was examined.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The first part of this three-part review on the relevance of laboratory testing of composites and adhesives deals with approval requirements for composite materials. We compare the in vivo and in vitro literature data and discuss the relevance of in vitro analyses. The standardized ISO protocols are presented, with a focus on the evaluation of physical parameters. These tests all have a standardized protocol that describes the entire test set-up. The tests analyse flexural strength, depth of cure, susceptibility to ambient light, color stability, water sorption and solubility, and radiopacity. Some tests have a clinical correlation. A high flexural strength, for instance, decreases the risk of fractures of the marginal ridge in posterior restorations and incisal edge build-ups of restored anterior teeth. Other tests do not have a clinical correlation or the threshold values are too low, which results in an approval of materials that show inferior clinical properties (e.g., radiopacity). It is advantageous to know the test set-ups and the ideal threshold values to correctly interpret the material data. Overall, however, laboratory assessment alone cannot ensure the clinical success of a product.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ABSTRACT: BACKGROUND: Fine particulate matter originating from traffic correlates with increased morbidity and mortality. An important source of traffic particles is brake wear of cars which contributes up to 20% of the total traffic emissions. The aim of this study was to evaluate potential toxicological effects of human epithelial lung cells exposed to freshly generated brake wear particles. RESULTS: An exposure box was mounted around a car's braking system. Lung cells cultured at the air-liquid interface were then exposed to particles emitted from two typical braking behaviours ("full stop" and "normal deceleration"). The particle size distribution as well as the brake emission components like metals and carbons was measured on-line, and the particles deposited on grids for transmission electron microscopy were counted. The tight junction arrangement was observed by laser scanning microscopy. Cellular responses were assessed by measurement of lactate dehydrogenase (cytotoxicity), by investigating the production of reactive oxidative species and the release of the pro-inflammatory mediator interleukin-8. The tight junction protein occludin density decreased significantly (p < 0.05) with increasing concentrations of metals on the particles (iron, copper and manganese, which were all strongly correlated with each other). Occludin was also negatively correlated with the intensity of reactive oxidative species. The concentrations of interleukin-8 were significantly correlated with increasing organic carbon concentrations. No correlation was observed between occludin and interleukin-8, nor between reactive oxidative species and interleukin-8. CONCLUSION: These findings suggest that the metals on brake wear particles damage tight junctions with a mechanism involving oxidative stress. Brake wear particles also increase pro-inflammatory responses. However, this might be due to another mechanism than via oxidative stress.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The two small asteroid-like bodies orbiting Mars, Phobos and Deimos, are low albedo and exhibit similar visible to near-infrared spectra. Determining the origin of these moons is closely tied to determining their composition. From available spectroscopic data Phobos exhibits two distinct types of materials across its surface, and data from both Mars Express and Mars Reconnaissance Orbiter have provided additional details about the properties of these materials and their spatial relation to one another. Although no prominent diagnostic absorptions have been detected, systematic weak features are seen in some data. An extensive regolith is observed to have developed on both moons with characteristics that may be unique due to their special environment in Mars orbit. Understanding the character and evolution of the regolith of Phobos and Deimos is central to interpreting the moons׳ physical and optical properties. The cumulative data available for compositional analyses across the surface of Phobos and Deimos, however, remain incomplete in scope and character and ambiguous in interpretation. Consequently the composition of the moons of Mars remains uncertain.