266 resultados para ceramic tiles
Resumo:
Nowadays, with increase amounts of sludge derived from the treatment of domestic sewage put pressure into research on systems for the adequate use of these materials. The aim of the present work is to study the use of sludge ash, from sintering and calcinated process, as a raw material for the ceramic industry. Using the sewage sludge ashes as ceramic raw material there will be no contamination of soil and underground water. Metals and toxic compounds like Al, Fe, Ba, Cr, Cu, Mn and Zn oxides were analyzed and characterized by X-ray fluorescence (XRF), scanning electron microscopy (SEM) and plasma emission spectroscopy (ICP-OES). The leached material was chemically analyzed where the integration of oxides into the ceramic matrix of sludge ash was observed. Residual decomposition was analyzed by TG, DTG and DTA curves.
Resumo:
An archeological artifact can be seen as a chronological element, which helps to determine the age of certain society and to understand the thinking, values and the way of life of this society. Thus, the classification of archeological artifacts is one of the approaches used to study the cultural system of antique societies trying to reconstruct their history. The "Centro de Museologia, Antropologia e Argueologia (CEMAARQ)" of the "Unesp Univ Estadual Paulista" in Presidente Prudente, São Paulo state, Brazil, develops projects within this context (identification and preservation). This is the case of the archeological site named "Lagoa São Paulo-02" discovered in 1993 at the margins of the Parana river in the region of Presidente Epitacio city, São Paulo state, Brazil. This site has ceramic fragments of different shapes and sizes that have a strong influence of traces of the Guarani culture, which is one of the Brazilian native populations. These samples were basically characterized via micro-Raman scattering and Fourier transform infrared absorption (FTIR) spectroscopies. The main objective was to identify the pigments used in the manufacture of the ceramic artifacts and to analyze the composition of the ceramic body to understand how the artifacts were made. Three pigments were found: red, black and white. For the red pigment were identified characteristic bands of hematite, an iron oxide found in the red rocks of the river banks that were eroded by water. The black pigment, probably, is due to the use of vegetal charcoal, which is found in nature as the product of burning organic material such as wood. For the white pigment, the FTIR spectra suggested the use of kaolin, either in the ceramic body or in the proper white pigment, due to the presence of the characteristic bands of the kaolinite. Complementary, the additives applied as anti-plastics were identified as charcoal and quartz, being the latter found in the rocks present in the archeological site. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Sugarcane bagasse ash (SCBA) is an industrial waste that contains silicon and aluminum oxides as the major components and iron, calcium, magnesium, and potassium oxides as the main minor components. In this paper, SCBA from one Brazilian factory was characterized and tested for its influence on the ceramic properties of clay/ash ceramic probes. Prismatic probes were pressed (18 MPa) using a ceramic mass mixed with 0%, 5%, 8%, and 10% ash. The probes were fired at temperatures between 800 degrees and 1200 degrees C. X-ray diffraction, X-ray fluorescence, thermal analysis (differential thermal analysis, thermo-gravimetric analysis/differential thermogravimetric analysis), and tests for texture (particle-size analysis), flexural strength, and linear shrinkage were carried out to characterize the samples. The results showed that the amount of ash to be incorporated will depend on mainly the composition of clay but also ash, and indicated that the clay used in this work can incorporate up to 10% weight of ash to produce solid bricks. The results also showed an improvement in ceramic/ash properties up to sintering temperatures higher than 1000 degrees C.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
A method has been developed to obtain quantitative information about grain size and shape from fractured surfaces of ceramic materials. One elaborated a routine to split intergranular and transgranular grains facets of ceramic fracture surfaces by digital image processing. A commercial ceramic (ALCOA A-16, Al2O3-1.5% of CrO) was used to test the proposed method. Microstructural measurements of grain shape and size taken from fracture surfaces have been compared through descriptive statistics of distributions, with the corresponding measurements from polished and etched surfaces. The agreement between results, with the expected bias on grain size values from fractures, obtained for both types of surfaces allowed to infer that this new technique can be used to extract the relevant microstructural information from fractured surfaces, thus minimising the time consuming steps of sample preparation. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
The non-ohmic and dielectric properties as well as the dependence on the microstructural features of CaCu(3)Ti(4)O(12)/CaTiO(3) ceramic composites obtained by conventional and microwave sintering were investigated. It was demonstrated that the non-ohmic and dielectric properties depend strongly on the sintering conditions. It was found that the non-linear coefficient reaches values of 65 for microwave-sintered samples and 42 for samples sintered in a conventional furnace when a current density interval of 1-10 mA cm(-2) is considered. The non-linear coefficient value of 65 is equivalent to 1500 for samples sintered in the microwave if a current interval of 5-30 mA is considered as is shortly discussed by Chung et al (2004 Nature Mater. 3 774). Due to a high non-linear coefficient and a low leakage current (90 mu A) under both processing conditions, these samples are promising for varistor applications. The conventionally sintered samples exhibit a higher relative dielectric constant at 1 kHz (2960) compared with the samples sintered in the microwave furnace (2100). At high frequencies, the dielectric constant is also larger in the samples sintered in the conventional furnace. Depending on the application, one or another synthesis methodology is recommended, that is, for varistor applications sintered in a microwave furnace and for dielectric application sintered in a conventional furnace.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The recent discovery of a ferroelectric monoclinic phase in the PbZr1-xTixO3 (PZT) system attained the attention of several researchers due to the possibility of understanding the relationships between structural features and piezoelectric properties. The nature of the monoclinic phase in some PZT compositions remains controversial and unclear. In this work, structural phase transitions of PbZr0.52Ti0.48O3 ceramic were investigated by infrared spectroscopy as a function of temperature. Studies were centered on nu(1)-stretching modes and corresponding half width Wi as a function of temperature. The occurrence of the anomalies in the infrared spectra as a function of temperature suggests the following monoclinic ( LT) -> monoclinic ( HT) -> tetragonal phase transition were observed at 183 K and at 263 K.
