This work presents a new route of preparation of zirconium ceramic foams based on the thermostimulated sol-gel process. This method produces gelled bodies with up to 90% of porosity in the wet gel and can be used to make complex-shaped components. Unfortunately, the shrinkage during the drying step allows to a catastrophic reduction (50%) of the foam porosity. To improve the foam stability we carried out a systematic study of the effect of gel foam aging on the drying process. Samples were aged in closed vessel at 25 C during different time period (from 6 to 240 h). The shrinkage and the mass loss during drying at 50 C were measured in situ, using a non-contact technique performed with a special apparatus. The results show that the total linear shrinkage decreases from 46% to 8% as the aging period increase from 6 to 240 h. This behavior is followed by a small change of total mass loss, from 42 to 54%. It indicates that by aging the structural stiffness of the foams increases due to secondary condensation reactions. Thus, by controlling the aging period, the porosity can be increased from 67 to 75% and the average size of mesopores of dried foams can be screened from 0.3 to 0.9 mum. Finally, these results demonstrate that the thermostimulated sol-gel transition provides a potential route to ceramic foams manufacture.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

SnO2 varistors doped with CoO, Cr2O3 and Nb2O5 were prepared by evaporation and decomposition of suspensions. The composition of the varistors was optimized to improve electrical properties, such as nonlinearity, leakage current and electrical stability. The best results were achieved with the following composition: 99.15% SnO2 +0.75% CoO+0.05% Cr2O3 +0.05% Nb2O5. Samples showed high density, reaching 99.5% of the theoretical density, as well as an homogeneous microstructure. The nonlinear coefficient was higher than 30 in the current range from 10(-7) to 10(-2) A/cm(2). The leakage current was 0.86 mu A/cm(2). These samples showed high stability of electrical parameters when they were exposed to high current of 27 mA/cm(2) for different time periods up to 30 min. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work we present evidence that water molecules are actively involved on the control of binding affinity and binding site discrimination of a drug to natural DNA. In a previous study, the effect of water activity (a(w)) on the energetic parameters of actinomycin-D intercalation to natural DNA was determined using the osmotic stress method (39). This earlier study has shown evidence that water molecules act as an allosteric regulator of ligand binding to DNA via the effect of water activity on the long-range stability of the DNA secondary structure. In this work we have carried out DNA circularization experiments using the plasmid pUC18 in the absence of drugs and in the presence of different neutral solutes to evaluate the contribution of water activity to the energetics of DNA helix unwinding. The contribution of water to these independent reactions were made explicit by the description of how the changes in the free energy of ligand binding to DNA and in the free energy associated with DNA helix torsional deformation are linked to a(w) via changes in structural hydration. Taken together, the results of these studies reveal an extensive linkage between ligand binding affinity and site binding discrimination, and long range helix conformational changes and DNA hydration, This is strong evidence that water molecules work as a classical allosteric regulator of ligand binding to the DNA via its contribution to the stability of the double helix secondary structure, suggesting a possible mechanism by which the biochemical machinery of DNA processing takes advantage of the low activity of water into the cellular milieu.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A method based an ion exchange(IE)-atomic absorption spectrometry(AAS) coupled by flow techniques, allowing the determination of formation constants of, at least, the first species of complex systems, in aqueous solution, was developed.The IE-AAS coupling reduces significantly the number of experimental steps in comparison with IE batch methods, resulting in an important increase in analytical rate. The method is simple both from experimental and computational points of view, making possible its utilization by workers without special expertise in the field of complex equilibria in solution. on the other hand, taking into account mainly the amount of hollow cathode lamps available to date, the developed procedure may be applied, within certain limitations, to the study of many systems whose features prevent the use of traditional approaches.