3 resultados para Anatase TiO
em AMS Tesi di Dottorato - Alm@DL - Università di Bologna
Resumo:
This thesis wad aimed at the study and application of titanium dioxide photocatalytic activity on ceramic materials. As a matter of fact, photocatalysis is a very promising method to face most of the problems connected with the increasing environmental pollution. Furthermore, titanium dioxide, in its anatase crystallographic phase, is one of the most investigated photocatalytic material and results to be perfectly compatible with silicate body mixes. That goal was pursued by two different strategies: 1. the addition to a body mix used for heavy clay products of several titania powders, with different mean crystallite size, surface area, morphology and anatase/rutile ratio and a titania nanosuspension as well. The titania addition followed two procedures: bulk and spray addition over the ceramic samples surface. Titania was added in two different percentages: 2.5 and 7.5 wt.% in both of the methods. The ceramic samples were then fired at three maximum temperatures: 900, 950 and 1000 °C. Afterwards, the photocatalytic activity of the prepared ceramic samples was evaluated by following the degradation of an organic compound in aqueous medium, under UV radiation. The influence of titania morphological characteristics on the photoactivity of the fired materials was studied by means of XRD and SEM observations. The ceramic samples, sprayed with a slip containing 7.5 wt.% of titania powder and fired at 900 °C, have the best photoactivity, with a complete photo-decomposition of the organic compound. At 1000 °C no sample acted as a photocatalyst due to the anatase-to-rutile phase transformation and to the reaction between titania and calcium and iron oxides in the raw materials. 2. The second one foresaw the synthesis of TiO2-SiO2 solid solutions, using the following stoichiometry: Ti1-xSixO2 where x = 0, 0.1, 0.3 and 0.5 atoms per formula unit (apfu). The mixtures were then fired following two thermal cycles, each with three maximum temperatures. The effect of SiO2 addition into the TiO2 crystal structure and, consequently, on its photocatalytic activity when fired at high temperature, was thoroughly investigated by means of XRD, XPS, FE-SEM, TEM and BET analysis. The photoactivity of the prepared powders was assessed both in gas and liquid phase. Subsequently, the TiO2-SiO2 solid solutions, previously fired at 900 °C, were sprayed over the ceramic samples surface in the percentage of 7.5 wt.%. The prepared ceramic samples were fired at 900 and 1000 °C. The photocatalytic activity of the ceramic samples was evaluated in liquid phase. Unfortunately, that samples did not show any appreciable photoactivity. In fact, samples fired at 900 °C showed a pretty low photoactivity, while the one fired at 1000 °C showed no photoactivity at all. This was explained by the excessive coarsening of titania particles. To summarise, titania particle size, more than its crystalline phase, seems to have a relevant role in the photocatalytic activity of the ceramic samples.
Resumo:
The worldwide demand for a clean and low-fuel-consuming transport promotes the development of safe, high energy and power electrochemical storage and conversion systems. Lithium-ion batteries (LIBs) are considered today the best technology for this application as demonstrated by the recent interest of automotive industry in hybrid (HEV) and electric vehicles (EV) based on LIBs. This thesis work, starting from the synthesis and characterization of electrode materials and the use of non-conventional electrolytes, demonstrates that LIBs with novel and safe electrolytes and electrode materials meet the targets of specific energy and power established by U.S.A. Department of Energy (DOE) for automotive application in HEV and EV. In chapter 2 is reported the origin of all chemicals used, the description of the instruments used for synthesis and chemical-physical characterizations, the electrodes preparation, the batteries configuration and the electrochemical characterization procedure of electrodes and batteries. Since the electrolyte is the main critical point of a battery, in particular in large- format modules, in chapter 3 we focused on the characterization of innovative and safe electrolytes based on ionic liquids (characterized by high boiling/decomposition points, thermal and electrochemical stability and appreciable conductivity) and mixtures of ionic liquid with conventional electrolyte. In chapter 4 is discussed the microwave accelerated sol–gel synthesis of the carbon- coated lithium iron phosphate (LiFePO 4 -C), an excellent cathode