Resumo:
A method has been developed to obtain quantitative information about grain size and shape from fractured surfaces of ceramic materials. One elaborated a routine to split intergranular and transgranular grains facets of ceramic fracture surfaces by digital image processing. A commercial ceramic (ALCOA A-16, Al2O3-1.5% of CrO) was used to test the proposed method. Microstructural measurements of grain shape and size taken from fracture surfaces have been compared through descriptive statistics of distributions, with the corresponding measurements from polished and etched surfaces. The agreement between results, with the expected bias on grain size values from fractures, obtained for both types of surfaces allowed to infer that this new technique can be used to extract the relevant microstructural information from fractured surfaces, thus minimising the time consuming steps of sample preparation. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
The non-ohmic and dielectric properties as well as the dependence on the microstructural features of CaCu(3)Ti(4)O(12)/CaTiO(3) ceramic composites obtained by conventional and microwave sintering were investigated. It was demonstrated that the non-ohmic and dielectric properties depend strongly on the sintering conditions. It was found that the non-linear coefficient reaches values of 65 for microwave-sintered samples and 42 for samples sintered in a conventional furnace when a current density interval of 1-10 mA cm(-2) is considered. The non-linear coefficient value of 65 is equivalent to 1500 for samples sintered in the microwave if a current interval of 5-30 mA is considered as is shortly discussed by Chung et al (2004 Nature Mater. 3 774). Due to a high non-linear coefficient and a low leakage current (90 mu A) under both processing conditions, these samples are promising for varistor applications. The conventionally sintered samples exhibit a higher relative dielectric constant at 1 kHz (2960) compared with the samples sintered in the microwave furnace (2100). At high frequencies, the dielectric constant is also larger in the samples sintered in the conventional furnace. Depending on the application, one or another synthesis methodology is recommended, that is, for varistor applications sintered in a microwave furnace and for dielectric application sintered in a conventional furnace.
Resumo:
This paper reports on the phase transformation during the preparation of Ni-25Nb, Ni-25Ta, Ni-20Nb-5Ta and Ni-15Nb-10Ta (at-%) powders by high-energy ball milling from elemental powders. The milling process was performed in a planetary ball milling using stainless steel balls and vials, rotary speed of 300rpm, and a ball-to-powder of 10:1. To minimize contamination and spontaneous ignition the powders were handled under argon atmosphere in a glove box. The milled powders were characterized by means of X-ray diffraction techniques. Results indicated that the Ni atoms were preferentially dissolved into the Nb (and/or Ta) lattice at the initial milling times, which contributed to change the relative intensity on the diffraction peaks. After the dissolution of Nb (and/or Ta) into the Ni lattice, the Ni peaks were moved to the direction of lower diffraction angles in Ni-25Nb, Ni-25Ta, Ni-20Nb-5Ta, Ni-15Nb-10Ta powders, indicating that the mechanical alloying was achieved.
Resumo:
This work discusses on the structural evaluation of mechanically alloyed and heat-treated Ti-25at%Si powders. The milling process was conducted in a planetary ball mill using stainless steel balls/vials, 200 rpm and ball-to-powder weight ratio of 5:1, whereas the heat treatment was conducted under Ar atmosphere at 1100 C for 4 h. Samples were characterized by X-ray diffraction, differential scanning calorimetry, scanning electron microscopy and energy dispersive spectrometry. The Si peaks disappeared after milling for 30h, indicating that the Si atoms were dissolved into the Ti lattice in order to form an extended solid solution. The Ti peaks were broadened and their intensities reduced for longer milling times whereas a halo was formed in Ti-25Si powders milled for 200h suggesting that an amorphous structure was achieved. The crystallite size was decreased with increasing milling times. A large Ti3Si amount was found in mechanically alloyed Ti-25at%Si powders after heating at 1100 degrees C for 4h.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The present work reports on the structural evaluation of mechanically alloyed Ti-xZr-22Si-11B (x = 5, 7, 10, 15 and 20 at-%) powders. Milled powders and hot-pressed alloys were characterized by X-ray diffraction, electron scanning microscopy, and electron dispersive spectrometry. The Si and B atoms were preferentially dissolved into the Ti and Zr lattices during ball milling of Ti-xZr-22Si-11B (x = 7, 10, 15 and 20 at-%) powders, and extended solid solutions were achieved. The displacement of Ti peaks was more pronounced to the direction of lower diffraction angles with increasing Zr amounts in mechanically alloyed Ti-Zr-Si-B powders, indicating that the Zr atoms were also dissolved into the Ti lattice.
