371 resultados para Solution heat treatment


Relevância:

80.00% 80.00%

Publicador:

Resumo:

The effects of heat treatment on morphologies and microstructures of Al 2024 and Al 7050 alloys, used as aircraft components, were studied by metallographic techniques. Light microscopy (LM) and quantitative image analysis were used to characterize the precipitate dispersion and morphology for these alloys. The application of the scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) combined techniques for studying these multiphase systems makes it possible to distinguish and quantify the different phases in the surface structure. Xray diffraction also permitted a qualitative comparison of the structures before and after heat treatments.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Neste trabalho foi realizada a caracterização mecânica e microestrutural de um aço microligado com estrutura multifásica. Foi aplicado tratamento térmico pré-determinado, objetivando a formação de uma microestrutura multifásica no material. Na caracterização microestrutural foram utilizados ataques químicos à base de metabissulfito de sódio e ácido pícrico, enquanto a caracterização mecânica foi realizada através de ensaios de tração. Os resultados demonstram o elevado potencial dos aços multifásicos em aplicações que necessitem de valores superiores de resistência e ductilidade, pois tanto para temperatura isotérmica de 400ºC quanto para 350ºC houve um ganho no limite de resistência à tração ficando em torno de 786MPa e 773MPa respectivamente, representando um aumento de 15,5% e 13,6% com relação ao material fornecido.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

