18 resultados para duraliner II
em Repositório Institucional UNESP - Universidade Estadual Paulista "Julio de Mesquita Filho"
Resumo:
Objectives: This study investigated the effect of microwave disinfection (650 W/6 min) on the flexural strength of five hard chairside reline resins (Kooliner, Duraliner II, Tokuso Rebase Fast, Ufi Get Hard, New Truliner) and one denture base resin (Lucitone 550).Methods: Thirty-two specimens (3.1x10x64 mm) from each acrylic resin were produced and divided into four groups of eight specimens each. The flexural test was performed after polymerization (G1), after two cycles of microwave disinfection (G2), after 7 days storage in water at 37 degrees C (G3) and after seven cycles of microwave disinfection (G4). Specimens from group G4 were microwaved daily being stored in water at 37 degrees C between exposures. The specimens were placed in three-point bend fixture in a MTS machine and loaded until failure. The flexural values (MPa) were submitted to ANOVA and Tukey's test (p=0.05).Results: Two cycles of microwave disinfection promoted a significant increase in flexural strength for materials Kooliner and Lucitone 550. After seven cycles of microwave disinfection, materials Kooliner and New Truliner showed a significant increase (p<0.05) in flexural values. The flexural strength of the material Tokuso Rebase was not significantly affected by microwave irradiation. Seven cycles of microwave disinfection resulted in a significant decrease in the flexural strength of material Duraliner II. Material Ufi Get Hard was the only resin detrimentally affected by microwave disinfection after two and seven cycles.Conclusions: Microwave disinfection did not adversely affect the flexural strength of all tested materials with the exception of material Ufi Get Hard. (c) 2005 Elsevier Ltd. All rights reserved.
Glass transition temperature of hard chairside reline materials after post-polymerisation treatments
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Objectives. This study compared the residual monomer (RM) in four hard chair-side reline resins (Duraliner II-D, Kooliner-K, Tokuso Rebase Fast-TRF and Ufi Gel hard-UGH) and one heat-polymerized denture base resin (Lucitone 550-L), which was processed using two polymerization cycles (short-LS and long-LL). It was also investigated the effect of two after polymerization treatments on this RM content.Methods. Specimens (n = 18) of each material were produced following the manufacturers' instructions and then divided into three groups. Group I specimens were left untreated (GI-control). Specimens of group II (GII) were given post-polymerization treatment by microwave irradiation. In group III (GIII), specimens were submitted to immersion in water at 55 degrees C (reline resins-10 min; denture base resin L-60min). The RM was analyzed using high performance liquid chromatography (HPLC) and expressed as a percentage of RM. Data were analyzed by two-way ANOVA followed by Tukey's test (alpha = 0.05).Results. Comparing control specimens, statistical differences were found among all materials (p < 0.05), and the results can be arranged as K (1.52%) > D (0.85%) > UGH (0.45%) > LL (0.24%) > TRF (0.14%) > LS (0.08%). Immersion in hot water (GIII) promoted a significant (p < 0.05) reduction in the RM for all materials evaluated compared to control (GI), with the exception of LL specimens. Materials K, UGH and TRF exhibited significantly (p < 0.05) lower values of RM after microwave irradiation (GII) than in the control specimens.Significance. The reduction in RM promoted by water-bath and microwave post-polymerization treatments could improve the mechanical properties and biocompatibility of the relining and denture base materials. (c) 2006 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Statement of problem. Microwave postpolymerization has been Suggested as a method to improve the mechanical strength of repaired denture base materials. However, the effect of microwave heating oil the flexural strength of the autopolymerizing denture reline resins has not been investigated.Purpose. This study analyzed the effect of microwave postpolymerization on the flexural strength of 4 autopolymerizing reline resins (Duraliner II, Kooliner, Ufi Gel Hard, and Tokuso Rebase Fast) and 1 heat-polymerized resin (Lucitone 550).Material and methods. For each material, 80 specimens (64 X 10 X 3.3 mm) were polymerized according to the manufacturer's instructions and divided into 10 groups (n = 8). Control group specimens remained as processed. Before testing, the specimens were Subjected to postpolymerization in a microwave oven using different power (500, 5,50, or 650 W) and time (3, 4, or 5 Minutes) settings. Load measurements (newtons) were made at a crosshead speed of 5 mm/min using a 3-point bending device with a span of 50 mill. The flexural strength values were calculated in MPa. Data analyses included 3-way and 2-way analysis of variance and the Tukey Honestly Significant Difference test (alpha=.05).Results. The flexural strengths of resins Duraliner 11 and Kooliner were significantly increased (P=.0015 and P=.0046, respectively) with the application of microwave irradiation using different time/power combinations. The materials Lucitone 550, Tokuso Rebase Fast, and Ufi Gel Hard demonstrated no significant strength improvement compared to the corresponding control. Only after microwave postpolymerization irradiation for 3 minutes at 550 W did Lucitione 550 show significantly higher flexural strength than Tokuso Rebase Fast and Ufi Gel Hard relining resins.Conclusion. Microwave postpolymerization irradiation can be an effective method for increasing the flexural strength of Duraliner II (at 650 W) and Kooliner (at 550 W and 650 W for 5 minutes).
