28 resultados para Hydrophobic silica
Resumo:
Abstract We demonstrate the use of Fourier transform infrared spectroscopy (FTIRS) to make quantitative measures of total organic carbon (TOC), total inorganic carbon (TIC) and biogenic silica (BSi) concentrations in sediment. FTIRS is a fast and costeffective technique and only small sediment samples are needed (0.01 g). Statistically significant models were developed using sediment samples from northern Sweden and were applied to sediment records from Sweden, northeast Siberia and Macedonia. The correlation between FTIRS-inferred values and amounts of biogeochemical constituents assessed conventionally varied between r = 0.84–0.99 for TOC, r = 0.85– 0.99 for TIC, and r = 0.68–0.94 for BSi. Because FTIR spectra contain information on a large number of both inorganic and organic components, there is great potential for FTIRS to become an important tool in paleolimnology.
Resumo:
The uptake of silica (Si) and gold (Au) nanoparticles (NPs) engineered for laser-tissue soldering in the brain was investigated using microglial cells and undifferentiated and differentiated SH-SY5Y cells. It is not known what effects NPs elicit once entering the brain. Cellular uptake, cytotoxicity, apoptosis, and the potential induction of oxidative stress by means of depletion of glutathione levels were determined after NP exposure at concentrations of 10(3) and 10(9)NPs/ml. Au-, silica poly (ε-caprolactone) (Si-PCL-) and silica poly-L-lactide (Si-PLLA)-NPs were taken up by all cells investigated. Aggregates and single NPs were found in membrane-surrounded vacuoles and the cytoplasm, but not in the nucleus. Both NP concentrations investigated did not result in cytotoxicity or apoptosis, but reduced glutathione (GSH) levels predominantly at 6 and 24h, but not after 12 h of NP exposure in the microglial cells. NP exposure-induced GSH depletion was concentration-dependent in both cell lines. Si-PCL-NPs induced the strongest effect of GSH depletion followed by Si-PLLA-NPs and Au-NPs. NP size seems to be an important characteristic for this effect. Overall, Au-NPs are most promising for laser-assisted vascular soldering in the brain. Further studies are necessary to further evaluate possible effects of these NPs in neuronal cells.
Resumo:
We present an independent calibration model for the determination of biogenic silica (BSi) in sediments, developed from analysis of synthetic sediment mixtures and application of Fourier transform infrared spectroscopy (FTIRS) and partial least squares regression (PLSR) modeling. In contrast to current FTIRS applications for quantifying BSi, this new calibration is independent from conventional wet-chemical techniques and their associated measurement uncertainties. This approach also removes the need for developing internal calibrations between the two methods for individual sediments records. For the independent calibration, we produced six series of different synthetic sediment mixtures using two purified diatom extracts, with one extract mixed with quartz sand, calcite, 60/40 quartz/calcite and two different natural sediments, and a second extract mixed with one of the natural sediments. A total of 306 samples—51 samples per series—yielded BSi contents ranging from 0 to 100 %. The resulting PLSR calibration model between the FTIR spectral information and the defined BSi concentration of the synthetic sediment mixtures exhibits a strong cross-validated correlation ( R2cv = 0.97) and a low root-mean square error of cross-validation (RMSECV = 4.7 %). Application of the independent calibration to natural lacustrine and marine sediments yields robust BSi reconstructions. At present, the synthetic mixtures do not include the variation in organic matter that occurs in natural samples, which may explain the somewhat lower prediction accuracy of the calibration model for organic-rich samples.
Resumo:
The aim of this study was to evaluate in humans the amount of new bone after sinus floor elevation with a synthetic bone substitute material consisting of nanocrystalline hydroxyapatite embedded in a highly porous silica gel matrix. The lateral approach was applied in eight patients requiring sinus floor elevation to place dental implants. After elevation of the sinus membrane, the cavities were filled with 0.6-mm granules of nanocrystalline hydroxyapatite mixed with the patient's blood. A collagen membrane (group 1) or a platelet-rich fibrin (PRF) membrane (group 2) was placed over the bony window. After healing periods between 7 and 11 months (in one case after 24 months), 16 biopsy specimens were harvested with a trephine bur during implant bed preparation. The percentage of new bone, residual filler material, and soft tissue was determined histomorphometrically. Four specimens were excluded from the analysis because of incomplete biopsy removal. In all other specimens, new bone was observed in the augmented region. For group 1, the amount of new bone, residual graft material, and soft tissue was 28.7% ± 5.4%, 25.5% ± 7.6%, and 45.8% ± 3.2%, respectively. For group 2, the values were 28.6% ± 6.90%, 25.7% ± 8.8%, and 45.7% ± 9.3%, respectively. All differences between groups 1 and 2 were not statistically significant. The lowest and highest values of new bone were 21.2% and 34.1% for group 1 and 17.4% and 37.8% for group 2, respectively. The amount of new bone after the use of nanocrystalline hydroxyapatite for sinus floor elevation in humans is comparable to values found in the literature for other synthetic or xenogeneic bone substitute materials. There was no additional beneficial effect of the PRF membrane over the non-cross-linked collagen membrane.
