234 resultados para FREQUENCY UPCONVERSION
Resumo:
Red, green, and blue emission through frequency upconversion and energy-transfer processes in tellurite glasses doped with Tm3+ and Er3+ excited at 1.064 mum is investigated. The Tm3+/Er3+-codoped samples produced intense upconversion emission signals at around 480, 530, 550 and 660 nm. The 480 nm blue emission was originated from the (1)G(4)-->H-3(6) transition of the Tm3+ ions excited by a multiphoton stepwise phonon-assisted excited-state absorption process. The 5 30, 5 50 nm green and 660 mn red upconversion luminescences were identified as originating from the H-2(11/2), S-4(3/2) --> I-4(15/2) and F-4(9/2) --> I-4(15/2) transitions of the Er3+ ions, respectively, populated via efficient cross-relaxation processes and excited-state absorption. White light generation employing a single infrared excitation source is also examined. (C) 2003 Elsevier B.V. (USA). All rights reserved.
Resumo:
Frequency upconversion luminescence in erbium-doped PbGeO3-PbF2-CdF2-based transparent glass ceramics (TGC) under 980 nm infrared excitation is investigated. Upconversion emission signals around 410, 525, 550, 660, and 850 nm were generated and identified as due to the H-2(9/2) H-2(11/2), S-4(3/2), and F-4(9/2) transitions to the I-4(15/2) ground-state, and S-4(3/2)-I-4(13/2), respectively. The erbium ions excited-state emitting levels were populated via a combination of stepwise ground-state absorption (GSA), excited-state absorption (ESA), and cross-relaxation processes. The results also disclosed that both blue (410 nm) and red (660 nm) upconversion emission signals in the transparent glass ceramic sample presented twice as much intensity as compared to its vitreous counterpart. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Enhanced frequency upconversion (UC) emission was studied in Yb3+/Er3+ co-doped PbO-GeO2 glass containing silver nanoparticles (NPs). Optical excitation was achieved with a laser operating at 980 nm in resonance with the Yb3+ transition F-4(5/2)-> F-4(7/2). The intensity of the whole UC spectrum from 400 to 700 nm was intensified due to the influence of silver NPs. The green and red emissions were enhanced by more than 300%. Emission bands centered at 408 nm and 480 nm were also detected corresponding to the H-2(9/2)-> I-4(15/2) and F-4(7/2)-> I-4(15/2) transitions of Er3+ ion. An intensity enhancement of approximate to 150% due to the NPs was measured. For the first time the influence of silver NPs on the blue emission of Yb3+/Er3+ co-doped PbO-GeO2 glass is reported. The large enhancement in the whole UC spectrum is due to the increased local field in the Er3+ ions locations and the proximity between the luminescence wavelengths and the NPs surface plasmon resonance. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Cooperative energy-transfer upconversion luminescence in Tb 3+/Yb 3+-codoped PbGeO 3-PbF 2-CdF 2 vitroceramic and its precursor glass under resonant and off-resonance infrared excitation, is investigated. Bright UV-visible emission signals around 384, 415, 438 nm, and 473-490, 545, 587, and 623 nm, identified as due to the 5D 3( 5G 6 → 7F J(J=6,5,4) and 5D 4 → 7F J(J=6,5,4,3) transitions, respectively, were readily observed. The results indicate that cooperative energy-transfer between ytterbium and terbium ions followed by excited-state absorption are the dominant upconversion excitation mechanisms herein involved. The comparison of the upconversion process in a vitroceramic sample and its glassy precursor revealed that the former present much higher upconversion efficiency. The dependence of the upconversion emission upon pump power, temperature, and doping content is also examined.
Resumo:
The infrared-to-visible frequency upconversion was investigated in Er 3+-doped Ga10Ge25S65 glass and in the transparent glass-ceramic obtained by heat-treatment of the glass above its glass-transition temperature. Continuous-wave and pulsed lasers operating at 980 nm and 1480 nm were used as excitation sources. The green (2H 11/2 → 4I15/2; 4S3/2 → 4I15/2) and red (4F9/2 → 4I15/2) photoluminescence (PL) signals due to the Er3+ ions were characterized. The PL decay times were influenced by energy transfer among Er3+ ions, by cross-relaxation processes and by energy transfer from the Er3+ ions to the host material. The PL from the Er3+ ions hosted in the crystalline phase was distinguished only when the glass-ceramic was excited by the 1480 nm pulsed laser. The excitation pathways responsible for the green and red PL bands are discussed to explain the differences between the spectra observed under continuous-wave and pulsed excitation. © 2013 American Institute of Physics.
