Mechanical strength of polyethylene terephthalate (PET) fibres and polymethyl methacrylate (PMMA) matrix composites were studied with particular interest on the effects of oxygen and argon plasma treated fibres. PET. fibres were treated in a radio frequency plasma reactor using argon or oxygen for different treatment times to increase the interface adhesion. Fibre volume fraction was measured through digital image analysis. Elastic moduli resulted between 3 GPa for untreated to 6 GPa for treated composites. Tensile tests on PET fibres showed that plasma treatment caused a decrease in average tensile strength compared to untreated fibres. Fracture analysis confirmed the increase in interfacial adhesion due to plasma treatment. (c) 2004 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work, in situ alpha-SiAlON-SiC ceramic composites were obtained,by, liquid phase sintering, using SiC as reinforcement. Different beta-SiC powder contents (0-20 wt.%), were added to Si3N4-AlN-RE2O3. powder mixtures, and compacted by cold isostatic pressing. The samples were sintered at 1950 degrees C for 1 h, in N-2 atmosphere. Sintered: samples were characterized by relative density, weight loss, X-ray diffraction and scanning electron microscopy. Furthermore, mechanical properties such as hardness and fracture toughness were determined by Vickers indentation method. Lattice parameters of the alpha' phase did not considerably change with increase of SiC content. However, morphology, average grain size and aspect ratio of the alpha' phase were considerably changed with increase of the SiC content. These behavior influences significantly the mechanical properties of this hard ceramic composite. (C) 2006 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Composites of aerosil fumed silica and tetraethoxysilane-derived sonogel were prepared by changing the aerosil content between 0 and 30wt% with respect to the silica content in the original tetraethoxysilane (TEOS). The structural characteristics were studied by density and Vickers microhardness measurements and analyzed by means of small-angle X-ray scattering (SAXS). The structure of the composite aerosil/TEOS-derived sonogel can be described as inclusions of the aerosil particles embedded in the matrix of the TEOS-derived sonogel, forming an aerosil/matrix interfacial surface inside the composite. The weakening of the bonding of aerosil/matrix interface, as suggested by the reported decrease in microhardness, increases the fracture toughness of the composite. The additive effect of the aerosil particles on the structure of the sonogel accounts for the increase of the bulk density and reduction of the specific surface of the composite. Some internal structure associated with the microclusters making up the sonogels is apparent from systematic deviations from Porod's law found in the system with small aerosil contents. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In order to cooperate in minimizing the problems of the current and growing volume of waste, this work aims at the production of panels made from industrial waste -thermoplastic (Polypropylene - PP; Polyethylene - PE and Acrylonitrile Butadiene Styrene - ABS) reinforced with agro-industrial waste - pupunha palm waste (shells and sheaths). The properties of the panels were evaluated: density, thickness swelling, water absorption and moisture content. It was used the ASTM D1037; EN 317; and ANSI A208.1 standards regarding particle boards. The best results in physical tests were treatments 1 (100% waste plastic), 6 (60% plastic waste and 40% waste of pupunha) and 7 (70% waste plastic and 30% waste of pupunha). The best results in the mechanical tests were treatments 3 (30% de residuos plasticos e 70% de residuos da pupunha), 4 (40% de residuos plasticos c 60% de residuos da pupunha) and 5 (50% de residuos plasticos e 50% de residuos da pupunha). For mechanical tests it was concluded that the results of modulus of rupture and of modulus of elasticity the best treatments were those with more fibers. In the tensile tests perpendicular to the surface, it is clear that using more waste plastics leads to the best results. It was concluded that the waste can be used as raw material for the production of alternative materials mainly in civil construction and furniture industries, and it can be employed in urban or rural environment, given the concept of eco-efficient products.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Aramid fiber reinforced polymer composites have been used in a wide variety of applications, such as aerospace, marine, sporting equipment and in the defense sector, due to their outstanding properties at low density. The most widely adopted procedure to investigate the repair of composites has been by repairing damages simulated in composite specimens. This work presents the structural repair influence on tensile and fatigue properties of a typical aramid fiber/epoxy composite used in the aerospace industry. According to this work, the aramid/epoxy composites with and without repair present tensile strength values of 618 and 680MPa, respectively, and tensile modulus of 26.5 and 30.1 GPa, respectively. Therefore, the fatigue results show that in loads higher than 170 MPa, both composites present a low life cycle (lower than 200,000 cycles) and the repaired aramid/epoxy composite presented low fatigue resistance in low and high cycle when compared with non-repaired composite. With these results, it is possible to observe a decrease of the measured mechanical properties of the repaired composites.