132 resultados para Dental restoration wear

em Repositório Institucional UNESP - Universidade Estadual Paulista "Julio de Mesquita Filho"


Relevância:

100.00% 100.00%

Publicador:

Resumo:

A quantitative study was made about the effects caused by ionizing irradiation on materials used for dental restoration (amalgams, compound resins and compomere), aiming to alleviate in bearers of head and neck cancer, the possible harmful effects of radiotherapy perceived when the repaired teething is within the radiation field. Research also encourages further studies for new alternative materials to be used in dental repair of patients submitted to radiotherapy for head and neck cancer. Test samples were submitted to a gamma radiation beam coming from a cobalt-therapy source and analyzed according to the X-ray fluorescence technique, comparing the chemical composition of the samples before and after irradiation. Radiation detectors such as an ionization chamber and a Geiger-Muller were used to measure the rate of residual dose. Gamma spectrometry with Nal detectors was also performed on the same samples. Results showed that there was no significant change in the chemical composition and that at post-irradiation, samples did not exhibit radiation emission, that is to say they had not become radioactive.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This randomized clinical trial sought to evaluate the performance of two packable composites over a period of 36 months. A total of 39 Class I and II restorations were placed in the permanent teeth of 20 patients. Using United States Public Health Services criteria, two investigators evaluated the restorations immediately after placement and again after 12 and 36 months, examining color match, marginal discoloration, marginal integrity, recurrent caries, proximal contact, anatomical shape, surface texture, and postoperative sensitivity. It was concluded that the packable composites evaluated showed satisfactory clinical performance after three years.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

To compare the abrasion wear resistance and superficial roughness of different glass ionomer cements used as restorative materials, focusing on a new nanoparticulate material. Material and Method: Three glass ionomer cements were evaluated: Ketac Molar, Ketac N100 and Vitremer (3M ESPE, St. Paul, MN, USA), as well as the Filtek Z350 (3M ESPE, St. Paul, MN, USA). For each material were fabricated circular specimens (n=12), respecting the handling mode specified by the manufacturer, which were polished with sandpaper disks of decreasing grit. The wear was determined by the amount of mass (M) lost after brushing (10,000 cycles) and the roughness (Ra) using a surface roughness tester. The difference between the Minitial and Mfinal (ΔM) as well as beroughness of aesthetic restorative materials: an in vitro comparison. SADJ. 2001; 56(7): 316-20. 11. Yip HK, Peng D, Smales RJ. Effects of APF gel on the physical structure of compomers and glass ionomer cements. Oper. Dent. 2001; 26(3): 231-8. 12. Ma T, Johnson GH, Gordon GE. Effects of chemical disinfectants on the surface characteristics and color of denture resins. J Prosthet Dent 1997; 77(2): 197-204. 13. International organization for standardization. Technical specification 14569-1. Dental Materials – guidance on testing of wear resistance – PART I: wear by tooth brushing. Switzerland: ISO; 1999. 14. Bollen CML, Lambrechts P, Quirynen M. Comparison of surface roughness of oral hard materials to the threshold surface roughness for bacterial plaque retention: a review of the literature. Dent Mater.1997; 13(4): 258-9. 15. Kielbassa AM, Gillmann C, Zantner H, Meyer-Lueckel H, Hellwig E, Schulte-Mönting J. Profilometric and microradiographic studies on the effects of toothpaste and acidic gel abrasivity on sound and demineralized bovine dental enamel. Caries Res. 2005; 39(5): 380-6. 16. Tanoue N, Matsumara H, Atsuta M. Wear and surface roughness of current prosthetic composites after toothbrush/dentifrice abrasion. J Prosthet Dent. 2000; 84(1): 93-7. 17. Heath JR, Wilson HJ. Abrasion of restorative materials by toothpaste. J Oral Rehabil. 1976; 3(2): 121-38. 18. Frazier KB, Rueggeberg FA, Mettenburg DJ. Comparasion of wearresistance of class V restorative materials. J Esthet Dent. 1998; 10(6): 309-14. 19. Momoi Y, Hirosakil K, Kohmol A, McCabe JF. In vitro toothebrushdentifrrice abrasion of resin-modified glass ionomers. Dent Mater. 1997; 13(2): 82-8. 20. Turssi CP, Magalhães CS, Serra MC, Rodrigues Jr.AL. Surface roughness assessment of resin-based materials during brushing preceded by pHcycling simulations. Oper Dent. 2001; 26(6): 576-84. 21. Wang L, Cefaly DF, Dos Santos JL, Dos Santos JR, Lauris JR, Mondelli RF, et al. In vitro interactions between lactic acid solution and art glassionomer cements. J Appl Oral Sci. 2009; 17(4): 274-9. 22. Carvalho FG, Fucio SB, Paula AB, Correr GM, Sinhoreti MA, PuppinRontani RM. Child toothbrush abrasion effect on ionomeric materials. J Dent Child (Chic). 2008; 75(2): 112-6. 23. Coutinho E, Cardoso MV, De Munck J, Neves AA, Van Landuyt KL, Poitevin A, et al. Bonding effectiveness and interfacial characterization of a nano-filled resin-modified glass-ionomer. Dent Mater. 2009; 25(11): 1347-57. tween Rainitial and Rafinal (ΔRa) were also used for statistical analysis (α=0.05). Results: Except for the composite, significant loss of mass was observed for all glass ionomer cements and the ΔM was comparable for all of them. Significant increase in roughness was observed only for Vitremer and Ketac N100. At the end of the brushing cycle, just Vitremer presented surface roughness greater than the composite resin. Conclusion: All glass ionomer cements showed significant weight loss after 10,000 cycles of brushing. However, only Vitremer showed an increase of roughness greater than the Z350 resin, while the nanoparticulate cement Ketac N100 showed a smooth surface comparable to the composite.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

