4 resultados para Lead alloys.

em Universidade Federal do Pará


Relevância:

20.00% 20.00%

Publicador:

Resumo:

ABSTRACT: Analytical procedures for U-Pb isotope dilution analyses at the Pará-Iso isotope geology laboratory of the Federal University of Pará (UFPA) are described in detail. The procedures are applied to zircon, titanite, rutile, apatite, columbite-tantalite and whole rock. Reagent preparation and chemical processing are done in clean-room conditions. Samples are dissolved using Teflon™ microcapsules in steel jacket Teflon™ Parr Instrument™ bomb or Teflon™ screw cap containers. U and Pb are separated using anion exchange AG 1x8 resin columns. Typical blanks for mineral sample amounts of 0.01 to 1.0 mg are less than 1 pg U and 20-30 pg Pb. Isotope analysis of the U and Pb from the same filament are carried out using a Finnigan MAT 262 mass-spectrometer in static and dynamic modes. The current analytical level is demonstrated on analyses of international standard zircon 91500 with three different 235U-205Pb and 235U-208Pb isotope tracers and whole rock standards. Results of analyses of two zircon samples are also presented.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

No presente trabalho, é realizada uma seqüência de experimentos com ligas hipoeutéticas Al-Ni para analisar a solidificação unidirecional vertical ascendente em condições transitórias de fluxo de calor. Abordagens experimentais são desenvolvidas para a determinação quantitativa de variáveis térmicas de solidificação, tais como: tempos locais de solidificação; velocidades de deslocamento das isotermas liquidus; taxas de resfriamento à frente da isoterma liquidus e gradientes térmicos à frente da interface sólido / líquido. O trabalho analisa também a dependência dos espaçamentos dendríticos secundários em relação às variáveis térmicas de solidificação e ao teor de soluto das ligas, além de relacionar estes parâmetros com a resistência à corrosão destas ligas. Esses parâmetros dendríticos experimentais, referentes à solidificação das ligas Al - 1, 1,4 e 1,8 % Ni, não puderam ser comparados com os principais modelos teóricos de crescimento dendrítico da literatura, pois, para as ligas em estudo há uma escassez de propriedades termofísicas, impossibilitando assim esta comparação. O comportamento corrosivo é analisado pela técnica de polarização potenciodinâmica e técnica de polarização potenciodinâmica cíclica conduzidas em solução de 3,5% NaCl em temperatura ambiente, estruturas dendríticas mais grosseiras tendem a aumentar as taxas de corrosão das ligas hipoeutéticas do sistema Al-Ni. Os resultados experimentais obtidos através de ensaios de corrosão são correlacionados com a microestrutura dendrítica. Dessa forma, são determinadas tendências experimentais de crescimento dendrítico e resistência à corrosão para a solidificação unidirecional vertical ascendente.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Experiments were conducted to investigate the influence of thermal parameters on the columnar to equiaxed transition during the horizontal unsteady-state directional solidification of Al-Si alloys. The parameters analyzed include the heat transfer coefficients, growth rates, cooling rates, temperature gradients and composition. A combined theoretical and experimental approach is developed to determine the solidification thermal variables considered. The increasing solute content in Al-Si alloys was not found to affect significantly the experimental position of the CET which occurred for cooling rates in the range between 0.35 and 0.64 K/s for any of three alloy compositions examined. A comparative analysis between the results of this work and those from the literature proposed to analyze the CET during upward vertical solidification of Al-Si alloys is reported and the results have shown that the end of the columnar region during horizontal directional solidification is abbreviated as a result of about six times higher thermal gradient than that verified during upward unidirectional solidification of alloys investigated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

O presente estudo descreve a ocorrência de intoxicação por chumbo em bovinos e galinhas no Pará, Brasil. Em um lote composto de 80 bezerros de um rebanho leiteiro, 10 animais ficaram doentes e nove morreram, e um animal se recuperou após ser removido do piquete. Após a inspeção deste piquete, foi observada a presença de baterias de caminhões usados para armazenar a energia captada por painéis solares. Os sinais clínicos observados nos bezerros incluíam dificuldade respiratória, corrimento nasal, salivação excessiva, opacidade da córnea, pressão da cabeça contra objetos e decúbito. As galinhas tinham diminuída oviposição e os ovos produzidos eram com cascas malformadas ou tinham a casca mais fina. Os achados de necropsia e as alterações histopatológicas observadas nos bovinos eram de pouco significado, com exceção de um animal que mostrou leve astrocitose no córtex cerebral. Em uma das galinhas, na histopatologia renal observou-se leve necrose tubular aguda multifocal. As concentrações de chumbo médios nos fígados e rins dos bovinos eram 93,91mg/kg e 209,76mg/kg, respectivamente, e a concentração média no fígado de galinhas foi 105,02mg/ kg. Concluiu-se que a fonte de contaminação por chumbo nesses bezerros e galinhas eram placas de bateria de caminhão, aos quais os animais tiveram acesso na pastagem.