Resumo:
The selection and use of hard chairside reline resins must be made with regard to dimensional stability, which will influence the accuracy of fit of the denture base. This study compared the dimensional change of two hard chairside reline resins (Duraliner II and Kooliner) and one heat-curing denture base resin (Lucitone 550). A stainless steel mold with reference dimensions (AB, CD) was used to obtain the samples. The materials were processed according to the manufacturer's recommendations. Measurements of the dimensions were made after processing and after the samples had been stored in distilled water at 37° C for eight different periods of time. The data were recorded and then analyzed with analysis of variance. All materials showed shrinkage immediately after processing (p < 0.05). The only resin that exhibited shrinkage after 60 days of storage in water was Duraliner II; these changes could be clinically significant in regard of tissue fit.
Resumo:
STATEMENT OF PROBLEM: Because water sorption of autopolymerizing acrylic reline resins is accompanied by volumetric change, it is a physical property of importance. As residual monomer leaches into the oral fluids and causes tissue irritation, low solubility of these resins is desired. Another requirement is a satisfactory bond between the autopolymerizing acrylic resins and the denture base acrylic resin. PURPOSE: This study compared the water sorption, solubility, and the transverse bond strength of 2 autopolymerizing acrylic resins (Duraliner II and Kooliner) and 1 heat-polymerizing acrylic resin (Lucitone 550). MATERIAL AND METHODS: The water sorption and solubility test was performed as per International Standards Organization Specification No. 1567 for denture base polymers. Bond strengths between the autopolymerizing acrylic resins and the heat-polymerizing acrylic resin were determine with a 3-point loading test made on specimens immersed in distilled water at 37 degrees C for 50 hours and for 30 days. Visual inspection determined whether failures were adhesive or cohesive. RESULTS: Duraliner II acrylic resin showed significantly lower water sorption than Kooliner and Lucitone 550 acrylic resins. No difference was noted in the solubility of all materials. Kooliner acrylic resin demonstrated significantly lower transverse bond strength to denture base acrylic resin and failed adhesively. The failures seen with Duraliner II acrylic resin were primarily cohesive in nature. CONCLUSIONS: Autopolymerizing acrylic reline resins met water sorption and solubility requirements. However, Kooliner acrylic resin demonstrated significantly lower bond strength to denture base acrylic resin.
Resumo:
Due to gradual resorption of the edentulous ridge bone, removable prostheses often require denture base relines to improve fit and stability. This research evaluated the bond strength between one heat-cured acrylic resin (Lucitone 550®) and two hard chairside reline resins, after two different periods of storage in water (50 h and 30 days). The bond strength was evaluated using a tensile test. The mode of failure, adhesive or cohesive, was also recorded. The results submitted to the Kruskal-Wallis test indicated that the highest tensile strengths were achieved with intact Lucitone 550® denture base resin in both periods of storage in water. After 50 h of storage in water, Duraliner II® reline material exhibited the highest bond strength to the denture base resin. After 30 days of storage in water, Duraliner II® reline resin demonstrated a significant reduction in adhesion, showing lower tensile bond strength than Kooliner® material. Both hard chairside reline materials failed adhesively across Lucitone 550® denture base resin, in both periods of time. © 1999 Blackwell Science Ltd.
Resumo:
Statement of problem. Little data are available regarding the effect of heat-treatments on the dimensional stability of hard chairside reline resins. Purpose. The objective of this in vitro study was to evaluate whether a heat-treatment improves the dimensional stability of the reline resin Duraliner II and to compare the linear dimensional changes of this material with the heat-polymerized acrylic resin Lucitone 550. Material and methods. The materials were mixed according to the manufacturer's instructions and packed into a stainless steel split mold (50.0 mm diameter and 0.5 mm thickness) with reference points (A, B, C, and D). Duraliner II specimens were polymerized for 12 minutes in water at 37°C and bench cooled to room temperature before being removed from the mold. Twelve specimens were made and divided into 2 groups: group 1 specimens (n=6) were left untreated, and group 2 specimens (n=6) were submitted to a heat-treatment in a water bath at 55°C for 10 minutes and then bench cooled to room temperature. The 6 Lucitone specimens (control group) were polymerized in a water bath for 9 hours at 71°C. The specimens were removed after the mold reached the room temperature. A Nikon optical comparator was used to measure the distances between the reference points (AB and CD) on the stainless steel mold (baseline readings) and on the specimens to the nearest 0.001 mm. Measurements were made after processing and after the specimens had been stored in distilled water at 37°C for 8 different periods of time. Data were subjected to analysis of variance with repeated measures, followed by Tukey's multiple comparison test (P<.05). Results. All specimens exhibited shrinkage after processing (control, -0.41%; group 1, -0.26%; and group 2, -0.51%). Group 1 specimens showed greater shrinkage (-1.23%) than the control (-0.23%) and group 2 (-0.81%) specimens after 60 days of storage in water (P<.05). Conclusion. Within the limitations of this study, a significant improvement of the long-term dimensional stability of the Duraliner II reline resin was observed when the specimens were heat-treated. However, the shrinkage remained considerably higher than the denture base resin Lucitone 550. Copyright © 2002 by The Editorial Council of The Journal of Prosthetic Dentistry.