OBJECTIVE: The aim of this study was to evaluate the resistance to fracture of intact and restored human maxillary premolars. METHOD AND MATERIALS: Thirty noncarious human maxillary premolars, divided into three groups of 10, were submitted to mechanical tests to evaluate their resistance to fracture. Group 1 consisted of intact teeth. Teeth in group 2 received mesio-occlusodistal cavity preparations and were restored with direct resin composite restorations. Teeth in group 3 received mesio-occlusodistal cavity preparations and were restored with ceromer inlays placed with the indirect technique. After restoration, teeth were stored at 37 degrees C for 24 hours and then thermocycled for 500 cycles at temperatures of 5 degrees C and 55 degrees C. RESULTS: Statistical analysis revealed that group 3 (178.765 kgf) had a significantly greater maximum rupture load than did group 1 (120.040 kgf). There was no statistically significant difference between groups 1 and 2 or between groups 2 and 3. CONCLUSION: Class II cavity preparations restored with indirect ceromer inlays offered greater resistance to fracture than did intact teeth. The fracture resistance of teeth restored with resin composite was not significantly different from that of either the ceromer or intact teeth.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The objective of this in vitro study was to quantitatively assess the effects of bleaching with 10 and 15% carbamide peroxide (CP) on restoration materials by performing superficial microhardness analysis. Acrylic cylindrical containers (4 x 2 mm) were filled with the following restoration products: Charisma (Heraues Kulzer, Vila Santa Catarina, São Paulo, Brazil), Durafill VS (Heraeus Kulzer), Vitremer (3M, Sumaré, São Paulo, Brazil), Dyract (Dentsply, Petrópolis, Rio de Janeiro, Brazil), and Permite C (SDI, São Pauio, São Paulo, Brazil). Sixty samples were prepared of each restoration material. Twenty samples received bleaching treatment with 10% CP, 20 samples received bleaching treatment with 15% CP, and 20 samples were kept submerged in artificial saliva, which was replaced daily. The treatment consisted of immersion of the specimens in 1 cm3 of CP at 10 and 15% for 6 hours per day during 3 weeks, whereupon the test specimens were washed, dried, and kept immersed in artificial saliva for 18 hours. Then the test and control specimens were analyzed using a microhardness gauge. The Knoop Hardness Number (KHN) was taken for each test and control specimen at five different locations by applying a 25 g force for 20 seconds. The values obtained were transformed into KHNs and the mean was calculated. The data were submitted to statistical analysis by analysis of variance and Tukey test, p < .05. The means/standard deviations were as follows: Charisma: CP 10% 38.52/4.08, CP 15% 34.31/6.13, saliva 37.36/4.48; Durafill VS: CP 10% 18.65/1.65, CP 15% 19.38/2.23, saliva 18.27/1.43; Dyract AP: CP 10% 30.26/2.81, CP 15% 28.64/5.44, saliva 33.88/3.46; Vitremer: CP 10% 28.15/3.04, CP 15% 17.40/3.11, saliva 40.93/4.18; and Permite C: CP 10% 183.50/27.09, CP 15% 159.45/5.78, saliva 215.80/26.15. A decrease in microhardness was observed for the materials Dyract AP, Vitremer, and Permite C after treatment with CP at 10 and 15%, whereas no effect on either of the two composites (Charisma and Durafill) was verified. CLINICAL SIGNIFICANCE: The application of the carbamide peroxide gels at 10 and 15% did not alter the microhardness of the composite resins Charisma and Durafill. In situ and clinical studies are necessary to enable one to conclude that the reduction in microhardness of the materials effectively results in clinical harm to the restorations.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Purpose: Tissue reactions to 4 different implant surfaces were evaluated in regard to the development and progression of ligature-induced peri-implantitis. Materials and Methods: In 6 male mongrel dogs, a total of 36 dental implants with different surfaces (9 titanium plasma-sprayed, 9 hydroxyapatite-coated, 9 acid-etched, and 9 commercially pure titanium) were placed 3 months after mandibular premolar extraction. After 3 months with optimal plaque control, abutment connection was performed. Forty-five days later, cotton ligatures were placed around the implants to induce peri-implantitis. At baseline and 20, 40, and 60 days after placement, the presence of plaque, peri-implant mucosal redness, bleeding on probing, probing depth, clinical attachment loss, mobility, vertical bone loss, and horizontal bone loss were assessed. Results: The results did not show significant differences among the surfaces for any parameter during the study (P > .05). All surfaces were equally susceptible to ligature-induced peri-implantitis over time (P < .001). Correlation analysis revealed a statistically significant relationship between width of keratinized tissue and vertical bone loss (r 2 = 0.81; P = .014) and between mobility and vertical bone loss (r 2 = 0.66; P = .04), both for the titanium plasma-sprayed surface. Discussion and Conclusions: The present data suggest that all surfaces were equally susceptible to experimental peri-implantitis after a 60-day period.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Single nucleotide polymorphisms in the promoter region of the human interleukin (IL)-2 (T-330G) and IL-6 (G-174C) genes have modified the transcriptional activity of these cytokines and are associated with several diseases. The aim of this study was to investigate the possible relationship between these single nucleotide polymorphisms and early implant failure. A sample of 74 nonsmokers was divided into 2 groups: test group comprising 34 patients (mean age 49.3 years) with ĝ‰¥1 implants that failed and control group consisting of 40 patients (mean age 43.8 years) with ĝ‰¥1 healthy implants. Genomic deoxyribonucleic acid from oral mucosa was amplified by polymerase chain reaction and analyzed by restriction fragment length polymorphism. Monte Carlo simulations (P < 0.05) were used to assess differences in allele and genotypes frequencies of the single nucleotide polymorphisms between the 2 groups. No significant differences were observed in the allele and genotypes distribution of both polymorphisms when the 2 groups were compared. The results indicate that polymorphisms in the IL-2 (T-330G) and IL-6 (G-174C) genes are not associated with early implant failure, suggesting that the presence of those single nucleotide polymorphisms does not constitute a genetic risk factor for implant loss in the studied population. Copyright © 2005 by Lippincott Williams & Wilkins.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

