Fractal dimensions of grain boundary region in doped SnO2 ceramics were determined based on previously derived fractal model. This model considers fractal dimension as a measure of homogeneity of distribution of charge carriers. Application of the derived fractal model enables calculation of fractal dimension using results of impedance spectroscopy. The model was verified by experimentally determined temperature dependence of the fractal dimension of SnO2 ceramics. Obtained results confirm that the non-Debye response of the grain boundary region is connected with distribution of defects and consequently with a homogeneity of a distribution of the charge carriers. Also, it was found that C-T-1 function has maximum at temperature at which the change in dominant type of defects takes place. This effect could be considered as a third-order transition.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Lead-Cadmium fluorosilicate stable glasses were prepared and the vitreous domain region determined in the composition diagram. Characteristic temperatures were obtained from thermal analysis and the structural studies performed illustrate clearly the role played by lead atoms in the glasses crystallization behavior and the glass-forming ability of cadmium atoms. The occurrence of either a cubic lead fluoride or a lead-cadmium fluoride solid solution in crystallizing samples was found to be dependent on Er3+ doping. The optically active ions were found to concentrate in the crystalline phase and in fact play the role of nucleating agent as suggested from X-ray diffraction and EXAFS measurements. (C) 2002 Elsevier B.V. Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives. The aim of this study was to evaluate the effect of mechanical cycling on the biaxial flexural strength of two densely sintered ceramic materials.Methods. Disc shaped zirconia (In-Ceram Zirconia) and high alumina (Procera AllCeram) ceramic specimens (diameter: 15 min and thickness: 1.2 mm) were fabricated according to the manufacturers' instructions. The specimens from each ceramic material (N = 40, n = 10/per group) were tested for flexural strength either with or without being subjected to mechanical cycling (20,000 cycles under 50 N load, immersion in distilled water at 37 degrees C) in a universal testing machine (1 mm/min). Data were statistically analyzed using two-way ANOVA and Tukey's test (alpha = 0.05).Results. High alumina ceramic specimens revealed significantly higher flexural strength values without and with mechanical cycling (647 +/- 48 and 630 +/- 143 MPa, respectively) than those of zirconia ceramic (497 +/- 35 and 458 +/- 53 MPa, respectively) (p < 0.05). Mechanical cycling for 20,000 times under 50 N decreased the flexural strength values for both high alumina andSignificance. High alumina ceramic revealed significantly higher mean flexural strength values than that of zirconia ceramic tested in this study either with or without mechanical cycling conditions. (C) 2005 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The temperature dependence of the electrical conductivity and the F-19 nuclear magnetic resonance (NMR) of PbGeO3-PbF2CdF, glasses and glass ceramics are investigated. The measured conductivity values of the glasses are above 10(-5) Skin at 500 K, and increase with increasing lead fluoride content. Activation energies extracted from the conductivity data are in the range 0.59-0.73 eV. Results are consistent with the hypothesis that in these oxyfluoride glasses lead fluoride rich clusters are dispersed in a metagermanate based matrix providing increasing mobility pathways for conducting ions. The conductivity of a sample of the glass ceramic of composition (mol%) 60PbGeO(3-)20PbF(2)-20CdF(2) was found to be smaller than that in the corresponding glass, suggesting that there are poor ionic conducting regions in the interface between the nanometer sized crystals. The temperature dependence of the F-19 relaxation times, measured in the range 100-800 K, exhibit the qualitative features associated with high fluorine mobility in both, glass and glass ceramics materials. We suggest that de-convolution of the spin-lattice relaxation rates observed in the glass ceramics shows that the observed high temperature rate maximum is associated with the diffusional motions of the fluorine ions in beta-PbF2 crystals. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, the use of a natural yttrium oxide and rare earth oxide solid solution (CRE2O3) as stabilizers of the alpha-Si3N4 phase to form alpha-SiAlON has been investigated. This oxide mix is produced at FAENQUIL-DEMAR, at a cost of only 20% of pure commercial Y2O3. Two alpha-SiAlONs using pure Y2O3 or CRE2O3 have been prepared, using mixes of 20% by volume of a molar fraction of 9:1 of AlN to Y2O3 or AlN to CRE2O3, respectively, with 80% alpha-Si3N4. Samples were gas pressure-sintered at 1900 degreesC, under 1.5 MPa of N-2 for 60 min. Both compositions yielded alpha-SiAlON ceramics with high relative densities (98% t.d.), hardness of 18 GPa and fracture toughness of 5 Mpa m(1/2), with homogeneous microstructures composed of elongated alpha-SiAlON grains with aspect ratios of 5. It is concluded that the mixed rare earth concentrate (CRE2O3) can be used to produce alpha-SiAlON ceramics with similar microstructures and mechanical properties of alpha-SiAlON ceramics fabricated using pure Y2O3, but with the advantage of its lower production cost. (C) 2004 Elsevier B.V All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper reports on a study of the: effect of replacing CoO by MnO2 on the sintering and electrical propel-ties of the 98.95% SnO2 + (1 - x)% CoO + x% MnO2 + 0.05% Ta2O5 system. All the samples were compacted into pellets and sintered at 1300 degrees C for 1 h, when they reached densities of about 98% of the theoretical density. An X-ray diffraction (XRD) analysis showed no other detectable phases other than SnO2. Current-voltage characterization indicated varistor behavior in the systems. The non-linear coefficient (alpha) and breakdown electric field (Eb) increased as the amount of MnO2 was increased. The results are explained in terms of an electric barrier modification, due to the presence of adsorbed negative oxygen species at the grain boundary inter face. (C) 2000 Elsevier B.V. B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent oxyfluoride glasses and beta-PbF(2) nanocrystals containing glass-ceramics were prepared with varying Eu(3+) content (0.3, 0.4, 0.5 and 0.6%). The effect of Eu(3+) content on the preparation of glass-ceramics was investigated. From differential scanning calorimetry, the T(x)-T(g)(T(x)-temperature of the onset of crystallization; T(g)-glass transition temperature) parameter for glasses has shown slight variation, and an exothermic peak near T(g) called the ceramization temperature (T(c)) has been observed. Heat treatments were performed at this temperature to obtain transparent glass-ceramics containing beta-PbF(2) nanocrystals, identified by x-ray diffraction. Heat treatments for different periods of time were performed and were observed to be very important in the control of the crystal size and of the crystallization rate. Based upon the absorption spectra, the scattering level due to the presence of beta-PbF(2) nanocrystals in the glass-ceramics was observed to be similar to that for the mother glasses. Detailed analysis of emission spectra and decay time measurements led to the identification of Eu(3+) ions as the beta-PbF(2) crystalline phase. Excitation spectra at 70 K show the interaction of Eu(3+) ions with the fluorogermanate network.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, we describe the preparation of glass ceramics in the Ga2S3 - GeS2 - CsCl system Visible and infrared transmitting glass ceramics were reproducibly obtained by appropriated heat treatment of the base glass Crystals with controllable size of about 40 nm were homogeneously generated in the glassy matrix X-ray diffraction characterizations have shown that gallium acts as nucleating agent in this material, giving rise to alpha-Ga2S3 crystals Improved thermo-mechanical properties such as dilatation coefficient and resistance to fracture propagation have been observed in the prepared glass ceramics

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives. Evaluate the flexural strength (sigma) and subcritical crack growth (SCG) under cyclic loading of glass-infiltrated alumina-based (IA, In-Ceram Alumina) and zirconia-reinforced (IZ, In-Ceram Zirconia) ceramics, testing the hypothesis that wet environment influences the SCG of both ceramics when submitted to cyclic loading.Methods. Bar-shaped specimens of IA (n = 45) and IZ ( n = 45) were fabricated and loaded in three-point bending (3P) in 37 degrees C artificial saliva (IA(3P) and IZ(3P)) and cyclic fatigued (F) in dry (D) and wet (W) conditions (IA(FD), IA(FW), IZ(FD), IZ(FW)). The initial sigma and the number of cycles to fracture were obtained from 3P and F tests, respectively. Data was examined using Weibull statistics. The SCG behavior was described in terms of crack velocity as a function of maximum stress intensity factor (K(Imax)).Results. The Weibull moduli (m = 8) were similar for both ceramics. The characteristic strength (sigma(0)) of IA and IZ was and 466 MPa 550 MPa, respectively. The wet environment significantly increased the SCG of IZ, whereas a less evident effect was observed for IA. In general, both ceramics were prone to SCG, with crack propagation occurring at K(I) as low as 43-48% of their critical K(I). The highest sigma of IZ should lead to longer lifetimes for similar loading conditions.Significance. Water combined with cyclic loading causes pronounced SCG in IZ and IA materials. The lifetime of dental restorations based on these ceramics is expected to increase by reducing their direct exposure to wet conditions and/or by using high content zirconia ceramics with higher strength. (C) 2010 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)