Colloidal nanoparticles are additives to improve or modify several properties of thermoplastic or elastic polymers. Usually colloid-polymer mixtures show phase separation due to the depletion effect. The strategy to overcome this depletion demixing was to prepare surface-modified colloidal particles, which can be blended with linear polymer chains homogeneous. A successful synthesis strategy for the preparation of hairy nanospheres was developed by grafting polystyrene macromonomer chains onto polyorganosiloxane microgels. The number of hairs per particle with a core radius of approximately 10nm exceeded 150 hairs in all cases. The molecular weight of the hairs variied between 4000-18000g/mol.The compatibility of these hairy spheres mixed with linear polymer chains was investigated by AFM, TEM and SAXS. Homogeneous mixtures were found if the molecular weight of the polymer hairs on the particle surface is at least as large as the molecular weight of the matrix chains. If the chains are much shorter than the hairs, the colloidal hair corona is strongly swollen by the matrix polymer, leading to a long-range soft interparticle repulsion ('wet brush'). If hairs and chains are comparable in length, the corona shows much less volume swelling, leading to a short-range repulsive potential similar to hard sphere systems ('dry brush'). Polymerketten und Kolloidpartikel entmischen aufgrund von Depletion-Wechselwirkungen. Diese entropisch bedingte Entmischung konnte durch das Ankoppeln von Polymerhaaren verschiedenen Molekulargewichts auf die Kugeloberflächen der Kolloide bis zu hohen Konzentrationen vermieden werden. Zur Darstellung sphärischer Bürsten und haariger Tracerpartikel wurde eine neue Synthesestrategie ausgearbeitet und erfolgreich umgesetzt.Das Kompatibilitätsverhalten dieser sphärischen Bürsten in der Schmelze von Polymerketten als Matrix wurde mittels Elektronenmikroskopie und Kleinwinkelröntgenstreuung untersucht. Die Mischungen setzten sich aus sphärischen Bürsten und Matrixketten mit unterschiedlichen Molekulargewichten zusammen.Es zeigte sich, daß die Mischbarkeit entschieden durch das Verhältnis von Haarlänge zu Länge der Matrixketten beeinflußt wird.Aus den Untersuchungen des Relaxationsverhaltens mittels Rheologie und SAXS ergibt sich, daß das Konzept der 'dry brush'- und 'wet brush'-Systeme auf diese Mischungen übertragbar ist. Die Volumenquellung der Haarcorona durch die Matrixketten ist, wie die Experimente gezeigt haben, bereits im Fall von Polymeren mit relativ niedrigen Molekulargewichten zu beobachten. Sie ist umso stärker ausgeprägt, je größer das Längenverhältnis zwischen Polymerhaaren und Matrixketten ist. Die Quellung bedeutet eine Vergrößerung des effektiven Radius der Partikel und entspricht somit einer Erhöhung des effektiven Volumenbruchs. Dies führt zur Ausbildung einer höheren Ordnung und zu einem Einfrieren der Relaxation dieser strukturellen Ordnung führt.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In dieser Arbeit wurden zwei Wege zur sauer katalysierten Synthese von Polyorganosiloxan-Kern-Schale-Nanopartikeln mit monomodaler Größenverteilung erarbeitet. Zum einen führt eine Erhöhung der Rührergeschwindigkeit auf 14000 rpm unter Verwendung eines Ultrathorax, während der ersten Stunde der Kondensation des Kernes zu Nanokugeln mit einer monomodalen Größenverteilung mit einem hydrodynamischen Radius von 33.1 nm +/- 22%. Zum anderen eröffnete die Reduktion des Flottenverhältnisses S, d.h. des Verhältnisses von Tensid- zu Monomermenge, von S=0.02 auf S=0.001 einen zweiten Weg zur Synthese von Nanokugeln mit monomodaler Größenverteilung. Der Radius dieser Kugeln beträgt 54.2 nm +/- 20%. Durch diese beiden Synthesewege sind Polyorganosiloxan-Nanokugeln in zwei verschiedenen Größen zugänglich. Durch 29Si-NMR-Messungen der Kerndispersion