102 resultados para poly glutamic acid film
Resumo:
It is shown that the adsorption and morphological properties of layer-by-layer films of poly(o-methoxyaniline) (POMA) alternated with poly(vinyl sulfonic acid) (PVS) are affected dramatically by different treatments of the POMA solutions employed to prepare the films. Whereas the dimension of the globular structures seen by atomic force microscopy increases non monotonically during film growth in parent POMA solution, owing to a competition of adsorption/desorption processes, it changes monotonically for the fractionated POMA. The roughness of the latter films depends on the concentration of the solution and saturates at a given size of the scan window. This allowed us to apply scaling laws that indicated a self-affine mechanism for adsorption of the treated POMA.
Resumo:
A film of poly-L-lysine (PLL) adheres better to the surface of a glassy carbon electrode when the PLL is partially cross-linked by means of glutaraldehyde. A film composition of 97.5% PLL/2.5% glutaraldehyde gives good adhesion and retains the anionic exchange capability of the PLL. The performance of the film was tested with hexacyanoferrate(III) using electrochemical and nonelectrochemical accumulation.
Resumo:
In this work we investigate the effect from the solution concentration on aggregation in layer-by-layer (LBL) films of poly(omethoxyaniline) (POMA) alternated with poly(vinyl sulfonic acid). Films are adsorbed on hydrophilized glass substrates and characterized with UV-Vis spectroscopy and atomic force microscopy. The formation of aggregates is favored in more concentrated solutions, leading to an increase in the diameter of the domains. This is caused by stronger polymer-polymer interactions under high concentrations. The size of POMA aggregates in solution is estimated to be larger than in LBL films, which is surprising because one should expect aggregates from solution to coalesce into larger aggregates in the deposited films. This unexpected result may be explained by a swelling effect of aggregates in the aqueous POMA solutions, consistent with other reports in the literature which consider the aggregates in solution to be made up of smaller aggregates. Upon adsorption on a solid substrate to form the LBL film, a molecular reorganization probably takes place, resulting in smaller aggregates. It is also found that the size distribution of the POMA domains in the LBL films is determined by the concentration of the solution. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Natural or synthetic materials may be used to aid tissue repair of fracture or pathologies where there has been a loss of bone mass. Polymeric materials have been widely studied, aiming at their use in orthopaedics and aesthetic plastic surgery. Polymeric biodegradable blends formed from two or more kinds of polymers could present faster degradation rate than homopolymers. The purpose of this work was to compare the biological response of two biomaterials: poly(L-lactic acid)PLLA and poly(L-lactic acid)PLLA/poly(ethylene oxide)PEO blend. Forty four-week-old rats were divided into two groups of 20 animals, of which one group received PLLA and the other PLLA/PEO implants. In each of the animals, one of the biomaterials was implanted in the proximal epiphysis of the right tibia. Each group was divided into subgroups of 5 animals, and sacrificed 2, 4, 8 and 16 weeks after surgery, respectively. Samples were then processed for analysis by light microscopy. Newly formed bone was found around both PLLA and PLLA/PEO implants. PLLA/PEO blends had a porous morphology after immersion in a buffer solution and in vivo implantation. The proportion 50/50 PLLA/PEO blend was adequate to promote this porous morphology, which resulted in gradual bone tissue growth into the implant.
Preparation and characterization of castor oil-based polyurethane/poly(o- methoxyaniline) blend film
Resumo:
Blends made up of castor oil-based polyurethane (PU) and poly(o-methoxyaniline) (POMA) were obtained in the form of films by casting and characterized by FTIR, UV-Vis-NIR spectroscopy, and electrical conductivity measurements. Doping was carried out by immersing the films in 1.0M HCl aqueous solution. Chemical bonds between NCO group of PU and NH group of POMA were observed by means of FTIR spectra. The UV-Vis-NIR spectra indicated that the presence of the PU in the blend does not affect doping and formation of the POMA phase. The electrical conductivity research was in the range of 10-3 S/cm. © 2007 Wiley Periodicals, Inc.
