Resumo:
This in vitro study evaluated the performance of three ceramic and two commonly used polishing methods on two CAD/CAM ceramics. Surface roughness and quality were compared. A glazed group (GLGR) of each ceramic material served as reference. One-hundred and twenty specimens of VITABLOCS Mark II (VITA) and 120 specimens of IPS Empress CAD (IPS) were roughened in a standardized manner. Twenty VITA and 20 IPS specimens were glazed (VITA Akzent Glaze/Empress Universal Glaze). Five polishing methods were investigated (n=20/group): 1) EVE Diacera W11DC-Set (EVE), 2) JOTA 9812-Set (JOTA), 3) OptraFine-System (OFI), 4) Sof-Lex 2382 discs (SOF) and 5) Brownie/Greenie/Occlubrush (BGO). Polishing quality was measured with a surface roughness meter (Ra and Rz values). The significance level was set at alpha=0.05. Kruskal Wallis tests and pairwise Wilcoxon rank sum tests with Bonferroni-Holm adjustment were used. Qualitative surface evaluation of representative specimens was done with SEM. On VITA ceramics, SOF produced lower Ra (p<0.00001) but higher Rz values than GLGR (p=0.003); EVE, JOTA, OFI and BGO yielded significantly higher Ra and Rz values than GLGR. On IPS ceramics, SOF and JOTA exhibited lower Ra values than GLGR (p<0.0001). Equivalent Ra but significantly higher Rz values occurred between GLGR and EVE, OFI or BGO. VITA and IPS exhibited the smoothest surfaces when polished with SOF. Nevertheless, ceramic polishing systems are still of interest to clinicians using CAD/CAM, as these methods are universally applicable and showed an increased durability compared to the investigated silicon polishers.
Resumo:
SUMMARY The aim of this study was to evaluate the influence of surface roughness on surface hardness (Vickers; VHN), elastic modulus (EM), and flexural strength (FLS) of two computer-aided design/computer-aided manufacturing (CAD/CAM) ceramic materials. One hundred sixty-two samples of VITABLOCS Mark II (VMII) and 162 samples of IPS Empress CAD (IPS) were ground according to six standardized protocols producing decreasing surface roughnesses (n=27/group): grinding with 1) silicon carbide (SiC) paper #80, 2) SiC paper #120, 3) SiC paper #220, 4) SiC paper #320, 5) SiC paper #500, and 6) SiC paper #1000. Surface roughness (Ra/Rz) was measured with a surface roughness meter, VHN and EM with a hardness indentation device, and FLS with a three-point bending test. To test for a correlation between surface roughness (Ra/Rz) and VHN, EM, or FLS, Spearman rank correlation coefficients were calculated. The decrease in surface roughness led to an increase in VHN from (VMII/IPS; medians) 263.7/256.5 VHN to 646.8/601.5 VHN, an increase in EM from 45.4/41.0 GPa to 66.8/58.4 GPa, and an increase in FLS from 49.5/44.3 MPa to 73.0/97.2 MPa. For both ceramic materials, Spearman rank correlation coefficients showed a strong negative correlation between surface roughness (Ra/Rz) and VHN or EM and a moderate negative correlation between Ra/Rz and FLS. In conclusion, a decrease in surface roughness generally improved the mechanical properties of the CAD/CAM ceramic materials tested. However, FLS was less influenced by surface roughness than expected.