konnte gezeigt werden, dass die Ursache der bimodalen Größenverteilung der Polyorganosiloxan-Nanokugeln in der Synthese der Kerndispersion zu finden ist. Aus den hieraus ermittelten Ergebnissen geht hervor, dass sich während der sauer katalysierten Kondensation von Diethoxydimethylsilan neben den PDMS-Ketten auch zyklische Kondensationsprodukte bilden. Die während der Reaktion fortschreitende Bildung von Zyklen - insbesondere von Vierringen - bewirkt eine Phasenseparation der Dispersion. Dies führt zur beobachteten Bildung der bimodalen Größenverteilung der Polyorganosiloxan-Nanokugeln. Wird die Rührergeschwindigkeit auf 14000 rpm während der ersten Stunde der Kondensation des Kernes erhöht, wird eine verminderte Ringbildung gefunden. Der erhöhte Energieeintrag und die damit verbundene bessere Durchmischung der Dispersion während der ersten Stunde der Kondensation des Kerns führt bevorzugt zum Kettenwachstum, so dass die Tendenz zur Ringbildung verringert wird. Es tritt keine Phasenseparation auf, wodurch die beobachtete monomodale Größenverteilung der Nanokugeln erklärt wird. Wird das Flottenverhältnis reduziert und somit der pH-Wert der Lösung erhöht, werden bevorzugt offenkettige PDMS-Produkte gebildet. Die Bildung von Vierringen erfolgt nicht, Ringe höherer Ordnung werden nur in untergeordneter Menge gebildet. Es erfolgt keine Phasenseparation der Dispersion und eine monomodale Größenverteilung der Polyorganosiloxan-Nanokugeln wird erhalten. Die durch Erniedrigung des Flottenverhältnisses synthetisierten Polyorganosiloxan-Nanokugeln zeigten in AFM-Experimenten interessante Eigenschaften. So ist es möglich, die Nanokugeln auf einer Mica-Oberfläche mittels der AFM-Spitze zu manipulieren, ohne sie hierbei sie degradieren. Die sauer katalysierte Synthese ermöglicht die Einführung von basenlabilen Hydridgruppen in die Polyorganosiloxan-Nanokugeln. Ausgehend von in organischen Lösungsmitteln redispergierbaren Polyorganosiloxan-Nanokugeln, deren Oberfläche mit Hydridgruppen funktionalisiert wurde, konnten durch Hydrosilylierung mit allylterminiertem Polyethylenoxid wasserlösliche potentielle Nanokontainer synthetisiert werden.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Plasmonic nanoparticles are great candidates for sensing applications with optical read-out. Plasmon sensing is based on the interaction of the nanoparticle with electromagnetic waves where the particle scatters light at its resonance wavelength. This wavelength depends on several intrinsic factors like material, shape and size of the nanoparticle as well as extrinsic factors like the refractive index of the surrounding medium. The latter allows the nanoparticle to be used as a sensor; changes in the proximate environment can be directly monitored by the wavelength of the emitted light. Due to their minuscule size and high sensitivity this allows individual nanoparticles to report on changes in particle coverage.rnrnTo use this single particle plasmon sensor for future sensing applications it has to meet the demand for detection of incidents on the single molecule level, such as single molecule sensing or even the detection of conformational changes of a single molecule. Therefore, time resolution and sensitivity have to be enhanced as today’s measurement methods for signal read-out are too slow and not sensitive enough to resolve these processes. This thesis presents a new experimental setup, the 'Plasmon Fluctuation Setup', that leads to tremendous improvements in time resolution and sensitivity. This is achieved by implementation of a stronger light source and a more sensitive detector. The new setup has a time resolution in the microsecond regime, an advancement of 4-6 orders of magnitude to previous setups. Its resonance wavelength stability of 0.03 nm, measured with an exposure time of 