Resumo:
In this paper, we demonstrate that the intrinsic electric field created by a poly(o-methoxyaniline) (POMA) cushion layer hinders the changes in molecular conformation of poly(p-phenylenevinylene) (PPV) in layer-by-layer with dodecylbenzene sulfonic acid (DBS). This was modeled with density functional theory (DFT) calculations where an energy barrier hampered molecular movements of PPV segments when they were subjected to an electric field comparable to that caused by a charged POMA layer. With restricted changes in molecular conformation, the PPV film exhibited Franck-Condon transitions and the photoexcitation spectra resembled the absorption spectra, in contrast to PPV/DBS films deposited directly on glass, with no POMA cushion. Other effects from the POMA cushion were the reduced number of structural defects, confirmed with Raman spectroscopy, and an enhanced PPV emission at high temperatures (300 K) in comparison with the films on bare glass. The positive effects from the POMA cushion may be exploited for enhanced opto-electronic devices, especially as the intrinsic electric field may assist in separating photoexcited electron-hole pairs in photovoltaic devices. © 2013 American Institute of Physics.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The physical properties of novel thermoplastic random copolyesters [-(CH2)(n)-COO-/-(CH2)(n)-COO-](x) made of long (n=12) and medium (n=8) chain length -hydroxyfatty esters [HO-(CH2)(n)-COOCH3] derived from bio-based vegetable oil feedstock are described. Poly(-hydroxy tridecanoate/-hydroxy nonanoate) P(-Me13-/-Me9-) random copolyesters (M-n=11,000-18,500 g/mol) with varying molar ratios were examined by TGA, DSC, DMA and tensile analysis, and WAXD. For the whole range of P(-Me13-/-Me9-) compositions, the WAXD data indicated an orthorhombic polyethylene-like crystal packing. Their melting characteristics, determined by DSC, varied with composition suggesting an isomorphic cocrystallization behavior. TGA of the P(-Me13-/-Me9-)s indicated improved thermal stability determined by their molar compositions. The glass transition temperature, investigated by DMA, was also found to vary with composition. The crystallinities of P(-Me13-/-Me9-)s however, were unaffected by the composition. The stiffness (Young's modulus) of these materials was found to be related to their degrees of crystallinity. (c) 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014, 131, 40492.
Resumo:
The synthesis of a series of omega-hydroxyfatty acid (omega-OHFA) monomers and their methyl ester derivatives (Me-omega-OHFA) from mono-unsaturated fatty acids and alcohols via ozonolysis-reduction/crossmetathesis reactions is described. Melt polycondensation of the monomers yielded thermoplastic poly(omega-hydroxyfatty acid)s [-(CH2)(n)-COO-](x) with medium (n = 8 and 12) and long (n = 17) repeating monomer units. The omega-OHFAs and Me-omega-OHFAs were all obtained in good yield (>= 80%) and purity (>= 97%) as established by H-1 NMR, Fourier Transform infra-red spectroscopy (FT-IR), mass spectroscopy (ESI-MS) and high performance liquid chromatography (HPLC) analyses. The average molecular size (M-n) and distribution (PDI) of the poly(omega-hydroxyfatty acid)s (P(omega-OHFA)s) and poly(omega-hydroxyfatty ester) s (P(Me-omega-OHFA) s) as determined by GPC varied with organo-metallic Ti(IV) isopropoxide [Ti(OiPr)(4)] polycondensation catalyst amount, reaction time and temperature. An optimization of the polymerization process provided P(omega-OHFA) s and P(Me-omega-OHFA) s with M-n and PDI values desirable for high end applications. Co-polymerization of the long chain (n = 12) and medium chain (n = 8) Me-omega-OHFAs by melt polycondensation yielded poly(omega-hydroxy tridecanoate/omega-hydroxy nonanoate) random co-polyesters (M-n = 11000- 18500 g mol(-1)) with varying molar compositions.
Resumo:
Voltammetry has been employed to study the influence of systematic additions of citric acid on the E-I curves of Tin in 0.5 M NaClO4, in order to verify the film growth in the presence of the organic acid and the inhibition of the pitting corrosion of the metal. The minimum concentration of the organic acid needed to change the GI curves is 10(-2) M, in the pH range 1.0-4.0. At pH 3.0 and 4.0, the scan rate dependence on current density, in the potential region of formation and reduction of the film, showed that in a first stage adsorption occurs. In a second stage, the v(1/2) dependence found can he explained by ohmic resistance control. The formation of tin/citric acid complexes, 10(-2) M, is suggested. The pitting inhibition may be due to the formation of a mixed layer of tin in citric acid concentrations higher than 10(-2) oxide and tin citrate complexes on the electrode surface. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
AgSIE was used for the direct analysis of folic acid (FA), with a detection limit and lower level of quantitation of 6.8 x10-10 mol L-1 and 2.3 x 10 8 mol L-1. The analysis in fresh and processed fruits was done without any sample pretreatment. In strawberry and acerola juices, FA concentration level values were below the method detection limit. FA was detectable in peach (77.7 0.4 mg L-1 and 64.4 0.5 mgL-1), Persian lime (45.4 0.7 mg L-1), pineapple Hawaii (66.2 0.4 mgL-1), pear pineapple (35.3 0.6 mgL-1), cashew (54.4 0.5 mgL-1) , passion fruit (73.2 0.3 mgL-1), and apple (84.4 0.5 mg L-1 ).
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)