529 resultados para dentin microhardness


Relevância:

20.00% 20.00%

Publicador:

Resumo:

This in situ/ex vivo study assessed the effect of different concentrations of fluoride in dentifrices on dentin subjected to erosion or to erosion plus abrasion. Ten volunteers took part in this crossover and double-blind study performed in 3 phases (7 days). They wore acrylic palatal appliances containing 4 bovine dentin blocks divided in two rows: erosion and erosion plus abrasion. The blocks were subjected to erosion by immersion ex vivo in a cola drink (60 s, pH 2.6) 4 times daily. During this step, the volunteers brushed their teeth with one of three dentifrices D (5,000 ppm F, NaF, silica); C (1,100 ppm F, NaF, silica) and placebo (22 ppm F, silica). Then, the respective dentifrice slurry (1: 3) was dripped on dentin surfaces. While no further treatment was performed in one row, the other row was brushed using an electric toothbrush for 30 s ex vivo. The appliances were replaced in the mouth and the volunteers rinsed with water. Dentin loss was determined by profilometry and analyzed by 2-way ANOVA/Bonferroni test (alpha = 0.05). Dentin loss after erosive-abrasive wear was significantly greater than after erosion alone. Wear was significantly higher for the placebo than for the D and C dentifrices, which were not significantly different from each other. It can be concluded that the presence of fluoride concentrations around 1,100 ppm in dentifrices is important to reduce dentin wear by erosion and erosion + abrasion, but the protective effect does not increase with fluoride concentration. Copyright (C) 2008 S. Karger AG, Basel.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This in situ study evaluated the interaction between caries and erosion processes. In the first phase, enamel specimens were subjected to erosion without dental plaque (EO) or to erosion with plaque (EP); in the second phase, they were subjected to erosion plus cariogenic challenge (EC) or cariogenic challenge (CO), both with plaque accumulation. Cross-sectional hardness data (10-330 mu m depth) were tested using ANOVA (alpha = 0.05). EO and EP showed surface softening to 10 mu m depth. CO and EC produced subsurface lesions, of similar depth (up to 220 mu m), with CO showing higher integrated loss of hardness than EC, indicating that cariogenic and erosive challenges did not have an additive effect. Copyright (C) 2010 S. Karger AG, Basel

