Resumo:

Purpose: Bioactive glass and bioactive glass-ceramic cone implants were placed in the rabbit eviscerated socket to assess their biocompatibility. Methods: Fifty-one Norfolk albino rabbits underwent evisceration of the right eye followed by implantation of cones made from Bioglass® 45S5 (control group) and two types of bioactive glass-ceramic (Biosilicate®), a single- and a two-phase bioactive glass-ceramic implants into the scleral cavity. Postoperative reactions, animal behavior and socket conditions were monitored daily. Clinical exam, biochemical evaluations, and orbit computed tomographic scan were done at 7, 90, and 180 days post-procedure. After that, the animals were euthanized, and the orbital content was removed and prepared to light microscopy with morphometric evaluation and scanning electron microscopy examination. Statistical analysis was done by parametric and non-parametric analysis of variance, complemented by Dunn's and Tukey's tests (p<0.05). Results: All animals did not develop systemic toxicity throughout the experimental period and also did not have orbit infection, implant migration or extrusion. Morphological analysis demonstrated pseudocapsule around all implants. Bioglass® and single-phase Biosilicate® implants induced less inflammation and pseudocapsule formation than two-phase Biosilicate® cones. Seven days post-procedure, the inflammatory reaction was intense and gradually decreased throughout the experiment. Tissue reaction was least intense in animals receiving Bioglass® implants. Conclusions: We observe discrete differences among the studied materials, with best responses obtained with use of Bioglass® 45S5 and single-phase Biosilicate®. The authors agree these implants might be useful in the management of the anophthalmic socket. © 2012 Informa Healthcare USA, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The bovine bone and sintetic hydroxyapatite (HA) bioceramics are reference materials to employment as a bone substitute, however, their slow rate of degradation and its low rate of bioactivity index (Ib) are presented as limiting factors for application as bone graft. In contrast, the bioglass is a resorbable and osteoinductive material. the present work objective the development of composites of dispersed bovine bone or sintetic HA in silicate-phosphate bioglass, seeking to obtain a biomaterial with properties suitable for application as bone grafts. The composites were prepared by mixing between the powder components followed by sintering for 1h. Were used HA and bioglass (45S5) with particle size <240μm. The tested proportions of HA/45S5 were 20/80, 30/70 and 40/60 (wt%). The composites characterization was made employing scanning electron microscopy, Infra-Red Spectrometry and hydrolytic resistance test. The test results indicate the potential use of the materials developed for applications such as bone graft. © (2012) Trans Tech Publications, Switzerland.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na 2O and CaO or by adding P 2O 5 to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a controlled two-stage heat treatment process. Rods (2 mm x 4 mm) were produced using the conventional lost-wax casting technique. Osteoconductive 45S5 bioglass was used as a reference material. Biocompatibility and osteoconductivity were investigated by implantation into healing defects (2 mm) in the midshaft of rabbit femora. Tissue response was investigated using conventional histology and scanning electron microscopy. Histological and histomorphometric evaluation of specimens after 12 weeks implantation showed significantly more bone contact with the surface of 45S5 bioglass implants when compared with other test materials. When the bone contact for each material was compared between experimental time points, the Glass-Ceramic 2 (CaO rich) group showed significant difference (p = 0.027) at 4 weeks, but no direct contact at 12 weeks. Histology and backscattered electron photomicrographs showed that modified fluorcanasite glass-ceramic implants had greater osteoconductivity than the parent stoichiometric composition. Of the new materials, fluorcanasite glass-ceramic implants modified by the addition of P 2O 5 showed the greatest stimulation of new mineralized bone tissue formation adjacent to the implants after 4 and 12 weeks implantation. © 2010 Wiley Periodicals, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Introduction: The radiographic characteristics of a biomaterial, such as its density, may influence the evaluation of the results obtained following its clinical use. Objective: The aim of this study was to evaluate the radiographic density of biomaterials used as bone substitutes, inserted into dental sockets and bone defects in created in the jaws of pigs. The influence of a soft tissue simulator on the results was also evaluated. Material and method: Two and three-millimeter-deep bone defects were created in the pigs mandible and the right first molar extraction socket were used. Commercial samples of five biomaterials were tested: Hydroxyapatite, Lyophilized Bovine Bone, 45S5 bioglass (generic), PerioGlass and β-Tri-Calcium Phosphate, and compared to a positive (mandibular bone) and negative (empty alveolar bone defects) controls. Radiographic images were acquired with and without a 10 mm thick soft-tissue simulator. Result: The results for the extraction sockets showed no differences between the biomaterials and the negative control. For the bone defects, the depth of the defect density influenced the density, both in the negative control (p < 0.01) and biomaterials (p < 0.05) groups. The soft- tissue simulator did not alter the results. Conclusion: The type of the evaluated defect can interfere in the radiographic features presented by each biomaterial, while the simulation of soft tissues was not statistically significant.