17 resultados para Fractal Image Coding
em Reposit
Resumo:
Jet impingement erosion test rig has been used to erode titanium alloy specimens (Ti-4Al-4V). Eroded surface profiles have been obtained by vertical sectioning method for light microscopy observation. Mixed fractals have been measured from profile images by a digital image processing and analysis technique. The use of this technique allows glimpsing a quantitative correlation among material properties, fractal surface topography and erosion phenomena. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
This work is an example of the improvement on quantitative fractography by means of digital image processing and light microscopy. Two techniques are presented to investigate the quantitative fracture behavior of Ti-4Al-4V heat-treated alloy specimens, under Charpy impact testing. The first technique is the Minkowski method for fractal dimension measurement from surface profiles, revealing the multifractal character of Ti-4Al-4V fracture. It was not observed a clear positive correlation of fractal values against Charpy energies for Ti-4Al-4V alloy specimens, due to their ductility, microstructural heterogeneities and the dynamic loading characteristics at region near the V-notch. The second technique provides an entire elevation map of fracture surface by extracting in-focus regions for each picture from a stack of images acquired at successive focus positions, then computing the surface roughness. Extended-focus reconstruction has been used to explain the behavior along fracture surface. Since these techniques are based on light microscopy, their inherent low cost is very interesting for failure investigations.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Objective. Pixel intensity values (PI) and fractal dimensions (FD) were compared in selected mandibular regions on digital panoramic images of normal, osteopenic, and osteoporotic perimenopausal and postmenopausal women to evaluate their relative efficacies in detecting osteoporotic-associated bone density changes.Study design. Standardized mandibular angle, body, and canine/premolar (C/PM) regions on 54 charge-coupied device (CCD) digital panoramic images of normal and potentially osteoporotic postmenopausal women were analyzed for PI and FD. Lumbar spine and femoral neck dual-energy x-ray absorptiometry QXA) on each patient served as the reference standard examination. Pearson correlation coefficients and analysis of variance (ANOVA) were performed.Results. There was significant correlation among PI measurements (P < 0.01), and no significant correlation between FD. C/PM had significantly lower PI than control C/PM (P = 0.049).Conclusions. Osteoporotic changes in mandibular C/PM cancellous bone were detected in our study population on CCD digital panoramic images by using a robust image analysis paradigm. Future automated application of such image analysis could enable widespread, cost effective screening for osteoporosis in dental settings.
Resumo:
This paper presents the study of computational methods applied to histological texture analysis in order to identify plant species, a very difficult task due to the great similarity among some species and presence of irregularities in a given species. Experiments were performed considering 300 ×300 texture windows extracted from adaxial surface epidermis from eight species. Different texture methods were evaluated using Linear Discriminant Analysis (LDA). Results showed that methods based on complexity analysis perform a better texture discrimination, so conducting to a more accurate identification of plant species. © 2009 Springer Berlin Heidelberg.
Resumo:
Due to the increased incidence of skin cancer, computational methods based on intelligent approaches have been developed to aid dermatologists in the diagnosis of skin lesions. This paper proposes a method to classify texture in images, since it is an important feature for the successfully identification of skin lesions. For this is defined a feature vector, with the fractal dimension of images through the box-counting method (BCM), which is used with a SVM to classify the texture of the lesions in to non-irregular or irregular. With the proposed solution, we could obtain an accuracy of 72.84%. © 2012 AISTI.