Resumo:
OBJECTIVE The first objective of this pilot study was to evaluate the impact of the hydrophilicity on the early phases of osseointegration. The second objective was to compare two hydrophilic implant surfaces with different geometries, surface roughness, and technologies achieving hydrophilicity. MATERIAL AND METHODS Twelve weeks after extraction, all four quadrants of nine minipigs received three dental implants, alternating between hydrophilic microrough surfaces (INICELL and SLActive) and a conventional hydrophobic microrough surface. After 5, 10, and 15 days of submerged healing, ground sections were prepared and subjected to histologic and histomorphometric analysis. RESULTS The histologic analysis revealed a similar healing pattern among the hydrophilic and hydrophobic implant surfaces, with extensive bone formation occurring between day 5 and day 10. With BIC values of greater than 50% after 10 days, all examined surfaces indicated favorable osseointegration at this very early point in healing. At day 15, the mean new bone-to-implant contact (newBIC) of one hydrophilic surface (INICELL; 55.8 ± 14.4%) was slightly greater than that of the hydrophobic microrough surface (40.6 ± 20.2%). At day 10 and day 15, an overall of 21% of the implants had to be excluded from analysis due to inflammations primarily caused by surgical complications. CONCLUSION Substantial bone apposition occurs between day 5 and day 10. The data suggest that the hydrophilic surface can provoke a slight tendency toward increased bone apposition in minipigs after 15 days. A direct comparison of two hydrophilic surfaces with varying geometries is of limited relevance.
Resumo:
No Abstract
Resumo:
A set of optimized deposition conditions for the inner wall coating of fused silica tubes with amorphous selenium was elaborated. The method is based on the vapor transport deposition of pure elemental selenium on a cooled substrate held at liquid nitrogen temperatures. Morphological and structural examination of the deposited layer was performed by optical microscopy and X-ray diffraction studies. Neutron activated selenium was used to monitor the deposition pattern and its stability under high gas flows. Monte Carlo simulations allowed the estimation of the different Se species composing the amorphous phase, at the given experimental deposition conditions. The versatility of the coating method presented in this work allows for the coating of tubes of different lengths and diameters, opening the way for several applications of amorphous selenium films in various fields.
Resumo:
Introduction: Laser tissue fusion has a large potential for minimal invasive tissue fusion in different surgical specialties. We have developed a combined endovascular minimal invasive surgical technique to fuse blood vessels for bypass surgery. However, the main difficulty was to achieve reproducible results as the main tensile strength is a result of protein denaturation. We therefore aimed to develop a quantitative, reproducible tissue fusion using polycapsulated silica core nanoparticles containing indocyanine green (Si@PCL/ICG). Methods: In a first step we developed mesoporous indocyanine green (ICG) containing nanoparticles and assessed their heating profile. Furthermore the stability to light exposure and ICG degradation was measured. In a second phase Si@PCL/ICG nanoparticles for embedding into a biodegradeable implant was developed and characterized using differential scanning calomeritry technique (DSC). Results: ICG containing mesoporous silica nanoparticles showed a sufficient increase in temperature up to 80°C suitable for laser tissue fusion. However, long-term stability of ICG mesoporous nanoparticles is lost after 7 days of light exposure. In contrast Si@PCL/ICG nanoparticles demonstrated a strong heating capacity as well as a good DSC profile for laser tissue fusion and long-term stability of 3 weeks. Furthermore Si@PCL/ICG nanoparticles can be directly dispersed in spin-coated polycaprolactone polymer. Conclusion: Si@PCL/ICG nanoparticles have good long-term stability and polymer embedding properties suitable for laser tissue fusion.