130 resultados para fluoride (halide) phosphate tellurite glass


Relevância:

40.00% 40.00%

Publicador:

Resumo:

In this work, we present a new photochromic tungstate based glass which have both absorption coefficient and refractive index modified under laser exposure. The photosensitive effect is superficial under ultraviolet (UV) irradiation but occurs in the entire volume of the glass under visible irradiation. The effect can be obtained in any specific point inside the volume using an infrared femtosecond laser. In addition, the photosensitive phenomenon can be erased by specific heat treatment. This glass can be useful to substitute actual data storage supports and is a promising material for 3-dimensional (3D) and holographic optical storage.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Diode-pumped Yb-doped glass lasers have received considerable attention for applications such as high-power beam production or femtosecond pulses generation. In this paper, we evaluate the laser potential of three different glass families doped with Yb3+ : alkali lead fluorborate (PbO-PbF2-B2O3), heavy metal oxide (Bi2O3-PbO-Ga2O3) and niobium tellurite (TeO2-Nb2O5-K2O-Li2O). Spectroscopic properties were studied for the samples and calculations of the minimum laser pump intensity (I-min), saturation fluence (U-sat) and the theoretical limit of peak power (P-max) are also presented. A comparison of laser properties of these three different glasses and their importance is shown and analyzed. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Objective. The aim of this in vitro study was to evaluate the interaction between two sources of fluoride (restorative systems and dentifrices) in inhibiting artificial root caries development. Methods. One hundred and eighty tooth segments were embedded in polyester resin, and sanded flat. Cylindrical cavities 1.0 mm-deep and 1.5 mm-diameter were prepared in root dentin and randomly restored by fluoride-containing restorative systems: Ketac-fil/Espe (Ke), Fuji II LC/GC Corp (Fj), F2000/3M (F2), Surefil/Dentsply (Su) or a control: Filtek Z250/3M (Z2). Ten experimental groups were made to test the association among the five restorative systems and two dentifrices: with F - (Sensodyne Baking Soda) or without F- (Sensodyne Original) (n = 18). After surface polishing, a 1 mm-wide margin around the restorations was demarcated and initial dentin surface Knoop microhardness values (KHNi) were obtained. The specimens were submitted to a pH-cycling model, and to applications of slurries of dentifrice. Afterwards the final dentin surface Knoop microhardness values (KHNf) were measured. Results. The differences between KHNi and KHNf, and the covariate KHNi were considered by the ANCOVA and Tukey's test (α = 0.05). The interaction between restorative system and dentifrice was statistically significant (p = 0.0026). All restorative systems provided some protection against artificial caries challenge when associated with the fluoride-containing dentifrice treatment. The means (standard deviation) of reductions in Knoop hardness values for systems associated with the fluoride-containing dentifrice were: Ke: 40.0(1.02)a, Fj: 41.9(1.02)b, F2: 43.3(1.04)c, Su: 43.5(1.00)c, Z2: 44.0(1.02)c; and with the non-fluoride-containing dentifrice were: Ke: 42.9(1.02)a, Fj: 44.7(1.01)b, F2: 45.2(1.09)bc, Su: 46.0(0.99)c, Z2: 46.6(0.99)c (statistical differences were expressed by different letters). Conclusion. The cariostatic effect shown by the fluoride-containing dentifrice could enhance that shown by Ketac-fil and Fuji II LC, and could mask that shown by F2000. © 2002 Elsevier Science Ltd. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The release of fluoride from restorative materials (Vitremer, Ketac-Fil, Fuji II LC and Freedom) was evaluated during two 15-day periods, before and after a topical application of acidulated phosphate fluoride gel (APF). For each material, 6 specimens were made, which were immersed in 2 ml of deionized water. The fluoride concentration dosages in the solutions were read at intervals of 24 hours for 15 days. After this period, the specimens of each material received treatment with APF gel for 4 minutes and the fluoride released was analyzed at 24-hour intervals during the following 15 days. The analysis of variance and the Tukey test (p < 0.05) showed that the total mean fluoride released during the initial 15 days was greater for Vitremer and Ketac-Fil and lower for Fuji II LC and Freedom; and in the final 15 days there was a difference in release readings, with the greatest value for Vitremer, followed by Fuji II LC, Ketac-Fil and Freedom. The comparison of the results between the 1st day and the 16th day (after gel application) showed a greater fluoride release on the 16th day for Vitremer, Fuji II LC and Freedom and was equal for Ketac-Fil. Although all the materials evaluated gained fluoride with the application of APF, the data suggest that the resin-modified ionomers are more efficient in releasing fluoride to the medium than the other materials.