10 ms, is an improvement of a factor of 20 even though the exposure time is 3000 times shorter than in previous reports. Thus, previously unresolvable wavelength changes of the plasmon sensor induced by minor local environmental alteration can be monitored with extremely high temporal resolution.rnrnUsing the 'Plasmon Fluctuation Setup', I can resolve adsorption events of single unlabeled proteins on an individual nanorod. Additionally, I monitored the dynamic evolution of a single protein binding event on a millisecond time scale. This feasibility is of high interest as the role of certain domains in the protein can be probed by a study of modified analytes without the need for labels possibly introducing conformational or characteristic changes to the target. The technique also resolves equilibrium fluctuations in the coverage, opening a window into observing Brownian dynamics of unlabeled macromolecules. rnrnA further topic addressed in this thesis is the usability of the nanoruler, two nanospheres connected with a spacer molecule, as a stiffness sensor for the interparticle linker under strong illumination. Here, I discover a light induced collapse of the nanoruler. Furthermore, I exploit the sensing volume of a fixed nanorod to study unlabeled analytes diffusing around the nanorod at concentrations that are too high for fluorescence correlation spectroscopy but realistic for biological systems. Additionally, local pH sensing with nanoparticles is achieved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Die Bioverkapselung ist eine faszinierende Methode, um biologische Materialien einschließlich Zellen in Siliziumdioxid, Metalloxiden oder hybriden Sol-Gel-Polymeren zu immobilisieren. Bisher wurde nur die Sol-Gel-Vorläufertechnologie genutzt, um Bakterien- oder Hefezellen in Siliziumdioxid zu immobilisieren. Hierfür wurden verschiedene Reagenzien als wässrige Vorläufer getestet, um poly(Silicate) auf Biomolekülen (Bhatia et al., 2000) oder Zellen (Liu und Chen 1999; Coradin und Livage, 2007) zu bilden. Einer der erfolgreichsten bisherigen Methoden verwendet eine Mischung aus Silicaten und kolloidalem Silica. Diese initialen Vorläufer werden durch die Zugabe von Salzsäure neutralisiert, was die Gelbildung fortschreiten lässt und die Verkapselung von Bakterien in einem Silica-Netzwerk zur Folge hat (Nassif et al., 2003). Mit der Entdeckung von Silicatein, einem Enzym, das aus Demospongien isoliert wurde und die Bildung von poly(Silicat) katalysiert, wurde es möglich, poly(Silicat) unter physiologischen Bedingungen zu synthetisieren. Silicatein wurde rekombinant in E. coli hergestellt und ist in der Lage, bei Raumtemperatur, neutralem pH-Wert und in wässrigen Puffersystemen aus Siliziumalkoxiden poly(Silicat) zu bilden (Krasko et al., 2000; Müller et al., 2007b; Zhou et al., 1999). In vivo katalysiert Silicatein die Synthese der Silicathülle der Schwamm-Spiculae (Skelettelemente; Müller et al., 2005b; Müller et al., 2007a; Müller et al., 2007b; Schröder et al., 2007a). Dieses Biosilica wurde in Form von Silica-Nanospheren mit Durchmessern zwischen 100 nm und 250 nm organisiert vorgefunden (Pisera 2003; Tahir et al., 2005). Mit dieser Arbeit konnte gezeigt werden, dass Escherichia coli erfolgreich mit dem Silicatein-Gen transformiert werden kann. Das Level der Proteinexpression kann in Anwesenheit von Isopropyl-β-D-thiogalaktopyranosid (IPTG) effizient erhöht werden, indem man die Bakterienzellen gleichzeitig mit Kieselsäure inkubiert. Dieser Effekt konnte sowohl auf Ebene der Synthese des rekombinanten Proteins durch Western Blot als auch durch Immunfluoreszenzmikroskopie nachgewiesen werden. Das heterolog produzierte Silicatein besitzt enzymatische Aktivität und kann die Polymerisation von Kieselsäure katalysieren. Dies konnte sowohl durch Färbung mit Rhodamin123, als