Resumo:
OBJECTIVES: The objective of the study was to evaluate the efficacy of an additional usage of a diamond-coated curette on surface roughness, adhesion of periodontal ligament (PDL) fibroblasts, and of Streptococcus gordonii in vitro. MATERIALS AND METHODS: Test specimens were prepared from extracted teeth and exposed to instrumentation with conventional Gracey curettes with or without additional use of diamond-coated curettes. Surface roughness (Ra and Rz) was measured before and following treatment. In addition, the adhesion of PDL fibroblasts for 72 h and adhesion of S. gordonii ATCC 10558 for 2 h have been determined. RESULTS: Instrumentation with conventional Gracey curettes reduced surface roughness (median Ra before: 0.36 μm/after: 0.25 μm; p < 0.001; median Rz before: 2.34 μm/after: 1.61 μm; p < 0.001). The subsequent instrumentation with the diamond-coated curettes resulted in a median Ra of 0.31 μm/Rz of 2.06 μm (no significance in comparison to controls). The number of attached PDL fibroblasts did not change following scaling with Gracey curettes. The additional instrumentation with the diamond-coated curettes resulted in a two-fold increase in the number of attached PDL fibroblasts but not in the numbers of adhered bacteria. CONCLUSIONS: Treatment of root surfaces with conventional Gracey curettes followed by subsequent polishing with diamond-coated curettes may result in a root surface which provides favorable conditions for the attachment of PDL fibroblasts without enhancing microbial adhesion. CLINICAL RELEVANCE: The improved attachment of PDL fibroblasts and the limited microbial adhesion on root surfaces treated with scaling with conventional Gracey curettes followed by subsequent polishing with diamond-coated curettes may favor periodontal wound healing.
Resumo:
CONTEXT: A polymorphism of the GH receptor (GHR) gene resulting in genomic deletion of exon 3 (GHR-d3) has been associated with responsiveness to GH therapy. However, the data reported so far do vary according to the underlying condition, replacement dose, and duration of the treatment. OBJECTIVE, DESIGN: The aim of this study was to analyze the impact of the GHR genotypes in terms of the initial height velocity (HV) resulting from treatment and the impact upon adult height in patients suffering from severe isolated GH deficiency. CONTROLS, PATIENTS, SETTING: A total of 181 subjects (peak stimulated GH
Resumo:
Susceptibility of different restorative materials to toothbrush abrasion and coffee staining Objective: The aim of this study was to evaluate the susceptibility of different restorative materials to surface alterations after an aging simulation. Methods: Specimens (n=15 per material) of five different restorative materials (CER: ceramic/Vita Mark II; EMP: composite/Empress Direct; LAV: CAD/CAM composite/Lava Ultimate; COM: prefabricated composite/Componeer; VEN: prefabricated composite/Venear) were produced. Whereas CER was glazed, EMP and LAV were polished with silicon polishers, and COM and VEN were left untreated. Mean roughness (Ra and Rz) and colorimetric parameters (L*a*b*), expressed as colour change (E), were measured. The specimens underwent an artificial aging procedure. After baseline measurements (M1), the specimens were successively immersed for 24 hours in coffee (M2), abraded in a toothbrushing simulator (M3), immersed in coffee (M4), abraded (M5) and repeatedly abraded (M6). After each aging procedure (M2-M6), surface roughness and colorimetric parameters were recorded. Differences between the materials regarding Ra/Rz and E were analysed with a nonparametric ANOVA analysis. The level of significance was set at α=0.05. Results: The lowest roughness values were obtained for CER. A significant increase in Ra was detected for EMP, COM and VEN compared to CER. The Ra/Rz values were found to be highly significantly different for the materials and measuring times (M) (p<0.0001). Regarding E most alterations were found for EMP and COM, whereas CER and LAV remained mostly stable. The E values were significantly different for the materials and M (p<0.0001). Conclusion: The ceramic and the CAD/CAM composite were the most stable materials with regard to roughness and colour change and the only materials that resulted in Ra values below 0.2 μm (the clinically relevant threshold). Venears and Componeers were more inert than the direct composite material and thus might be an alternative for extensive restorations in the aesthetic zone.
