Amorphous and crystalline powder of PLT phase was synthesized by using the Pechini method. Infrared (FTIR) analysis of the polymeric resin shows intense bands of organic materials from 250 to 1620 cm(-1). X-ray diffraction (XRD) and Raman spectra of calcined powder at different temperatures show amorphous phase at 450 degrees C/3 h, semi-crystalline phase at 550 degrees C/3 h and a crystalline phase at 800 degrees C/3 h. Luminescence effect was observed in amorphous powder calcined from 300 to 350 degrees/3 h with broad absorption peaks in 579 nm at 300 degrees C/3 h and 603 rum at 350 degrees C/3 h, respectively. The photoluminescence effect is attributed to emissions of Ti -> 0 directly from the oxygen 2p orbital (valence band) to the titanate 3d orbital (conduction bands). (c) 2004 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this work is to report on the luminescence properties of BaZnSiO4 activated by Eu3+ and Mn2+ ions. Doped and undoped powder samples were prepared by solid-state reaction starting from oxides and carbonates or Ba2SiO4:Eu3+ and Zn2SiO4:Mn2+ precursors. X-ray diffraction powder data, IR vibrational, and UV-vis luminescence spectroscopies were carried out. Results showed that doped and undoped samples from both types of precursors have the same structure and crystallize with a superstructure of hexagonal kalsilite. Vibrational spectroscopy has confirmed the formation of a silicate group, which outlines differences between products and silicate precursors. The observed luminescence assigned to Eu3+ and Mn2+ transitions covered most parts of the visible spectrum, an important requirement for phosphors in fluorescent low-pressure mercury vapor lamps.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of binary diphenylphosphinates with Eu3+ and Gd3+ were prepared. The compounds have the general formula Gd1-xEux(DPP)(3), where x ranges from 0 to 1. The spectroscopic measurements show interesting behavior. The intensity of the D-5(0) --> F-7(2) transitions decreases relative to D-5(0) --> F-7(1) With an increase in europium dispersion. Inside the temporal domain, the same decrease is observed with increasing delay after excitation. The lifetimes are also affected, which can be seen in the x = 1 compound, where the decay is a first-order process and lifetime values are 4.81 ms. In the binary compound, as an effect of dispersion, the lifetime of the D-5(0) level measured at the D-5(0) --> F-7(1) transition increases with europium dispersion, and the average along the series is 6.25 ms. The decay measured at the D-5(0) --> F-7(2) transitions reveals a second-order process with lifetimes ranging from 1.90 to 6.00 ms. (C) 2001 Elsevier B.V. B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper presents an analysis and discussion, based on cooperative game theory, for the allocation of the cost of losses to generators and demands in transmission systems. We construct a cooperative game theory model in which the players are represented by equivalent bilateral exchanges and we search for a unique loss allocation solution, the Core. Other solution concepts, such as the Shapley Value, the Bilateral Shapley Value and the Kernel are also explored. Our main objective is to illustrate why is not possible to find an optimal solution for allocating the cost of losses to the users of a network. Results and relevant conclusions are presented for a 4-bus system and a 14-bus system. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Infrared-to-visible and infrared-to-infrared frequency upconversion processes in Yb3+-Tm3+ doped PbO-GeO2 glasses containing silver nanoparticles (NPs) were investigated. The experiments were performed by exciting the samples with a diode laser operating at 980 nm (in resonance with the Yb3+ transition F-2(7/2)-> F-2(5/2)) and observing the photoluminescence (PL) in the visible and infrared regions due to energy transfer from Yb3+ to Tm3+ ions followed by excited state absorption in the Tm3+ ions. The intensified local field in the vicinity of the metallic NPs contributes for enhancement in the PL intensity at 480 nm (Tm3+ :(1)G(4)-> H-3(6)) and at 800 nm (Tm3+ : H-3(4) -> H-3(6)). (C) 2009 American Institute of Physics. [doi:10.1063/1.3211300]

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)