Resumo:
Slightly < 111 >-oriented 0.65Pb(Mg1/3Nb2/3)03-0.35PbTiO(3) ceramic was prepared using fine powders obtained by means of an alternative and promising chemical oxide precursor method. High quality samples with improved structural, microstructural, dielectric and ferroelectric properties were obtained. The dielectric constant value (epsilon similar to 2577) measured at 1 kHz is compared to unpoled < 112 > grain-oriented ceramics while the remanent polarization (P-r similar to 19-1 mu cm(-2)) is compared with random grain-oriented ceramics. These results point out the viability to produce ferroelectric PMN-PT ceramics of very good quality using powder precursors prepared from this chemical method. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Flexible piezo- and pyroelectric composite was made in the thin film form by spin coating. Lead Zirconate Titanate (PZT) ceramic powder was dispersed in a castor oil-based polyurethane (PU) matrix, providing a composite with 0-3 connectivity. The dielectric data, measured over a wide range of frequency (10(-5) Hz to 105 Hz), shows a loss peak around 100 Hz related with impurities in the polymer matrix. There is also an evidence of a peak in the range 10(-4) Hz, possibly originating from the glass transition temperature T of the polymer. The pyroelectric coefficient at 34 K is 7.0x10(-5) C(.)m(-2.)K(-1) which is higher than that of P-PVDF (1X10(-5) C(.)m(-2.)K(-1)).
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The thermoluminescence (TL) response of Dy and Li doped 20CaB(4)O(7)-80CaB(2)O(4) (Wt%) glass-ceramic irradiated with ultraviolet (UV) radiation was studied. In order to act as TL activator ions, the Dy and Li ions were included in the matrix during the melting process to increase its TL efficiency. A single crystalline CaB2O4 phase was present in the glass-ceramic as determined by X-ray diffraction (XRD). The glass-ceramic 20CaB(4)O(7)-80CaB(2)O(4):Dy,Li wt% (named 20CBO7:Dy,Li) is a newly prepared TL material. Its thermoluminescent dosimetric characteristics have shown a linear response under UV radiation exposure and a good TL signal reproducibility, thus proving to be a promising material for using as an ultraviolet radiation dosimeter. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Purpose: This three-dimensional finite element analysis study evaluated the effect of different material combinations on stress distribution within metal-ceramic and all-ceramic single implant-supported prostheses. Materials and Methods: Three-dimensional finite element models reproducing a segment of the maxilla with a missing left first premolar were created. Five groups were established to represent different superstructure materials: GP, porcelain fused to gold alloy; GR, modified composite resin fused to gold alloy; TP, porcelain fused to titanium; TR, modified composite resin fused to titanium; and ZP, porcelain fused to zirconia. A 100-N vertical force was applied to the contact points of the crowns. All models were fixed in the superior region of bone tissue and in the mesial and distal faces of the maxilla section. Stress maps were generated by processing with finite element software. Results: Stress distribution and stress values of supporting bone were similar for the GP, GR, TP, and ZP models (1,574.3 MPa, 1,574.3 MPa, 1,574.3 MPa, and 1,574.2 MPa, respectively) and different for the TR model (1,838.3 MPa). The ZP model transferred less stress to the retention screw (785 MPa) than the other groups (939 MPa for GP, 961 MPa for GR, 1,010 MPa for TP, and 1,037 MPa for TR). Conclusion: The use of different materials to fabricate a superstructure for a single implant-supported prosthesis did not affect the stress distribution in the supporting bone. The retention screw received less stress when a combination of porcelain and zirconia was used. Int J Oral Maxillofac Implants 2011;26:1202-1209