In order to prolong the clinical longevity of resilient denture relining materials and reduce plaque accumulation, incorporation of antimicrobial agents into these materials has been proposed. However, this addition may affect their properties. Objective: This study evaluated the effect of the addition of antimicrobial agents into one soft liner (Soft Confort, Dencril) on its peel bond strength to one denture base (QC 20, Dentsply). Material and Methods: Acrylic specimens (n=9) were made (75x10x3 mm) and stored in distilled water at 37 degrees C for 48 h. The drug powder concentrations (nystatin 500,000U - G2; nystatin 1,000,000U - G3; miconazole 125 mg - G4; miconazole 250 mg - G5; ketoconazole 100 mg - G6; ketoconazole 200 mg - G7; chlorhexidine diacetate 5% - G8; and 10% chlorhexidine diacetate - G9) were blended with the soft liner powder before the addition of the soft liner liquid. A group (G1) without any drug incorporation was used as control. Specimens (n=9) (75x10x6 mm) were plasticized according to the manufacturers' instructions and stored in distilled water at 37 degrees C for 24 h. Relined specimens were then submitted to a 180-degree peel test at a crosshead speed of 10 mm/min. Data (MPa) were analyzed by analysis of variance (alpha=0.05) and the failure modes were visually classified. Results: No significant difference was found among experimental groups (p=0.148). Cohesive failure located within the resilient material was predominantly observed in all tested groups. Conclusions: Peel bond strength between the denture base and the modified soft liner was not affected by the addition of antimicrobial agents.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Denture fractures are common in daily practice, causing inconvenience to the patient and to the dentists. Denture repairs should have adequate strength, dimensional stability and color match, and should be easily and quickly performed as well as relatively inexpensive. Objective: The aim of this study was to evaluate the flexural strength of acrylic resin repairs processed by different methods: warm water-bath, microwave energy, and chemical polymerization. Material and methods: Sixty rectangular specimens (31x10x2.5 mm) were made with warm water-bath acrylic resin (Lucitone 550) and grouped (15 specimens per group) according to the resin type used to make repair procedure: 1) specimens of warm water-bath resin (Lucitone 550) without repair (control group); 2) specimens of warm water-bath resin repaired with warm water-bath; 3) specimens of warm water-bath resin repaired with microwave resin (Acron MC); 4) specimens of warm water-bath resin repaired with autopolymerized acrylic resin (Simplex). Flexural strength was measured with the three-point bending in a universal testing machine (MTS 810 Material Test System) with load cell of 100 kgf under constant speed of 5 mm/min. Data were analyzed statistically by Kruskal-Wallis test (p<0.05). Results: The control group showed the best result (156.04 +/- 1.82 MPa). Significant differences were found among repaired specimens and the results were decreasing as follows: group 3 (43.02 +/- 2.25 MPa), group 2 (36.21 +/- 1.20 MPa) and group 4 (6.74 +/- 0.85 MPa). Conclusion: All repaired specimens demonstrated lower flexural strength than the control group. Repairs with autopolymerized acrylic resin showed the lowest flexural strength.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objective: The aim of this study was to evaluate the fracture strength and failure mode of flared bovine roots restored with different intraradicular posts. Material and Methods: Fifty bovine incisors with similar dimensions were selected and their roots were flared until 1.0 mm of dentin wall remained. Next, the roots were allocated into five groups (n=10): GI-cast metal post-and-core; GII-fiber posts plus accessory fiber posts; GIII-direct anatomic post; GIV-indirect anatomic post and GV-control (specimens without intraradicular post). A polyether impression material was used to simulate the periodontal ligament. After periodontal ligament simulation, the specimens were subjected to a compressive load at a crosshead speed of 0.5 mm/min in a servo-hydraulic testing machine (MTS 810) applied at 135 to the long axis of the tooth until failure. The data (N) were subjected to ANOVA and Tukey's post-hoc test (alpha=0.05). Results: GI