139 resultados para Denture soft lining materials
Resumo:
Objective:This study investigated the efficacy of different techniques for the union of fragments of a denture before repair and on the accuracy of the reposition.Materials and methods:For this study, 20 maxillary dentures made with Lucitone 550 heat-cured resin were used. Points were determined with a scanner on the cusp of the teeth, as a measurement of the segments. After digitisation, each model was exported to the AUTOCAD R 14 program and two-dimensional measurements of the distances between the marked points were made. After the initial analysis, the dentures were fractured into two segments using an impact test machine. For the repair, maxillary dentures were divided into two groups; in the first, the repair was carried out using Kerr's sticky wax and in the second group, Super Bonder was used to join the fragments, with subsequent inclusion of DENTSPLY((R)) Repair Material resin. After the repair, the points of the maxillary dentures were measured again. The numerical values obtained were tabulated to compare the measurements before fracture and after the repair. For statistical analysis, analysis of variance was employed, using a single factor and double factor, followed by the Tukey test with a reliability of 95%.Results:The results demonstrated a statistically significant difference between the materials used to join the dentures for repair, where the dentures were joined with sticky wax presented a larger variation in the distances between the points.Conclusion:The variation in distances between the points is influenced by the agent of repair.
Resumo:
Purpose: This study assessed masticatory efficiency and duration of the masticatory cycle in 14 asymptomatic patients with severe bone resorption. All patients had worn complete dentures for over 10 years. Recall visits were scheduled at 5 months and 1 year after receiving new dentures.Materials and Methods: Fourteen patients were evaluated in this study. The Research Diagnostic Criteria questionnaire and tests of the efficiency and duration of the masticatory cycle were performed with artificial food before, 5 months after, and 1 year after new dentures were delivered. Masticatory efficiency was assessed using a sieve system; artificial food was ground for 35 masticatory cycles and monitored by the operator.Results: Masticatory efficiency at 5 months was significantly improved for the 0.42-mm mesh. An improvement in masticatory efficiency and a reduction in mastication time were observed with the new dentures after 1 year.Conclusion: The results of this study indicated that 5 months did not allow enough time to demonstrate improved muscular capacity and ability after receiving new dentures. After 1 year, the duration of the masticatory cycle was reduced, and masticatory efficiency was significantly improved.
Resumo:
Purpose: This study evaluated the influence of distal extension removable partial denture associated with implant in cases of different bone level of abutment tooth, using 2D finite element analysis.Materials and Methods: Eight hemiarch models were simulated: model A-presenting tooth 33 and distal extension removable partial denture replacing others teeth, using distal rest connection and no bone lost; model B-similar to model A but presenting distal guide plate connection; model C-similar to model A but presenting osseointegrated implant with ERA retention system associated under prosthetic base; model D-similar to model B but presenting osseointegrated implant as described in model C; models E, F, G, and H were similar to models A, B, C, and D but presenting reduced periodontal support around tooth 33. Using ANSYS 9.0 software, the models were loaded vertically with 50 N on each cusp tip. For results, von Mises Stress Maps were plotted.Results: Maximum stress value was encountered in model G (201.023 MPa). Stress distribution was concentrated on implant and retention system. The implant/removable partial denture association decreases stress levels on alveolar mucosa for all models.Conclusions: Use of implant and ERA system decreased stress concentrations on supporting structures in all models. Use of distal guide plate decreased stress levels on abutment tooth and cortical and trabecular bone. Tooth apex of models with reduced periodontal support presented increased stress when using distal rest. (Implant Dent 2011;20:192-201)
Resumo:
Purpose: The purpose of this study was to compare the artificial tooth positional changes following the flasking and polymerization of complete dentures by a combination of two flasking methods and two polymerization techniques using computer graphic measurements.Materials and Methods: Four groups of waxed complete dentures (n = 10) were invested and polymerized using the following techniques: (1) adding a second investment layer of gypsum and conventional water bath polymerization (Control), (2) adding a second investment layer of gypsum and polymerization with microwave energy (Gyp-micro), (3) adding a second investment layer of silicone (Zetalabor) and conventional polymerization (Silwater), and (4) adding a second investment layer of silicone and polymerization with microwave energy (Silmicro). For each specimen, six segments of interdental distances (A to F) were measured to determine the artificial tooth positions in the waxed and polymerized stages using software program AutoCad R14. The mean values of the changes were statistically compared by univariate ANOVA with Tukey post-hoc test at 5% significance.Results: There were no significant differences among the four groups, except for segment D of the Silmicro group (-0.004 +/- 0.032 cm) in relation to the Gypwater group (0.044 +/- 0.031 cm) (p < 0.05), which presented, repectively, expansion and shrinkage after polymerization.Conclusions: Within the limitations of this study, it was concluded that although the differences were not statistically significant, the use of a silicone investment layer when flasking complete dentures resulted in the least positional changes of the artificial teeth regardless of the polymerization technique.