auch durch Reaktion der nicht polymerisierten, freien Kieselsäure mit dem ß-Silicomolybdato-Farbsystem (Silicomolybdänblau) nachgewiesen werden. Elektronenmikroskopische Untersuchungen zeigten, dass nur die silicateinexprimierenden Bakterien während des Wachstums in Anwesenheit von Kieselsäure eine viskose Hülle um Zelle herum bilden. Ebenfalls konnte gezeigt werden, dass Silicatein-α aus Suberites domuncula nach Transformation in E. coli an die Zelloberfläche dieser Zellen transportiert wurde und dort seine enzymatische Funktion beibehielt. Die Silicathülle wurde mittels Raster-Elektronenmikroskopie (REM) analysiert. Die Bakterien, die Silicatein exprimierten und poly(Silicat) an ihrer Oberfläche synthetisierten, zeigten die gleichen Wachstumsraten wie die Bakterien, die das Gen nicht enthielten. Schlussfolgernd lässt sich sagen, dass die silicateinvermittelte Verkapselung von Bakterien mit poly(Silicat) die Bandbreite der Anwendung von Bakterien für die Produktion von rekombinanten Proteinen verbessern, erweitern und optimieren könnte.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Plasmonische Metallnanopartikel bündeln, verstärken und beeinflussen Licht auf nanoskopischer Ebene. Diese grundlegende Eigenschaft kommt von koheränten, kollektiven Schwingungen der Leitungsbandelektronen, die von einfallendem Licht resonant angeregt und lokalisierte Oberflächenplasmonenresonanz (LSPR) oder ‚Partikelplasmonen‘ genannt werden. Plasmonen in Metallnanopartikeln wurden bisher z.B. zur Erkennen von pathogenen Biomolekülen, bei der photothermischen Therapie und zur Verbesserung der Effizienz von Solarzellen verwendet. In dieser Arbeit werde ich meinen Fokus auf die Synthese und Funktionalisierung von Goldnanopartikeln zur Anwendung als Sensoren legen.rnrnKürzliche Verbesserungen in der nasschemischen Synthese haben zur Herstellung von Goldnanopartikel mit unterschiedlichen Formen und Größen geführt, die sich in ihren Sensoreigenschaften unterscheiden. Unter den unterschiedlichen Sensorgeometrien sind Goldnanostäbchen die bevorzugte Form zur Biomolekül-Sensorik durch LSPR. Nanostäbchen werden durch eine positiv geladene CTAB-Schicht stabilisiert, die Proteine bei neutralem pH-Wert anziehen kann. Die Adsorption und Desorption von Proteinen an der Nanopartikeloberfläche und damit die Bindungskinetiken von Proteinen kann auf Einzelmolekülebene erforscht werden. Ich zeige hier eine Studie mit hoher örtlicher und zeitlicher Auflösung um einzelne Bindungsereignisse von Fibronectin auf Goldnanostäbchen darzustellen.rnrnGoldnanostäbchen müssen mit spezifischen biologischen Erkennungselementen funktionalisiert werden um eine Analyterkennung oder Proteinwechselwirkung zu erreichen. Ich funktionalisiere Goldnanostäbchen mit kurzen DNA-Sequenzen (Aptamer-Sequenzen und NTA konjugierten Polihymidinen) und habe anhand diese unterschiedlich sensitiven Partikel eine Studie mit verschiedenen Analyten (oder Protein-Protein Wechselwirkungen) erfolgreich durchgeführt.rn rnPlasmonen von Nanopartikel-Clustern koppeln miteinander, was ihre Resonanzenergie ändert. Der kontrollierte Zusammenbau von Nanopartikeln zu Dimeren oder höher geordneten Strukturen wie ‚Core-Satellites‘ können dazu dienen ihre Sensitivität zu erhöhen. Diese Cluster bieten eine hohe Sensitivität auf Grund der Anwesenheit von plasmonischen Hotspots in der Lücke zwischen zwei Partikeln. Die Plasmonkopplung ist ein Phänomen, das abhängig vom Abstand zweier Partikel zueinander ist und bildet somit die Basis von sogenannten Plasmon-Linealen. Ich habe eine Strategie entwickelt um Dimere aus Hsp90 funktionalisierten Goldnanosphären zu bilden. Diese Technik wird nicht durch Ausbleichen oder das Blinken von Farbstoffen limitiert und ich zeige zum ersten Mal wie man dadurch dynamische Proteinkonformationen untersuchen kann.rn