and GIV presented higher fracture strength (p<0.05) than GII. GIII presented intermediate values without statistically significant differences (p>0.05) from GI, GII and GIV. Control specimens (GV) produced the lowest fracture strength mean values (p<0.05). Despite obtaining the highest mean value, GI presented 100% of unfavorable failures. GII presented 20% of unfavorable failures. GIII, GIV and GV presented only favorable failures. Conclusions: Although further in vitro and in vivo studies are necessary, the results of this study showed that the use of direct and indirect anatomic posts in flared roots could be an alternative to cast metal post-and-core.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objectives: To compare the fracture resistance of bovine teeth after intracoronal bleaching with sodium percarbonate (SPC) or sodium perborate (SP) mixed with water or 20% hydrogen peroxide (HP). Materials and methods: Fifty extracted bovine teeth were divided into four experimental groups (G1G4) and one control (n = 10) after endodontic treatment. Following root canal obturation, a glass ionomer barrier was placed at the cementoenamel junction. After that, the pulp chambers were filled with: G1 SP with water; G2 SP with 20% HP; G3 SPC with water; and G4 SPC with 20% HP. No bleaching agent was used in the control group. Coronal access cavities were sealed with glass ionomer and specimens were immersed in artificial saliva. The bleaching agents were replaced after 7 days, and teeth were kept in artificial saliva for an additional 7 days, after which the pastes were removed and the coronal access cavities were restored with glass ionomer. Crowns were subjected to compressive load at a cross head speed of 0.5 mm min-1 applied at 135 degrees to the long axis of the root by an EMIC DL2000 testing machine, until coronal fracture. Data were statistically analysed by anova and Tukey test. Results: No differences in fracture resistance were observed between the experimental groups (P > 0.05). However, all experimental groups presented lower fracture resistance than the control group (P < 0.05). Conclusion: SPC and SP led to equal reduction on fracture resistance of dental crowns, regardless of being mixed with water or 20% HP.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The purpose of this study was to investigate the bond strength of fiber post previously laser treated root canals. Forty single-rooted bovine teeth were endodontically treated, randomly and equally divided into two main groups according to the type of pretreatment: G1: 2.5% NaOCl (control group); and G2: Er,Cr:YSGG laser. Each group was further subdivided into 2 groups based on the category of adhesive systems/ luting materials used: a: an etch-and-rinse resin cement (Single Bond/RelyX ARC; 3M ESPE), and b: a self-adhesive resin cement (Rely X Unicem; 3M ESPE). Three 1.5 mm thick slabs were obtained per root and the push-out test was performed at a crosshead speed of 0.5 mm/min until post dislodgement occurred. Data were analyzed by ANOVA and post-hoc Tukey's test at a pre-set alpha of 0.05. Analysis of variance showed no statistically significant difference (p > 0.05) among the groups G1a (25.44 ± 2.35) and G1b (23.62 ± 3.48), G2a (11.77 ± 2.67) and G2b (9.93 ± 3.37). Fractures were observed at the interface between the dentin and the resin in all groups. The Er,Cr:YSGG laser irradiation did not influence on the bond strength of the resin cements and the etch-and-rinse resin cement had better results on bond strength than self-adhesive resin cement.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Objective: The aim of this in vitro study was to evaluate the bond strength of different root canal sealers to dentin. Material and Methods: Forty extracted single-rooted human teeth were examined and the coronal and middle thirds of the canals were prepared with a 1.50 mm post drill (FibreKor Post System, Pentron). The teeth were allocated in two experimental groups, irrigated with 2.5% NaOCl+17% EDTA or saline solution (control group) and instrumented using Race rotary files (FKG) to a size #40 at the working length. Then, the groups were divided into four subgroups and filled with Epiphany sealer (Group 1), EndoREZ (Group 2), AH26 (Group 3) and Grossman's Sealer (Group 4). After 2 weeks of storage in 100% humidity at 37 degrees C, all teeth were sectioned