We report the structural and magnetic properties of Co2MnO 4, partially substituted by Bi at the octahedral site. Bismuth enhances ferromagnetism due to a decrease of the Co2+-Co2+ antiferromagnetic interactions and an increase of the Mn3+-Mn 4+ exchanges. Spurious phases (magnetic and/or nonmagnetic oxides) can easily form because of the large differences between the ionic radii of Bi3+ and Co3+, hiding or altering the intrinsic physical properties of the main BixCo2-xMnO4 phase. An easy way to eliminate the secondary phases is using acid reagents. Short-time etching of Bi0.1Co1.9MnO4 using nitric acid was successfully used, keeping most of the properties of the initial compound, with no alteration of the crystallographic structure. Final stoichiometry was respected (∼Bi0.08Co1.82MnO4), meaning that the material after etching definitely contains bismuth elements in its structure and the observed properties are intrinsic to the oxide spinel. Additional experiments were performed as a function of the synthesis conditions, showing that an optimal pH value of 7 allowed the best magnetic response of the non-doped material. © 2013 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: The Stroke remains one of the major chronic diseases worldwide, and is considered a major cause of disability, which results not only in persistent neurological deficits, but also in the high physical deconditioning, nevertheless there are not many forms of assessing functional capacity in this population. We aimed to investigate the feasibility of the Six Minute Walk Teste and the Six-Minute Step Test (6MST) in post-stroke patients and compare the behavior of physiological variables during the 6MST and the Six-Minute Walk Test (6MWT), by correlating the functional performance obtained in both tests. Method. The 6MWT was carried out according to the American Thoracic Society (ATS) and the 6MST was performed in six minutes in order to compare it to the 6MWT in a 20 cm step. Was included post-stroke individuals able to walk without aid. All of them did the 6MWT and the 6MST. Results: 12 patients participated in the study. There was no statistical difference in the parameters analyzed when tests were compared. There was poor correlation between the functional performance in both tests. Conclusion: The 6MWT and the 6MST is feasible for post-stroke patients and physiological responses are equal during the performance of both tests. However, there was no correlation with respect to functional performance, which was assessed by the distance walked in the 6MWT and by the number of steps climbed in the 6MST. © 2013 da Silva et al.; licensee BioMed Central Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives: To evaluate the null hypotheses that hydrofluoric (HF) acid etching time would neither decrease the biaxial flexural strength of a glass-based veneering ceramic nor enhance it after silane and unfilled resin (UR) applications. Methods: Disc-shaped IPS e.max ZirPress specimens were allocated into 12 groups: G1-control (no-etching), G2-30 s, G3-60 s, G4-90 s, G5-120 s, G6-60 s + 60 s. Groups (G7-G12) were treated in the same fashion as G1-G6, but followed by silane and UR applications. Surface morphology and roughness (Ra and Rq) of the ceramics were assessed by means of scanning electron microscopy (SEM) and profilometry, respectively. Flexural strength was determined by biaxial testing. Data were analyzed by two-way ANOVA and the Sidak test (α = 0.05). Weibull statistics were estimated and finite element analysis (FEA) was carried out to verify the stress concentration end areas of fracture. Results: The interaction (etching time vs. surface treatment) was significant for Ra (p = 0.008) and Rq (0.0075). Resin-treated groups presented significantly lower Ra and Rq than non-treated groups, except for the 60 s group (p < 0.005). SEM revealed that etching affected the ceramic microstructure and that the UR was able to penetrate into the irregularities. A significant effect of etching time (p = 0.029) on flexural strength was seen. G7-G12 presented higher strength than G1-G6 (p < 0.0001). None of experimental groups failed to show 95% confidence intervals of σ 0 and m overlapped. FEA showed lower stress concentration after resin treatment. Significance: HF acid etching time did not show a damaging effect on the ceramic flexural strength. Moreover, the flexural strength could be enhanced after UR treatment. © 2013 Academy of Dental Materials.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Pós-graduação em Ciências Odontológicas - FOAR

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Pós-graduação em Ciências Odontológicas - FOAR

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Besides possessing good mechanical properties, dental materials should present a good biological behavior and should not injure the involved tissues. Bond strength and biocompatibility are both highly significant properties of dentin adhesives. For that matter, these properties of four generations of adhesive systems (Multi-Purpose/Single Bond/SE Plus/Easy Bond) were evaluated.Eighty bovine teeth had their dentin exposed (500- and 200-mu m thickness). Adhesive was applied on the dentin layer of each specimen. Following that, the microshearing test was performed for all samples. A dentin barrier test was used for the cytotoxicity evaluation. Cell cultures (SV3NeoB) were collected from testing materials by means of 200- or 500-mu m-thick dentin slices and placed in a cell culture perfusion chamber. Cell viability was measured 24 h post-exposition by means of a photometrical test (MTT test).The best bonding performance was shown by the single-step adhesive Easy Bond (21 MPa, 200 mu m; 27 MPa, 500 mu m) followed by Single Bond (15.6 MPa, 200 mu m; 23.4 MPa, 500 mu m), SE Plus (18.2 MPa, 200 mu m; 20 MPa, 500 mu m), and Multi-Purpose (15.2 MPa, 200 mu m; 17.9 MPa, 500 mu m). Regarding the cytotoxicity, Multi-Purpose slightly reduced the cell viability to 92 % (200 mu m)/93 % (500 mu m). Single Bond was reasonably cytotoxic, reducing cell viability to 71 % (200 mu m)/64 % (500 mu m). The self-etching adhesive Scotchbond SE decreased cell viability to 85 % (200 mu m)/71 % (500 mu m). Conversely, Easy Bond did not reduce cell viability in this test, regardless of the dentin thickness.Results showed that the one-step system had the best bond strength performance and was the least toxic to pulp cells. In multiple-step systems, a correct bonding technique must be done, and a pulp capping strategy is necessary for achieving good performance in both properties.The study showed a promising system (one-step self-etching), referring to it as a good alternative for specific cases, mainly due to its technical simplicity and good biological responses.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study evaluated the effect on micro-tensile bond strength (mu-TBS) of laser irradiation of etched/unetched dentin through an uncured self-etching adhesive. Dentinal surfaces were treated with Clearfil SE Bond Adhesive (CSE) either according to the manufacturer's instructions (CSE) or without applying the primer (CSE/NP). The dentin was irradiated through the uncured adhesive, using an Nd: YAG laser at 0.75 or 1 W power settings. The adhesive was cured, composite crowns were built up, and the teeth were sectioned into beams (0.49 mm(2)) to be stressed under tension. Data were analyzed using one-way ANOVA and Tukey statistics (alpha = 5%). Dentin of the fractured specimens and the interfaces of untested beams were observed under scanning electron microscopy (SEM). The results showed that non-etched irradiated surfaces presented higher mu-TBS than etched and irradiated surfaces (p < 0.05). Laser irradiation alone did not lead to differences in mu-TBS (p > 0.05). SEM showed solidification globules on the surfaces of the specimens. The interfaces were similar on irradiated and non-irradiated surfaces. Laser irradiation of dentin through the uncured adhesive did not lead to higher mu-TBS when compared to the suggested manufacturer's technique. However, this treatment brought benefits when performed on unetched dentin, since bond strengths were higher when compared to etched dentin.