Objectives: This study aimed to assess dimensional changes in acrylic resin base and artificial teeth position after water storage and thermocycling using computer graphics measurements. Methods: Twenty-four waxed replicas were obtained from a previous upper complete denture. For linear measurements, points in cusps tips of left central incisor and second premolars and molars were marked in one of the prostheses with graphite and transferred to the others using an acrylic resin guide. The prostheses were scanned after waxing, polymerization and treatments and the images were exported to “AutoCad 2002 Today®” software for measurements. Results: There was no statistically significant difference in changes of each segment for each group and between the phases evaluated after polymerization and thermocycling. In groups I and III, the values after polymerization are higher than those after treatment, which suggests shrinkage while the prostheses in group II have expanded. Conclusion: The three groups exhibited artificial teeth movement after tests in comparison to the polymerized prosthesis. The prostheses submitted to water storage in kiln at 36ºC during seven days showed different behavior than the other groups.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Purpose: In order to assist in the selection of artificial teeth for complete dentures, this study aimed to assess the relationship between horizontal and vertical measurements of the face and the morphology of the maxillary central incisor. Materials and Methods: This was a study of 50 plaster casts and 100 teleradiographs - 50 in lateral norm and 50 in frontal norm, belonging to 50 individuals, Caucasian, with a naturally optimal occlusion, matching at least four of the six keys of Andrews. Images of the upper central incisors were obtained by scanning the plaster casts (three-dimensional) and subjectively classified by three examiners as oval, triangular or quadrangular. Facial measures (vertical and horizontal) were defined by means of teleradiographs. In order to check inter-examiner agreement on the classification of central incisor, the Kappa test was used. To verify whether data had normal distribution, the Kolmogorov-Smirnov test was used ( P > 0.2) was used. One-way analysis of variance was employed to assess the association between variables (P > 0.05). Results: When vertical measurements were compared with the three incisor shapes, there was no statistically significant difference (P > 0.05): Triangular (0.54), oval (0.63) and quadrangular (0.51). Similarly, no difference (P > 0.05) was found for facial width (139.08, 143.37, 141.65), maxillary width (76.68, 78.99, 76.91) and mandibular width (103.47, 105.50, 103.11). Conclusions: The majority of cases showed that horizontal and vertical measurements of the face cannot be used as a reference for determining the morphology of the maxillary central incisor crown. It is relevant to analyze and compare other morphological structures to improve the oral health-related quality of life for the conventional denture wearer.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Purpose: This study aimed to evaluate the effect of different storage periods in artificial saliva and thermal cycling on Knoop hardness of 8 commercial brands of resin denture teeth. Methods: Eigth different brands of resin denture teeth were evaluated (Artplus group, Biolux group, Biotone IPN group, Myerson group, SR Orthosit group, Trilux group, Trubyte Biotone group, and Vipi Dent Plus group). Twenty-four teeth of each brand had their occlusal surfaces ground flat and were embedded in autopolymerized acrylic resin. After polishing, the teeth were submitted to different conditions: (1) immersion in distilled water at 37 ± 2 °C for 48 ± 2. h (control); (2) storage in artificial saliva at 37 ± 2 °C for 15, 30 and 60 days, and (3) thermal cycling between 5 and 55 °C with 30-s dwell times for 5000 cycles. Knoop hardness test was performed after each condition. Data were analyzed with two-way ANOVA and Tukey's test (α= .05). Results: In general, SR Orthosit group presented the highest statistically significant Knoop hardness value while Myerson group exhibited the smallest statistically significant mean (P< .05) in the control period, after thermal cycling, and after all storage periods. The Knoop hardness means obtained before thermal cycling procedure (20.34 ± 4.45 KHN) were statistically higher than those reached after thermal cycling (19.77 ± 4.13 KHN). All brands of resin denture teeth were significantly softened after storage period in artificial saliva. Conclusion: Storage in saliva and thermal cycling significantly reduced the Knoop hardness of the resin denture teeth. SR Orthosit denture teeth showed the highest Knoop hardness values regardless the condition tested. © 2010 Japan Prosthodontic Society.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Statement of problem. To select the width of denture teeth, the distance between the marks indicating the location of the canines is usually measured around the curvature of the wax occlusal rim; however, most manufacturers' mold charts provide the measurements of the artificial 6 anterior teeth as if they were on a straight line.Purpose. The purpose of this study was to investigate whether the curve distance between the distal surfaces of the maxillary canines can be related to the combined width (straight measurement) of the 6 anterior teeth in 4 ethnic groups.Material and methods. Maxillary stone casts were obtained for 160 dentate subjects of 4 ethnic groups (40 whites, 40 blacks, 40 multiracial - descendants of white and black parents, and 40 Asians). The width of each maxillary anterior tooth was measured on the casts with sliding calipers. The combined width of the 6 anterior teeth (CW) corresponded to the sum of the width of each anterior tooth. The curve distance between the distal surfaces of the canines (CD) was measured by using dental tape and sliding calipers. The Pearson correlation coefficient and