523 resultados para Acrylic resin denture teeth
Resumo:
Objectives: The purpose of this study was to investigate the effect of thermal cycling and disinfection on the colour change of denture base acrylic resin. Materials and Methods: Four different brands of acrylic resins were evaluated (Onda Cryl, QC 20, Classico and Lucitone). All brands were divided into four groups (n=7) determined according to the disinfection procedure (microwave, Efferdent, 4% chlorhexidine or 1% hypochlorite). The treatments were conducted three times a week for 60days. All specimens were thermal cycled between 5 and 55°C with 30-s dwell times for 1000 cycles before and after disinfection. The specimens' colour was measured with a spectrophotometer using the CIE L*a*b* system. The evaluations were conducted at baseline (B), after first thermal cycling (T 1), after disinfection (D) and after second thermal cycling (T 2). Colour differences (ΔE) were calculated between T 1 and B (T 1B), D and B (DB), and T 2 and B (T 2B) time-points. Results: The samples submitted to disinfection by microwave and Efferdent exhibited the highest values of colour change. There were significant differences on colour change between the time-points, except for the Lucitone acrylic resin. Conclusions: The thermal cycling and disinfection procedures significantly affected the colour stability of the samples. However, all values obtained for the acrylic resins are within acceptable clinical parameters. © 2012 The Gerodontology Society and John Wiley & Sons A/S.
Resumo:
The aim of this study was to evaluate the hardness, roughness and mass loss of an acrylic denture base resin after in vitro exposure to four disinfectant solutions. Forty specimens (Clássico, Brazil) were prepared and randomly assigned to 4 groups n = 10) according to the disinfectant solution: G1: control, stored in distilled water at 37 degrees C; G2: 1% sodium hypochlorite; G3: 2% glutaraldehyde; G4: 4% chlorhexidine. G2 to G4 were immersed for 60 minutes in the disinfectant solution. Measurements were carried out both before and after immersion in the solution. The surface was analyzed with a surface roughness tester (Surfcorder SE 1700 KOZAKALAB), a microdurometer FM-700 (Future Tech) and a scanning electron microscope (DSM 962-ZEISS). Loss of mass was determined with a digital weighing scale. After disinfection procedures, values were analyzed statistically. The acrylic denture base resin may be vulnerable to surface changes after in vitro immersion in the disinfectant solutions studied.
Resumo:
Objective: This study investigated the effect of experimental photopolymerized coatings, containing zwitterionic or hydrophilic monomers, on the hydrophobicity of a denture base acrylic resin and on Candida albicans adhesion. Methods: Acrylic specimens were prepared with rough and smooth surfaces and were either left untreated (control) or coated with one of the following experimental coatings: 2-hydroxyethyl methacrylate (HE); 3-hydroxypropyl methacrylate (HP); and 2-trimethylammonium ethyl methacrylate chloride (T); and sulfobetaine methacrylate (S). The concentrations of these constituent monomers were 25%, 30% or 35%. Half of the specimens in each group (control and experimentals) were coated with saliva and the other half remained uncoated. The surface free energy of all specimens was measured, regardless of the experimental condition. C. albicans adhesion was evaluated for all specimens, both saliva conditioned and unconditioned. The adhesion test was performed by incubating specimens in C. albicans suspensions (1 × 10 7 cell/mL) at 37 °C for 90 min. The number of adhered yeasts were evaluated by XTT (2,3-bis[2-methoxy-4-nitro-5-sulfophenyl]-5-[{phenylamino} carbonyl]-2H-tetrazolium-hydroxide) method. Results: For rough surfaces, coatings S (30 or 35%) and HP (30%) resulted in lower absorbance values compared to control. These coatings exhibited more hydrophilic surfaces than the control group. Roughness increased the adhesion only in the control group, and saliva did not influence the adhesion. The photoelectron spectroscopy analysis (XPS) confirmed the chemical changes of the experimental specimens, particularly for HP and S coatings. Conclusions: S and HP coatings reduced significantly the adhesion of C. albicans to the acrylic resin and could be considered as a potential preventive treatment for denture stomatitis. © 2012 Elsevier Ltd.