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Erbium Er3+ and ytterbium Yb3+ codoped fluoro-phosphate glasses belonging to the system NaPO3-YF 3-BaF2-CaF2 have been prepared by the classical melt-quenching technique. Glasses containing up to 10 wt% of erbium and ytterbium fluorides have been obtained and characterized using differential scanning calorimetry (DSC) and UV-visible and near-infrared spectroscopy. Transparent and homogeneous glass-ceramics have been then reproducibly synthetized by appropriate heat treatment above glass transition temperature of a selected parent glass. Structural investigations of the crystallization performed through X-ray diffractometry (XRD) and scanning electron microscopy (SEM) have evidenced the formation of fluorite-type cubic crystals based during the devitrification process. Finally, infrared to visible up-conversion emission upon excitation at 975 nm has been studied on the Er3+ and Yb 3+ codoped glass-ceramics as a function of thermal treatment time. A large enhancement of intensity of the up-conversion emissions-about 150 times- has been observed in the glass-ceramics if compared to the parent glass one, suggesting an incorporation of the rare-earth ions (REI) into the crystalline phase. © 2012 The American Ceramic Society.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Purpose: This longitudinal clinic study evaluated the effect of a glass ionomer sealant (GIS) and a fluoride varnish (FV) in the prevention of dental decay on newly erupted permanent molars of children with and without caries experience. Materials and methods: Eighty children, aged 6-8 years, with all four newly erupted first permanent molars, were divided into two groups. Group 1 consisted of 53 children without caries experience and group 2 consisted of 27 children with dental caries experience. Permanent molars of the right side were sealed with GIS and the fluoride varnish was applied on the other two permanent first molars. Evaluation of GIS retention and the effectiveness of both materials in the prevention of dental caries were performed after 6, 12 and 18 months. Results: After 18 months, of the 299 teeth, 271 (91%) showed no caries lesions and 28 presented caries lesions (9%). Teeth sealed with GIS had more carious lesions (15) than teeth with fluoride varnish (13). Most of the teeth (70%) that presented carious lesions were in group 2. Of the 138 sealed teeth, only one showed GIS to be totally present, 95 were partially present and 42 teeth were absent. Conclusion: The caries-preventive effect was very similar between both treatments. The presence of dental caries prevailed in the children with caries experience. © 2013 Informa Healthcare.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This study evaluated the influence of different forms of heat treatment on a pre-hydrolyzed silane to improve the adhesion of phosphate monomer-based (MDP) resin cement to glass ceramic. Resin and feldspathic ceramic blocks (n=48, n=6 for bond test, n=2 for microscopy) were randomly divided into 6 groups and subject to surface treatments: G1: Hydrofluoric acid (HF) 9.6% for 20 s + Silane + MDP resin cement (Panavia F); G2: HF 9.6% for 20 s + Silane + Heat Treatment (oven) + Panavia F; G3: Silane + Heat Treatment (oven) + Panavia F; G4: HF 9.6% for 20 s + Silane + Heat Treatment (hot air) + Panavia F; G5: Silane + Heat Treatment (hot air) + Panavia F; G6: Silane + Panavia F. Microtensile bond strength (MTBS) test was performed using a universal testing machine (1 mm/min). After debonding, the substrate and adherent surfaces were analyzed using stereomicroscope and scanning electron microscope (SEM) to categorize the failure types. Data were analyzed statistically using two-way test ANOVA and Tukey's test (=0.05). Heat treatment of the silane containing MDP, with prior etching with HF (G2: 13.15 ± 0.89a; G4: 12.58 ± 1.03a) presented significantly higher bond strength values than the control group (G1: 9.16 ± 0.64b). The groups without prior etching (G3: 10.47 ± 0.70b; G5: 9.47 ± 0.32b) showed statistically similar bond strength values between them and the control group (G1). The silane application without prior etching and heat treatment resulted in the lowest mean bond strength (G6: 8.05 ± 0.37c). SEM analysis showed predominantly adhesive failures and EDS analysis showed common elements of spectra (Si, Na, Al, K, O, C) characterizing the microstructure of the glass-ceramic studied. Heat treatment of the pre-hydrolyzed silane containing MDP in an oven at 100 °C for 2 min or with hot air application at 50 ± 5 ºC for 1 min, was effective in increasing the bond strength values between the ceramic and resin cement containing MDP.