regression analysis were used to evaluate the relationship between CD and CW in each ethnic group (alpha=.05).Results. The mean CD and CW values (in mm) obtained were: whites (CD=52.12; CW=45.65); blacks (CD=56.10; CW=48.13); multiracial (CD=53.58; CW=46.54); and Asians (CD=53.29; CW=46.60). Significant (P<.001) correlations between CD and CW measurements were observed for all ethnic groups studied (whites, r=0.957; blacks, r=0.803; multiracial, r=0.917; and Asians, r=0.881). The following linear regression equations were obtained: whites [CD=1.1(CW)+0.3]; blacks [CD=0.95(CW)+9.3]; multiracial [CD=1.2(CW)-1.1]; and Asians [CD=1.0(CW)+5].Conclusions. The curve distance between the distal surfaces of the maxillary canines can be accurately related to the combined width of the 6 anterior teeth in the selection of denture teeth for the studied ethnic groups. (J Prosthet Dent 2012;107:400-404)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study evaluated the fracture resistance of teeth submitted to internal bleaching and restored with different non-metallic post. Eighty mandibular incisors were endodontically treated and randomly divided in 10 groups (n = 8): G1- restored with composite resin (CR), G2- CR + fiber-reinforced composite post (FRC, Everstick post, Sticktech) cemented with resin cement self-etch adhesive (RCS, Panavia F 2.0, Kuraray), G3- CR + FRC + self-adhesive resin cement (SRC, Breeze, Pentral Clinical), G4- CR+ glass fiber post (GF, Exacto Post, Angelus) + RCS, G5- CR + GF + SRC. The G6 to G10 were bleached with hydrogen peroxide (HP) and restored with the same restorative procedures used for G1 to G5, respectively. After 7 days storage in artificial saliva, the specimens were submitted to the compressive strength test (N) at 0.5 mm/min cross-head speed and the failure pattern was identified as either reparable (failure showed until 2 mm below the cement-enamel junction) or irreparable (the failure showed <2 mm or more below the cement-enamel). Data were analyzed by ANOVA and Tukey test (α = 0.05). No significant difference (p < 0.05) was found among G1 to G10. The results suggest that intracoronal bleaching did not significantly weaken the teeth and the failure patterns were predominately reparable for all groups. The non-metallic posts in these teeth did not improve fracture resistance.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Purpose: This investigation studied the effects of 3 surface treatments on the shear bond strength of a light-activated composite resin bonded to acrylic resin denture teeth. Materials and Methods: The occlusal surfaces of 30 acrylic resin denture teeth were ground flat with up to 400-grit silicon carbide paper. Three different surface treatments were evaluated: (1) the flat ground surfaces were primed with methyl methacrylate (MMA) monomer for 180 seconds; (2) light-cured adhesive resin was applied and light polymerized according to the manufacturer's instructions; and (3) treatment 1 followed by treatment 2. The composite resin was packed on the prepared surfaces using a split mold. The interface between tooth and composite was loaded at a cross-head speed of 0.5 mm/min until failure. Results: Analysis of variance indicated significant differences between the surface treatments. Results of mean comparisons using Tukey's test showed that significantly higher shear bond strengths were developed by bonding composite resin to the surfaces that were previously treated with MMA and then with the bonding agent when compared to the other treatments. Conclusion: Combined surface treatment of MMA monomer followed by application of light-cured adhesive resin provided the highest shear bond strength between composite resin and acrylic resin denture teeth.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study aimed to evaluate the durability of adhesion between acrylic teeth and denture base acrylic resin. The base surfaces of 24 acrylic teeth were flatted and submitted to 4 surface treatment methods: SM1 (control): No SM; SM2: application of a methyl methacrylate-based bonding agent (Vitacol); SM3: air abrasion with 30-μm silicone oxide plus silane; SM4: SM3 plus SM2. A heat-polymerized acrylic resin was applied to the teeth. Thereafter, bar specimens were produced for the microtensile test at dry and thermocyled conditions (60 days water storage followed by 12,000 cycles). The results showed that bond strength was significantly affected by the SM (P < .0001) (SM4 = SM2 > SM3 > SM1) and storage regimens (P < .0001) (dry > thermocycled). The methyl methacrylate-based adhesive showed the highest bond strength.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The aim of this study was to investigate whether the artificial aging by thermal cycling had influenced the marginal adaptation of class V restorations with/without chlorhexidine application in the bond process. Twelve intact human third molars were used. Class V cavity preparations were performed on the buccal surface and the teeth received 35% phosphoric acid-etching procedure (Ultradent Products Inc., South Jordan, Utah, USA). Subsequently, the samples were divided in two groups: Untreated acid-etched dentin and chlorhexidine application as an adjunct in the bond process. The adhesive Single Bond 2 (3M ESPE, St. Paul, MN, USA) was used after 2% chlorhexidine application, and the restorations were performed with FiltekTM Z350 XT (3M ESPE) composite resin. The specimens were submitted to artificial aging by thermal cycling with 3,000 cycles. Analyzes were performed on scanning electron microscopy using replicas of marginal adaptation in percentage of continuous margin before and after the artificial aging. The data were analyzed by paired test and the results showed statistically significant differences in the percentage of continuous margin with/without chlorhexidine treatment before and after thermal cycling. This study concluded that the artificial aging by thermal cycling influenced the marginal adaptation of mixed class V composite restorations.