466 resultados para DENTAL RESINS
Resumo:
The disinfection of dental prostheses by immersion in a chemical solution should be capable of rapid inactivation of pathogenic microorganisms, without causing any adverse effect on the denture base resins. This study evaluated the effect of disinfection immersion on the transverse strength of two heat-cured resins. The denture base resins (Lucitone 550 and QC 20) were polymerized according to the manufacturers' instructions. After polymerization, the specimens were polished, and then stored in water at 37 degreesC for 50 +/- 2 h prior immersion in one of the following solutions for 10 min: 4% chlorhexidine, 1% sodium hypochlorite and 3.78% sodium perborate. The specimens were submitted to disinfection twice, simulating when dentures come from the patient and before being returned to the patient. Ten specimens were made for each group. The transverse strength was evaluated by a 3-point bend test. The flexural strength of the two denture base acrylic resins evaluated remained unaffected after immersion in the three solutions evaluated. In general, the QC 20 resin specimens exhibited lower transverse strength than the Lucitone 550 resin specimens, regardless of immersion solutions.
Resumo:
Objective. To identify and quantify the camphorquinone (CQ) used in different brands of composite resins as a function of the shade analyzed.Materials and methods. Filtek Z250 A3 (FZA3), Filtek Z-250 Incisal (FZI), Pyramid Enamel A1 (PEA1), Pyramid Enamel Translucent (PET), Filtek Supreme A3E (FSA3) and Filtek Supreme GT (FSGT) were used. Five hundred milligrams of each resin were weighed and then dissolved in 1.0 ml of methanol. The samples were centrifuged to accelerate the sedimentation of the inorganic particles. 0.8 ml of the supernatant solution was collected with a pipette and assessed under gas chromatography coupled to the mass spectrometer (GC-MS). The results were compared to pure CQ solutions, used as a standard. Student's t-test, (p = 0.05) significant at the level of 5%, compared the results of each brand shade.Results. A smaller amount of camphorquinone was found in Filtek Z-250 (FZI) resin incisal shade when compared to (FZA3) A3 shade. on the other hand, Filtek Supreme resin featured a statistically larger camphorquinone amount in the incisal shade. in Pyramid Enamel resin camphorquinone was found only in shade Al, while the photoinitiator used in the Translucent shade was not identified.Significance. Based on the data obtained, it is possible to conclude that a single composite resin brand may feature differences in amount and type of photoinitiator used. (C) 2006 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
This article discusses the development of a test bench and a methodology for the study of composite resin abrasive wear. To evaluate the operation of the test bench and to compare the proposed methodology with other existing ones, a study was made of the five composites most commonly used by dentists.The one-way ANOVA method and the Tukey test were used to statistically analyze the results by multiple comparisons of the groups of resins tested. Using the proposed methodology, these resins were classified in an increasing order of abrasive wear strength, as follows: Charisma (the lowest abrasive wear strength), Tetric, TPH, Herculite and Z-100 (the highest abrasive wear strength) (P < 0.05). In comparison to other methodologies, the results of the proposed methodology presented the lowest coefficient of variation. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
A quantitative study was made about the effects caused by ionizing irradiation on materials used for dental restoration (amalgams, compound resins and compomere), aiming to alleviate in bearers of head and neck cancer, the possible harmful effects of radiotherapy perceived when the repaired teething is within the radiation field. Research also encourages further studies for new alternative materials to be used in dental repair of patients submitted to radiotherapy for head and neck cancer. Test samples were submitted to a gamma radiation beam coming from a cobalt-therapy source and analyzed according to the X-ray fluorescence technique, comparing the chemical composition of the samples before and after irradiation. Radiation detectors such as an ionization chamber and a Geiger-Muller were used to measure the rate of residual dose. Gamma spectrometry with Nal detectors was also performed on the same samples. Results showed that there was no significant change in the chemical composition and that at post-irradiation, samples did not exhibit radiation emission, that is to say they had not become radioactive.
Resumo:
The aim of this study was to evaluate the shear bond strength of brackets bonded with different restorative systems and compare it with that afforded by an established orthodontic bonding system. Seventy human bicuspids were used, divided into five different groups with 14 teeth each. Whereas a specific orthodontic bonding resin (Transbond (TM) XT) was used in the control group, the restorative systems Charisma, Tetric Ceram, TPH Spectrum and Z100 were used in the other four groups. Seven days after bonding the brackets to the samples, shear forces were applied under pressure in a universal testing machine. The data collected was evaluated using the ANOVA test and, when a difference was identified, the Tukey test was applied. A 5% level of significance was adopted. The mean results of the shear bond strength tests were as follows: Group 1 (Charisma), 14.98 MPa; Group 2 (Tetric Ceram), 15.16 MPa; Group 3 (TPH), 17.70 MPa; Group 4 (Z100), 13.91 MPa; and Group 5 or control group (Transbond (TM) XT), 17.15 MPa. No statistically significant difference was found among the groups. It was concluded that all tested resins have sufficient bond strength to be recommended for bonding orthodontic brackets.
Resumo:
The purpose of this study was to examine histologically the effects of propolis topical application to dental sockets and skin wounds. After topical application of either a 10% hydro-alcoholic solution of propolis or 10% hydro-alcoholic solution alone, cutaneous wound healing and the socket wound after tooth extraction were examined. The rats were sacrificed at 3, 6, 9, 15 and 21 days after the operation. The specimens were subjected to routine laboratory studies after staining with hematoxylin and eosin. It was concluded that topical application of propolis hydro-alcoholic solution accelerated epithelial repair after tooth extraction but had no effect on socket wound healing.