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Complete and partial loss of maxillary bone may jeopardize oral physiology and generate complications as oral-sinus-nasal communication. Palatal obturator prostheses are a treatment alternative for rehabilitation of these patients. The aim of this study was to assess stress distribution, through photoelasticity, on palatal obturator prostheses associated with different attachment systems (o'ring, bar clip, and o'ring/bar clip) of implants and submitted to relining. Two photoelastic models were fabricated according to an experimental maxillary model with oral-sinus-nasal communication. One model did not present implants, whereas the other included 2 implants with 13.0 mm in length in the left ridge. Four colorless maxillary obturator prostheses were fabricated and relined with soft silicone. One of these prostheses presented no attachment system, whereas the remaining prostheses included attachment systems adapted to the implants. The assembly (model/attachment system/prosthesis) was positioned in a circular polariscope during loading with 100 N at 10 mm/s. The results were based on observation during the experiment and photographic records of stress on the photoelastic model. The bar clip system exhibited the highest stress concentration followed by o'ring/bar clip and o'ring systems. The attachment systems presented different stress distribution with greater concentration surrounding the implants and homogenous stress distribution on the photoelastic model without implants. The highest concentration of fringes occurred, in ascending order, with o'ring, o'ring/bar clip, and bar clip systems.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Objectives: This in situ study evaluated the effect of an erosive challenge on different restorative materials and on enamel restored with these materials, as well as the ability of these materials to protect the adjacent enamel against erosion.Methods: Ten volunteers wore palatal devices with eight bovine enamel blocks, randomly selected and distributed into two vertical rows, corresponding to the following groups: GI/GV, resin-modified glass ionomer; GII/GVI, conventional glass ionomer; GIII/GVII, composite resin; GIV/GVIII, amalgam. one row (corresponding to groups I-IV) was immersed in a cola drink and the other row (corresponding to groups V-VIII) was subjected to saliva only. The palatal device was continuously worn for 7 days and only half of the appliance (groups I-IV) was immersed in the soft drink (Coca-Cola (R), 150 mL) for 5 min, three times a day. The study variables comprised the wear (profilometry, mu m) and the percentage of surface microhardness change (%SMHC). Data were tested for significant differences by two-way ANOVA and Tukey's tests (p < 0.05).Results: Considering the restorative materials, for %SMHC and wear, there were no differences among the materials and between the saliva and the erosive challenge. For enamel analyses, the erosive challenge promoted a higher wear and %SMHC of the enamel than did the saliva. There were no significant differences in wear and %SMHC of the enamel adjacent to the different restorative materials.Conclusion: This research data suggest that there is little %SMHC and wear of the studied restorative materials and none of them had a preventive effect against erosion on adjacent enamel, which showed a pronounced wear. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Objectives: This study investigated the effect of relining, water storage and cyclic loading on the ultimate flexural strength (FSU) and on the flexural strength at the proportional limit (FSPl) of a denture base acrylic resin (Lucitone 550-L).Methods: Rectangular bars of L were made (64 mm x 10 mm x 2 mm) and relined (1.3 mm) with four relining resins (Kooliner-K, Ufi Gel Hard-UGH, Tokuso Rebase Fast-TR and New Truliner-NT). In addition, specimens relined with L and intact L specimens were made (64 mm x 10 mm x 3.3 mm). A three-point flexural test was applied on the specimens (n = 10) after (1) polymerization; (2) water storage (30 days); (3) cyclic loading (10,000 cycles at 5 Hz) and (4) water storage (30 days) + cyclic loading. Data (MPa) were analyzed with three-way ANOVA and Tukey's HSD tests (alpha = 0.05). To test for a possible correlation between FSU and FSPl, a linear regression coefficient 'r' was calculated.Results: After water storage, L-UGH and L-TR demonstrated an increased FSU (41.4950.64 MPa and 49.95-57.36 MPa, respectively) (P < 0.05). Only L-TR demonstrated an increased FSPl (20.58-24.21 MPa) after water storage (P < 0.05). L-L had the highest FSU (between 78.57 and 85.09 MPa) and FSPl (between 31.30 and 34.17 MPa) (P < 0.05). The cyclic loading decreased the FSU and FSPl of all materials (P < 0.05). Regression analysis showed a strong linear correlation between the two variables (r = 0.941).Conclusions: Water storage improved the FSU of L-UGH and L-TR and the FSPl of L-TR. L-L produced the highest FSU and FSPl. The FSU and FSPl of all materials were detrimentally influenced by cyclic loading.