Resumo:
BACKGROUND AND AIM There is a lack of suitable in vitro models to evaluate various treatment modalities intending to remove subgingival bacterial biofilm. Consequently, the aims of this in vitro-study were: a) to establish a pocket model enabling mechanical removal of biofilm and b) to evaluate repeated non-surgical periodontal treatment with respect to biofilm removal and reformation, surface alterations, tooth hard-substance-loss, and attachment of periodontal ligament (PDL) fibroblasts. MATERIAL AND METHODS Standardized human dentin specimens were colonized by multi-species biofilms for 3.5 days and subsequently placed into artificially created pockets. Non-surgical periodontal treatment was performed as follows: a) hand-instrumentation with curettes (CUR), b) ultrasonication (US), c) subgingival air-polishing using erythritol (EAP) and d) subgingival air-polishing using erythritol combined with chlorhexidine digluconate (EAP-CHX). The reduction and recolonization of bacterial counts, surface roughness (Ra and Rz), the caused tooth substance-loss (thickness) as well as the attachment of PDL fibroblasts were evaluated and statistically analyzed by means of ANOVA with Post-Hoc LSD. RESULTS After 5 treatments, bacterial reduction in biofilms was highest when applying EAP-CHX (4 log10). The lowest reduction was found after CUR (2 log10). Additionally, substance-loss was the highest when using CUR (128±40 µm) in comparison with US (14±12 µm), EAP (6±7 µm) and EAP-CHX (11±10) µm). Surface was roughened when using CUR and US. Surfaces exposed to US and to EAP attracted the highest numbers of PDL fibroblasts. CONCLUSION The established biofilm model simulating a periodontal pocket combined with interchangeable placements of test specimens with multi-species biofilms enables the evaluation of different non-surgical treatment modalities on biofilm removal and surface alterations. Compared to hand instrumentation the application of ultrasonication and of air-polishing with erythritol prevents from substance-loss and results in a smooth surface with nearly no residual biofilm that promotes the reattachment of PDL fibroblasts.
Resumo:
DNAzymes (Dz) 8–17 and 10–23 are two widely studied and well-characterized RNA-cleaving DNA catalysts. In an effort to further improve the understanding of the fragile interactions and dynamics of the enzymatic mechanism, this study examines the catalytic efficiency of minimally modified DNAzymes. Five single mutants of Dz8–17 and Dz10–23 were prepared by replacing the adenine residues in the corresponding catalytic cores with 3-deazaadenine units. Kinetic assays were used to assess the effect on the catalytic activity and thereby identify the importance of hydrogen bonding that arises from the N3 atoms. The results suggest that modifications at A15 and A15.0 of Dz8–17 have a significant influence and show a reduction in catalytic activity. Modification at each location in Dz10–23 results in a decrease of the observed rate constants, with A12 appearing to be the most affected with a reduction of ∼80% of kobs and ∼25% of the maximal cleavage rate compared to the wild-type DNAzyme. On the other hand, modification of A12 in Dz8–17 showed an ∼130% increase in kobs, thus unraveling a new potential site for the introduction of chemical modifications. A pH-profile analysis showed that the chemical cleavage step is rate-determining, regardless of the presence and/or location of the mutation. These findings point towards the importance of the N3-nitrogens of certain adenine nucleotides located within the catalytic cores of the DNAzymes for efficient catalytic activity and further suggest that they might directly partake in maintaining the appropriate tertiary structure. Therefore, it appears that minor groove interactions constitute an important feature of DNAzymes as well as ribozymes.
