56 resultados para Step etching
Resumo:
Major blood stage antimalarial drugs like chloroquine and artemisinin target the heme detoxification process of the malaria parasite. Hemozoin formation reactions in vitro using the Plasmodium falciparum histidine-rich protein-2 (Pfhrp-2), lipids, and auto-catalysis are slow and could not explain the speed of detoxification needed for parasite survival. Here, we show that malarial hemozoin formation is a coordinated two component process involving both lipids and histidine-rich proteins. Hemozoin formation efficiency in vitro is 1-2% with Pfhrp-2 and 0.25-0.5% with lipids. We added lipids after 9h in a 12h Pfhrp-2 mediated reaction that resulted in sixfold increase in hemozoin formation. However, a lipid mediated reaction in which Pfhrp-2 was added after 9h produced only twofold increase in hemozoin production compared to the reaction with Pfhrp-2 alone. Synthetic peptides corresponding to the Pfhrp-2 heme binding sequences, based on repeats of AHHAAD, neither alone nor in combination with lipids were able to generate hemozoin in vitro. These results indicate that hemozoin formation in malaria parasite involves both the lipids and the scaffolding proteins. Histidine-rich proteins might facilitate hemozoin formation by binding with a large number of heme molecules, and facilitating the dimer formation involving iron-carboxylate bond between two heme molecules, and lipids may then subsequently assist the mechanism of long chain formation, held together by hydrogen bonds or through extensive networking of hydrogen bonds.
Resumo:
PURPOSE To evaluate the bonding of simplified adhesive systems to sound and caries-affected dentin of primary teeth with microtensile (µTBS) and nanoleakage (NL) tests. MATERIALS AND METHODS Occlusal cavities were prepared in 36 sound second primary molars. Half of the specimens were submitted to pH cycling to simulate caries-affected dentin. Teeth were randomly restored with one of three materials: the etch-and-rinse adhesive system Adper Single Bond 2 (SB), the two-step self-etching adhesive system Adper SE Plus (SE), and the one-step self-etching adhesive system Adper Easy One (EASY). After storage for 24 h, specimens with cross-sectional areas of 0.8 mm2 were prepared for microtensile testing (1 mm/min). One stick from each tooth was immersed in silver nitrate solution (24 h) and allowed to develop for 8 h in order to score the nano leakage with SEM. The fracture pattern was evaluated using a stereomicroscope (400X). The µTBS means were analyzed by two-way ANOVA and Tukey's post-hoc test. For NL, the Kruskal- Wallis and Mann-Whitney tests were used (α < 0.05). RESULTS SB (35.5 ± 3.5) showed the highest µTBS value to sound dentin, followed by EASY (26.3 ± 1.9) and SE (18.2 ± 6.5) (p < 0.05). No difference among materials was observed for caries-affected dentin (SB: 17.8 ± 4.2; SE: 13.9 ± 3.2; EASY: 14.4 ± 4.2, p > 0.05). For all groups, adhesive/mixed fracture prevailed. Caries affected dentin promoted silver nitrate uptake into the adhesive interface; however, with SE, the nano leakage was more pronounced than in the other adhesive systems, even in sound dentin. CONCLUSION Caries-affected dentin negatively influences the bond strength and nano leakage of the two-step etch-and-rinse and one-step self-etching adhesive systems tested in primary teeth.
Resumo:
BACKGROUND: Zirconia (ZrO2 ) has received interest as a dental material; however, little information is available on the impact of surface modifications on the osseointegration of zirconia implants. PURPOSE: The aim of the present study was to determine the effect of acid or alkaline etching of sandblasted ZrO2 implants on bone apposition in vivo. METHODS: Cylindrical ZrO2 implants with two circumferential grooves were placed in the maxilla of 12 miniature pigs. Biopsies were harvested after 1, 2, 4, and 8 weeks of healing. Undecalcified toluidine blue-stained ground sections were produced. The bone-to-implant contact, the bone area, and the presence of multinucleated giant cells were determined by histomorphometry. An uncorrected explorative statistical analysis was performed. RESULTS: Acid etching but not alkaline etching of sandblasted ZrO2 implants caused more bone-to-implant contact than sandblasted ZrO2 implants. The bone area was unaffected by the surface modifications. Acid and alkaline etching both increased the formation of multinucleated giant cells at the implant surface. CONCLUSIONS: This study provides a scientific basis to further investigate the impact of acid etching of sandblasted ZrO2 implants on osseointegration and the role of multinucleated giant cells in this process.