A survey was sent to 70 Brazilian dental schools evaluating techniques and restorative materials being taught for Class I and II preparation in posterior primary teeth by Pediatric Dentistry courses. After a 54% response rate, marked teaching diversity was found among Brazilian dental schools. Amalgam continues to be taught, but a tendency of preference towards more esthetic-like materials was observed.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The objective of this in vitro study was to evaluate demineralization around restorations. Class V preparations were made on the buccal and lingual surfaces of each tooth. TPH (Group 1), Fuji II LC (Group 2), Tetric (Group 3), Dyract (Group 4), GS 80 (Group 5) and Chelon Fil (Group 6) were randomly placed in equal numbers of teeth. The teeth were submitted to a pH-cycling model associated with a thermocycling model. Sections were made and the specimens were examined for the presence of demineralization under polarized light microscopy. Demineralization was significantly reduced with Chelon Fil (Group 6). Furthermore, a similar inhibitory effect on the development of demineralization was observed in Groups 2, 4 and 5.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objectives: To compare the response of human dental pulp capped with a mineral trioxide aggregate (MTA) and Ca(OH) 2 powder. Methods and Material: Pulp exposures were performed on the occlusal floor of 40 permanent premolars. The pulp was then capped with either Ca(OH) 2 powder (CH) or MTA and restored with resin composite. After 30 days (groups CH30 and MTA30) and 60 days (groups CH60 and MTA60), the teeth were extracted and processed for HE and categorized in a histological score system. The data were subjected to Kruskal-Wallis and Conover tests (α=0.05). Results: In regard to dentin bridge formation, CH30 showed a tendency towards superior performance compared to MTA30 (p>0.05), although the products showed comparable results at day 60. In the item Inflammation and General State of the Pulp (p>0.05), CH showed a tendency towards presenting a higher inflammatory response. In the item Other Pulpal Findings, MTA and Ca(OH) 2 showed equal and excellent performance after 30 and 60 days (p>0.05). Conclusion: After 30 days, Ca(OH) 2 powder covered with calcium hydroxide cement showed faster hard tissue bridge formation compared to MTA. After 60 days, Ca(OH) 2 powder or MTA materials showed a similar and excellent histological response with the formation of a hard tissue bridge in almost all cases with low inflammatory infiltrate. © Operative Dentistry, 2008.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Child temperament has been studied in various researches and may be useful to predict how a child responds to dental treatment, especially very young children. The purpose of the present longitudinal study was to evaluate the behavioral manifestation of children aged 0 to 3 years, considering different types of dental situation. A total of 169 children were selected and the following data were collected: the age of the child, gender, age of the mother, number of dental visits and their respective dates, stimuli offered to the child, and behavioral response to these stimuli. The children and their respective behaviors were divided into five groups according to the dental situation offered: control, missed visits, fluoride varnish, restoration, and dental trauma. The data were submitted to descriptive and inferential analysis using the chi-square test, with the level of significance set at 5%. Analysis of the different situation offered to infants during routine dental care revealed a predominance of collaborating and partially collaborating behavior, and age at the time of dental care influenced the behavior of the infants, irrespective of the stimulus group. The different types of dental situation provoked changes in the behavioral response of the children of certain age groups, especially in the dental trauma group.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