Resumo:
Zielsetzung: Das Ziel dieser Studie war, den Einfluss von drei Politursystemen auf die Oberflächenrauigkeit von verschiedenen Materialien für computer-aided design/computer-aided manufacturing (CAD/CAM) Restaurationen mittels Profilometrie sowie die mikromechanischen Eigenschaften der Materialien mittels Mikrohärtemessgerät zu analysieren. Materialien und Methoden: Von dem CAD/CAM-Kompositmaterial Paradigm MZ100 (3M ESPE), der CAD/CAM-Feldspatkeramik VITABLOCS Mark II (VITA Zahnfabrik) und den CAD/CAM-Hybridmaterialien Lava Ultimate (3M ESPE), VITA ENAMIC (VITA Zahnfabrik) und AMBARINO High-Class (Creamed) wurden je 60 Prüfkörper zugeschnitten, gekennzeichnet und standardisiert aufgerauht. Die standardisierte Aufrauhung wurde mit Baseline-Rauigkeitsmessungen überprüft (Ra und Rz; µm). Die Prüfkörper wurden mit einem von drei Politursystemen poliert (n=20 pro CAD/CAM-Material): 1) Sof-Lex Scheiben (Disc-System, 3 Politurschritte: medium, fein und superfein; 3M ESPE), 2) VITA Polishing Set Clinical (Silikonpolitursystem, 2 Politurschritte: medium und fein; VITA Zahnfabrik) oder 3) KENDA Nobilis (Silikonpolierer, 1 Politurschritt (universal); KENDA Dental). Nach Politur der Prüfkörper wurden Ra und Rz sowie die mikromechanischen Eigenschaften Oberflächenhärte (VHN; Vickers Härte) und Elastizitätsmodul (EM; GPa) gemessen. In den darauf folgenden sechs Monaten wurden die Prüfkörper in Leitungswasser gelagert und insgesamt sechs Mal einem maschinellem Zahnbürsten zugeführt. Anschliessend wurden erneut Ra und Rz sowie VHN und EM gemessen. Ra-, Rz-, VHN- und EM-Werte wurden mittels nichtparametrischer ANOVA global analysiert und die p-Werte mittels Bonferroni-Holm Korrektur für multiples Testen korrigiert. Als post-hoc Tests wurden Kruskal-Wallis-Tests sowie exakte Wilcoxon Rangsummen-Tests verwendet und die p-Werte wurden nicht korrigiert. Das Signifikanzniveau wurde auf α=0,05 festgelegt. Resultate: Für alle drei CAD/CAM-Hybridmaterialien ergaben Sof-Lex Scheiben nach der Politur die tiefste Oberflächenrauigkeit (d. h. die tiefsten Ra- und Rz-Werte), gefolgt von KENDA Nobilis und von dem VITA Polishing Set Clinical. Bei dem CAD/CAM-Kompositmaterial sowie bei der CAD/CAM-Feldspatkeramik ergaben Sof-Lex Scheiben und KENDA Nobilis ähnliche Resultate, gefolgt von dem VITA Polishing Set Clinical. Bei einigen CAD/CAM-Materialien zeigten sich – zum Teil in Abhängigkeit des Politursystems – nach maschinellem Zahnbürsten und Lagerung signifikant höhere Ra- und Rz-Werte. Die CAD/CAM-Materialien zeigten unabhängig des Politursystems und der Lagerung signifikant verschiedene VHN- und EM-Werte. Bei einigen CAD/CAM-Materialien zeigten sich – zum Teil ebenfalls in Abhängigkeit des Politursystems – nach maschinellem Zahn-bürsten und Lagerung signifikant tiefere VHN- und EM-Werte. Schlussfolgerungen: Die Wahl des Politursystems beeinflusste die Oberflächenrauigkeit der CAD/CAM-Materialien markant, wobei Sof-Lex Scheiben insgesamt die besten Politurresultate zeigten, gefolgt von dem Silikonpolierer KENDA Nobilis. Von der Verwendung des Silikonpolitursystems VITA Polishing Set Clinical muss eher abgeraten werden. Das CAD/CAM-Kompositmaterial Paradigm MZ100 und die CAD/CAM-Hybridmaterialien Lava Ultimate und AMBARINO High-Class als weichere und elastischere Materialien liessen sich insgesamt besser polieren, waren aber bezüglich mechanischer Eigenschaften anfälliger auf Lagerung als die härtere CAD/CAM-Feldspatkeramik VITABLOCS Mark II und das CAD/CAM-Hybridmaterial VITA ENAMIC.