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study evaluated the effect of different light energy densities on conversion degree (CD) and Knoop hardness number (KHN) of RelyX ARC (RLX) resin cement. After manipulation according to the manufacturer's instructions, RLX was inserted into a rubber mold (0.8 mm X 5 mm) and covered with a Mylar strip. The tip of the lightcuring unit (LCU) was positioned in contact with the Mylar surface. Quartz-tungsten-halogen (QTH) and light-emitting diode (LED) LCUs with light densities of 10, 20 and 30 J/cm2 were used to light-cure the specimens. After light curing, the specimens were stored dry in lightproof containers at 37°C. After 24 hours, the CD was analyzed by FT-Raman and, after an additional 24-hours, samples were submitted to Knoop hardness testing. The data of the CD (%) and KHN were submitted to two-way ANOVA and the Tukey's test (α=0.05). QTH and LED were effective light curing units. For QTH, there were no differences among the light energy densities for CD or KHN. For LED, there was a significant reduction in CD with the light energy density set at 10 J/cm2. KHN was not influenced by the lightcuring unit and by its light energy density. © Operative Dentistry.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Aims and objectives: The behavior of polymer-matrix composite is dependent on the degree of conversion. The aim of this study was to evaluate the degree of conversion of two resin cements following storage at 37°C immediately, 24 and 48 hours, and 7 days after light-curing by FTIR analysis. Materials and methods: The specimens were made in a metallic mold and cured with blue LED with power density of 500 mW/cm2 for 30 seconds. The specimens were pulverized, pressed with KBr and analyzed with FTIR following storage times. Statistical analysis used: ANOVA (two-way) and Tukey's post hoc. Results: To the polymer-matrix composites between 24 and 48 hours does not show a significant increase (p > 0.05), however, the highest values were found after 7 days. Conclusion: The polymer-matrix composites used in this study showed similarity on the degree of conversion and increased of according to the time of storage.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

BACKGROUND AND GOAL: Patients infected with hepatitis C virus (HCV) with elevated low-density lipoprotein (LDL) levels achieve higher sustained virologic response (SVR) rates after peginterferon (PegIFN)/ribavirin treatment versus patients with lower LDL. Our aim was to determine whether SVR rates in patients with low/elevated LDL can be improved by dose intensification. STUDY: In PROGRESS, genotype 1 patients with baseline HCV RNA≥400,000 IU/mL and body weight ≥85 kg were randomized to 48 weeks of 180 μg/wk PegIFN α-2a (40 kDa) plus ribavirin (A: 1200 mg/d; B: 1400/1600 mg/d) or 12 weeks of 360 μg/wk PegIFN α-2a followed by 36 weeks of 180 μg/wk, plus ribavirin (C: 1200 mg/d; D: 1400/1600 mg/d). This retrospective analysis assessed SVR rates among patients with low (<100 mg/dL) or elevated (≥100 mg/dL) LDL. Patients with high LDL (n=256) had higher baseline HCV RNA (5.86×10 IU/mL) versus patients with low LDL (n=262; 4.02×10 IU/mL; P=0.0003). RESULTS: Multiple logistic regression analysis identified a significant interaction between PegIFN α-2a dose and LDL levels on SVR (P=0.0193). The only treatment-related SVR predictor in the nested multiple logistic regression was PegIFN α-2a dose among patients with elevated LDL (P=0.0074); therefore, data from the standard (A+B) and induction (C+D) dose arms were pooled. Among patients with low LDL, SVR rates were 40% and 35% in the standard and induction-dose groups, respectively; SVR rates in patients with high LDL were 44% and 60% (P=0.014), respectively. CONCLUSIONS: Intensified dosing of PegIFN α-2a increases SVR rates in patients with elevated LDL even with the difficult-to-cure characteristics of genotype 1, high baseline viral load, and high body weight. Copyright © 2013 by Lippincott Williams & Wilkins.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The aim of this study was to evaluate the compressive strength of microhybrid (Filtek™ Z250) and nanofilled (Filtek™ Supreme XT) composite resins photo-activated with two different light guide tips, fiber optic and polymer, coupled with one LED. The power density was 653 mW cm -2 when using the fiber optic light tip and 596 mW cm-2 with the polymer. After storage in distilled water at 37 ± 2 °C for seven days, the samples were subjected to mechanical testing of compressive strength in an EMIC universal mechanical testing machine with a load cell of 5 kN and speed of 0.5 mm min-1. The statistical analysis was performed using ANOVA with a confidence interval of 95% and Tamhane's test. The results showed that the mean values of compressive strength were not influenced by the different light tips (p > 0.05). However, a statistical difference was observed (p < 0.001) between the microhybrid composite resin photo-activated with the fiber optic light tip and the nanofilled composite resin. Based on these results, it can be concluded that microhybrid composite resin photo-activated with the fiber optic light tip showed better results than nanofilled, regardless of the tip used, and the type of the light tip did not influence the compressive strength of either composite. Thus, the presented results suggest that both the fiber optic and polymer light guide tips provide adequate compressive strength to be used to make restorations. However, the fiber optic light tip associated with microhybrid composite resin may be an interesting option for restorations mainly in posterior teeth. © 2013 Astro Ltd.