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives: the purpose of this study is to employ optical microscopy to measure the thickness of the hybrid layer and the penetration (tags) of an aggressive self-etching adhesive system into sound dentin.Methods: occtusat cavities were prepared in 40 extracted human posterior teeth. The prepared teeth were randomly assigned to four experimental groups with 10 specimens each. The self-etching adhesive system Adper Prompt L-Pop was applied to the dentin surface as follows: Group 1: cavosurface enamel was etched for 60 s and dentin for 20 s with 35% phosphoric acid get, immediately followed by application of the self -etching adhesive with a brush to the entire cavity for 15 s; Groups 2, 3, and 4: no pre-etching was performed, and the self -etching adhesive was applied to both enamel and dentin for 15, 30 and 45 s, respectively. After curing, the cavities were fitted with composite resin Fittek Z250. Afterwards, the teeth were decalcified and the restorations were carefully removed for later embedding in paraffin. The specimens were serially sectioned at 6 mu m of thickness and sequentially mounted in glass slides. These sections were stained with Brown and Brenn staining for posterior analysis and measurement of the hybrid layer and resin tags on a tight microscope with a micrometric ocular 40/075. The results were submitted to analysis of variance at the 5% level.Results: whenever there was significance, the Tukey test was applied at the 5% level. The specimens receiving application of acid etching before the selfetching. adhesive displayed a larger thickness of the hybrid layer; on the other hand, specimens receiving only application of the self -etching adhesive on dentin for 15, 30 and 45 s exhibited similar thickness of the hybrid layer. As regards the resin tags, no statistically significant differences could be found between the study groups.Conclusions: it could be concluded that the increase in the time of application of the self-etching adhesive Adper Prompt L-Pop did not significantly influence the formation and thickness of hybrid layer, as well as its penetration into the sound dentin surface. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives. To evaluate the response of the pulpo-dentin complex following application of a resin-modified glass-ionomer cement or an adhesive system in deep cavities performed in human teeth.Methods. Deep class V cavities were prepared on the buccal surface of 26 premolars. In Group I the cavity walls (dentin) and enamel were conditioned with 32% phosphoric acid and the dentin adhesive system One Step (Bisco, Inc., Itasca, IL, USA) was applied. In Groups 2 and 3, before total etching and application of bonding agent, the cavity floor was lined with the resin-modified glass-ionomer cement-Vitrebond (3M ESPE Dental Products Division, St. Paul, MN, USA) or the calcium hydroxide cement-Dycal (control group, Dentsply, Mildford, DE, USA), respectively. The cavities were restored using light-cured Z-100 composite resin (3M ESPE). The teeth were extracted between 5 and 30 days and prepared for microscopic assessment. Serial sections were stained with H/E, Masson's trichrome, and Brown and Brenn techniques.Results. In Group 1, the inflammatory response was more evident than in Groups 2 and 3. Diffusion of dental material components across dentinal tubules was observed only in Group 1, in which the intensity of the pulp response increased as the remaining dentin thickness decreased. Bacteria were evidenced in the lateral walls of two samples (Group 2) which exhibited no inflammatory response or tissue disorganization.Conclusions. Based on the experimental conditions, it was concluded total acid etching followed by application of One Step bonding agent cannot be recommended as adequate procedures. In this clinical condition the cavity walls should be lined with a biocompatible dental material, such as Vitrebond or Dycal. 2003 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study evaluated the surface microhardness of four glass ionomer cements and a composite resin (Fuji IX, Ketac Molar, Vidrion R, Vitromolar and Z 250). Ten specimens of each glass ionomer cement with 8.0 mm diameter and 5.0 mm high dimensions were made and Vicker's microhardness measurements were taken at 1 day and 1 week after initial setting reaction. The results were analyzed using Student's T test and Tukey test (p < 0.05) and demonstrated that the values of microhardness increased after 1 week, with the exception of Fuji IX. Resin composite Z250 presented the greatest values for microhardness.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objective. The aim of this study was to investigate the influence of shortening the etching time on the bond strength of a conventional and a self-etching primer adhesive system used in primary tooth dentin.Methods. Flat dentin surfaces were obtained from 24 primary molars, randomly assigned to 4 experimental groups. The adhesive systems Single Bond and Clearfil SE Bond were applied in two groups according to the manufacturers' recommendations. In the other two groups, the adhesives were applied after half-time of acid etching, 7 s for Single Bond and 10 s for Clearfil SE Primer. Resin crowns were built up and after 24 h storage in water at 37 &DEG; C, the teeth were sectioned to produce beams with cross-sectional area of approximately 0.49 mm(2). Specimens were tested in tension at 0.5 mm/min until failure. Fractured specimens were analyzed to determine the failure mode.Results. Tensile bond strengths for Single Bond in primary dentin were higher than for Clearfil SE Bond. Shortening of acid etching time improved bond strength only for Single Bond, while no statistically significant difference was observed for Clearfil SE Bond when both etching times were compared.Significance. No detrimental effect on bond strength was observed when the time of acid etching was shortened in 50%. Shortening the time for a procedure in a small child without compromising the quality of the work is a very important finding for the practicing pediatric dentist. © 2004 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: To analyze the smear layer and the hybrid layer in noncarious and carious dentin prepared by different cutting instruments and restored with composite resin. Study design: Cavities were randomly prepared in 160 specimens (noncarious and artificial carious dentin) by high-speed diamond tips (KG Sorensen 1013), air abrasion system (Prepstart, Danville Engineering), ultrasonic tip (CVDentus 8.3231-1), and ultrasonic tip associated with ultrasonic cavitation by water for 10 s. Half of the cavities in each group were conditioned with 37% phosphoric acid for 15 s. The amount of smear layer and dentinal tubules present were analyzed using scanning electron microscopy and graded from 0 to 3. Cavities were prepared in another 20 noncarious specimens and 20 carious specimens and restored with adhesive composite resin system. The restorations were hemisected longitudinally and analyzed using scanning electron microscopy to evaluate the hybrid layer and resinous prolongation characteristics, using scores ranging from 1 to 6. Results: The data were statistically analyzed using Kruskal-Wallis and Dunn tests at 5% of significance level. There was evidence that the most efficient smear layer removal was the acid etching in the noncarious dentin and the water ultrasonic cavitation in the carious dentin. The hybrid layer formed on the noncarious and carious dentin prepared by the ultrasonic tip was more regular than in the specimens prepared by high-speed diamond tip, with many resinous prolongations. Conclusion: The ultrasonic tip seems to be a promising tool for carious dentin cavity preparation. Microsc. Res. Tech. 73:597-605, 2010. (C) 2009 Wiley-Liss, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)