A polymeric complex [Eu(α-tpc)3(α-Htpc) 2]n and its characterization by single crystal X-ray and thermal analysis, infrared and photoluminescence spectroscopies are described. The compound crystallizes in the monoclinic Cc space group. The asymmetric unit is formed from a europium ion bonded to one carboxyl oxygen of five different thiophene carboxylic moieties. Three of these moieties are deprotonated and bridge between neighboring europium ions giving rise to an infinite polymer along the c axis. Besides the europium characteristic emission lines, the emission spectra show unambiguously the crystal size effect on the 5D0 → 7F0 transition. The complex thermal decomposition at 220 C leads to a stable luminescent complex in which the 5D0 → 7F4 transition reveals a monomeric characteristic. The Judd-Ofelt intensity parameters to the polymeric and the monomeric compound with the same ligand and coordination number were compared. © 2013 Published by Elsevier Ltd.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Hybrid Eu3+-doped silica-poliethyleneoxide (PEO) nanocomposites with covalent bonds between the inorganic (siloxane) and organic (PEO) phases have been obtained by sol-gel process. These materials are transparent, flexible and present high Eu3+ luminescence output. Their luminescence properties, local environment around europium ions and structure have been investigated as a function of europium content. EXAFS measurements indicate that the increase in Eu-doping induces a decrease in Eu3+ coordination number. An increase in symmetry degree around the metal ion is also observed for increasing Eu3+ concentration, while non radiative decay paths from the D-5(0) excited state become more important. SAXS results suggest the preferential interaction of europium ions with ether-type oxygens of the polymer chains. However, the existence of interactions between the cations and the carbonyl groups from urea bridges located at the siloxane-PEO interface can not be excluded.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Used as catalysts even in organic and inorganic molecules, as additives on catalysts, electrochromic films on smart windows the tungsten trioxide have been largely studied on the lasts decades, but there is just a few about it's luminescence. Using as precursors nitric acid and sodium tungstate the tungsten trioxide were been prepared thru wet process then treating on thermic and hydrothermal treatments. Where been evaluated the effects of methodology, nitric acid concentration, duration and temperature of treatments. The samples were characterized by X-ray diffraction (XRD), Raman scattering spectroscopy (RSS), Fourier transformed infrared spectroscopy, photoluminescence spectroscopy (PLS) and X-ray excited optical luminescence (XEOL). Hydrated phases of tungsten trioxide were obtained through hydrothermal treatments and the non-hydrated phases occur with thermic treatments. The acid concentration has the ability to determine the major phase formed as well the temperature determine the hydratation of the product. With lower temperatures dihydrate phase were preferable formed and with the rise of temperature, the water molecules were lost up to the fractionary hydratation and then the non-hydrated phase with higher temperatures depending on the atmosphere used on the thermal treatment. Doping the system with europium ions even substituting tungsten or in the interstices of the matrix were not been successful, as well the XEOL spectroscopy intensity were null and quite low for ultraviolet and visible excitation photoluminescence because of oxygen defect levels localized into the prohibited band.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The synthesis and characterization of a new organic ligand monooctyldiphenylphosphinate (L) is described, as well as a new Eu(3+) diketonate complex [Eu(tta)(3)(L)(2)] (tta = thenoyltrifluoracetone). The ligand (L) was formed by substitution reaction (80% yield) and characterized by uni- and bidimensional (1)H, (13)C and (31)P NMR experiments, to confirm its molecular structure. The coordination of (L) to Eu(3+) in the complex [Eu(tta)(3)(L)(2)] was confirmed by FT-IR spectra. The emission spectra present the same profile when excited in Eu(3+) or in the ligands, suggesting an energy transfer from ligands to Eu(3+) ions. The emission spectra of the precursor [Eu(tta)(3)(H(2)O)(2)], and [Eu(tta)(3)(L(2))] present bands arising from f-f intra-configurational transitions. The only (5)D(0)-(7)F(0) transition shows the presence of at least one site without symmetry center. The FWHM of such transition is 7 cm(-1) and 57 cm(-1) for [Eu(tta)(3)(H(2)O)(2)] and [Eu(tta)(3)(L)(2)] complexes, respectively. This widening is provided by the presence of large groups around Eu(3+) ion. The calculated intensity parameters Omega(2) and Omega(4) show that the interaction features between center-ion and ligand are different; the small value of Omega(4) is related to long range effects of alkyl chain. The Langmuir isotherms of this ligand and complex have been investigated although their hydrolysis in water subphase does not allow stable monolayers. (C) 2009 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim

