221 resultados para superconducting phase transition width
em Repositório Institucional UNESP - Universidade Estadual Paulista "Julio de Mesquita Filho"
Resumo:
We study the phase transition from a dx2-y2 to a dx2-y2+dxy superconductor using the tight-binding model of two-dimensional cuprates. As the temperature is lowered past the critical temperature Tc, first a dx2-y2 superconducting phase is created. With further reduction of temperature, the dx2-y2+dxy phase is created at temperature T=Tc1. We study the temperature dependencies of the order parameter, specific heat, and spin susceptibility in these mixed-angular-momentum states on a square lattice and on a lattice with orthorhombic distortion. The above-mentioned phase transitions are identified by two jumps in specific heat at Tc and Tc1. ©1999 The American Physical Society.
Resumo:
The temperature dependencies of specific heat and spin susceptibility of a coupled dx2-y2 + idxy superconductor in the presence of a weak dxy component are investigated in the tight-binding model (1) on square lattice and (2) on a lattice with orthorhombic distortion. As the temperature is lowered past the critical temperature Tc, first a less ordered dx2-y2 superconductor is created, which changes to a more ordered dx2-y2 + idxy superconductor at Tcl(< Tc). This manifests in two second order phase transitions identified by two jumps in specific heat at Tc and Tc1. The temperature dependencies of the superconducting observables exhibit a change from power-law to exponential behavior as temperature is lowered below Tc1 and confirm the new phase transition. © 1998 Published by Elsevier Science B.V. All rights reserved.
Resumo:
The FePt alloy undergoes the cubic to tetragonal lattice transformation in the ferromagnetic state. We calculated the electronic structure for both cubic and tetragonal structures using the FPLAPW method with APW + lo. Comparing the density of states of the cubic and tetragonal structures, it is expected that the lattice transformation is caused by the band Jahn-Teller effect. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The discovery of a new monoclinic phase in the PbZr1-xTixO3 (PZT) system in the vicinity of the morphotropic phase boundary (MPB), previously considered as a region where the rhombohedral and tetragonal phases of PZT coexist, was recently reported. Investigations of this new phase were reported using different techniques such as high-resolution synchrotron x-ray powder diffraction and Raman spectroscopy. The main objective has been to define a new phase diagram of PZT. In this context, infrared spectroscopic studies were performed in the vicinity of the MPB and studies were initially centred on a PZT sample with x = 0.49 mol% Ti content. Results suggested that the monoclinic --> tetragonal phase transition occurs at 237 K, confirming the use of IR as a useful technique to investigate this phase transition.
Resumo:
Recently, the observation of a new monoclinic phase in the PbZr1-xTixO3 (PZT) system in the vicinity of the morphotropic phase boundary was reported. Investigations of this new phase were reported using different techniques such as high-resolution synchrotron x-ray powder diffraction and Raman spectroscopy. In this work, the monoclinic --> tetragonal phase transition in PbZr0.50Ti0.50O3 ceramics was studied using infrared spectroscopy between 1000 and 400 cm(-1). The four possible nu(1)-stretching modes (Ti-O and Zr-O stretch) in the BO6 octahedron in the ABO(3) structure of PZT in this region were monitored as a function of temperature. The lower-frequency mode nu(1)-(Zr-O) remains practically unaltered, while both intermediate nu(1)-(Ti-O) modes decrease linearly as temperature increases from 89 to 263 K. In contrast, the higher-frequency nu(1)-(Ti-O) and nu(1)-(Zr-O) modes present anomalous behaviour around 178 K. The singularity observed at this mode was associated with the monoclinic --> tetragonal phase transition in PbZr0.50Ti0.50O3 ceramics.
