Objectives: The purpose of this study was to investigate the effect of thermal cycling and disinfection on the colour change of denture base acrylic resin. Materials and Methods: Four different brands of acrylic resins were evaluated (Onda Cryl, QC 20, Classico and Lucitone). All brands were divided into four groups (n=7) determined according to the disinfection procedure (microwave, Efferdent, 4% chlorhexidine or 1% hypochlorite). The treatments were conducted three times a week for 60days. All specimens were thermal cycled between 5 and 55°C with 30-s dwell times for 1000 cycles before and after disinfection. The specimens' colour was measured with a spectrophotometer using the CIE L*a*b* system. The evaluations were conducted at baseline (B), after first thermal cycling (T 1), after disinfection (D) and after second thermal cycling (T 2). Colour differences (ΔE) were calculated between T 1 and B (T 1B), D and B (DB), and T 2 and B (T 2B) time-points. Results: The samples submitted to disinfection by microwave and Efferdent exhibited the highest values of colour change. There were significant differences on colour change between the time-points, except for the Lucitone acrylic resin. Conclusions: The thermal cycling and disinfection procedures significantly affected the colour stability of the samples. However, all values obtained for the acrylic resins are within acceptable clinical parameters. © 2012 The Gerodontology Society and John Wiley & Sons A/S.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Colour stability of resin and silicone is an important factor for longevity of facial prostheses. The aim of this study was to evaluate the colour stability of resins and silicone for facial prostheses. Three brands of acrylic resin and one of facial silicone were evaluated considering pigment incorporation for the colourless materials. Ten samples of each material were fabricated and submitted to measurements of chromatic alteration initially and after 90 and 180 days of weathering natural through visual analysis and spectrophotometry. Data were evaluated by ANOVA and Tukey test (p < 0.05). Statistically significant colour alteration was observed among some materials regardless of the period. The materials did not present a statistical difference between 90 and 180 days except for the pigmented heat-polymerized resin. The colour difference between pigmented Silastic MDX4-4210 and colourless Silastic was statistically significant (p < 0.01) in both periods as well as between pigmented and colourless heat-polymerized resin, and between the resins Rapidaflex and Lentaflex. The visual method demonstrated colour alteration in all materials evaluated during the first 90 days of ageing. All materials exhibited colour alteration due to exposure to environment. © 2012 Informa UK, Ltd.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)