106 resultados para Textile fibers.
Resumo:
We have studied the possibility of associating fluorescence microscopy and hematoxylin-eosin staining for the identification of elastic fibers in elastin-rich tissues. Elastic fibers and elastic laminae were consistently identified by the proposed procedure, which revealed itself to be easy and useful for the determination of such structures and their distribution. The fluorescence properties of stained elastic fibers are due to eosin staining as revealed by fluorescence analysis of the dye in solution, with no or only minor contribution by the elastin autofluorescence. The main advantage of this technique resides in the possibility of studying the distribution of elastic fibers in file material without further sectioning and staining. The use of the confocal laser scanning microscope greatly improved the resolution and selectivity of imaging elastic fibers in different tissues. The determination of the three-dimensional distribution and structure of elastic fiber and laminae using the confocal laser scanning microscope was evaluated and also produced excellent results.
Resumo:
A high performance liquid chromatography ( HPLC) method with electrochemical detection (ED) was developed for the determination of benzidine, 3,3-dimethylbenzidine, o-toluidine and 3,3-dichlorobenzidine in the wastewater of the textile industry. The aromatic amines were eluted on a reversed phase column Shimadzu Shimpack C-18 using acetonitrile + ammonium acetate (1 x 10(-4) mol L-1) at a ratio 46: 54 v/v as mobile phase, pumped at a flow rate of 1.0 mL min(-1). The electrochemical oxidation of the aromatic amines exhibits well-defined peaks at a potential range of +0.45 to +0.78 V on a glassy carbon electrode. Optimum working potentials for amperometric detection were from 0.70 V to +1.0 V vs. Ag/AgCl. Analytical curves for all the aromatic amines studied using the best experimental conditions present linear relationship from 1 x 10(-8) mol L-1 to 1.5 x 10(-5) mol L-1, r = 0.99965, n = 15. Detection limits of 4.5 nM (benzidine), 1.94 nM (o-toluidine), 7.69 nM (3,3-dimethylbenzidine), and 5.15 nM (3,3-dichlorobenzidine) were achieved, respectively. The detection limits were around 10 times lower than that verified for HPLC with ultra violet detection. The applicability of the method was demonstrated by the determination of benzidine in wastewater from the textile industry dealing with an azo dye processing plant.
Resumo:
This article reports on a series of experiments with polyethylene terepthalate (PET) treated in a radio frequency plasma reactor using argon and oxygen as a gas fuel, for treatment times equal to 5 s, 20 s, 30 s, and 100 s. The mechanical strength modification of PET fibers, evaluated by tensile tests on monofilaments, showed that oxygen and argon plasma treatment resulted in a decrease in the average tensile strength compared with the untreated fibers. This reduction in tensile strength is more significant for argon plasma and is very sensitive to the treatment time for oxygen plasma. Scanning electron microscopy (SEM) used to analyze the effects of cold plasma treatment on fiber surfaces indicates differences in roughness profiles depending on the type of treatments, which were associated with variations in mechanical strength. Differences in the roughness profile, surveyed through an image analysis method, provided the distance of roughness interval, D-ri. This parameter represents the number of peaks contained in a unit length and was introduced to correlate fiber surface condition, before and after cold plasma treatments, and average tensile strength. Statistical analysis of experimental data, using Weibull cumulative distribution and linear representation, was performed to explain influences of treatment time and environmental effects on mechanical properties. The shape parameter, alpha, and density parameter, beta, from the Weibull distribution function were used to indicate the experimental data range and to confirm the mechanical performance obtained experimentally.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Polypropylene powder and sisal fibers were oxygen plasma treated, and the mechanical properties of their composites were tested. Two main effects were investigated: the incorporation of oxygen polar groups in the polypropylene surface and the surface degradation and chain scission of both polypropylene and sisal fibers. Prior to these treatments, three reactor configurations were tested to investigate the best condition for both effects to occur in PP film. Results showed that polypropylene-cellulose adhesion forces are about an order of magnitude higher for PP film treatments at 13.56 MHz than at 40 kHz owing to much higher chain scission at lower frequencies, although it probably also occurs at high frequency and high power. Polypropylene powder treated with oxygen plasma in optimum conditions for polar group incorporation did not result in improvement in any composite mechanical property, probably owing to the polymer melting. Sisal fibers and PP powder treated In conditions of surface degradation did not improve flexural or tensile properties but resulted in higher impact resistance, comparable to the improvement obtained with the addition of compatibilizer.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
In order to cooperate in minimizing the problems of the current and growing volume of waste, this work aims at the production of panels made from industrial waste -thermoplastic (Polypropylene - PP; Polyethylene - PE and Acrylonitrile Butadiene Styrene - ABS) reinforced with agro-industrial waste - pupunha palm waste (shells and sheaths). The properties of the panels were evaluated: density, thickness swelling, water absorption and moisture content. It was used the ASTM D1037; EN 317; and ANSI A208.1 standards regarding particle boards. The best results in physical tests were treatments 1 (100% waste plastic), 6 (60% plastic waste and 40% waste of pupunha) and 7 (70% waste plastic and 30% waste of pupunha). The best results in the mechanical tests were treatments 3 (30% de residuos plasticos e 70% de residuos da pupunha), 4 (40% de residuos plasticos c 60% de residuos da pupunha) and 5 (50% de residuos plasticos e 50% de residuos da pupunha). For mechanical tests it was concluded that the results of modulus of rupture and of modulus of elasticity the best treatments were those with more fibers. In the tensile tests perpendicular to the surface, it is clear that using more waste plastics leads to the best results. It was concluded that the waste can be used as raw material for the production of alternative materials mainly in civil construction and furniture industries, and it can be employed in urban or rural environment, given the concept of eco-efficient products.