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Pectinmethylesterase (PME) was extracted from guava fruit (Psidium guajava L.), cultivar Paluma, by 70% ammonium sulphate saturation and partially purified by gel filtration on Sephadex G100. Gel filtration showed PME isoenzymes with different values of molecular mass. Two samples were examined: concPME (70% saturation by ammonium sulphate) and Iso4 PME (one of the isoforms from gel filtration with the greatest specific activity). Optimum pH of the enzyme (for both samples) was 8.5 and optimum temperature ranged from 75 and 85 degrees C. The optimum sodium chloride concentration was 0.15 M. The K-M and V-max ranged from 0.32 to 0.23 mg m1(-1) and 244 to 53.2 mu mol/min, respectively, for concPME and Iso4PME. The activation energies (E-a) were 64.5 and 103 kJ/mol, respectively, for concPME and Iso4PME. Guava PME, cv Paluma, is a very thermostable enzyme, showing great heat stability at all temperatures studied. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tibia segmental defect healing in sheep were clinically, radiographically and histologically evaluated. Twelve young sheep aged four to five months were divided into two groups, G1 and G2. A 3.5 cm long segmental defect was created in the right tibial diaphysis with maintenance of the periosteum. The bone defects in both groups were stabilized with a bone plate combined with a titanium cage. In G1 the cage was filled with pieces of autologous cortical bone graft. In G2 it was filled with a composite biomaterial which consisted of inorganic bovine bone, demineralized bovine bone, a pool of bovine bone morphogenetic proteins bound to absorbable ultra-thin powdered hydroxyapatiteand bone-derived denaturized collagen. Except for one G1 animal, all of them showed normal limb function 60 days after surgery. Radiographic examination showed initial formation of periosteal callus in both groups at osteo-tomy sites, over the plate or cage 15 days postoperatively. At 60 and 90 days callus remodeling occurred. Histological and morphometric analysis at 90 days after surgery showed that the quantity of implanted materials in G1 and G2 were similar, and the quantity of new bone formation was less (p = 0.0048) and more immature in G1 than G2, occupying 51 +/- 3.46% and 62 +/- 6.26% of the cage space, respectively. These results suggest that the composite biomaterial tested was a good alternative to autologous cartical bone graft in this experimental ovine tibial defect. However, additional evaluation is warranted prior to its clinical usage.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The cubic perovskite related material CaCu3Ti4O12 has attracted a great deal of attention due to the high values of the static dielectric constant, of order 104, approximately constant in the temperature range 100-600 K. The substitution of Ca by Cd results in a similar temperature dependence but a static dielectric constant more than one order of magnitude lower. A theoretical electronic structure study is performed on CaCu3Ti4O12 (CCTO) and CdCu3Ti4O12 (CdCTO) using a tight binding with overlap method. Although the calculations are performed in a paramagnetic configuration, excellent agreement with experiment was found for the calculated band gap of CCTO. In spite of the fact that the band structures of both systems look practically the same, a significant difference is found in the calculated bond strength of Ca-O and Cd-O pairs, driven by the presence of Ti, with Ca-O interaction in CCTO loosened with respect to Cd-O interaction in the cadmium compound. It is suggested that O vacancies are more easily formed in CCTO, this being related to the lower electronegativity of Ca as compared to Cd. The formation of oxygen vacancies could be the origin of the difference in the static dielectric constant of the two compounds.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Sunflower oil (SO) and high-oleic sunflower oil (HOSO) were used to prepare fried potatoes by either discontinuous or continuous laboratory frying. Fried potatoes that had been fried in oils of differing quality were stored at 60 degrees C for up to 30 d and evaluated for polar compounds, polymers, peroxide value, oil stability index, and alpha-tocopherol content. Results obtained through the various methods applied were consistent and indicated that the length of the induction period could not be explained only on the basis of the degree of unsaturation or polar compound levels in fried potatoes before storage. alpha-Tocopherol content also had a significant influence as potatoes fried in HOSO, with 16% polar compounds and only 10 mg/kg alpha-tocopherol at the starting point of storage, were oxidized more rapidly than potatoes fried in SO with a comparatively higher degradation level, 19% polar compounds, and 100 mg/kg alpha-tocopherol.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The cathodic behaviour of oxides formed on titanium electrodes in physiological solutions at potentials between 3 and 5 V (vs. SCE) was studied by cyclic voltammetry. In case of anodic polarization at potentials higher than 3 V (vs. SCE), a cathodic peak at similar to 0.4 V (vs. SCE) appears in the cathodic scan, which could be due to the reduction of unstable peroxides. The results show that this peak depends on the anodic potential and the oxidation time. This behaviour supposedly is due to the formation of unstable titanium peroxides like TiO3 during anodization. Based on repetitive oxidation-reduction processes can be concluded that the created amount of TiO3 inside of the TiO2 surface layer seems to be constant. (c) 2006 Elsevier Ltd. All rights reserved.