material for LIBs thanks to its intrinsic safety and tolerance to abusive conditions, which showed excellent electrochemical performance in terms of specific capacity and stability. In chapter 5 are presented the chemical-physical and electrochemical characterizations of graphite and titanium-based anode materials in different electrolytes. We also characterized a new anodic material, amorphous SnCo alloy, synthetized with a nanowire morphology that showed to strongly enhance the electrochemical stability of the material during galvanostatic full charge/discharge cycling. Finally, in chapter 6, are reported different types of batteries, assembled using the LiFePO 4 -C cathode material, different anode materials and electrolytes, characterized by deep galvanostatic charge/discharge cycles at different C-rates and by test procedures of the DOE protocol for evaluating pulse power capability and available energy. First, we tested a battery with the innovative cathode material LiFePO 4 -C and conventional graphite anode and carbonate-based electrolyte (EC DMC LiPF 6 1M) that demonstrated to surpass easily the target for power-assist HEV application. Given that the big concern of conventional lithium-ion batteries is the flammability of highly volatile organic carbonate- based electrolytes, we made safe batteries with electrolytes based on ionic liquid (IL). In order to use graphite anode in IL electrolyte we added to the IL 10% w/w of vinylene carbonate (VC) that produces a stable SEI (solid electrolyte interphase) and prevents the graphite exfoliation phenomenon. Then we assembled batteries with LiFePO 4 -C cathode, graphite anode and PYR 14 TFSI 0.4m LiTFSI with 10% w/w of VC that overcame the DOE targets for HEV application and were stable for over 275 cycles. We also assembled and characterized ―high safety‖ batteries with electrolytes based on pure IL, PYR 14 TFSI with 0.4m LiTFSI as lithium salt, and on mixture of this IL and standard electrolyte (PYR 14 TFSI 50% w/w and EC DMC LiPF 6 50% w/w), using titanium-based anodes (TiO 2 and Li 4 Ti 5 O 12 ) that are commonly considered safer than graphite in abusive conditions. The batteries bearing the pure ionic liquid did not satisfy the targets for HEV application, but the batteries with Li 4 Ti 5 O 12 anode and 50-50 mixture electrolyte were able to surpass the targets. We also assembled and characterized a lithium battery (with lithium metal anode) with a polymeric electrolyte based on poly-ethilenoxide (PEO 20 – LiCF 3 SO 3 +10%ZrO 2 ), which satisfied the targets for EV application and showed a very impressive cycling stability. In conclusion, we developed three lithium-ion batteries of different chemistries that demonstrated to be suitable for application in power-assist hybrid vehicles: graphite/EC DMC LiPF 6 /LiFePO 4 -C, graphite/PYR 14 TFSI 0.4m LiTFSI with 10% VC/LiFePO 4 -C and Li 4 T i5 O 12 /PYR 14 TFSI 50%-EC DMC LiPF 6 50%/LiFePO 4 -C. We also demonstrated that an all solid-state polymer lithium battery as Li/PEO 20 –LiCF 3 SO 3 +10%ZrO 2 /LiFePO 4 -C is suitable for application on electric vehicles. Furthermore we developed a promising anodic material alternative to the graphite, based on SnCo amorphous alloy.
Resumo:
This work was based on the synthesis and characterization of innovative crystals for biomedical and technological applications. Different types of syntheses were developed in order to obtain crystals with high photocatalytic properties. A hydrothermal synthesis was also processed to correlate the chemical-physical characteristics with synthesis parameters obtaining synthesis of nanoparticles of titanium dioxide with different morphology, size and crystalline phase depending on the variation of the synthesis parameters. Also a synthesis in water at 80 °C temperature and low pressure was developed from which anatase containing a small percentage of brookite nanoparticles were obtained, presenting a high photocatalytic activity. These particles have been used to obtain the microcrystals formed by an inorganic core of hydroxyapatite surface covered by TiO2 nanoparticles. Micrometer material with higher photocatalytic has been produced. The same nanoparticles have been functionalized with resorcinol oxidized in order to increase the photocatalytic efficiency. Photodegradation test results have confirmed this increase. Finally, synthetic nanoparticles with a waterless synthesis using formic acid and octanol, through esterification "in situ" were synthesized. Nanoparticles superficially covered by carboxylic residues able to bind a wide range of molecules to obtain further photocatalytic properties were obtained.