Resumo:
Purpose: To evaluate the influence of water bath and microwave postpolymerization treatments on the cytotoxicity of 6 hard reline acrylic resins. Materials and Methods: The materials tested were Tokuso Rebase Fast (TR), Ufi Gel Hard (UGH), Duraliner II (D), Kooliner (K), New Truliner (NT), and Light Liner (LL). LL resin was additionally tested with an air-barrier coating (LLABC). Nine disks of each material (10 × 1 mm) were made and divided into 3 groups: group 1 (no postpolymerization treatment); group 2 (postpolymerization in microwave oven); group 3 (postpolymerization in water bath at 55°C for 10 minutes). L929 cells were cultured in 96-well plates and incubated for 24 hours in Eagle's medium. Eluates prepared from the disks or medium without disks (control) replaced the medium. Cytotoxicity was assessed by both dehydrogenase succinic activity (MTT) assay and incorporation of radioactive 3H-thymidine assay. Tests were carried out in quadruplicate and repeated twice. Differences between groups were determined by analysis of variance with Tukey multiple-comparison intervals (α = .05). Results: For MTT assay, the postpolymerization treatments had no effect on the cytotoxicity of all materials (P > .05). For 3H-thymidine assay, the postpolymerization treatments significantly decreased the cytotoxicity of UGH (P < .05). The cytotoxicity of K, NT, LL, and LLABC increased after microwave irradiation (P < .05). TR, NT, and LLABC showed an increase in cytotoxicity after water bath (P < .05). Conclusion: When assessed by MTT assay, the cytotoxicity of the materials was not affected by postpolymerization treatments. 3H-Thymidine assay showed that the cytotoxicity of the resins was not improved by the postpolymerization treatments, with the exception of UGH.
Resumo:
Purpose: To evaluate the effect of 2 postpolymerization treatments on toothbrushing wear (weight loss) and surface roughness of 3 autopolymerized reline resins-Duraliner II (D) (Reliance Dental), Kooliner (K) (Coe Laboratories), and Tokuso Rebase Fast (T) (Tokuyama Dental)-and 1 heat-polymerized resin, Lucitone 550 (L) (Dentsply International). Materials and Methods: Specimens (40 x 10 x 2mm) of each material (n = 24) were prepared and divided into 3 groups: control (no postpolymerization treatment); water bath (immersion in water at 55°C); and microwave (microwave irradiation). Specimens were dried until constant weight was achieved and the surface roughness (Ra) was measured. Tests were performed in a toothbrush machine using 20,000 strokes of brushing at a weight of 200 g, with the specimens immersed in 1:1 dentifrice/water slurry. Specimens were reconditioned to constant weight and the weight loss (mg) and surface roughness were evaluated. Data were analyzed by 2-way analysis of variance and followed by Tukey test (α = .05). Results: In the control group, the weight loss of materials D and T was lower (P < .05) than that of L. No differences among materials were found after postpolymerization treatments (P > .05). The weight loss of material T (control = 0.5 mg) was significantly increased (P < .05) after postpolymerization treatments (water bath = 1.9 mg; microwave = 1.8 mg). For materials K and T, the toothbrushed surface roughness was higher (P < .05) after microwave and waterbath postpolymerization treatments. Material L showed increased surface roughness after microwave postpolymerization treatment. Conclusion: The toothbrushing wear resistance of L was not superior to the reline resins. The postpolymerization treatments did not improve the toothbrushing wear resistance of the materials and produced an increased surface roughness for materials L, K, and T.