Relevância:

30.00% 30.00%

Publicador:

Resumo:

An investigation by optical spectroscopy of the Eu3 + and Er3 + active ions in the crystallized fluorozirconate matrix LaZr2F11 is presented. The D-5(1) --> F-7(0-5) emission lines of Eu3 + are used to extract the F-7(0-5) energy scheme and the observed extinctions permit the deduction of irreducible representations (IRREPS) associated with corresponding sub-levels in the D-2 symmetry. The crystal field analysis was carried out on a 387 x 387 basis set, comprising the F-7, D-5(1,2,3) F-5(1,2), (5)G(1,2,3) and P-3(1,2,3,4,5,6) terms of the Eu-3 (+) 4f(6) configuration. The deviation and rms are 6.8 and 7.9 cm (-1), respectively for 38 levels and ten parameters. The experimental crystal field parameters are in good agreement with the ab-initio ones. Moreover, the relative intensities of the D-5(0) --> F-7(2,3,4) emissions are well reproduced by an 'ab-initio' calculation, except for three lines. The Er3 + ions introduced in LaZr2F11, microcrystals also lie in an unique crystallographic site. A total of 31 energy levels were recorded and the crystal field analysis led to 6.6 and 7.8 cm (-1) for the deviation and rms, respectively, for nine variable parameters taken into account. The experimental CF parameters for Er3 + and Eu3 + are very similar, which seems to show that the host lattice contracts around the smaller Er3 + ion. The informations given by both Eu3 + and Eu3 + optical probes in LaZr2F11 are very consistent with the structure previously determined for the isotypic PrZr2F11 fluoride. (C) 2000 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A structure modeling of two families of sol-gel derived Eu3+-doped organic/inorganic hybrids based on the results of small-angle X-ray scattering experiments is reported. The materials are composed of poly(oxyethylene) chains grafted at one or both ends to siloxane groups and are called mono- and di-urethanesils, respectively. A theoretical function corresponding to a two-level hierarchical structure model fits well the experimental Scattering curves. The first level corresponds to small siloxane clusters embedded in a polymeric matrix. The secondary level is associated to the existence of siloxane cluster rich domains surrounded by a cluster-depleted polymeric matrix. Results show that increasing europium doping favors the growth of the secondary domains. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Rare earth (RE) ions have spectroscopic characteristics to emit light in narrow lines, which makes RE complexes with organic ligands candidates for full color OLED (Organic Light Emitting Diode) applications. In particular, beta-diketone rare earth (RE(3+)) complexes show high fluorescence emission efficiency due to the high absorption coefficient of the beta-diketone and energy transfer to the central ion. In this work, the fabrication and the electroluminescent properties of devices containing a double and triple-layer OLED using a new beta-diketone complex, [Eu(bmdm)(3)(tppo)(2)], as transporting and emitting layers are compared and discussed. The double and triple-layer devices based on this complex present the following configurations respectively: device 1: ITO/TPD (40 nm)/[Eu(bmdm)(3)(tppo)(2)] (40 nm)/Al (150 nm); device 2: ITO/TPD (40 nm)/[Eu(bmdm)(3) (tppo)(2)] (40 nm)/Alq(3) (20 nm)/Al (150 nm) and device 3: ITO/TPD (40 nm)/bmdm-ligand (40 nm)/Al (150 nm), were TPD is (N,N'-diphenyl-N,N'-bis(3-methylphenyl)-1,1-biphenil-4,4-diamine) and bmdm is butyl methoxy-dibenzoyl-methane. All the films were deposited by thermal evaporation carried out in a high vacuum system. These devices exhibit high intensity photo- (PL) and electro-luminescent (EL) emission. Electroluminescence spectra show emission from Eu(3+) ions attributed to the (5)D(0) to (7)F(J) (J = 0, 1, 2, 3 and 4) transitions with the hypersensitive (5)D(o) -> (7)F(2) transition (around 612 nm) as the most prominent one. Moreover, a transition from (5)D(1) to (7)F(1) is also observed around 538 nm. The OLED light emission was almost linear with the current density. The EL CIE chromaticity coordinates (X = 0.66 and Y = 0.33) show the dominant wavelength, lambda(d) = 609 nm, and the color gamut achieved by this device is 0.99 in the CIE color space. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