transversally into 2-mm-thick discs. Push-out tests were performed at a cross-head speed of 1 mm/min using a universal testing machine. The maximum load at failure was recorded and expressed in MPa. Results: Means (+/- SD) in root canals irrigated with 2.5% NaOCl and 17% EDTA were: G1 (21.6 +/- 6.0), G2 (15.2 +/- 3.7), G3 (14.6 +/- 4.5) and G4 (11.7 +/- 4.1). Two-way ANOVA and Tukey's test showed the highest bond strength for the Epiphany's group (p < 0.01) when compared to the other tested sealers. Saline solution decreased the values of bond-strength (p < 0.05) for all sealers. Conclusion: Epiphany sealer presented higher bond strength values to dentin in both irrigating protocols, and the use of 2.5% NaOCl and 17% EDTA increased the bond strength values for all sealers.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The Epiphany (TM) Sealer is a new dual-curing resin-based sealer and has been introduced as an alternative to gutta-percha and traditional root canal sealers. The canal filling is claimed to create a seal with the dentinal tubules within the root canal system producing a 'monoblock' effect between the sealer and dentinal tubules. Therefore, considering the possibility to incorporate the others adhesive systems, it is important to study the bond strength of the resulting cement. Forty-eight root mandibular canines were sectioned 8-mm below CEJ. The dentine discs were prepared using a tapered diamond bur and irrigated with 1% NaOCl and 17% EDTA. Previous the application Epiphany (TM) Sealer, the Epiphany (TM) Primer, AdheSE, and One Up Bond F were applied to the root canal walls. The LED and QTH (Quartz Tungsten Halogen) were used to photo-activation during 45 s with power density of 400 and 720 mW/cm(2), respectively. The specimens were performed on a universal testing machine at a cross-head speed of 1 mm/min until bond failure occurred. The force was recorded and the debonding values were used to calculate Push-out bond strength. The analysis of variance (ANOVA) and Tukey's post-hoc tests showed significant statistical differences (P < 0.05) to Epiphany (TM) Sealer/Epiphany (TM) Primer/QTH and EpiphanyTM Sealer/AdheSE/QTH, which had the highest mean values of bond strength. The efficiency of resin-based filling materials are dependent the type of light curing unit used including the power density, the polymerization characteristics of these resin-based filling materials, depending on the primer/adhesive used.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Portuguese chestnut (Castanea sativa) is used for forest products, raw nuts and processed flour, paste, and candy. We studied the influence on germination efficiency of seed with and without partial tegument removal combined with different substrate composition (coconut fiber, pine compost and vermiculite) at São Paulo State University, Campus of Botucatu, São Paulo, Brazil. Randomized blocks were used in a factorial scheme 3x2 (three substrates x two seed types) consisting of six treatments with five replications (twelve seeds). Seeds were sowed in expanded polystyrene trays, with 72 cells, and maintained at 25 C under controlled environment. Rate, time elapsed and speed of seed germination was submitted to ANOVA and the average compared using Tukey's 5% test of probability and curves adjusted based on Gompertz regression. Coconut fiber or vermiculite associated with seed without partial tegument removal showed the highest germination rate, and coconut fiber with or without partial tegument removal displayed the fastest speed of seed germination.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Tropidurid lizards have colonized a variety of Brazilian open environments without remarkable morphological variation, despite ecological and structural differences among habitats used. This study focuses on two Tropidurus sister-species that, despite systematic proximity and similar morphology, exhibit great ecological divergence and a third ecologically generalist congeneric species providing an outgroup comparison. We quantified jumping capacity and sprint speed of each species on sand and rock to test whether ecological divergence was also accompanied by differences in locomotor performance. Relevant physiological traits possibly associated with locomotor performance metabolic scopes and fiber type composition, power output and activity of the