149 resultados para Thermodynamics of polymer Blends


Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this work we report the surface modification of different engineering polymers, such as, polyethylene terephthalate (PET), polyethylene (PE) and polypropylene (PP) by an atmospheric pressure plasma jet (APPJ). It was operated with Ar gas using 10 kV, 37 kHz, sine wave as an excitation source. The aim of this study is to determine the optimal treatment conditions and also to compare the polymer surface modification induced by plasma jet with the one obtained by another atmospheric pressure plasma source the dielectric barrier discharge (DBD). The samples were exposed to the plasma jet effluent using a scanning procedure, which allowed achieving a uniform surface modification. The wettability assessments of all polymers reveal that the treatment leads to reduction of more than 40 degrees in the water contact angle (WCA). Changes in surface composition and chemical bonding were analyzed by x-ray photoelectron spectroscopy (XPS) and Fourier-Transformed Infrared spectroscopy (FTIR) that both detected incorporation of oxygen-related functional groups. Surface morphology of polymer samples was investigated by Atomic Force Microscopy (AFM) and an increase of polymer roughness after the APPJ treatment was found. The plasma-treated polymers exhibited hydrophobic recovery expressed in reduction of the O-content of the surface upon rinsing with water. This process was caused by the dissolution of low molecular weight oxidized materials (LMWOMs) formed on the surface as a result of the plasma exposure. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The failure of facial prostheses is caused by limitations in the properties of existing materials, especially flexibility and durability. Therefore, this study evaluated the marginal deterioration of a silicone used for fabrication of facial prostheses (Silastic MDX4-4210, Dow Corning Corporation, Midland, MI, USA) according to the influence of artificial aging, daily disinfection, and 2 types of pigmentation. Thirty specimens were fabricated and subdivided in 6 groups: without pigmentation, pigmented with make-up powder and iron oxide, and evaluated with and without the action of the disinfectant. Analysis of marginal deterioration was performed on a scanning electron microscope (magnification, ×5000) immediately 6 months and 1 year after fabrication of specimens, following the guidelines of ASTM International. After visual analysis of the photomicrographs, it was noticed that all groups presented marginal deterioration and alterations in surface texture with time. The use of disinfection did not contribute to the marginal deterioration of polymer (silicone), regardless of the pigmentation and artificial aging.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

O trabalho teve como objetivo avaliar a sobrevivência do clone H13 de Eucalyptus urograndis sob dois manejos hídricos de viveiro, plantados em dois solos, com e sem a adição de polímero hidroabsorvente (hidrogel). O plantio foi realizado em vasos mantidos em estufa, com dois tipos de solo: um arenoso e outro argiloso. Cada vaso recebeu 2,5 L de solo, um litro de água e o hidrogel na proporção de 0,4 g vaso-1 (120 mL de gel). O delineamento experimental adotado foi o inteiramente casualizado, com três repetições. Os sintomas de estresse, nos vários níveis avaliados, sempre se manifestaram primeiro nas plantas no solo argiloso, de modo mais acentuado naquelas que foram mantidas sem estresse de água na fase de viveiro. Isso garantiu que as plantas sobrevivessem por um período menor sem água, variando de 14 a 20 dias (com e sem hidrogel, respectivamente), enquanto, no solo arenoso, a sobrevivência foi maior, de 29 a 34 dias (com e sem hidrogel, respectivamente). Apesar da não significância estatística, os resultados com o hidrogel possibilitam, em ambos os solos, maior flexibilidade operacional na intervenção com novas irrigações.

Relevância:

100.00% 100.00%

Publicador:

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Cellulose macro- and nanofibers have gained increasing attention due to the high strength and stiffness, biodegradability and renewability, and their production and application in development of composites. Application of cellulose nanofibers for the development of composites is a relatively new research area. Cellulose macro- and nanofibers can be used as reinforcement in composite materials because of enhanced mechanical, thermal, and biodegradation properties of composites. Cellulose fibers are hydrophilic in nature, so it becomes necessary to increase their surface roughness for the development of composites with enhanced properties. In the present paper, we have reviewed the surface modification of cellulose fibers by various methods. Processing methods, properties, and various applications of nanocellulose and cellulosic composites are also discussed in this paper.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The [(Mn4O5)-O-IV(terpy)(4)(H2O)(2)](6+) complex, show great potential for electrode modification by electropolymerization using cyclic voltammetry. The voltammetric behavior both in and after electropolymerization process were also discussed, where the best condition of electropolymerization was observed for low scan rate and 50 potential cycles. A study in glass electrode for better characterization of polymer was also performed. Electrocatalytic process by metal centers of the conducting polymer in H2O2 presence with an increase of anodic current at 0.85 V vs. SCE can be observed. The sensor showed great response from 9.9 x 10(-5) to 6.4 x 10(-4) mol L-1 concentration range with a detection limit of 8.8 x 10(-5) mol L-1, where the electrocatalytic mechanism was based on oxidation of H2O2 to H2O with consequently reduction of Mn-IV to Mn-III. After, the Mn-III ions are oxidized electrochemically to Mn-IV ions. (C) 2012 Elsevier Ltd .... Selection and/or peer-review under responsibility of the Symposium Cracoviense Sp. z.o.o.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The styrene levels of polystyrene (PS) glasses from the most consumed brands of disposable glasses intended for water and coffee in Brazil were determined. A GC-FID method was developed and validated, showing good precision and accuracy. The method was successfully used to determine styrene in 11 PS glass brands. The styrene levels ranged from 1.68 to 43.69 mg/100 g glass, depending on the kind of polymer, thickness, and glass brand. It could be used to control the content of styrene in the polymer. The migration of styrene from the glasses into water and 20 % ethanol was not detected.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

O interesse da indústria de alimentos por produtos desenvolvidos a partir de farinhas acrescidas de proteína não se deve somente às suas características nutricionais, senão também às suas propriedades funcionais e reológicas, as quais definem as suas aplicações comerciais. Este trabalho teve por objetivo avaliar o efeito de parâmetros operacionais do processo de extrusão sobre as propriedades de pasta de misturas de farinha de mandioca e caseína. O processo de extrusão seguiu o delineamento 'central composto rotacional' para três fatores: teor de proteína (2,5 a 9,5%), umidade (14,5 a 19,5%) e temperatura de extrusão (65 a 135 ºC). As misturas antes e após a extrusão foram analisadas no Rapid Visco Analyser (RVA) quanto a: viscosidade inicial, pico de viscosidade, quebra de viscosidade, viscosidade final e tendência à retrogradação. Os resultados obtidos nas misturas antes da extrusão mostraram aumento dos valores de viscosidade com o aumento da concentração de proteína até o ponto central (6%) e, nos teores mais elevados de proteína, ocorreu redução destes. Após a extrusão, observou-se que o teor de proteína foi a variável de maior efeito sobre as propriedades de pasta, seguida pela umidade das misturas.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)