This article reports a study of the thermal stability and morphological changes in tin oxide nanobelts grown in the orthorhombic SnO phase. The nanobelts were heat-treated in a differential scanning calorimetry (DSC) furnace at 800 degrees C for I It in argon, oxygen, or synthetic air atmospheres. The samples were then characterized by DSC, X-ray diffraction (XRD), high resolution transmission electron microscopy (HRTEM), and high resolution field emission scanning electron microscopy (FE-SEM). The results confirmed that the orthorhombic SnO phase is thermodynamically unstable, causing the belts to transform into the SnO2 phase when heat-treated. During the phase transition, if oxygen is available in the furnace atmosphere, nanofibers grow at the edge of nanobelts at about 50 degrees of the belts' growth direction, while particles grow on the belt surface in the absence of oxygen. Although the decomposition process reduces the nanobelt cell volume by 22%, most belts remain monocrystalline after the heat treatment. The results confirm that phase transition is a decomposition process, which explains the morphological changes in the belts based on metallic tin generated in the process.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Objective-To evaluate the effects of epidural administration of 3 doses of dexmedetomidine on isoflurane minimum alveolar concentration (MAC) and characterize changes in bispectral index (BIS) induced by nociceptive stimulation used for MAC determination in dogs.Animals-6 adult dogs.Procedures-Isoflurane-anesthetized dogs received physiologic saline (0.9% NaCl) solution (control treatment) or dexmedetomidine (1.5 [DEX1.5], 3.0 [DEX3], or 6.0 [DEX6] mu g/kg) epidurally in a crossover study. Isoflurane MAC (determined by use of electrical nociceptive stimulation of the hind limb) was targeted to be accomplished at 2 and 4.5 hours. Changes in BIS attributable to nociceptive stimulation and cardiopulmonary data were recorded at each MAC determination.Results-With the control treatment, mean +/- SD MAC values did not change over time (1.57 +/- 0.23% and 1.55 +/- 0.25% at 2 and 4.5 hours, respectively). Compared with the control treatment, MAC was significantly lower at 2 hours (13% reduction) but not at 4.5 hours (7% reduction) in DEX1.5-treated dogs and significantly lower at 2 hours (29% reduction) and 4.5 hours (13% reduction) in DEX3-treated dogs. The DEX6 treatment yielded the greatest MAC reduction (31 % and 22% at 2 and 4.5 hours, respectively). During all treatments, noxious stimulation increased BIS; but changes in BIS were correlated with increases in electromyographic activity.Conclusions and Clinical Relevance-In dogs, epidural administration of dexmedetomidine resulted in dose-dependent decreases in isoflurane MAC and that effect decreased over time, Changes in BIS during MAC determinations may not represent increased awareness because of the possible interference of electromyographic activity.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Objective-To evaluate the cardiorespiratory and intestinal effects of the muscarinic type-2 (M-2) antagonist, methoctramine, in anesthetized horses.Animals-6 horses.Procedure-Horses were allocated to 2 treatments in a randomized complete block design. Anesthesia was maintained with halothane (1% end-tidal concentration) combined with a constant-rate infusion of xylazine hydrochloride (1 mg/kg/h, IV) and mechanical ventilation. Hemodynamic variables were monitored after induction of anesthesia and for 120 minutes after administration of methoctramine or saline (0.9% NaCl) solution (control treatment). Methoctramine was given at 10-minute intervals (10 mug/kg, IV) until heart rate (HR) increased at least 30% above baseline values or until a maximum cumulative dose of 30 mug/kg had been administered. Recovery characteristics, intestinal auscultation scores, and intestinal transit determined by use of chromium oxide were assessed during the postanesthetic period.Results-Methoctramine was given at a total cumulative dose of 30 mug/kg to 4 horses, whereas 2 horses received 10 mug/kg. Administration of methoctramine resulted in increases in HR, cardiac output, arterial blood pressure, and tissue oxygen delivery. Intestinal auscultation scores and intestinal transit time (interval to first and last detection of chromium oxide in the feces) did not differ between treatment groups.Conclusions and Clinical Relevance-Methoctramine improved hemodynamic function in horses anesthetized by use of halothane and xylazine without causing a clinically detectable delay in the return to normal intestinal motility during the postanesthetic period. Because of their selective positive chronotropic effects, M-2 antagonists may represent a safe alternative for treatment of horses with intraoperative bracycardia.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Nanostructures on implant surfaces have been shown to enhance osseointegration; however, commonly used evaluation techniques are probably not sufficiently sensitive to fully determine the effects of this process. This study aimed to observe the osseointegration properties of nanostructured calcium phosphate (CaP)-coated implants, by using a combination of three-dimensional imaging and conventional histology. Titanium implants were coated with stable CaP nanoparticles using an immersion technique followed by heat treatment. Uncoated implants were used as the control. After topographical and chemical characterizations, implants were inserted into the rabbit femur. After 2 and 4 weeks, the samples were retrieved for micro-computed tomography and histomorphometric evaluation. Scanning electron microscopy evaluation indicated that the implant surface was modified at the nanoscale by CaP to obtain surface textured with rod-shaped structures. Relative to the control, the bone-to-implant contact for the CaP-coated implant was significantly higher at 4 weeks after the implant surgery. Further, corresponding 3-D images showed active bone formation surrounding the implant. 