229 resultados para Glass ionomer
Resumo:
The purpose of this work was to evaluate the biological compatibility of the Sealapex, Apexit, Sealer 26 and Ketac Endo endodontic cements. Polyethylene tubes containing these cements were implanted in the subcutaneous tissue of 40 (forty) rats. The animals were sacrificed after 14 and 90 days. A descriptive analysis of the reactions found in the connective tissue by contact with the cements was performed. The magnitude of inflammatory infiltrate, the presence and predominance of cell types and their distribution as to the filling material and reparative phenomena, such as fibroblastic and angioblastic proliferation and formation of fibrous capsules, were subjectively measured. After 90 days, all cements presented statistically significant reduction of the inflammatory reaction, presence of a fibrous tissue capsule in contact with the opening of the tubes containing the filling materials, and reduction of fibroblastic proliferation. Angioblastic proliferation decreased only for the Sealer 26 and Ketac Endo groups. All cements tested were either partially or totally phagocyted, and the mildest inflammatory response was found for the Sealer 26 group at both evaluation periods.
Resumo:
This in vitro study evaluated the demineralization around restorations class V made on the buccal and lingual surfaces of teeth when using different restorative materials. Thirty extracted teeth were randomly divided into 3 groups (n=10) according to the restorative material: Group I - Fuji II LC (GC America Inc., Alsip, Illinois, USA), Group II - Tetric (Ivoclar Vivadent AG, Schaan, Liechtenstein) and Group III - Chelon Fil (3M/ESPE., Seefeld, Germany). The teeth were submitted to a pH-cycling model associated to a thermocycling model. Sections were made and the specimens were analyzed under a polarized light microscopy as for the presence of demineralization. Measurements were performed and the results were subjected to statistical analysis using Anova and Tukey´s Test (α=0.05). Mean values of demineralization depth (µm) according to each positions showed that the demineralization was significantly reduced when Chelon Fil (Group III) was used for all depths, when compared to fluoridated resin materials. Also, it was verified that non-fluoridated resin material, composite resin Tetric, had the lowest inhibitory effect on the development of demineralization.
Resumo:
Objectives: The objective of this study was to evaluate the clinical performance of 124 non-carious cervical lesion restorations at 12 months. Materials And Methods: Three study groups were formed according to the material and technique used. All teeth received 37% phosphoric acid etching in enamel and dentin. The teeth of Group I received the conventional adhesive system Scotch Bond Multi Purpose, followed by resin composite Filtek Z350; teeth of Group II were restored with resin-modified glass-ionomer cement Fuji II LC; teeth of Group III were restored with the same resin-modified glass-ionomer cement however, before it was inserted, 2 coats of primer of the Scotch Bond Multi Purpose adhesive system were applied to dentinal tissue. The teeth were evaluated by 2 examiners with regard to the factors of retention, marginal adaptation, marginal discoloration, color alteration, presence of marginal caries lesion, anatomic shape, and sensitivity. Results: Application of the Kruskal-Wallis test showed no statistically significant difference for anatomic shape, marginal discoloration, color alteration, caries lesion, marginal adaptation, and sensitivity among the three study groups, but the variable retention presented statistically significant difference at 12 months, with Group III presenting a behavior superior to that of Group II but similar to that of Group I. Conclusion: The analyzed restorations of non-carious cervical lesions presented a good clinical performance at 12 months.
Resumo:
Introduction and objective: Glass ionomer cement, which was first introduced in Dentistry in 1972, presents good qualities such as aesthetics, fluoride release and adhesion to dental tissues. Because of its preventive characteristics regarding to dental caries, glass ionomer cement has been used for Atraumatic Restorative Treatment (ART), as reported by Frencken and Holmgren [6], meeting the principles announced by the World Health Organization (WHO) for application to large population groups without regular access to dental care. Material and methods: In this present study, the abrasive wear strength of two glass-ionomer cements (Vidrion R® and ChemFlex®) was evaluated through toothbrushing machine. Classic® toothbrushes with soft bristles and Sorriso® dentifrice were also used for the study. Results: Student-t test showed significant difference between both groups, with tobs value = 9.4411 at p < 0.05. Conclusion: It can be concluded that the wear rate caused by toothbrush/dentifrice was higher for Vidrion R® (52.00 mg) than ChemFlex® (5.57 mg).