Resumo:
Purpose: Potential effects on hardness and roughness of a necessary and effective disinfecting regimen (1% sodium hypocholorite and 4% chlorhexidine) were investigated for two hard chairside reline resins versus a heat-polymerizing denture base acrylic resin. Materials and Methods: Two standard hard chairside reliners (Kooliner and Duraliner II), one heat-treated chairside reliner (Duraliner II +10 minutes in water at 55°C), and one standard denture base material (Lucitone 550) were exposed to two disinfecting solutions (1% sodium hypochlorite; 4% chlorhexidine gluconate), and tested for two surface properties [Vickers hardness number (VHN, kg/mm2); Roughness (Ra, μm)] for different times and conditions (1 hour after production, after 48 hours at 37 ± 2°C in water, after two disinfection cycles, after 7 days in disinfection solutions, after 7 days in water only). For each experimental condition, eight specimens were made from each material. Data were analyzed by analysis of variance followed by Tukey's test, and Student's t-test (p= 0.05). Results: For Kooliner (from 6.2 ± 0.3 to 6.5 ± 0.5 VHN) and Lucitone 550 (from 16.5 ± 0.4 to 18.4 ± 1.7 VHN), no significant changes in hardness were observed either after the disinfection or after 7 days of immersion, regardless of the disinfectant solution used. For Duraliner II (from 4.0 ± 0.1 to 4.2 ± 0.1 VHN), with and without heat treatment, a small but significant increase in hardness was observed for the specimens immersed in the disinfectant solutions for 7 days (from 4.3 ± 0.2 to 4.8 ± 0.5 VHN). All materials showed no significant change in roughness (Kooliner: from 0.13 ± 0.05 to 0.48 ± 0.24 μm; Duraliner II, with and without heat treatment: from 0.15 ± 0.04 to 0.29 ± 0.07 μm; Lucitone 550: from 0.44 ± 0.19 to 0.49 ± 0.15 μm) after disinfection and after storage in water for 7 days. Conclusions: The disinfectant solutions, 1% sodium hypochlorite and 4% chlorhexidine gluconate, caused no apparent damage on hardness and roughness of the materials evaluated. Copyright © 2006 by The American College of Prosthodontists.
Resumo:
Purpose: This study assessed the shear bond strength of 4 hard chairside reline resins (Kooliner, Tokuso Rebase Fast, Duraliner II, Ufi Gel Hard) to a rapid polymerizing denture base resin (QC-20) processed using 2 polymerization cycles (A or B), before and after thermal cycling. Materials and Methods: Cylinders (3.5 mm x 5.0 mm) of the reline resins were bonded to cylinders of QC-20 polymerized using cycle A (boiling water-20 minutes) or B (boiling water; remove heat-20 minutes; boiling water-20 minutes). For each reline resin/polymerization cycle combination, 10 specimens (groups CAt e CBt) were thermally cycled (5 and 55°C; dwell time 30 seconds; 2,000 cycles); the other 10 were tested without thermal cycling (groups CAwt ad CBwt). Shear bond tests (0.5 mm/min) were performed on the specimens and the failure mode was assessed. Data were analyzed by 3-way ANOVA and Newman-Keuls post-hoc test (α=.05). Results: QC-20 resin demonstrated the lowest bond strengths among the reline materials (P<.05) and mainly failed cohesively. Overall, the bond strength of the hard chairside reline resins were similar (10.09±1.40 to 15.17±1.73 MPa) and most of the failures were adhesive/cohesive (mixed mode). However, Ufi Gel Hard bonded to QC-20 polymerized using cycle A and not thermally cycled showed the highest bond strength (P<.001). When Tokuso Rebase Fast and Duraliner II were bonded to QC-20 resin polymerized using cycle A, the bond strength was increased (P=.043) after thermal cycling. Conclusions: QC-20 displayed the lowest bond strength values in all groups. In general, the bond strengths of the hard chairside reline resins were comparable and not affected by polymerization cycle of QC-20 resin and thermal cycling.
Resumo:
This study evaluated the effect of water-bath and microwave post-polymerization treatments on the flexural strength and Vickers hardness of four autopolymerizing reline resins (Duraliner II-D, Kooliner-K, Tokuso Rebase Fast-TR and Ufi Gel Hard C-UGH) and one heat-polymerized acrylic resin (Lucitone 550-L), processed using two polymerization cycles (short cycle - 90 minutes at 73°C and 100°C for 30 minutes; and long cycle - 9 hours at 71°C). For each material, thirty specimens (64 x 10 x 3.3 mm) were made and divided into 3 groups (n=10). Specimens were tested after: processing (control group); water-bath at 55°C for 10 minutes (reline materials) or 60 minutes (L); and microwave irradiation. Flexural strength tests were performed at a crosshead speed of 5 mm/min using a three-point bending device with a span of 50 mm. The flexural strengths values were calculated in MPa. One fragment of each specimen was submitted to Vickers hardness test. Data were analyzed by 2-way ANOVA followed by Tukey's HSD test (α=0.05). L microwaved specimens (short cycle) exhibited significantly higher flexural strength means than its respective control group (p<0.05). Water-bath promoted a significant increase (p<0.05) in flexural strength of K and L (long cycle). The hardness of the tested materials was not influenced by the post-polymerization treatments. Post-polymerization treatments could be used to improve the flexural strength of some materials tested.
Resumo: