59 resultados para Restorative material
em Repositório Institucional UNESP - Universidade Estadual Paulista "Julio de Mesquita Filho"
Resumo:
The usefulness of fluoride-releasing restorations in secondary caries prevention may be questioned because of the presence of other common sources of fluoride and because of ageing of the restorations. This study tested the hypothesis that glass-ionomer cement restorations, either aged or unaged, do not prevent secondary root caries, when fluoride dentifrice is frequently used. Sixteen volunteers wore palatal appliances in two phases of 14 days, according to a 2 x 2 crossover design. In each phase the appliance was loaded with bovine root dentine slabs restored with either glass-ionomer or resin composite, either aged or unaged. Specimens were exposed to cariogenic challenge 4 times/day and to fluoridated dentifrice 3 times/day. The fluoride content in the biofilm (FB) formed on slabs and the mineral loss (Delta Z) around the restorations were analysed. No differences were found between restorative materials regarding the FB and the Delta Z, for either aged (p = 0.792 and p = 0.645, respectively) or unaged (p = 1.00 and p = 0.278, respectively) groups. Under the cariogenic and fluoride dentifrice exposure conditions of this study, the glass-ionomer restoration, either aged or unaged, did not provide additional protection against secondary root caries. Copyright (c) 2006 S. Karger AG, Basel.
Resumo:
Purpose: The aim of this study was to assess the contributions of some prosthetic parameters such as crown-to-implant (C/I) ratio, retention system, restorative material, and occlusal loading on stress concentrations within a single posterior crown supported by a short implant. Materials and Methods: Computer-aided design software was used to create 32 finite element models of an atrophic posterior partially edentulous mandible with a single external-hexagon implant (5 mm wide × 7 mm long) in the first molar region. Finite element analysis software with a convergence analysis of 5% to mesh refinement was used to evaluate the effects of C/I ratio (1:1; 1.5:1; 2:1, or 2.5:1), prosthetic retention system (cemented or screwed), and restorative material (metal-ceramic or all ceramic). The crowns were loaded with simulated normal or traumatic occlusal forces. The maximum principal stress (σmax) for cortical and cancellous bone and von Mises stress (σvM) for the implant and abutment screw were computed and analyzed. The percent contribution of each variable to the stress concentration was calculated from the sum of squares analysis. Results: Traumatic occlusion and a high C/I ratio increased stress concentrations. The C/I ratio was responsible for 11.45% of the total stress in the cortical bone, whereas occlusal loading contributed 70.92% to the total stress in the implant. The retention system contributed 0.91% of the total stress in the cortical bone. The restorative material was responsible for only 0.09% of the total stress in the cancellous bone. Conclusion: Occlusal loading was the most important stress concentration factor in the finite element model of a single posterior crown supported by a short implant.
Resumo:
Os cimentos ionoméricos representam importante opção de material restaurador em Odontologia e sua adesão à estrutura dental, diminuindo a infiltração marginal, somada à liberação de flúor, inibindo o metabolismo de microrganismos acidogênicos e favorecendo a remineralização dental, podem diminuir a ocorrência de cárie secundária. A aplicação tópica de géis acidulados ou neutros contendo flúor tem sido largamente utilizada em Odontologia. No entanto, este procedimento pode afetar a integridade dos materiais restauradores, aumentando sua rugosidade e a retenção de placa bacteriana. Dessa forma, o presente estudo avaliou o período de tempo no qual o cimento ionomérico Vitremer mantém sua capacidade inibitória sobre Streptococcus mutans ATCC 25175 e a adesão dos mesmos sobre a superfície do material, bem como a influência da aplicação tópica de flúor acidulado e neutro sobre esses parâmetros microbiológicos e as características superficiais daquele material. Verificou-se que a atividade antimicrobiana do cimento ionomérico Vitremer se mantém por aproximadamente quatro dias e não é recuperada com o uso de flúor gel acidulado ou neutro. Observou-se, também, que Streptococcus mutans ATCC 25175 adere ao material restaurador testado sendo que a aplicação tópica de flúor não influenciou esta adesão. As características superficiais desses materiais não se alteraram com a aplicação dos géis.
Resumo:
The aim of this study was to evaluate the effects of carbamide peroxide (CP) on surfaces of different restorative materials. Porcelain, composite resin, glass ionomer, and amalgam were analyzed in this study. Surface roughness (Ra) was measured before and after treatment with 10% and 15% CP. Fifteen percent CP increased Ra values in both the glass ionomer and amalgam subgroups, while 10% CP increased Ra values in the glass ionomer subgroup only. Changes in restorative material surfaces can be more severe when bleaching is completed without a clinician's supervision. Hence, thorough patient examinations must be done before, during, and after bleaching treatment. Int J Prosthodont 2011;24:155-157
Resumo:
This in vitro study evaluated the effect of erosive pH cycling on the percentage of surface micro-hardness change (%SMHC) and wear of different restorative materials and bovine enamel restored with these materials. Eighty enamel specimens were randomly divided into eight groups according to the restorative materials and immersion media used: GI/GV-resin-modifled glass-ionomer, GII/GVI-conventional glass-ionomer, GIII/GVII-resin composite and GIV/GVIII-amalgam. Over a period of seven days, groups GI to GIV were immersed in a cola drink (ERO) for 5 minutes, 3x/day and kept in artificial saliva between erosive cycles. Groups GV to GVIII were immersed in artificial saliva (SAL) throughout the entire experimental period (control). Data were tested for significant differences using ANOVA and Tukey's tests (p < 0.05). For %SMHC, considering the restorative materials, no significant differences were detected among the materials and immersion media. Mean wear was higher for the resin modified glass ionomer cement when compared to conventional cement, but those materials did not significantly differ from the others. For enamel analyses, erosive pH cycling promoted higher wear and %SMHC compared to saliva. There were no significant differences in wear and %SMHC of enamel around the different restorative materials, regardless of the distance from the restorative material (50, 150 or 300 mu m). In conclusion, there were only subtle differences among the materials, and these differences were not able to protect the surrounding enamel from erosion.
Resumo:
Objective. The aim of this in vitro study was to evaluate the interaction between two sources of fluoride (restorative systems and dentifrices) in inhibiting artificial root caries development. Methods. One hundred and eighty tooth segments were embedded in polyester resin, and sanded flat. Cylindrical cavities 1.0 mm-deep and 1.5 mm-diameter were prepared in root dentin and randomly restored by fluoride-containing restorative systems: Ketac-fil/Espe (Ke), Fuji II LC/GC Corp (Fj), F2000/3M (F2), Surefil/Dentsply (Su) or a control: Filtek Z250/3M (Z2). Ten experimental groups were made to test the association among the five restorative systems and two dentifrices: with F - (Sensodyne Baking Soda) or without F- (Sensodyne Original) (n = 18). After surface polishing, a 1 mm-wide margin around the restorations was demarcated and initial dentin surface Knoop microhardness values (KHNi) were obtained. The specimens were submitted to a pH-cycling model, and to applications of slurries of dentifrice. Afterwards the final dentin surface Knoop microhardness values (KHNf) were measured. Results. The differences between KHNi and KHNf, and the covariate KHNi were considered by the ANCOVA and Tukey's test (α = 0.05). The interaction between restorative system and dentifrice was statistically significant (p = 0.0026). All restorative systems provided some protection against artificial caries challenge when associated with the fluoride-containing dentifrice treatment. The means (standard deviation) of reductions in Knoop hardness values for systems associated with the fluoride-containing dentifrice were: Ke: 40.0(1.02)a, Fj: 41.9(1.02)b, F2: 43.3(1.04)c, Su: 43.5(1.00)c, Z2: 44.0(1.02)c; and with the non-fluoride-containing dentifrice were: Ke: 42.9(1.02)a, Fj: 44.7(1.01)b, F2: 45.2(1.09)bc, Su: 46.0(0.99)c, Z2: 46.6(0.99)c (statistical differences were expressed by different letters). Conclusion. The cariostatic effect shown by the fluoride-containing dentifrice could enhance that shown by Ketac-fil and Fuji II LC, and could mask that shown by F2000. © 2002 Elsevier Science Ltd. All rights reserved.