enzymes citrate synthase, pyruvate kinase and lactate dehydrogenase of the iliofibularis muscle - were also compared among the three Tropidurus species. We found that the two sister-species exhibited remarkable differences in jumping performance, while Tropidurus oreadicus, the more distantly related species, exhibited intermediate values. Tropidurus psamonastes, a species endemic to sand dunes, exhibited high absolute sprint speeds on sand, jumped rarely and possessed a high proportion of glycolytic fibers and low activity of citrate synthase. The sister-species Tropidurus itambere, endemic to rocky outcrops, performed a large number of jumps and achieved lower absolute sprint speed than T. psamonastes. This study provides evidence of rapid divergence of locomotor parameters between sister-species that use different substrates, which is only partially explained by variation in physiological parameters of the iliofibularis muscle.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Foi avaliado o possível efeito de tratamentos superficiais em pinos de fibra de carbono lisos, quando comparados aos pinos serrilhados, na retenção à resina composta empregada na confecção de núcleos de preenchimento. Foram utilizados cinqüenta pinos de fibra de carbono, divididos em cinco grupos: os quatro primeiros grupos eram constituídos por pinos do tipo liso, cujas superfícies foram tratadas, e o último grupo por dez pinos do tipo serrilhado. Foram desenvolvidas matrizes de resina acrílica com um leito ajustado para conter o pino, com um alargamento na porção coronária para posterior preenchimento com resina composta. Após o tratamento superficial, todos os pinos receberam camadas de primer, foram secos e então ajustados à matriz de resina, colocando-se a resina composta autopolimerizável na porção coronária para um núcleo de preenchimento de 3 mm. As amostras foram submetidas a termociclagem e armazenadas em água destilada por uma semana. Os espécimes foram testados por meio de ensaios mecânicos de tração, à velocidade de 0,5 mm/min, até o deslocamento do conjunto ou a fratura da resina do núcleo. As conclusões foram as seguintes: a) o tratamento superficial nos grupos tratados por meio de jateamento (Grupo A), pontas diamantadas marcadoras de profundidade para facetas laminadas (Grupo C) e alteração da morfologia da extremidade coronária (Grupo D) conferiu aos pinos lisos valores de retenção comparáveis aos dos pinos serrilhados (Grupo E) nos ensaios de tração, porém sem diferença estatisticamente significativa entre estes grupos; b) os pinos tratados por meio de pontas diamantadas de granulação média (Grupo B) obtiveram valores de retenção menores que os demais grupos.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Statement of problem. Different combinations of Co-Cr alloys bonded to ceramic have been used in dentistry; however, the bond strength of ceramic to metal can vary because of different compositions of these alloys.Purpose. The purpose of this study was to evaluate the shear bond strength of a dental ceramic to 5 commercially available Co-Cr alloys.Material and methods. Five Co-Cr alloys (IPS d.SIGN 20, IPS d.SIGN 30, Remanium 2000, Heranium P, and Wirobond C) were tested and compared to a control group of an Au-Pd alloy (Olympia). Specimen disks, 5 mm high and 4 mm in diameter, were fabricated with the lost-wax technique. Sixty specimens were prepared using opaque and dentin ceramics (VITA Omega 900), veneered, 4 mm high and 4 mm in diameter, over the metal specimens (n = 10). The shear bond strength test was performed in a universal testing machine with a crosshead speed of 0.5 mm/min. After shear bond testing, fracture surfaces were evaluated in a stereomicroscope under x25 magnification. Ultimate shear bond strength (MPa) data were analyzed with 1-way ANOVA and the Tukey HSD test (alpha = .05).Results. The mean (SID) bond strengths (MPa) were: 61.4 (7.8) for Olympia; 94.0 (18.9) for IPS 20; 96.8 (10.2) for I PS 30; 75.1 (12.4) for Remanium; 71.2 (14.3) for Heranium P; and 63.2 (10.9) for Wirobond C. Mean bond strengths for IPS 20 and IPS 30 were not significantly different, but were significantly (P<.001) higher than mean bond strengths for the other 4 alloys, which were not significantly different from each other.Conclusions. Bond strength of a dental ceramic to a Co-Cr alloy is dependent on the alloy composition.