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The objective of this work was to evaluate the effect of the addition of bamboo laminas of the species Dendrocalamus giganteus to three-layer medium density particleboard (MDP). These laminas were glued onto both the top and the bottom of each panel. With the manufactured panels laminated with bamboo, mechanical tests based on the Brazilian Standard ABNT NBR 14810 were carried out to determine the modulus of rupture (MOR) in static bending and the tensile strength parallel-to-surface. These mechanical tests were realized in particleboards of eucalyptus and in reinforced particleboard, both produced in the laboratory. The modulus of rupture and tensile strength parallel-to-surface of the laminated MDP had values close to those that have been reported. The reinforcements increased the values of these studied properties. Nevertheless, this fact indicated the possibility to produce a stronger MDP using bamboo lamina as surface layers. These results show the possibility of using coatedbamboo MDP for utilization in large spans, for example, in flooring for mezzanines with finish on both sides, and for robust furniture as bookshelves, beds, tables, etc.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Carbon fiber reinforced carbon composites can be made by iterative liquid impregnation or gas phase carbon deposition routes. In both cases, at the final processing stage the carbon fiber is embedded in carbon matrix which results in unique properties such as low density, high thermal conductivity and thermal shock resistance, low thermal expansion and high modulus, in relation to other refractory materials. In the present study assembled three-directional and four-directional preforms, having 50% volume of pores, were densified by iterative cycles of thermoset resin impregnation followed by pyrolysis under inert atmosphere, until appropriate densities were achieved. The thermoset resin is converted in a carbon matrix during pyrolysis. The iterative manufacturing process of the carbon fiber reinforced carbon composites is evaluated by means of nondestructive techniques based on X-ray computed tomography and electrical resistivity. X-ray computed tomography gives a general mapping view of the filling pores of the preforms which impacts results of the electrical resistivity. After six processing cycles and heat treatments up to 2000?, the final densities of the three-directional and four-directional carbon fiber reinforced carbon composites were 1.16g/cm(3) and an electrical resistivity of approximate to 0.07m. The configuration of preforms, three-directional or four-directional, did not alter the densification profile, in terms of increasing density and reducing porosity during the processing cycles.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Biodegradable polymers are starting to be introduced as raw materials in the food-packaging market. Nevertheless, their price is very high. Starch, a fully biodegradable and bioderived polymer is a very interesting alternative due to its very low price. However, the use of starch as the polymer matrix for the production of rigid food packaging, such as trays, is limited due to its poor mechanical properties, high hidrophilicity and high density. This work presents two strategies to overcome the poor mechanical properties of starch. First, the plasticization of starch with several amounts of glycerol to produce thermoplastic starch (TPS) and second, the production of biocomposites by reinforcing TPS with promising fibers, such as barley straw and grape waste. The mechanical properties obtained are compared with the values predicted by models used in the field of composites; law of mixtures, Kerner-Nielsen and Halpin-Tsai. To evaluate if the materials developed are suitable for the production of food-packaging trays, the TPS-based materials with better mechanical properties were compared with commercial grades of oil-based polymers, polypropylene (PP) and polyethylene-terphthalate (PET), and a biodegradable polymer, polylactic acid (PLA).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Specimens of aluminum-based composites reinforced by silicon carbide nanoparticles (Al/SiCnp) produced by powder metallurgy (PM) were anodized under voltage control in tartaric-sulfuric acid (TSA). In this work, the influence of the amount of SiCnp on the film growth during anodizing was investigated. The current density versus time response and the morphology of the porous alumina film formed at the composite surface are compared to those concerning a commercial aluminum alloy (AA1050) anodized under the same conditions. The processing method of the aluminum alloys influences the efficiency of the anodizing process, leading to a lower thicknesses for the unreinforced Al-PM alloy regarding the AA1050. The current density versus time response is strongly dependent on the amount of SiCnp. The current peaks and the steady-state current density recorded at each voltage step increases with the SiCnp volume fraction due to the oxidation of the SiCnp. The formation mechanism of the anodic film on Al/SiCnp composites is different from that occurring in AA1050, partly due the heterogeneous distribution of the reinforcement particles in the metallic matrix, but also to the entrapment of SiCnp in the anodic film.