Resumo:
This study evaluated the potential of plasma treatments to modify the surface chemistry and hydrophobicity of a denture base acrylic resin to reduce the Candida glabrata adhesion. Specimens (n=54) with smooth surfaces were made and divided into three groups (n=18): control - non-treated; experimental groups - submitted to plasma treatment (Ar/50W; AAt/130W). The effects of these treatments on chemical composition and surface topography of the acrylic resin were evaluated. Surface free energy measurements (SFE) were performed after the treatments and after 48h of immersion in water. For each group, half (n=9) of the specimens were preconditionated with saliva before the adhesion assay. The number of adhered C. glabrata was evaluated by cell counting after crystal violet staining. The Ar/50W and AAt/130W treatments altered the chemistry composition, hydrophobicity and topography of acrylic surface. The Ar/50W group showed significantly lower C. glabrata adherence than the control group, in the absence of saliva. After preconditioning with saliva, C. glabrata adherence in experimental and control groups did not differ significantly. There were significant changes in the SFE after immersion in water. The results demonstrated that Ar/50W treated surfaces have potential for reducing C. glabrata adhesion to denture base resins and deserve further investigation, especially to tailor the parameters to prolong the increased wettability. © 2012 Blackwell Verlag GmbH.
Resumo:
Purpose: The objectives of this study were to investigate the flexural strength (FS) and chemical interaction between 2-tert-butylaminoethyl methacrylate (TBAEMA) and a denture base acrylic resin. Materials and Methods: Specimens were divided into five groups according to the concentration of TBAEMA incorporated in acrylic resin Onda-Cryl (0%, 1%, 2%, 3%, 4%) and were submitted to Fourier transform infrared spectroscopy (FTIR), electron spectroscopy for chemical analysis (XPS-ESCA), and differential scanning calorimetry (DSC) analyses. FS of the specimens was tested, and results were analyzed by ANOVA/Tukey's test (α < 0.05). Results: Different nitrogen ratios were observed on specimens' surfaces: 0.36%, 0.54%, 0.35%, and 0.20% for groups 1%, 2%, 3%, and 4%, respectively. FTIR indicated copolymerization of acrylic resin and TBAEMA, and DSC results demonstrated a decrease in glass transition temperature (Tg). Significant differences were found for FS (p < 0.05). The mean values were 91.1 ± 5.5,A 77.0 ± 13.1,B 67.2 ± 12.5,B 64.4 ± 13.0,B and 67.2 ± 5.9B MPa for groups 0%, 1%, 2%, 3% and 4%, respectively (same superscript letters indicate no significant difference). Conclusions: The incorporation of TBAEMA in acrylic resin resulted in copolymerization and the presence of amine groups on specimens' surfaces, and in decreases of Tg and FS. © 2012 by the American College of Prosthodontists.
Resumo:
Objective In studies on Candida albicans adhesion to surfaces, diverse protocols have been used for collection and preparation of saliva samples. Thus, this study investigated whether variations in the centrifugation parameters and number of donors of saliva would influence the adhesion of C. albicans to a denture base resin. Methods Resin acrylic samples (n = 72) were made and then divided into four groups: (a) control – specimens were left without preconditioning in saliva; (b) three experimental groups, in which the specimens were preconditioned with saliva collected from 15 volunteers and centrifuged at 12 000 g for 5 min (G1); from 15 volunteers and centrifuged at 18 000 g for 30 min (G2); and from one volunteer and centrifuged at 12 000 g for 5 min (G3). Candida adhesion was evaluated by both the 2,3-bis(2-methoxy-4-nitro-5-sulfophenyl)-5-[(phenylamino) carbonyl]-2H-tetrazolium hydroxide (XTT) reduction method and crystal violet staining. Data were analyzed by one-way analyses of variance (P = 0.05). Results For XTT reduction assay, groups G2, G3, and control were not significantly different, whereas group G1 showed significantly higher absorbance value than control. For crystal violet staining there were no significant differences among all groups. Conclusion Variations in the centrifugation parameters and number of donors of saliva may influence C. albicans adhesion to denture base resins.
Resumo:
Aim The aim of the present study was to evaluate the effect of surface roughness (roughness average [Ra] μm) on the hydrophobicity of a denture-base acrylic resin and the initial adherence and biofilm formation of Candida albicans (C. albicans). Methods Disk-shaped specimens were divided into six groups: Ra 0.05, Ra 0.2, Ra 0.4, Ra 0.8, Ra 1.5, and Ra 3.0. Water contact angles (WCA) were measured, and the specimens incubated with C. albicans for 90 min (initial adherence, n = 108) or 48 h (biofilm formation, n = 108). Adhered and biofilm cells were evaluated by c.f.u./mL and 2,3-bis-(2-methoxy-4-nitro-5-sulfophenyl)-2H-tetrazolium-5-carboxanilide (XTT), and the correlation between the two methods was evaluated. The surface of the specimens and cells (adhered and biofilm) were also analyzed by scanning electron microscopy (SEM). Results Groups Ra 0.05 and 3.0 exhibited the lowest (~75°) and the highest (~100°) WCA mean values, respectively. For both initial adherence and biofilm formation, no statistically-significant differences were observed among all groups, as determined by c.f.u./mL and XTT. A positive correlation between these two methods was found. SEM analysis showed the presence of scratches and valleys on the acrylic specimens and densely-packed yeast cells covering the entire surface. Conclusions Roughness significantly increased hydrophobicity (WCA), but had no effect on the number and metabolic activity of adherent and biofilm cells of C. albicans.
Resumo:
Purpose: To investigate the cumulative effects of brushing (B) or immersion (I), using different cleansing agents, on the surface roughness, hardness and color stability of a heat-polymerized denture resin, Lucitone 550 (L), and a hard chairside reline resin, Tokuyama Rebase Fast II (T). Methods: A total of 316 specimens (10 x 2 mm) were fabricated. The specimens (n= 9) were divided into brushing or immersion groups according to the following agents: dentifrice/distilled water (D), 1% sodium hypochlorite (Na0C1), Corega Tabs (Pb), 1% chlorhexidine gluconate (Chx), and 0.2% peracetic acid (Ac). Brushing and immersion were tested independently. Assays were performed after 1, 3, 21, 45 and 90 blushing cycles or immersion of 10 seconds each. Data were evaluated statistically by repeated measures ANOVA. Tukey's honestly significant difference (HSD) post-hoc test was used to determine differences between means (a= 0.05). Results: For L there was no statistically significant difference in roughness, except a significant decrease in roughness by brushing with D. T showed a significant effect on the roughness after 90 immersions with Ac. Hardness values decreased for L when specimens were immersed or brushed in Na0C1 and Pb. The hardness of T decreased with increases in the repetitions (immersion or brushing), regardless of the cleaning method. Values of color stability for L resin showed significant color change after brushing with and immersion in Ac and Pb. Brushing with D exhibited a higher incidence of color change. For T there were no significant differences between cleaning agents and repetitions in immersion. A color change was noted after three brushings with the Ac, Chx, and D. Brushing with dentifrice decreased roughness of L. Immersion in or brushing with Na0C1 and Pb decreased the hardness of L. For T, hardness decreased with increases in immersions or brushing. Color changes after the immersion in or brushing with cleaning agents were clinically acceptable according to National Bureau of Standards parameters for both resins.
Resumo:
Acrylic resin is a widely used material in clinical practice, and a satisfactory biocompatibility is essential. When the resin polymerization reaction is incomplete, residual monomers are released into the oral cavity. The aim of this study was to evaluate, through a literature review, the cytotoxicity caused by the denture base acrylic resin used, and its components. The selection of published studies was performed on the Pubmed database from January 2008 to July 2013. The keywords used were: cytotoxicity and acrylic resins, cytotoxicity and denture base resins and cytotoxicity and oral prosthesis. Inclusion criteria were: in vitro studies and literature reviews published in English that evaluated the acrylic resin cytotoxicity for denture base and its components. Studies with no reference to the search strategy were excluded. A total of 182 articles were found. Among these, only 13 were included for writing this review. The MTT test is the most common test used to evaluate acrylic resin cytotoxicity. Auto-polymerized resin is more cytotoxic than heat-polymerized resin because of its higher quantity of residual monomers which cause cell and tissue changes in the oral mucosa. However, more studies are necessary for the development of biocompatible materials.