Resumo:
This work reports the synthesis of the MgNb(2)O(6) and the ferroelectric lead magnesium niobate Pb(Mg(1/3)Nb(2/3))O(3) (PMN) using fine precursor powders obtained from a chemical Oxide Precursor Method (OPM). To obtain pyrochlore-free PMN ceramics, the synthesis of the precursor MgNb(2)O(6) powders was studied for 2-25 mol% excess of MgO and 10 mol% excess of PbO. Structural and microstructural properties of the sintered ceramics obtained by the cited method and by the classical columbite method were studied and compared. Results lead to good quality, pyrochlore-free PMN ceramic prepared by OPM, presenting greater grain size if compared with ceramic prepared by columbite method.
Resumo:
The recent discovery of a ferroelectric monoclinic phase in the PbZr1-xTixO3 (PZT) system attained the attention of several researchers due to the possibility of understanding the relationships between structural features and piezoelectric properties. The nature of the monoclinic phase in some PZT compositions remains controversial and unclear. In this work, structural phase transitions of PbZr0.52Ti0.48O3 ceramic were investigated by infrared spectroscopy as a function of temperature. Studies were centered on nu(1)-stretching modes and corresponding half width Wi as a function of temperature. The occurrence of the anomalies in the infrared spectra as a function of temperature suggests the following monoclinic ( LT) -> monoclinic ( HT) -> tetragonal phase transition were observed at 183 K and at 263 K.
Resumo:
Flexible piezo- and pyroelectric composite was made in the thin film form by spin coating. Lead Zirconate Titanate (PZT) ceramic powder was dispersed in a castor oil-based polyurethane (PU) matrix, providing a composite with 0-3 connectivity. The dielectric data, measured over a wide range of frequency (10(-5) Hz to 105 Hz), shows a loss peak around 100 Hz related with impurities in the polymer matrix. There is also an evidence of a peak in the range 10(-4) Hz, possibly originating from the glass transition temperature T of the polymer. The pyroelectric coefficient at 34 K is 7.0x10(-5) C(.)m(-2.)K(-1) which is higher than that of P-PVDF (1X10(-5) C(.)m(-2.)K(-1)).
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
In this paper, electrical and structural properties were reported for pyrochlore free (1-x)[Pb(Mg1/3Nb2/3)O-3] - xPbTiO(3) (PMN-PT) (with 35 mol% PbTiO3) ceramics obtained from fine powders. Dielectric studies were focused on the investigation of the complex dielectric permittivity (epsilon '-i epsilon '') as a function of frequency and temperature. The effects of the dc applied electric field on dielectric response were also investigated. Results revealed a field dependence dielectric anomaly in the dielectric permittivity curves (epsilon(T)) in the low dc electric field region, which in turn prevails in the whole analysed frequency interval. To the best of our knowledge, these properties for the PMN-PT ceramic system have not been reported before as in this work. The results were analysed within the framework of the current models found in the literature.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The thermoluminescence (TL) response of Dy and Li doped 20CaB(4)O(7)-80CaB(2)O(4) (Wt%) glass-ceramic irradiated with ultraviolet (UV) radiation was studied. In order to act as TL activator ions, the Dy and Li ions were included in the matrix during the melting process to increase its TL efficiency. A single crystalline CaB2O4 phase was present in the glass-ceramic as determined by X-ray diffraction (XRD). The glass-ceramic 20CaB(4)O(7)-80CaB(2)O(4):Dy,Li wt% (named 20CBO7:Dy,Li) is a newly prepared TL material. Its thermoluminescent dosimetric characteristics have shown a linear response under UV radiation exposure and a good TL signal reproducibility, thus proving to be a promising material for using as an ultraviolet radiation dosimeter. (C) 2007 Elsevier B.V. All rights reserved.