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Objectives. The purpose of this paper is to modify the conventional calcium fluoro-aluminosilicate glass, which is used in the formation of glass ionomer cements (CIGs) by the niobium addition and to study the properties of GICs obtained.Materials and methods. Sol-gel process was used to prepare the powder at lower temperature than fusion method. Glass-ceramic powder obtained in this way was used to prepare the GICs. The properties such as working and setting times, microhardness and diametral tensile strength were evaluated for the experimental GICs and a commercial luting cement.Results. The ideal powder:liquid (P:L) ratio determined to prepare the experimental GICs was equal to 1:1. The cements prepared using this ratio showed working and setting times similar to the commercial GICs. in mechanical tests it was observed that microhardness and diametral tensile strength of the experimental GICs decreased significantly with the reduction of P:L ratio. on the other hand, the results obtained in microhardness tests indicated that the presence of niobium was a positive factor.Significance. The chemical process allows the development of glass-ceramic powder at 600 degrees C which is the goal of the present paper. It was concluded that GICs containing niobium might be used in dental applications and these results encourage further researches on other compositions. (c) 2007 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Glass ionomer cements (GICs) are largely employed in Dentistry for several applications, such as luting cements for the attachment of crowns, bridges, and orthodontic brackets as well as restorative materials. The development of new glass systems is very important in Dentistry to improve of the mechanical properties and chemical stability. The aim of this study is the preparation of two glass systems containing niobium in their compositions for use as GICs. Glass systems based on the composition SiO2,Al2O3-Nb2O5-CaO were prepared by chemical route at 700degreesC. The XRD and DTA results confirmed that the prepared materials are glasses. The structures of the obtained glasses were compared to commercial material using FTIR, Al-27 and Si-29 MAS-NMR. The analysis of FTIR and MAS-NMR spectra indicated that the systems developed and commercial material are formed by SiO4 and AlO4 linked tetrahedra. These structures are essential to get the set time control and to have cements. These results encourage further applications of the experimental glasses in the formation of GICs. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Purpose: The purpose of this study was to comparatively assess the seven-year clinical performance of a one-bottle etch-and-rinse adhesive with resin composite (RC) and resin-modified glass ionomer (RMGI) restorations in noncarious cervical lesions.Methods and Materials: One operator placed 70 restorations (35 restorations in each group) in 30 patients under rubber dam isolation without mechanical preparation. The restorations were directly assessed by two independent examiners, using modified US Public Health Service criteria at baseline and 6, 12, 24, 60, and 84 months. The obtained data were tabulated and statistically analyzed using the Fisher and McNemar tests. A difference was significant if p<0.05.Results: Twenty patients were available for recall after seven years (66.6%), and 25 RC and 26 RMGI restorations out of 70 restorations were evaluated. Excellent agreement was registered for all criteria between examiners (kappa >= 0.85). Alfa and bravo scores were classified as clinically acceptable. The McNemar test detected significant differences within RC restorations between baseline and seven-year evaluations for anatomic form, marginal integrity, and retention (p<0.05). For RMGI restorations, a significant difference was identified for marginal integrity (p<0.05). As to material comparison, the Fisher exact showed a better retention performance for RMGI restorations than for RC restorations (p<0.05). Twelve composite restorations were dislodged (52.0% retention) and three ionomer restorations were lost (88.5% retention). The cumulative success rate for RC and RMGI was 30% and 58.1%, respectively.Conclusions: After seven years of service, the clinical performance of RMGI restorations was superior to that of the adhesive system/resin composite restorations in this study.