This study evaluated the Knoop hardness and polymerization depth of a dual-cured resin cement, light-activated at different distances through different thicknesses of composite resin. One bovine incisor was embedded in resin and its buccal surface was flattened. Dentin was covered with PVC film where a mold (0.8-mm-thick and 5 mm diameter) was filled with cement and covered with another PVC film. Light curing (40 s) was carried out through resin discs (2, 3, 4 or 5 mm) with a halogen light positioned 0, 1, 2 or 3 mm from the resin surface. After storage, specimens were sectioned for hardness measurements (top, center, and bottom). Data were subjected to split-plot ANOVA and Tukey's test (α=0.05). The increase in resin disc thickness decreased cement hardness. The increase in the distance of the light curing tip decreased hardness at the top region. Specimens showed the lowest hardness values at the bottom, and the highest at the center. Resin cement hardness was influenced by the thickness of the indirect restoration and by the distance between the light-curing unit tip and the resin cement surface.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

With the arrival of self-etch adhesives systems, there has been a rise in interest among clinicians, making it imperative for health professionals to have knowledge of the properties, characteristics, the association as well as the dental structures of these materials, in order to select them and use them correctly. The self-etch adhesive systems show good values of bond strength, microleakage and performance, and have therefore become an option in direct adhesive restorations. In the regard, this case study aims to describe the technique involving the use of selfetch adhesives system for direct restoration of anterior teeth.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objective: The prevalence of wearing and fracture of complete dentures was evaluated among edentulous patients treated in two dental schools in Brazil. Background: Acceptance and wearing of complete dentures are related to adaptive behaviour of edentulous patients. However, one reason that could interfere with the wearing dentures is their potential to fracture, which is still a common complication in denture rehabilitation practice. Material and methods: Two hundred and twenty-four edentulous patients rehabilitated with complete dentures from 2000 to 2005 in Araçatuba and Araraquara Dental School, University of State of São Paulo, were assessed in 2006 and 2007 to answer a questionnaire about wearing and fracture of their dentures. Statistical analysis were performed using Epi Info software and chi-squared test to compare maxillary and mandibular data (α = 0.05). Results: Almost 26% of the patients did not wear their dentures, and among the remainder, the majority wore the maxillary denture. About 30% of the dentures were fractured, with higher prevalence in the maxillary arch (p = 0.003). Conclusions: Discontinuation of wearing dentures was quite high, especially considering the treatment which was carried out in university clinics. Prevalence of fractures was also high, greater for the maxillary denture, and was one of the main reasons for non-wearing of complete dentures. © 2011 The Gerodontology Society and John Wiley & Sons A/S.