65 resultados para PVDF
Resumo:
Flexible piezo- and pyroelectric composite was made in the thin film form by spin coating. Lead Zirconate Titanate (PZT) ceramic powder was dispersed in a castor oil-based polyurethane (PU) matrix, providing a composite with 0-3 connectivity. The dielectric data, measured over a wide range of frequency (10(-5) Hz to 105 Hz), shows a loss peak around 100 Hz related with impurities in the polymer matrix. There is also an evidence of a peak in the range 10(-4) Hz, possibly originating from the glass transition temperature T of the polymer. The pyroelectric coefficient at 34 K is 7.0x10(-5) C(.)m(-2.)K(-1) which is higher than that of P-PVDF (1X10(-5) C(.)m(-2.)K(-1)).
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The phase transition from the non-polar a-phase to the polar beta-phase of poly(vinylidene fluoride) (PVDF) has been investigated using micro-Raman spectroscopy, which is advantageous because it is a nondestructive technique. Films of alpha-PVDF were subjected to stretching under controlled rates at 80 degrees C, while the transition to P-PVDF was monitored by the decrease in the Raman band at 794 cm(-1) characteristic of the a-phase, along with the concomitant increase in the 839 cm-1 band characteristic of the P-phase. The alpha ->beta transition in our PVDF samples could be achieved even for the sample stretched to twice (2 X -stretched) the initial length and it did not depend on the stretching rate in the range between 2.0 and 7.0 mm/min. These conclusions were corroborated by differential scanning calorimetry (DSC) and X-ray diffraction experiments for PVDF samples processed under the same conditions as in the Raman scattering measurements. Poling with negative corona discharge was found to affect the a-PVDF morphology, improving the Raman bands related to this crystalline phase. This effect is minimized for films stretched to higher ratios. Significantly, corona-induced effects could not be observed with the other experimental techniques, i.e., X-ray diffraction and infrared spectroscopy.
Resumo:
We report on light-emitting devices based on a green-phosphor compound (Mn-doped zinc silicate, Zn2SiO4: Mn) dispersed in a conductive polymeric blend (poly-o-methoxyaniline/polyvinylene fluoride, POMA/PVDF-TrFE). The devices exhibited high luminance in the green, good stability and homogeneous brilliance over effective areas up to 5 cm(2). The electroluminescence (EL) spectrum presented essentially the same characteristics as the photoluminescence (PL) and cathodoluminescence spectra, indicating that the light emission originates from decay of the same excited species, regardless of the excitation source. Operating characteristics were analyzed with current density - voltage (J - V) and luminance voltage ( L - V) curves to investigate the nature of the electroluminescence of the active material, which is still not completely understood.
Resumo:
Blends of poly(o-methoxyaniline) - POMA - and poly(vinylidene fluoride) - PVDF - of various compositions were prepared from organic solvent solutions. Flexible, free-standing and stretchable films were obtained by casting, which were characterized by conductivity measurements, electron microscopy and differential scanning calorimetry. As expected, the blends conductivity increases with increasing contents of the conducting polymer. The onset of the conductivity at low contents of conducting polymer indicates a low percolation threshold for the blends. Despite the presence of the conductive host, the blends displayed the crystalline spherulitic morphology and the beta-phase characteristic of pure PVDF. This morphology appears to be destroyed, however, if the film is stretched by zone-drawing.
Resumo:
A novel method is proposed for measuring the hysteresis loops of ferroelectric polymers. The samples need to have only one electrode and are poled by corona discharge in a constant current corona triode. It is shown how the sample surface potential and the charging current are related to the remanent polarization and coercive field, so that the hysteresis loops can be obtained. An illustrative example is given for samples of beta-PVDF for which the hysteresis cycles were remarkably close to those obtained with the traditional Sawyer-Tower circuit. Values of 80 MV/m and 70 mC/m2 were estimated for the coercive field and remanent polarization, respectively.
Resumo:
The nucleation and growth model, which is usually applied to switching phenomena, is adapted for explaining surface potential measurements on the P(VDF-TrFE) (polyvinylidene fluoride-trifluoroethylene) copolymer obtained in a constant current corona triode. It is shown that the growth is one-dimensional and that the nucleation rate is unimportant, probably because surface potential measurements take much longer than the switching ones. The surface potential data can therefore be accounted for by a growth model in which the velocity of growth varies exponentially with the electric field. Since hysteresis loops can be obtained from surface potential measurements, it is suggested that similar mechanisms can be used when treating switching and hysteresis phenomena, provided that account is taken of the difference in the time scale of the measurements.
Resumo:
Ferroelectric ceramic particles based on lead titanate zirconate (PZT) were dispersed in a polymer matrix based on castor oil. After the poling process, the pyroelectric activity of this composite was measured using a direct method in which a linear heating rate was applied to the pre-poled samples. The pyroelectric coefficient at 343 K is comparable with that of a PZT-poly(vinylidene fluoride) (PVDF) composite and significantly higher than that of PVDF. © 1998 Kluwer Academic Publishers.
Resumo:
This paper presents an ultrasonic method to measure small concentrations of water in lubricating oil. It uses an ultrasonic measurement cell composed by a piezoceramic emitter (5 and 10 MHz), and a large aperture PVDF receiver that eliminates diffraction effects. The propagation velocity, attenuation coefficient and density of several samples of water-in-oil emulsion were measured. The concentrations of water of the samples were in the range of 0 to 5% in volume, and the results showed that these low concentrations can be discriminated within a resolution of 0.2% in the studied range, using the measurement of the propagation velocity.
Resumo:
The study of the stable and the metastable ferroelectric polarization of poly(vinylidene fluoride), PVDF, was performed using two successive equal sign ramp voltages, mediated by a short-circuit period. Rates from 10 V/s up to 0.7 MV/s were used. Results showed that they follow different formation kinetics; that the stable part decreases for higher ramp voltage rates and its apparent coercive field increases.