Resumo:
Objectives: This study evaluated the effect of disinfection by immersion in sodium perborate (50 degrees C/10 min) or microwave irradiation (650 W/6 min) on the linear dimensional change (LDC) of four reline resins (Kooliner-K, New Truliner-N, Tokuso Rebase Fast-T, Ufi Gel Hard-U) and one heat-polymerizing denture base resin (Lucitone 550-L). Methods: Specimens (50.0 mm diameter, 0.5 mm thickness) were made using a split mold with reference points, and divided into two controls and four test groups (u = 8). The distances between the points were measured on the mold (baseline readings), and compared to those obtained from the specimens after: polymerization or immersion in water (37 degrees C) for 7 days (controls); 2 or 7 cycles of disinfection by immersion or microwave irradiation. Results: the two-way ANOVA and Tukey's test (alpha = 0.05) showed that microwave disinfection significantly increased the mean LDC of materials L (-1.43%), N (-1.27%) and K (-1.06%). Material N also exhibited a significant increase in LDC after two cycles of chemical disinfection (-0.73%). For U (-0.47%) and T (-0.21%) materials, no significant changes in LDC were found. Conclusions: Microwave disinfection increases the shrinkage of materials L, N, and K. The dimensional stability of resins U and T was not affected by the disinfection methods evaluated. (c) 2006 Wiley Periodicals, Inc.
Resumo:
This investigation studied the effects of disinfectant solutions on the hardness of acrylic resin denture teeth. The occlusal surfaces of 64 resin denture teeth were ground flat with abrasives up to 400-grit silicon carbide paper. Measurements were made after polishing and after the specimens were stored in water at 37 degreesC for 48 h. The specimens were then divided into four groups and immersed in chemical disinfectants (4% chlorhexidine; 1% sodium hypochlorite and sodium perborate) for 10 min. The disinfection methods were performed twice to simulate clinical conditions and hardness measurements were made. Specimens tested as controls were immersed in water during the same disinfection time. Eight specimens were produced for each group. After desinfection procedures, testing of hardness was also performed after the samples were stored at 37 degreesC for 7, 30, 60, 90 and 120 days. Data were analysed using two-way analysis of variance (anova) and Tukey's test at 95% confidence level. According to the results, no significant differences were found between materials and immersion solutions (P > 0.05). However, a continuous decrease in hardness was noticed after ageing (P < 0.05). It was conclude that the surfaces of both acrylic resin denture teeth softened upon immersion in water regardless the disinfecting solution.
Resumo:
During microwave disinfection, the dentures are exposed to water at high temperature and this may affect the bond between the denture teeth and the acrylic resin from which dentures are made. In this study, a shear test was used to evaluate the effect of microwave disinfection (650W/6 min) on the bond strength of two types of denture teeth to three acrylic resins, with different polymerization methods. The specimens were submitted to the shear tests (0.5 mm/min) after: immersion in water (37 degrees C) for 48 h or 8 days (controls); two or seven cycles of microwave disinfection (test groups). Data (MPa) were analyzed using three-way ANOVA and Tukey HSD test (alpha = 0.05). Microwave disinfection did not adversely affect the bond strength of all tested materials with the exception of QC-20 bonded to SR Vivodent PE, for which a significant reduction was recorded after seven cycles of irradiation. (C) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Objectives:Microleakage is a pre-stage of debonding between hard chairside relines and denture base acrylic resins. Therefore, it is important to assess them with regard to the longevity of the relined denture. This study investigated the effect of thermal cycling on the microleakage at the interface of three hard chairside reline resins and three denture base resins.Material and methods:Rectangular bars (12 mm x 3 mm x 3 mm) of Lucitone 550, Acron MC and QC 20 were made and relined with Kooliner, Tokuyama Rebase Fast II and Ufi Gel Hard, Lucitone 550, Acron MC and QC 20 resins. Specimens were divided into one control and two test groups (n = 10). In specimens of the control group, the microleakage was performed after the reline procedure. In Test Group 1, the specimens were stored for 24 h in distilled water at room temperature and in Test Group 2; the specimens were thermal cycled from 5 to 55 degrees C for 5000 cycles with a 30-s dwell time. Subsequently, all specimens were immersed in 50% silver nitrate solutions for 24 h. All specimens were sectioned longitudinally into three fractions and the lateral sections were examined (n = 20). Silver nitrate stain penetration was examined under a stereoscopic lens with x30 magnification, and the images were captured. Leica Qwin image analysis software was used to determine microleakage at the interface of the materials. Data were analysed using the Kruskal-Wallis test at a 95% level of significance.Results:For all cycles, there were no statistically significant differences between thermal cycled and non-thermal cycled groups (p > 0.05).Conclusion:It can be concluded that thermal cycling had no effect on the microleakage.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)