262 resultados para TiO2-ZrO2 composite
Resumo:
A series of V2O5/TiO2 samples was synthesized by sol-gel and impregnation methods with different contents of vanadia. These samples were characterized by x-ray diffraction (XRD), Raman spectroscopy, x-ray photoelectron spectroscopy (XPS), and electronic paramagnetic resonance (EPR). XRD detected rutile as the predominant phase for pure TiO2 prepared by the sol-gel method. The structure changed to anatase when the vanadia loading was increased. Also, anatase was the predominant phase for samples obtained by the impregnation method. Raman measurements identified two species of surface vanadium: monomeric vanadyl (V4+) and polymeric vanadates (V5+). XPS results indicated that Ti ions were in octahedral position surrounded by oxygen ions. The V/Ti atomic ratios showed that V ions were highly dispersed on the vanadia/titania surface obtained by the sol-gel method. EPR analysis detected three V4+ ion types: two of them were located in axially symmetric sites substituting for Ti4+ ions in the rutile structure, and the third one was characterized by magnetically interacting V4+ ions in the form of pairs or clusters. A partial oxidation of V4+ to V5+ was evident from EPR analysis for materials with higher concentrations of vanadium. (C) 2001 American Vacuum Society.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
An investigation was made into the photocatalytic activity of in situ synthesized TiO2 chemically modified by Pd(II) 2-aminothiazole complex for phenol degradation at different pH values. At longer reaction times, the bare titania presented far poorer pbotoactivity than the modified catalysts in the entire range of pH studied. The catalyst complexed with Pd(II) was more efficient than the metal-free Pd, irrespective of pH and reaction time, suggesting that metal plays an important role. A cooperative mechanism is proposed, involving the possible photoactivation of both TiO2 and sensitizer. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Foi avaliado o possível efeito de tratamentos superficiais em pinos de fibra de carbono lisos, quando comparados aos pinos serrilhados, na retenção à resina composta empregada na confecção de núcleos de preenchimento. Foram utilizados cinqüenta pinos de fibra de carbono, divididos em cinco grupos: os quatro primeiros grupos eram constituídos por pinos do tipo liso, cujas superfícies foram tratadas, e o último grupo por dez pinos do tipo serrilhado. Foram desenvolvidas matrizes de resina acrílica com um leito ajustado para conter o pino, com um alargamento na porção coronária para posterior preenchimento com resina composta. Após o tratamento superficial, todos os pinos receberam camadas de primer, foram secos e então ajustados à matriz de resina, colocando-se a resina composta autopolimerizável na porção coronária para um núcleo de preenchimento de 3 mm. As amostras foram submetidas a termociclagem e armazenadas em água destilada por uma semana. Os espécimes foram testados por meio de ensaios mecânicos de tração, à velocidade de 0,5 mm/min, até o deslocamento do conjunto ou a fratura da resina do núcleo. As conclusões foram as seguintes: a) o tratamento superficial nos grupos tratados por meio de jateamento (Grupo A), pontas diamantadas marcadoras de profundidade para facetas laminadas (Grupo C) e alteração da morfologia da extremidade coronária (Grupo D) conferiu aos pinos lisos valores de retenção comparáveis aos dos pinos serrilhados (Grupo E) nos ensaios de tração, porém sem diferença estatisticamente significativa entre estes grupos; b) os pinos tratados por meio de pontas diamantadas de granulação média (Grupo B) obtiveram valores de retenção menores que os demais grupos.
Resumo:
Purpose: To evaluate the flexural strength of two fixed dental prosthesis (FDP) designs simulating frameworks of adhesive fixed partial prostheses, reinforced or not by glass fiber.Materials and Methods: Forty specimens, made with composite resin, were divided into 4 groups according to the framework design and the presence of fiber reinforcement: A1 - occlusal support; A2: occlusal support + glass fiber; B1: occlusal and proximal supports; B2: occlusal and proximal supports + glass fiber. The specimens were subjected to the three-point bending test, and the data were submitted to two-way ANOVA and Tukey's test (5%).Results: Group A2 (97.9 +/- 38 N) was statistically significantly different from all other experimental groups, presenting a significantly lower mean flexural strength.Conclusion: The use of glass fibers did not improve the flexural strength of composite resin, and designs with occlusal and proximal supports presented better results than designs simulating only occlusal support.
Resumo:
Purpose: Existing composite restorations on teeth are often remade prior to the cementation of fixed dental prostheses. The aim of this study was to evaluate the effect of static and cyclic loading on ceramic laminate veneers adhered to aged resin composite restorations.Materials and Methods: Eighty sound maxillary incisors were collected and randomly divided into four groups: group 1: control group, no restorations; group 2: two Class III restorations; group 3: two Class IV restorations; group 4: complete composite substrate. Standard composite restorations were made using a microhybrid resin composite (Anterior Shine). Restored teeth were subjected to thermocycling (6000 cycles). Window preparations were made on the labial surface of the teeth for ceramic laminate fabrication (Empress II). Teeth were conditioned using an etch-and-rinse system. Existing composite restorations representing the aged composites were silica coated (CoJet) and silanized (ESPE-Sil). Ceramic laminates were cemented using a bis-GMA-based cement (Variolink Veneer). The specimens were randomly divided into two groups and were subjected to either static (groups 1a, 2a, 3a, 4a) or cyclic loading (groups 1b, 2b, 3b, 4b). Failure type and location after loading were classified. Data were analyzed using one-way ANOVA and Tukey's test.Results: Significantly higher fracture strength was obtained in group 4 (330 +/- 81 N) compared to the controls in group 1 (179 +/- 120 N) (one-way ANOVA, p < 0.05). Group lb survived a lower mean number of cyclic loads (672,820 cycles) than teeth of groups 2b to 4b (846x10(3) to 873x10(3) cycles). Failure type evaluation after the fracture test showed predominantly adhesive failures between dentin and cement, but after cyclic loading, more cohesive fractures in the ceramic were seen.Conclusion: Ceramic laminate veneers bonded to conditioned aged composite restorations provided favorable results. Surface conditioning of existing restorations may eliminate the necessity of removing aged composite restorations.