Resumo:
The radiopacity of esthetic restorative materials has been established as an important requirement, improving the radiographic diagnosis. The aim of this study was to evaluate the radiopacity of six restorative materials using a direct digital image system, comparing them to the dental tissues (enamel-dentin), expressed as equivalent thickness of aluminum (millimeters of aluminum). Five specimens of each material were made. Three 2-mm thick longitudinal sections were cut from an intact extracted permanent molar tooth (including enamel and dentin). An aluminum step wedge with 9 steps was used. The samples of different materials were placed on a phosphor plate together with a tooth section, aluminum step wedge and metal code letter, and were exposed using a dental x-ray unit. Five measurements of radiographic density were obtained from each image of each item assessed (restorative material, enamel, dentin, each step of the aluminum step wedge) and the mean of these values was calculated. Radiopacity values were subsequently calculated as equivalents of aluminum thickness. Analysis of variance (ANOVA) indicated significant differences in radiopacity values among the materials (P<0.0001). The radiopacity values of the restorative materials evaluated were, in decreasing order: TPH, F2000, Synergy, Prisma Flow, Degufill, Luxat. Only Luxat had significantly lower radiopacity values than dentin. One material (Degufill) had similar radiopacity values to enamel and four (TPH, F2000, Synergy and Prisma Flow) had significantly higher radiopacity values than enamel. In conclusion, to assess the adequacy of posterior composite restorations it is important that the restorative material to be used has enough radiopacity, in order to be easily distinguished from the tooth structure in the radiographic image. Knowledge on the radiopacity of different materials helps professionals to select the most suitable material, along with other properties such as biocompatibility, adhesion and esthetic.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
This in vitro study evaluated the demineralization around restorations class V made on the buccal and lingual surfaces of teeth when using different restorative materials. Thirty extracted teeth were randomly divided into 3 groups (n=10) according to the restorative material: Group I - Fuji II LC (GC America Inc., Alsip, Illinois, USA), Group II - Tetric (Ivoclar Vivadent AG, Schaan, Liechtenstein) and Group III - Chelon Fil (3M/ESPE., Seefeld, Germany). The teeth were submitted to a pH-cycling model associated to a thermocycling model. Sections were made and the specimens were analyzed under a polarized light microscopy as for the presence of demineralization. Measurements were performed and the results were subjected to statistical analysis using Anova and Tukey´s Test (α=0.05). Mean values of demineralization depth (µm) according to each positions showed that the demineralization was significantly reduced when Chelon Fil (Group III) was used for all depths, when compared to fluoridated resin materials. Also, it was verified that non-fluoridated resin material, composite resin Tetric, had the lowest inhibitory effect on the development of demineralization.
Resumo:
This incidence of postoperative sensitivity was evaluated in resin-based posterior restorations. Two hundred and ninety-two direct restorations were evaluated in premolars and molars. A total of 143 Class I and 149 Class 11 restorations (MO/OD and MOD) were placed in patients ranging in age from 30 to 50 years. After the cavity preparations were completed, a rubber dam was placed, and the preparations were restored using a total-etch system (Prime & Bond NT) and a resin-based restorative material (TPH Spectrum). The patients were contacted after 24 hours and 7, 30 and 90 days postoperatively and questioned regarding the presence of sensitivity and the stimuli that triggered that sensitivity. The Chi-square and Fisher's Exact Test were used for statistical analysis. Evaluation at 24 hours after restorative treatment revealed statistically significant differences among the types of cavity preparations restored and the occurrence of postoperative sensitivity (p=0.0003), with a higher frequency of sensitivity in Class H MOD restorations (26%), followed by Class II MO/DO (15%) and Class I restorations (5%). At 7, 30 and 90 days after restorative treatment, there was a decrease in the occurrence of sensitivity for all groups. The percentage of sensitivity among the groups was not significantly different. This study shows that the occurrence of sensitivity is correlated with the complexity of the restoration.
