1 resultado para Post-pressing time

em ArchiMeD - Elektronische Publikationen der Universität Mainz - Alemanha


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The behaviour of a polymer depends strongly on the length- and time scale as well as on the temperature rnat which it is probed. In this work, I describe investigations of polymer surfaces using scanning probe rnmicroscopy with heatable probes. With these probes, surfaces can be heated within seconds down to rnmicroseconds. I introduce experiments for the local and fast determination of glass transition and melting rntemperatures. I developed a method which allows the determination of glass transition and melting rntemperatures on films with thicknesses below 100 nm: A background measurement on the substrate was rnperformed. The resulting curve was subtracted from the measurement on the polymer film. The rndifferential measurement on polystyrene films with thicknesses between 35 nm and 160 nm showed rncharacteristic signals at 95 ± 1 °C, in accordance with the glass transition of polystyrene. Pressing heated rnprobes into polymer films causes plastic deformation. Nanometer sized deformations are currently rninvestigated in novel concepts for high density data storage. A suitable medium for such a storage system rnhas to be easily indentable on one hand, but on the other hand it also has to be very stable towards rnsurface induced wear. For developing such a medium I investigated a new approach: A comparably soft rnmaterial, namely polystyrene, was protected with a thin but very hard layer made of plasma polymerized rnnorbornene. The resulting bilayered media were tested for surface stability and deformability. I showed rnthat the bilayered material combines the deformability of polystyrene with the surface stability of the rnplasma polymer, and that the material therefore is a very good storage medium. In addition we rninvestigated the glass transition temperature of polystyrene at timescales of 10 µs and found it to be rnapprox. 220 °C. The increase of this characteristic temperature of the polymer results from the short time rnat which the polymer was probed and reflects the well-known time-temperature superposition principle. rnHeatable probes were also used for the characterization of silverazide filled nanocapsules. The use of rnheatable probes allowed determining the decomposition temperature of the capsules from few rnnanograms of material. The measured decomposition temperatures ranged from 180 °C to 225 °C, in rnaccordance with literature values. The investigation of small amounts of sample was necessary due to the rnlimited availability of the material. Furthermore, investigating larger amounts of the capsules using rnconventional thermal gravimetric analysis could lead to contamination or even damage of the instrument. rnBesides the analysis of material parameters I used the heatable probes for the local thermal rndecomposition of pentacene precursor material in order to form nanoscale conductive structures. Here, rnthe thickness of the precursor layer was important for complete thermal decomposition. rnAnother aspect of my work was the investigation of redox active polymers - Poly-10-(4-vinylbenzyl)-10H-rnphenothiazine (PVBPT)- for data storage. Data is stored by changing the local conductivity of the material rnby applying a voltage between tip and surface. The generated structures were stable for more than 16 h. It rnwas shown that the presence of water is essential for succesfull patterning.