ZnO:Eu3+ (0.1 and 3 at%) with average particle size of 500 nm were prepared by the Pechini method. Photoluminescence spectroscopy evidences that there is no energy transfer between ZnO and Eu3+ ion. The emission spectrum at 77 K shows that Eu3+ ions occupy at least three different sites in ZnO:Eu 3 at% sample. The experimental intensity parameter Omega(2) indicates that Eu3+ ions in the sample doped with 3 at% occupy sites where 4-configurational levels can better mix with opposite-parity states than those in the sample doped with 0.1 at%. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The aim of this work is to report on the luminescence properties of BaZnSiO4 activated by Eu3+ and Mn2+ ions. Doped and undoped powder samples were prepared by solid-state reaction starting from oxides and carbonates or Ba2SiO4:Eu3+ and Zn2SiO4:Mn2+ precursors. X-ray diffraction powder data, IR vibrational, and UV-vis luminescence spectroscopies were carried out. Results showed that doped and undoped samples from both types of precursors have the same structure and crystallize with a superstructure of hexagonal kalsilite. Vibrational spectroscopy has confirmed the formation of a silicate group, which outlines differences between products and silicate precursors. The observed luminescence assigned to Eu3+ and Mn2+ transitions covered most parts of the visible spectrum, an important requirement for phosphors in fluorescent low-pressure mercury vapor lamps.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Transparent oxyfluoride glasses and beta-PbF(2) nanocrystals containing glass-ceramics were prepared with varying Eu(3+) content (0.3, 0.4, 0.5 and 0.6%). The effect of Eu(3+) content on the preparation of glass-ceramics was investigated. From differential scanning calorimetry, the T(x)-T(g)(T(x)-temperature of the onset of crystallization; T(g)-glass transition temperature) parameter for glasses has shown slight variation, and an exothermic peak near T(g) called the ceramization temperature (T(c)) has been observed. Heat treatments were performed at this temperature to obtain transparent glass-ceramics containing beta-PbF(2) nanocrystals, identified by x-ray diffraction. Heat treatments for different periods of time were performed and were observed to be very important in the control of the crystal size and of the crystallization rate. Based upon the absorption spectra, the scattering level due to the presence of beta-PbF(2) nanocrystals in the glass-ceramics was observed to be similar to that for the mother glasses. Detailed analysis of emission spectra and decay time measurements led to the identification of Eu(3+) ions as the beta-PbF(2) crystalline phase. Excitation spectra at 70 K show the interaction of Eu(3+) ions with the fluorogermanate network.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work, a SiO2 spherical were prepared by the Stober Method and then recovered with a single layer of Eu2O3 oxide (SiO2@Eu2O3) obtained by the Polymeric Precursor Method. The SiO2@Eu2O3 powder was heated treated at 100, 300, 400, 500 and 800 A degrees C. The samples were characterized by the Scanning Electonic Microscopy (SEM), Thermal Analysis (TGA/DTA), and the luminescent properties of the SiO2@Eu2O3 powders were studied by their emission and excitation spectra as well as by the lifetime measurements of the Eu3+ D-5(0) -> aEuro parts per thousand F-7(2) transition. The SEM analysis shows that the silica prepared by the Stober Method is spherical with a particle size of 460 nm. The emission spectra of the SiO2@Eu2O3 powders presented the Eu3+ characteristics bands related to the D-5(0) -> aEuro parts per thousand F-7(J) (J = 0, 1, 2, 3, 4) transitions at 577, 591, 616, 649 and 695 nm, respectively. The band related to the D-5(0) -> aEuro parts per thousand F-7(2) transition is the most intense in the spectra, and its intensity decreases with the temperature enhancement. The decay curves of the SiO2@Eu2O3 samples presented monoexponential features, and the obtained lifetime values were higher than the Eu2O3 oxide. It was possible to conclude that the D-5(0) -> aEuro parts per thousand F-7(2) hypersensitive transition is strongly dependent on the Eu3+ surrounding.