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work, differential scanning calorimetry (DSC) was used to study effect of PbS impurity on crystallization mechanism of phosphate glasses. Bulk glasses presented one crystallization peak while powdered glasses presented two distinct crystallization peaks. For both undoped and doped glasses were determined the activation energies for the crystallization and the Avrami n parameters. The activation energies for undoped phosphate glass were 336 +/- 6 and 213 +/- 3 kJ mol(-1), respectively, associated with first and second crystallization peaks. For doped glass, the obtained energies were 373 +/- 9 and 286 +/- 7 kJ mol(-1). The calculated Avrami parameters, based on first crystallization peaks, for undoped and doped glasses were 2.25 +/- 0.01 and 1.75 +/- 0.02, respectively. These values suggest that the first DSC peak, in both glasses, may be associated with surface crystallization. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The purpose of this work is to study the 20Li(2)O-80TeO(2) glass using the differential scanning calorimetry (DSC) and X-ray diffraction (XRD) techniques in order to understand the crystallization kinetics on this glass matrix. To study the glass by DSC, screened samples with different particle sizes to resolve the observed asymmetrical crystallization peak were used. DSC curves for particles smaller than 38 mum in size show two distinct crystallization peaks, associated to distinct phase transformation in this glass, leading to activation energies at 301 and 488 kJ mol(-1). XRD analysis reveals that the first crystallization peak is attributed to TeO2 crystalline phase while the second one to the alpha-TeO3 and an unidentified phase.(C) 2004 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nucleation process and crystal growth for three samples of the (20-x)Li(2)O-80TeO(2)-xWO(3) glass system were studied using X-ray diffraction and differential scanning calorimetry techniques. X-ray diffraction data confirmed the amorphous characteristic of the as-quenched samples and indicated the growth of crystalline phases formed due to the thermal treatment for annealed samples. These results reveal the presence of three distinct gamma-TeO(2), alpha-TeO(2) and alpha-Li(2)Te(2)O(5) crystalline phases in the TL sample, and two distinct alpha-TeO(2) and gamma-TeO(2) crystalline phases in the TLW5 and TLW10 samples. The activation energy and the Avrami exponent were determined from DSC measurements. The activation energy values X-ray diffraction data of the TLW10 glass sample suggest that gamma-TeO(2) phase occur before the alpha-TeO(2). The results obtained for the Avrami exponent point to that the nucleation process is volumetric and that the crystal growth is two or three-dimensional.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In the present work, tellurite 20Li(2)O-80TeO(2) glasses were prepared with identical nominal composition under different glass-forming histories to produce a stressed and stress-free samples. X-ray Diffraction (XRD) and Differential Scanning Calorimetry (DSC) techniques were used to study the effects of the glass-forming histories on the thermal and structural properties of these glasses. The gamma-TeO2 (metastable), alpha-TeO2 and alpha-Li2Te2O5 phases were identified during the controlled devitrification in these glasses. The mestastable character of the gamma-TeO2 phase was clearly observed in the glass under stress but this effect is not so clear in the stress-free glass. The gamma-TeO2 and alpha-TeO2 phases crystallizes during the initial stages of crystallization in both studied glasses while the alpha-Li2Te2O5 phase crystallize in the final stages of the crystallization. The activation energies and Avrami exponent were calculated for both studied glasses with different particle size leading to E-3 > E-2 > E-1 for stressed glass and E-3 > E-2 approximate to E-1 for stress-free glass, where E-1, E-2 and E-3 were associated to the gamma-TeO2, alpha-TeO2 and alpha-Li2Te2O5 phases, respectively. The observed distinct (n) over bar (1) < <(n)over bar>(2) < <(n)over bar>(3) in both glasses is an indicative that nucleation and growth takes place by more than one mechanism in the early stages of the crystallization. (C) 2011 Elsevier B.V. All rights reserved.