Resumo:
The methodology for fracture analysis of polymeric composites with scanning electron microscopes (SEM) is still under discussion. Many authors prefer to use sputter coating with a conductive material instead of applying low-voltage (LV) or variable-pressure (VP) methods, which preserves the original surfaces. The present work examines the effects of sputter coating with 25 nm of gold on the topography of carbon-epoxy composites fracture surfaces, using an atomic force microscope. Also, the influence of SEM imaging parameters on fractal measurements is evaluated for the VP-SEM and LV-SEM methods. It was observed that topographic measurements were not significantly affected by the gold coating at tested scale. Moreover, changes on SEM setup leads to nonlinear outcome on texture parameters, such as fractal dimension and entropy values. For VP-SEM or LV-SEM, fractal dimension and entropy values did not present any evident relation with image quality parameters, but the resolution must be optimized with imaging setup, accompanied by charge neutralization. © Wiley Periodicals, Inc.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
The fracture surfaces express the sequence of events of energy release due to crack propagation by linking the relief of the fracture to the loading stresses. This study aims to evaluate the heterogeneity of the critical zone for the advancement of the crack along its entire length in a thermoset composite carbon fiber and epoxy matrix, fractured in DCB testing (Double Cantilever Beam) and ENF (End-Notched Flexure). Investigations were made from image stacks obtained by optical reflection of extended depth from focus reconstruction. The program NIH Image J was used to obtain elevation map and fully focused images of the fracture surface, whose topographies were quantitatively analyzed. The monofractal behavior for DCB samples was assessed as being heterogeneous along the crack front and along the crack for all the conditionings. For the samples fractured in ENF test, there was a strong positive correlation to the natural condition, considering the fibers at 0° for the monofractal dimension and structural dimension (Df and Ds). For fibers at 90° to crack propagation, there was a moderate positive correlation for the textural dimension of natural condition. However, for the samples under ultraviolet condition and those subjected to thermal cycles, there was no correlation between the fractal dimension and fracture toughness in mode II
Resumo:
Fracture surfaces are the fracture process marks, taht it is characterized by energy release guieded by failure mode. The fracture toughness express this energy em stress and strain terms in pre-cracked samples. The strectch zone is the characteristic region forms by the transition of fatigue fracture and final fracture and it width demonstrate the relation with failure energy release.The quantitative fractography is a broadly tool uses in failure surfaces characterization that it can point to a material’s aspect or a fracture process. The image processing works like an investigation tool, guinding a lot of studies in this area. In order to evaluate the characterization effectivity and it respectivity studies, it used 300M steel that it was thermal treated by an aeronautical process known and it characterized by tensile test and energy dispersive spectroscopy (EDS). The tensile test of this material, made by ASTM E8, allowed the head treatment effectivity confirmation, beyond of mechanics porperties determination. The EDS confirmed the material composition, beyond of base the discussion about fracture mechanism presence. The fracture toughness test has also made, that it works to obtain the fracture surfeaces studies below self-similarity and self-affinity approaches. In front of all the exposed it was possible to conclude that the fractal dimension works like a study parameter of fracture process, allowinf the relation of their values with changes in thickness, which interferes directly in material’s behaviour in fracture toughness approach
Resumo:
Aims: This study compared fractal dimension (FD) values on mandibular trabecular bone in digital and digitized images at different spatial and contrast resolutions. Materials and Methods: 12 radiographs of dried human mandibles were obtained using custom-fabricated hybrid image receptors composed of a periapical radiographic film and a photostimulable phosphor plate (PSP). The film/ PSP sets were disassembled, and the PSPs produced images with 600 dots per inch (dpi) and 16 bits. These images were exported as tagged image file format (TIFF), 16 and 8 bits, and 600, 300 and 150 dpi. The films were processed and digitized 3 times on a flatbed scanner, producing TIFF images with 600, 300 and 150 dpi, and 8 bits. On each image, a circular region of interest was selected on the trabecular alveolar bone, away from root apices and FD was calculated by tile counting method. Two-way ANOVA and Tukey’s test were conducted to compare the mean values of FD, according to image type and spatial resolution (α = 5%). Results: Spatial resolution was directly and inversely proportional to FD mean values and standard deviation, respectively. Spatial resolution of 150 dpi yielded significant lower mean values of FD than the resolutions of 600 and 300 dpi ( P < 0.05). A nonsignificant variability was observed for the image types ( P > 0.05). The interaction between type of image and level of spatial resolution was not signi fi cant (P > 0.05). Conclusion: Under the tested, conditions, FD values of the mandibular trabecular bone assessed either by digital or digitized images did not change. Furthermore, these values were in fluenced by lower spatial resolution but not by contrast resolution.