Supported ceramic membranes have been produced by the sol-casting procedure from aqueous colloidal suspensions prepared by the sol-gel route. Coatings on a tubular alumina support have been successfully performed leading to crack free layers. Samples have been sintered at 400, 500 and 600 degreesC, and the effect of heating treatment on the nanostructure and on the ultrafiltration properties are analyzed. The characterization has been done by high resolution scanning electron microscopy, nitrogen adsorption-desorption isotherms, water permeation and cut-off determination using polyethylene glycol standard solutions. The micrographs have revealed that grains and pore size increase with the temperature, whereas their shape remains invariant. This results is in agreements with N-2 adsorption-desorption analyses, which have revealed that the mean pore size diameter increases from 4 to 10 nm as the sintering temperature increases from 400 to 600 degreesC, while the total porosity remains constant. Furthermore, the tortuosity, calculated from water permeability, is essentially invariant with the sintering temperatures. The membranes cut-off, determined with a retention rate equal to 95%, are 3500, 6500 and 9000 g . mol(-1) for 400, 500 and 600 degreesC, respectively, showing that the permeation properties of SnO2 ultrafiltration membranes can easily be controlled by sintering condition.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Undoped x center dot alpha-Fe(2)O(3) y center dot CeO(2) and doped with praseodymium ceramic pigments were obtained by the sol-gel method after heat treatment at 800 degrees C for 2 h. These pigments were characterized by XRD, nitrogen adsorption, scanning electron microscopy, ultraviolet-visible absorption spectroscopy and colorimetrical measurements. Red and brown colors with several tonalities were observed after changes with Ce and Pr concentration.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent thin films of nanocrystalline anatase were obtained by dip-coating process using an ethanolic suspension of redispersed nanoparticles. This suspension was prepared by sol-gel route and their redispersability achieved by surface grafting of para-toluene-sulfonic acid and acetylacetone. The effects of the acetylacetone content on the powder redispersibility and on the structural evolution of films were determined by small angle X-ray scattering, X-ray reflectometry and X-ray diffraction for different firing temperatures. The results demonstrated that the porous structure of the studied films consist of agglomerates of primary particles with two levels of porosity. The control of the amount of capping ligand allows for a fine-tuning of the average pore size of the dried films. Upon increasing the firing temperature up to 500 degrees C, progressive increase in apparent density, average pore size of films and average crystallite size of powders were observed. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An application of photoacoustic technique is developed for determining the thermal diffusivity coefficient and the thermal conductivity of transparent materials. The backing material which supports the sample is made optically opaque, i.e., it entirely absorbs the incident light, and the converted heat diffuses through the sample heating the gas in contact with its opposite surface. The method is illustrated by fitting voltage amplitude and phase signals versus the chopping frequency in the photoacoustic cell, according to a theoretical model of heat diffusion. Thermal parameters obtained for three polymers compare very well with results from the literature. (C) 1995 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A tangential filtration process was implemented in this study using porous ceramic tubes made of alpha-alumina produced by the slip-casting technique. These tubes were sintered at 1450 degrees C and characterized by mercury intrusion porosimetry, which revealed a mean pore size of 0.5 mu m. The tubes were chemically impregnated with a zirconium citrate solution, after which they were calcined and heat treated at temperatures of up to 600 and 900 degrees C to eliminate volatile organic compounds and transform the zirconium citrate into zirconium oxide impregnated in the alumina in the form of nanoparticle agglomerates. The microporous pipes were tested on a microfiltration hydraulic system to analyze their performance in the demulsification of sunflower oil and water mixtures. The fluid-dynamic parameters of Reynolds number and transmembrane pressure were varied in the process. The volume of permeate was analyzed by measuring the Total Organic Carbon concentration (TOC), which indicated 99% of oil phase retention. The emulsified mixture was characterized by optical microscopy, while the morphology and composition of the impregnated microporous tubes were analyzed by scanning electron microscopy (SEM). Quantification of the TOC values for the tube impregnated once at 600 degrees C showed the best demulsification performance, with the concentration on permeate smaller than 10 mg/L. The impregnated tube sintered once at 900 degrees C presented low carbon concentration (smaller than 20 mg/L), has the advantage of presenting the greatest trans-membrane flux in relation to the other microporous tube. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Glasses with composition 60PbGeO(3)-10PbF(2)-30CdF(2) (mol%) have been obtained in the bulk form with a high stability against crystallization. After doping them with 0.5 mol% of Er3+ or Eu3+ and appropriate heat treatment transparent glass ceramics could be obtained. Electronic spectroscopy, X-ray diffraction and transmission electron microscopy measurements have been made. beta-PbF2: Er3+/Eu3+ Single crystals, 5-10 nm in size, are detected in the otherwise transparent composite medium, the size of the particles and absence of clustering allowing for the increased transparency of the final materials. (C) 1999 Elsevier B.V. B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work presents a new route of preparation of zirconium ceramic foams based on the thermostimulated sol-gel process. This method produces gelled bodies with up to 90% of porosity in the wet gel and can be used to make complex-shaped components. Unfortunately, the shrinkage during the drying step allows to a catastrophic reduction (50%) of the foam porosity. To improve the foam stability we carried out a systematic study of the effect of gel foam aging on the drying process. Samples were aged in closed vessel at 25 C during different time period (from 6 to 240 h). The shrinkage and the mass loss during drying at 50 C were measured in situ, using a non-contact technique performed with a special apparatus. The results show that the total linear shrinkage decreases from 46% to 8% as the aging period increase from 6 to 240 h. This behavior is followed by a small change of total mass loss, from 42 to 54%. It indicates that by aging the structural stiffness of the foams increases due to secondary condensation reactions. Thus, by controlling the aging period, the porosity can be increased from 67 to 75% and the average size of mesopores of dried foams can be screened from 0.3 to 0.9 mum. Finally, these results demonstrate that the thermostimulated sol-gel transition provides a potential route to ceramic foams manufacture.