3-D quantification and 2-D histology demonstrated statistical correlation; moreover, 3-D quantification indicated a statistical decrease in bone density in the non-coated control implant group between 2 and 4 weeks after the surgery. The application of 3-D evaluation further clarified the temporal characteristics and biological reaction of implants in bone. (C) 2011 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Objectives. This study characterized the feldspathic ceramic surfaces after various silanization protocols.Methods. Ceramic bars (2 mm x 4 mm x 10 mm) (N = 18) of feldpathic ceramic (VM7, VITA Zahnfabrik) were manufactured and finished. Before silane application, the specimens were ultrasonically cleaned in distilled water for 10 min. The ceramic specimens were randomly divided into nine groups (N = 2 per group) and were treated with different silane protocols. MPS silane (ESPE-Sil, 3M ESPE) was applied to all specimens and left to react at 20 degrees C for 2 min (G20). After drying, the specimens were subjected to heat treatment in an oven at 38 degrees C (G38), 79 degrees C (G79) or 100 degrees C (G100) for 1 min. Half of the specimens of each group were rinsed with water at 80 degrees C for 15 s (G20B, G38B, G79B, G100B). The control group (GC) received no silane. Attenuated total reflection infrared Fourier transform analysis (ATR FT-IR) was performed using a spectrometer. Thickness of silane layer was measured using a spectroscopic ellip-someter working in the lambda = 632.8 nm (He-Ne laser) at 70 degrees incidence angle. Surface roughness was evaluated using an optical profilometer. Specimens were further analyzed under the Scanning Electron Microscopy (SEM) to observe the topographic patterns.Results. ATR FT-IR analysis showed changes in Si-O peaks with enlarged bands around 940 cm(-1). Ellipsometry measurements showed that all post-heat treatment actions reduced the silane film thickness (30.8-33.5 nm) compared to G20 (40 nm). The groups submitted to rinsing in hot water (B groups) showed thinner silane films (9.8-14.4 nm) than those of their corresponding groups (without washing) (30.8-40 nm). Profilometer analysis showed that heat treatments (Ra approximate to 0.10-0.19 mu m; Rq approximate to 0.15-0.26 mu m) provided a smoother surface than the control group (Ra approximate to 0.48 mu m; Rq approximate to 0.65 mu m). Similar patterns were also observed in SEM images.Significance. Heat treatment after MPS silane application improved the silane layer network. Rinsing with boiling water eliminated the outmost unreacted regions of the silane yielding to thinner film thicknesses. (C) 2011 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Strontium zirconate (SrZrO3) powders have been synthesized by the polymeric precursor method after heat treatment at different temperatures for 2 h in oxygen atmosphere. The decomposition of precursor powder was followed by thermogravimetric analysis, X-ray diffraction (XRD) and Fourier transform Raman (FT-Raman). The UV-vis absorption spectroscopy measurements suggested the presence of intermediary energy levels in the band gap of structurally disordered powders. XRD, Rietveld refinement and FT-Raman revealed that the powders are free of secondary phases and crystallizes in the orthorhombic structure. (C) 2007 Elsevier Masson SAS. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The effect of Fe addition on the microstructural properties and the corrosion resistance of Al-Zn-Mg alloys submitted to different heat treatments (cast, annealed and aged), has been studied in chloride solutions using optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), energy-dispersive X-ray (EDX), cyclic polarization (CP) and open circuit potential (o.c.p.) measurements. The presence of 0.3% Fe in the alloy limited the growth of the MgZn2 precipitates, both in the annealed and in the quenched specimens. No effect of Cr on the grain size in the presence of Fe was found because of the accumulation of Cr in the Fe-rich particles. Fe in the Al-Zn-Mg alloys also made them more susceptible to pitting. Pitting occurred mainly near the Fe-rich particles both, under o.c.p. conditions in O-2-saturated solutions and during the CP.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Nanocrystalline Al(2)O(3)powders have been synthesized by the polymeric precursor method. A study of the evolution of crystalline phases of obtained powders was accomplished through X-ray diffraction, micro-Raman spectroscopy and refinement of the structures through the Rietveld method. The results obtained allow the identification of three steps on the gamma-Al2O3 to alpha-Al2O3 phase transition. The single-phase alpha-Al2O3 Powder was obtained after heat-treatment at 1050 degrees C for 2 h. A study of the morphology of the particles was accomplished through measures of crystallite size, specific surface area and transmission electronic microscopy. The particle size is closely related to gamma-Al2O3 to alpha-Al2O3 phase transition. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Synthesis of silver nanoparticles by thermal treatment of a silver-aspartarne complex under inert atmosphere is described. Spherical metallic silver naroparticles with average diameter of 5 +/-2 nm were obtained by thermal treatment of the complex [Ag(C14H17N2O5)] 1/2H(2)O at 185 degrees C. Thermogravimetric and infrared analysis of the product show the occurrence of an ester bond cleavage of the aspartame ligand followed by rearrangement and release of a molecule of formaldehyde (H2CO), which is transformed in two strong reducing molecules, H-2 and CO. For silver reduction, the presence of the formaldehyde molecules seems to be the key process for the metallic nanoparticles fort-nation. The maintenance of the ligand crystalline structure, with the exception of the ester group loss, was noted as essential for nanoparticles formation and size control. The ligand crystalline structure was completely lost at 200 degrees C and particle growth and coalescence were observed above 250 degrees C. (C) 2005 Elsevier B.V. All rights reserved.