Resumo:
This study evaluated the fracture resistance of endodontically treated teeth restored with prefabricated carbon fiber posts and varying quantities of coronal dentin. Sixty freshly extracted upper canines were randomly divided into groups of 10 teeth each. The specimens were exposed to 250,000 cycles in a controlled chewing simulator. All intact specimens were subjected to a static load (N) in a universal testing machine at 45 degrees to the long axis. Data were analyzed by 1-way analysis of variance and Tukey test (alpha = .05). Significant differences (P < .001) were found among the mean fracture forces of the test groups (positive control, 0 mm, 1 mm, 2 mm, 3 mm, and negative control groups: 1022.82 N, 1008.22 N, 1292.52 N, 1289.19 N, 1255.38 N, and 1582.11, respectively). These results suggested that the amount of coronal dentin did not significantly increase the fracture resistance of endodontically treated teeth restored with prefabricated carbon fiber post and composite resin core. (Oral Surg Oral Med Oral Pathol Oral Radiol Endod 2008;106:e52-e57)
Resumo:
The paper presents the results of an experimental study of interfacial failure in a multilayered structure consisting of a dentin/resin cement/quartz-fiber reinforced composite (FRC). Slices of dentin close to the pulp chamber were sandwiched by two half-circle discs made of a quartz-fiber reinforced composite, bonded with bonding agent (All-bond 2, BISCO, Schaumburg) and resin cement (Duo-link. BISCO, Schaumburg) to make Brazil-nut sandwich specimens for interfacial toughness testing. Interfacial fracture toughness (strain energy release rate, G) was measured as a function of mode mixity by changing loading angles from 0 degrees to 15 degrees. The interfacial fracture surfaces were then examined using Scanning Electron Microscopy (SEM) and Energy Dispersive X-ray Spectroscopy (EDX) to determine the failure modes when loading angles changed. A computational model was also developed to calculate the driving forces, stress intensity factors and mode mixities. Interfacial toughness increased from approximate to 1.5 to 3.2 J/m(2) when the loading angle increases from approximate to 0, 0 to 15 degrees. The hybridized dentin/cement interface appeared to be tougher than the resin cement/quartz-fiber reinforced epoxy. The Brazil-nut sandwich specimen was a suitable method to investigate the mechanical integrity of dentin/cement/FRC interfaces. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Objectives. This study compared the durability of repair bond strength of a resin composite to a reinforced ceramic after three repair systems.Methods. Alumina-reinforced feldspathic ceramic blocks (Vitadur-alpha(R)) (N=30) were randomly divided into three groups according to the repair method: PR-Porcelain Repair Kit (Bisco) [etching with 9.5% hydrofluoric acid + silanization + adhesive]; CJ-CoJet Repair Kit (3M ESPE) [(chairside silica coating with 30 mu m SiO2 + silanization (ESPE(R)-Sil) + adhesive (Visio(TM)-Bond)]; CL-Clearfil Repair Kit [diamond surface roughening, etching with 40% H3PO4 + Clearfil Porcelain Bond Activator + Clearfil SE Bond)]. Resin composite was photo-polymerized on each conditioned ceramic block. Non-trimmed beam specimens were produced for the microtensile bond strength (mu TBS) tests. In order to study the hydrolytic durability of the repair methods, the beam specimens obtained from each block were randomly assigned to two conditions. Half of the specimens were tested either immediately after beam production (Dry) or after long-term water storage (37 degrees C, 150 days) followed by thermocyling (12,000 cycles, 5-55 degrees C) in a universal testing machine (1 mm/min). Failure types were analyzed under an optical microscope and SEM.Results. mu TBS results were significantly affected by the repair method (p=0.0001) and the aging conditions (p=0.0001) (two-way ANOVA, Tukey's test). In dry testing conditions, PR method showed significantly higher (p < 0.001) repair bond strength (19.8 +/- 3.8 MPa) than those of CJ and CL (12.4 +/- 4.7 and 9.9 +/- 2.9, respectively). After long-term water storage and thermocycling, CJ revealed significantly higher results (14.5 +/- 3.1 MPa) than those of PR (12.1 +/- 2.6 MPa) (p < 0.01) and CL (4.2 +/- 2.1 MPa) (p < 0.001). In all groups when tested in dry conditions, cohesive failure in the composite accompanied with adhesive failure at the interface (mixed failures), was frequently observed (76%, 80%, 65% for PR, CJ and CL, respectively). After aging conditions, while the specimens treated with PR and CJ presented primarily mixed failure types (52% and 87%, respectively), CL group presented mainly complete adhesive failures at the interface (70%).Significance. Hydrolytic stability of the repair method based on silica coating and silanization was superior to the other repair strategies for the ceramic tested. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.