Resumo:
The purpose of the present work is to report studies on structural phase transition for PMN-xPT ferroelectric, with melt PbTiO3 composition around the MPB (x = 0.35 mol %), using infrared spectroscopy technique. The study was centered on monitoring the behavior of the 1-(NbO), 1-(TiO) and 1-(MgO) stretching modes as a function of temperature. The increasing as a function of temperature for 1-(TiO) and 1-(MgO) modes, observed between 230 and 300 K, can be related to the monoclinic (MC) + tetragonal (T) phase coexistence in the PMN-PT.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
This article reports a study of the thermal stability and morphological changes in tin oxide nanobelts grown in the orthorhombic SnO phase. The nanobelts were heat-treated in a differential scanning calorimetry (DSC) furnace at 800 degrees C for I It in argon, oxygen, or synthetic air atmospheres. The samples were then characterized by DSC, X-ray diffraction (XRD), high resolution transmission electron microscopy (HRTEM), and high resolution field emission scanning electron microscopy (FE-SEM). The results confirmed that the orthorhombic SnO phase is thermodynamically unstable, causing the belts to transform into the SnO2 phase when heat-treated. During the phase transition, if oxygen is available in the furnace atmosphere, nanofibers grow at the edge of nanobelts at about 50 degrees of the belts' growth direction, while particles grow on the belt surface in the absence of oxygen. Although the decomposition process reduces the nanobelt cell volume by 22%, most belts remain monocrystalline after the heat treatment. The results confirm that phase transition is a decomposition process, which explains the morphological changes in the belts based on metallic tin generated in the process.
Resumo:
The gel to liquid crystalline phase transition of the double-chained cationic dioctadecyldimethylammonium chloride and bromide (DODAX, X = Cl- or Br-) in aqueous vesicle dispersions prepared by non-sonication, sonication and extrusion has been investigated using high-sensitivity differential scanning calorimetry (DSC). The transition temperature (T-m) is a function of the preparation method, amphiphile concentration, vesicle curvature and nature of the counterion. DSC thermograms for DODAB and DODAC non-sonicated vesicle dispersions exhibit a single endothermic peak at T-m roughly independent of concentration up to 10 mM. Extrusion broadens the transition peak and shifts T-m downwards. Sonication, however, broadens slightly the transition peak and tends to shift T-m upwards suggesting that extrusion and sonication form vesicles with different characteristics. DODAC always exhibits higher T-m than DODAB irrespective of the preparation method. T-m changes as follows: T-m (sonicated) greater than or equal to T-m (non-sonicated) > T-m (extruded). Hysteresis of about 7 degrees C was observed for DODAB vesicle dispersions. (C) 2000 Elsevier B.V. Ireland Ltd. All rights reserved.
Resumo:
We combine the D0 measurement of the width difference between the light and heavy B-s(0) mass eigenstates and of the CP-violating mixing phase determined from the time-dependent angular distributions in the B-s(0)-> J/psi phi decays along with the charge asymmetry in semileptonic decays also measured with the D0 detector. With the additional constraint from the world average of the flavor-specific B-s(0) lifetime, we obtain Delta Gamma(s)equivalent to(Gamma(L)-Gamma(H))=0.13 +/- 0.09 ps(-1) and vertical bar phi(s)vertical bar=0.70(-0.47)(+0.39) or Delta Gamma(s)=-0.13 +/- 0.09 ps(-1) and vertical bar phi(s)vertical bar=2.44(-0.39)(+0.47). The data sample corresponds to an integrated luminosity of 1.1 fb(-1) accumulated with the D0 detector at the Fermilab Tevatron Collider.
Resumo:
We predict the loss of superfluidity in a Bose-Einstein condensate (BEC) trapped in a combined optical and axially-symmetric harmonic potentials during a resonant collective excitation initiated by a periodic modulation of the atomic scattering length a, when the modulation frequency equals twice the radial trapping frequency or multiples thereof. This classical dynamical transition is marked by a loss of superfluidity in the BEC and a subsequent destruction of the interference pattern upon free expansion. Suggestion for future experiment is made. (C) 2003 Elsevier B.V. B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)