Resumo:
BackgroundEndodontic treatment, involves removal of the dental pulp and its replacement by a root canal filling. Restoration of root filled teeth can be challenging due to structural differences between vital and non-vital root filled teeth. Direct restoration involves placement of a restorative material e.g. amalgam or composite directly into the tooth. Indirect restorations consist of cast metal or ceramic (porcelain) crowns. The choice of restoration depends on the amount of remaining tooth which may influence long term survival and cost. The comparative in service clinical performance of crowns or conventional fillings used to restore root filled teeth is unclear.ObjectivesTo assess the effects of restoration of endodontically treated teeth (with or without post and core) by crowns versus conventional filling materials.Search methodsWe searched the following databases: the Cochrane Oral Health Group's Trials Register, CENTRAL, MEDLINE via OVID, EMBASE via OVID, CINAHL via EBSCO, LILACS via BIREME and the reference lists of articles as well as ongoing trials registries. There were no restrictions regarding language or date of publication. Date of last search was 13 February 2012.Selection criteriaRandomised controlled trials (RCTs) or quasi-randomised controlled trials in participants with permanent teeth which have undergone endodontic treatment. Single full coverage crowns compared with any type of filling materials for direct restoration, as well as indirect partial restorations (e.g. inlays and onlays). Comparisons considered the type of post and core used (cast or prefabricated post), if any.Data collection and analysisTwo review authors independently assessed trial quality and extracted data.Main resultsOne trial judged to be at high risk of bias due to missing outcome data, was included. 117 participants with a root filled premolar tooth restored with a carbon fibre post, were randomised to either a full coverage metal-ceramic crown or direct adhesive composite restoration. At 3 years there was no reported difference between the non-catastrophic failure rates in both groups. Decementation of the post and marginal gap formation occurred in a small number of teeth.Authors' conclusionsThere is insufficient evidence to support or refute the effectiveness of conventional fillings over crowns for the restoration of root filled teeth. Until more evidence becomes available clinicians should continue to base decisions on how to restore root filled teeth on their own clinical experience, whilst taking into consideration the individual circumstances and preferences of their patients.
Resumo:
Light dynamics is a relevant phenomenon with respect to esthetic restorations, as incorrect analysis of the optical behavior of natural dentition may lead to potential clinical failures. The nature of incident light plays a major role in determining the amount of light transmission or reflection, and how an object is perceived depends on the nature of the light source. Natural teeth demonstrate translucency, opalescence, and fluorescence, all of which must be replicated by restorative materials in order to achieve clinical success. Translucency is the intermediary between complete opacity and complete transparency, making its analysis highly subjective. In nature, the translucency of dental enamel varies from tooth to tooth, and from individual to individual. Therefore, four important factors must be considered when appraising translucency. Presence or absence of color, thickness of the enamel, degree of translucency, and surface texture are essential components when determining translucency. State-of-the-art resin composites provide varying shades and opacities that deliver a more faithful reproduction of the chromaticity and translucency/opacity of enamel and dentin. This enables the attainment of individualized and customized composite restorations. The objective of this article is to provide a review of the phenomena of translucency and opacity in the natural dentition and composite resins, under the scope of optics, and to describe how to implement these concepts in the clinical setting.CLINICAL SIGNIFICANCEChoosing composite resins, based on optical properties alone, in order to mimic the properties of natural tooth structures, does not necessarily provide a satisfactory esthetic outcome. In many instances, failure ensues from incorrect analysis of the optical behaviors of the natural dentition as well as the improper use of restorative materials. Therefore, it is necessary to implement a technique that enables a restorative material to be utilized to its full potential to correctly replicate the natural teeth.(J Esthet Restor Dent 23:73-88, 2011).
Resumo:
Purpose: To evaluate the root fracture strength of human single-rooted premolars restored with customized fiberglass post-core systems after fatigue simulation. Methods: 40 human premolars had their crowns cut and the root length was standardized to 13 mm. The teeth were endodontically treated and embedded in acrylic resin. The specimens were distributed into four groups (n=10) according to the restorative material used: prefabricated fiber post (PFP), PFP+accessory fiber posts (PFPa), PFP+unidirectional fiberglass (PFPf), and unidirectional fiberglass customized post (CP). All posts were luted using resin cement and the cores were built up with a resin composite. The samples were stored for 24 hours at 37 degrees C and 100% relative humidity and then submitted to mechanical cycling. The specimens were then compressive-loaded in a universal testing machine at a crosshead speed of 0.5 mm/minute until fracture. The failure patterns were analyzed and classified. Data was submitted to one-way ANOVA and Tukey's test (alpha= 0.05). Results: The mean values of maximum load (N) were: PFP - 811.4 +/- 124.3; PFPa - 729.2 +/- 157.2; PFPf - 747.5 +/- 204.7; CP - 762.4 +/- 110. Statistical differences were not observed among the groups. All groups showed favorable restorable failures. Fiberglass customized post did not show improved fracture resistance or differences in failure patterns when compared to prefabricated glass fiber posts. (Am J Dent 2012;25:35-38).