Resumo:
Background: the purpose of this study was to histomorphometrically evaluate the response of periodontal tissues covering Class V resin restorations in dogs.Methods: After raising a mucoperiosteal flap, bony defects measuring 5 x 5 mm were created on the buccal aspect of the canines of five dogs followed by cavity preparations on the root surface measuring 3 x 3 x 1 mm. Before repositioning the flap to cover the bone defect, the cavities were restored with composite resin (CR) or resin-modified glass ionomer cement (RMGIC) or were left unrestored as control (C). The dogs were euthanized 90 days after surgery. Specimens comprising the tooth and periodontal tissues were removed, processed routinely, cut into longitudinal serial sections in the bucco-lingual direction, and stained with hematoxylin and eosin (H&E) or Masson's trichrome. The most central sections were selected for histomorphometric analysis.Results: Histomorphometric analysis revealed apical migration of epithelial tissue onto the restorative materials (RMGIC and CR). The C group presented significantly longer connective tissue attachment (P < 0.05) than the RMGIC and CR groups and significantly higher bone regeneration (P < 0.05) compared to the RMGIC group. Histologically, the cervical third (CT) of all groups had the most marked chronic inflammatory infiltrate.Conclusions: Within the limits of this study, it can be concluded that the restorative materials used exhibit biocompatibility; however, both materials interfered with the development of new bone and the connective tissue attachment process.
Resumo:
This study evaluated the effect of cycling various pH demineralizing solutions on the surface hardness, fluoride release and surface properties of restorative materials (Ketac-Fil Plus, Vitremer, Fuji II LC, Freedom and Fluorofil). Thirty specimens of each material were made and the surface hardness measured. The specimens were randomized into five groups according to the pH (4.3; 4.6; 5.0; 5.5 and 6.2) of the demineralizing solution. The specimens were submitted to pH-cycling for 15 days. The specimens remained in the demineralizing solution for six hours and in the remineralizing solution for 18 hours. Then, the surface hardness (SH) was remeasured and the surface properties were assessed. Fluoride release was determined daily. Data from SH and the percentage of alteration in surface hardness were analyzed by analysis of variance (p < 0.05); the Kruskal-Wallis test was performed for the fluoride release results. When hardness was compared, the variation in pH led to a positive correlation for glass ionomer cements and a negative correlation for fluoride release. For polyacid-modified resin composites, a negative correlation was found with regards to fluoride release; no significant correlation was observed for hardness. Surface properties were influenced: an acidic pH led to a greater alteration, except for polyacid-modified resin composites. The pH of the demineralizing solution influenced fluoride release from the tested materials. The pH variation altered hardness and surface properties of glass ionomer cements but did not influence polyacid-modified resin composites.
Resumo:
Os cimentos ionoméricos representam importante opção de material restaurador em Odontologia e sua adesão à estrutura dental, diminuindo a infiltração marginal, somada à liberação de flúor, inibindo o metabolismo de microrganismos acidogênicos e favorecendo a remineralização dental, podem diminuir a ocorrência de cárie secundária. A aplicação tópica de géis acidulados ou neutros contendo flúor tem sido largamente utilizada em Odontologia. No entanto, este procedimento pode afetar a integridade dos materiais restauradores, aumentando sua rugosidade e a retenção de placa bacteriana. Dessa forma, o presente estudo avaliou o período de tempo no qual o cimento ionomérico Vitremer mantém sua capacidade inibitória sobre Streptococcus mutans ATCC 25175 e a adesão dos mesmos sobre a superfície do material, bem como a influência da aplicação tópica de flúor acidulado e neutro sobre esses parâmetros microbiológicos e as características superficiais daquele material. Verificou-se que a atividade antimicrobiana do cimento ionomérico Vitremer se mantém por aproximadamente quatro dias e não é recuperada com o uso de flúor gel acidulado ou neutro. Observou-se, também, que Streptococcus mutans ATCC 25175 adere ao material restaurador testado sendo que a aplicação tópica de flúor não influenciou esta adesão. As características superficiais desses materiais não se alteraram com a aplicação dos géis.
Resumo:
The aim of this study was to evaluate the effects of carbamide peroxide (CP) on surfaces of different restorative materials. Porcelain, composite resin, glass ionomer, and amalgam were analyzed in this study. Surface roughness (Ra) was measured before and after treatment with 10% and 15% CP. Fifteen percent CP increased Ra values in both the glass ionomer and amalgam subgroups, while 10% CP increased Ra values in the glass ionomer subgroup only. Changes in restorative material surfaces can be more severe when bleaching is completed without a clinician's supervision. Hence, thorough patient examinations must be done before, during, and after bleaching treatment. Int J Prosthodont 2011;24:155-157
Resumo: