299 resultados para hydroxyapatite implants


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this study was to evaluate and compare the quantitative and qualitative inflammatory responses and bone formation potential after implantation of polyethylene tubes filled with a new calcium hydroxide containing sealer (MBPc) and Prolloot mineral trioxide aggregate (MIA). There were 48 Wistar rats divided in three groups: Group I (control group) empty polyethylene tubes were implanted in the extraction site; group II and III, polyethylene tubes were implanted filled with ProRoot mineral trioxide aggregate (MIA) and MBPc, respectively. At 7, 15, and 30 days after tube implantation, the animals were killed, the hemi-maxillas were removed and prepared to light microscopic analyses. The scores obtained were submitted to Kruskal-Wallis statistical test (p < 0.05). Significant differences between the materials were not observed. The results showed that both materials had similar biological response.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: Immunosuppressive agents may induce severe changes on bone metabolism and may impair the osseointegration process during the implant healing. No data are available concerning the influence of cyclosporin A on dental implants previously integrated to the bone. The aim of this study was to evaluate the influence of cyclosporin A administration on the mechanical retention of bone previously integrated to dental implants.Methods: Eighteen female New Zealand rabbits were submitted to an implant surgery. Each animal received one commercial dental implant of 10 x 3.75 mm. After 12 weeks of an undisturbed healing period, six animals were randomly sacrificed and the removal torque test was performed (group A). In addition, six animals were submitted to a daily injection of cyclosporin A in a dosage of 10 mg/kg (group C), and six animals received saline solution as a control (group B). After 12 weeks of cyclosporin A administration, groups B and C were sacrificed and submitted to a removal torque test in which higher values can be interpreted as higher mechanical bone retention to the implant surface or higher osseointegration.Results: the removal torque results were 30.5 (+/- 9.8) Ncm for group A, 50.17 (+/- 17.5) Ncm for group B, and 26 (+/- 7.8) Ncm for group C. The statistical analysis showed significant differences between groups A and B (P < 0.05) and groups B and C (P < 0.01).Conclusion: Cyclosporin A administration may impair the mechanical retention of dental implants previously integrated to the bone.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mechanical alloying has been used successfully to produce nanocrystalline powders of hydroxyapatite (HA) using three different procedures. The milled HA was studied by X-ray diffraction, Infrared, Raman scattering spectroscopy and Scanning Electron Microscopy (SEM). We obtained HA with different degrees of crystallinity and time of milling. The grain size analysis through SEM and XRD shows particles with dimensions of 36.9, 14.3 and 35.5 nm (for (R1), (R2) and (R3), respectively) forming bigger units with dimensions given by 117.2, 110.8 and 154.4 nm (for (R1), (R2) and (R3), respectively). The Energy-Dispersive Spectroscopy (EDS) analysis showed that an atomic ratio of Ca/P= 1.67, 1.83 and 1.50 for reactions (R1), (R2) and (R3), respectively. These results suggest that the R1 nanocrystalline ceramic is closer to the expected value for the ratio Ca/P for hydroxyapatite, which is 513 congruent to 1.67. The bioactivity analysis shows that all the samples implanted into the rabbits can be considered biocompatible, since they had been considered not toxic, bad not caused inflammation and reject on the part of the organisms of the animals, during the period of implantation. The samples implanted in rabbits had presented new osseous tissue formation with the presence of osteoblasts cells. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: This study investigated the influence of estrogen deficiency and its treatment with estrogen and alendronate on the removal torque of osseointegrated titanium implants.Methods: Fifty-eight female Wistar rats received a titanium implant in the tibia metaphysis. After 60 days, which was needed for implant osseointegration, the animals were randomly divided into five groups: control (CTLE; N = 10), sham surgery (SHAM; N = 12), ovariectomy (OVX; N = 12), ovariectomy followed by hormone replacement (EST; N = 12), and ovariectomy followed by treatment with alendronate (ALE; N = 12). The CTLE group was sacrificed to confirm osseointegration, whereas the remaining groups were submitted to sham surgery or ovariectomy according to their designations. After 90 days, these animals were also sacrificed. Densitometry of femur and lumbar vertebrae was performed by dual-energy x-ray absorptiometry (DXA) to confirm systemic impairment of the animals. All implants were subjected to removal torque.Results: Densitometric analysis of the femur and lumbar vertebrae confirmed a systemic impairment of the animals, disclosing lower values of bone mineral density for OVX. Analysis of the removal torque of the implants showed statistically lower values (P <0.05) for the OVX group in relation to the other groups. However, the group treated with alendronate (ALE group) presented significantly higher torque values compared to the others.Conclusion: According to this study, estrogen deficiency was observed to have a negative influence on the removal torque of osseointegrated implants, whereas treatment with alendronate

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper we report a study of the physicochemical, dielectric and piezoelectric properties of anionic collagen and collagen-hydroxyapatite (HA) composites, considering the development of new biomaterials which have potential applications in support for cellular growth and in systems for bone regeneration. The piezoelectric strain tensor element d(14), the elastic constant s(55) and the dielectric permittivity 8(11), were measured for the anionic collagen and collagen-HA films. The thermal analysis shows that the denaturation endotherm is at 59.47 degreesC for the collagen sample. The collagen-HA composite film shows two transitions, at 48.9 and 80.65 degreesC. The X-ray diffraction pattern of the collagen film shows a broad band characteristic of an amorphous material. The main peaks associated to the crystalline HA is present in the sample of collagen-HA. In the collagen-HA composite, one can also notice the presence of other peaks with low intensities which is an indication of the formation of other crystalline phases of apatite. The scanning electron photomicrograph of anionic collagen membranes shows very thin bundles of collagen. The scanning electron photomicrography of collagen-HA film also show deposits of hydroxyapatite on the collagen fibers forming larger bundles and suggesting that a collagenous structure of reconstituted collagen fibers could act as nucleators for the formation of apatite crystal similar to those of bone. The piezoelectric strain tensor element d(14) was measured for the anionic collagen, with a value of 0.062 pC N-1, which is in good agreement compared with values reported in the literature obtained with other techniques. For the collagen-HA composite membranes, a slight decrease of the value of the piezoelectricity (0.041 pC N-1) was observed. The anionic collagen membranes present the highest density, dielectric permittivity and lowest frequency constant f.L. (C) 2001 Elsevier B.V. B.V. All rights reserved.