Resumo:
IR-visible upconversion fluorescence spectroscopy and thermal effects in pr(3+)/Yb3+-codoped Ga2O3:La2S3 chalcogenide glasses excited at 1.064 mum is reported. Intense visible upconversion emission in the wavelength region of 480-680 nm peaked around 500, 550, 620 and 660 nm is observed. Upconversion excitation of the Pr3+ excited-state visible emitting levels is achieved by st combination of phonon-assisted absorption, energy-transfer and phonon-assisted excited-state absorption processes. A threefold upconversion emission enhancement induced by thermal effects when the codoped sample was heated in the temperature range of 20-200 degreesC is demonstrated. The thermal-induced enhancement is attributed to a multiphonon-assisted anti-Stokes process which takes place in the excitation of the ytterbium and excited-state absorption of the praseodymium. The thermal effect is modelled by conventional rate equations considering temperature-dependent effective absorption cross-sections for the F-2(7/2)-F-2(5/2) ytterbium transition and (1)G(4)-P-3(0) praseadymium excited-state absorption, and it is shown to agree very well with experimental results. Frequency upconversion in singly Pr3+-doped samples pumped at 836 nm and 1.064 mum in a two-beam configuration is also examined.
Resumo:
In this paper we investigate the energy transfer processes in TM3+/Er3+ doped telluride glass pumped at the commercial diode laser pump wavelength similar to 800 nm. Tailoring the rare-earths content in the glass matrix, seven main energy transfer channels within the doping range considered were identified, A 6-fold enhancement of the Er3+ visible frequency upconversion fluorescence at similar to 660 nm is observed due to the inclusion of Tm3+ ions. This is evidence of the relevant contribution of the route Er-1(I-4(11/2)) + Er-2(I-4(13/2)) -> Er-1(I-4(15/2)) + Er-2(F-4(9/2)) to the process. Energy migration among pumped I-4(9/2) level reducing the efficiency of the upconversion emission rate (H-3(11/2), S-4(3/2), and F-4(9/2)) is observed for Er3+ above 1.5 wt%. The rate equations regarding the observed energy transfer routes are determined and a qualitative analysis of the observed processes is reported. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
The influence of the temperature on the nucleation of silver nanoparticles (NPs) in Tm3+/Yb3+ codoped PbO-GeO2 glasses was studied in this work. The infrared-to-visible frequency upconversion (UC) luminescence of Tm3+ ions was used to probe the NPs nucleation and the results were correlated with the increase of the heat-treatment temperature. Emission spectra in the blue-red region were measured by exciting the samples with a cw 980 nm diode laser in resonance with the Yb3+ transition (F-2(7/2) -> F-2(5/2)). The results were correlated with transmission electron microscopy measurements and revealed the different behavior of the nucleation process as a function of temperature.The enhanced UC emission in the visible region is attributed to the increased local field in the proximity of the silver NPs combined with the Yb3+ -> Tm3+ energy transfer. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
The efficiency of energy transfer (ET) between Pr3+ ions in a fluoroindate glass is determined. ET rates, WET, were determined for dilute samples and the results show a dependence of WET on the Pr3+ concentration. ET processes which contribute to resonance fluorescence and frequency upconversion emission were studied. The origin of the interaction energy among the Pr3+ ions was determined to be dipole - dipole. © 1998 Elsevier Science B.V. All rights reserved.
Resumo:
We report optical gain at 382 and 414 nm from Nd3+-doped fluroindate glasses after excitation with lasers operating either at 583 or 532 nm. Stimulated emission due to a frequency upconversion process results in increase of the emitted violet and blue light intensity and emission line narrowing. Large optical gain is measured by pump-probe spectroscopy using samples with various Nd3+ concentrations. © 1999 American Institute of Physics.
Resumo:
Optical absorption and fluorescence were investigated in Tm3+ doped fluoroindate glass. The spectroscopic parameters for transitions in the 4f11 configuration were determined. The fluorescence study revealed the origin of the frequency upconversion process as well as allowed to quantify the interaction between Tm3+ ions.
Resumo:
Fabrication and optical characterization of Tm3+/Yb3+ codoped PbO-GeO2 (PGO) pedestal-type waveguides are investigated in this work. It is important to mention that, to the best of authors' knowledge, the use of PGO pedestal-type waveguide has not been studied before. PGO thin films codoped with Tm3+ and Yb3+ were obtained through RF magnetron sputtering technique. The pedestal profile was obtained using conventional optical lithography procedures, followed by plasma etching and sputtering deposition. The profile of Tm3+/Yb3+ codoped PGO waveguides was observed by means of Scanning Electron Microscopy (SEM) measurements. Also the infrared and infrared-to-visible frequency upconversion luminescences of Tm3+ ions were measured exciting the samples with a cw 980 nm diode laser. Propagation losses around 11 dB/cm and 9 dB/cm were obtained at 630 and 1050 nm, respectively, for waveguides in the 20-100 μm width range. Single-mode propagation was observed for waveguides width up to 12 μm and 7 μm, at 1050 nm and 630 nm, respectively; larger waveguides width provided multi-mode propagation. The present results corroborate the possibility of using Tm3+/Yb3+ codoped PGO thin films as active waveguide for photonic applications. © 2013 Elsevier B.V. All rights reserved.