Resumo:
Fabrication of an interim prosthesis is an important procedure in oral rehabilitation because it aids in determining the esthetics, phonetics, and occlusal relationship of the definitive restoration. The typical material (acrylic resin) used in interim prostheses commonly fails due to fractures. During extended oral rehabilitation with fixed partial prostheses, high strength interim prostheses are often required to protect hard and soft tissues, avoid dental mobility, and to allow the clinician and patient a chance to evaluate cosmetics and function before the placement of the definitive prosthesis. Furthermore, a satisfactory interim prosthesis can serve as a template for the construction of the definitive prosthesis. The maintenance of this prosthesis is important during treatment for protection of teeth and occlusal stability. Procedures to reinforce interim prostheses help to improve performance and esthetics in long-term treatment. Due to the low durability of acrylic resin in long-term use, the use of reinforcing materials, such as metal castings or spot-welded stainless steel matrix bands, is indicated in cases of extensive restoration and long-term treatment. This paper describes an easy technique for fabricating a fixed interim prosthesis using acrylic resin and a cast metallic reinforcement.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Denture fractures are common in daily practice, causing inconvenience to the patient and to the dentists. Denture repairs should have adequate strength, dimensional stability and color match, and should be easily and quickly performed as well as relatively inexpensive. Objective: The aim of this study was to evaluate the flexural strength of acrylic resin repairs processed by different methods: warm water-bath, microwave energy, and chemical polymerization. Material and methods: Sixty rectangular specimens (31x10x2.5 mm) were made with warm water-bath acrylic resin (Lucitone 550) and grouped (15 specimens per group) according to the resin type used to make repair procedure: 1) specimens of warm water-bath resin (Lucitone 550) without repair (control group); 2) specimens of warm water-bath resin repaired with warm water-bath; 3) specimens of warm water-bath resin repaired with microwave resin (Acron MC); 4) specimens of warm water-bath resin repaired with autopolymerized acrylic resin (Simplex). Flexural strength was measured with the three-point bending in a universal testing machine (MTS 810 Material Test System) with load cell of 100 kgf under constant speed of 5 mm/min. Data were analyzed statistically by Kruskal-Wallis test (p<0.05). Results: The control group showed the best result (156.04 +/- 1.82 MPa). Significant differences were found among repaired specimens and the results were decreasing as follows: group 3 (43.02 +/- 2.25 MPa), group 2 (36.21 +/- 1.20 MPa) and group 4 (6.74 +/- 0.85 MPa). Conclusion: All repaired specimens demonstrated lower flexural strength than the control group. Repairs with autopolymerized acrylic resin showed the lowest flexural strength.
Resumo:
The selection and use of hard chairside reline resins must be made with regard to dimensional stability, which will influence the accuracy of fit of the denture base. This study compared the dimensional change of two hard chairside reline resins (Duraliner II and Kooliner) and one heat-curing denture base resin (Lucitone 550). A stainless steel mold with reference dimensions (AB, CD) was used to obtain the samples. The materials were processed according to the manufacturer's recommendations. Measurements of the dimensions were made after processing and after the samples had been stored in distilled water at 37° C for eight different periods of time. The data were recorded and then analyzed with analysis of variance. All materials showed shrinkage immediately after processing (p < 0.05). The only resin that exhibited shrinkage after 60 days of storage in water was Duraliner II; these changes could be clinically significant in regard of tissue fit.
Resumo:
STATEMENT OF PROBLEM: Because water sorption of autopolymerizing acrylic reline resins is accompanied by volumetric change, it is a physical property of importance. As residual monomer leaches into the oral fluids and causes tissue irritation, low solubility of these resins is desired. Another requirement is a satisfactory bond between the autopolymerizing acrylic resins and the denture base acrylic resin. PURPOSE: This study compared the water sorption, solubility, and the transverse bond strength of 2 autopolymerizing acrylic resins (Duraliner II and Kooliner) and 1 heat-polymerizing acrylic resin (Lucitone 550). MATERIAL AND METHODS: The water sorption and solubility test was performed as per International Standards Organization Specification No. 1567 for denture base polymers. Bond strengths between the autopolymerizing acrylic resins and the heat-polymerizing acrylic resin were determine with a 3-point loading test made on specimens immersed in distilled water at 37 degrees C for 50 hours and for 30 days. Visual inspection determined whether failures were adhesive or cohesive. RESULTS: Duraliner II acrylic resin showed significantly lower water sorption than Kooliner and Lucitone 550 acrylic resins. No difference was noted in the solubility of all materials. Kooliner acrylic resin demonstrated significantly lower transverse bond strength to denture base acrylic resin and failed adhesively. The failures seen with Duraliner II acrylic resin were primarily cohesive in nature. CONCLUSIONS: Autopolymerizing acrylic reline resins met water sorption and solubility requirements. However, Kooliner acrylic resin demonstrated significantly lower bond strength to denture base acrylic resin.