581 resultados para Moist dentin


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Odontomas are developmental disturbances which manifest in the form of denticles or amorphous informes masses comprising all dental tissues, especially enamel and dentin, with variable amounts of pulp and cement. We describe here two clinical cases of odontomas in children, focusing on diagnostic means and the importance of early treatment of these lesions. The standard treatment for the two present cases was surgical removal.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Purpose: To evaluate the pullout strength of a glass fiber-reinforced composite post (glass FRC) cemented with three different adhesive systems and one resin cement. The null hypothesis was that pullout strengths yielded by the adhesive systems are similar. Materials and Methods: Thirty bovine teeth were selected. The size of the specimens was standardized at 16 mm by sectioning off the coronal portion and part of the root. The specimens were divided into three groups, according to the adhesive system, which were applied following the manufacturers' instructions: G1, ScotchBond Multi-Purpose Plus; G2, Single Bond; G3, Tyrian SPE/One-Step Plus. The glass FRCs (Reforpost) were etched with 37% H3PO4 for 1 min and silanized (Porcelain Primer). Thereafter, they were cemented with the dual resin cement En-Force. The specimens were stored for 24 h, attached to an adapted device, and submitted to the pullout test in a universal testing machine (1 mm/min). The data were submitted to the one-way ANOVA and Tukey's test (α = 0.05). Results: G1 (30.2 ± 5.8 Kgf) displayed the highest pullout strength (p < 0.001) when compared to G2 (18.6 ± 5.8 Kgf) and G3 (14.3 ± 5.8 Kgf), which were statistically similar. Analysis of the specimens revealed that all failures occurred between the adhesive system and the root dentin (pullout of the post cement), regardless of group. Conclusion: The multiple-bottle, total-etch adhesive system provided higher pullout strength of the glass FRC when compared to the single-bottle, total-etch, and single-step self-etching adhesive systems. The null hypothesis was rejected (p < 0.001).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this study was to determine the cutting ability of chemical vapor deposition (CVD) diamond burs coupled to an ultrasonic dental unit handpiece for minimally invasive cavity preparation. One standard cavity was prepared on the mesial and distal surfaces of 40 extracted human third molars either with cylindrical or with spherical CVD burs. The cutting ability was compared regarding type of substrate (enamel and dentin) and direction of handpiece motion. The morphological characteristics, width and depth of the cavities were analyzed and measured using scanning electron micrographs. Statistical analysis using the Kruskal-Wallis test (p < 0.05) revealed that the width and depth of the cavities were significantly greater when they were prepared on dentin. Wider cavities were prepared when the cylindrical CVD bur was used, and deeper cavities resulted from preparation with the spherical CVD bur. The direction of handpiece motion did not influence the size of the cavities, and the CVD burs produced precise and conservative cutting.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Background: Excisional biopsies of gingival overgrowths, performed with safety margins, frequently result in mucogingival defects. These defects may produce esthetic problems and increase the chances of dentin hyperesthesia and its possibility of hindering oral hygiene. Methods: Two clinical cases are reported in which gingival overgrowths were removed by excisional biopsy, resulting in unsightly defects. The first clinical case presents an invasive approach for the treatment of a recurrent pyogenic granuloma in the anterior maxilla, and the second depicts a complete removal of a peripheral odontogenic fibroma in the posterior maxilla. In both situations, the soft-tissue defects were repaired by periodontal plastic surgery, including a laterally positioned flap and a coronally positioned flap, respectively. Results: Periodontal plastic surgery successfully restored the defects that resulted from biopsies, and no recurrence has been noticed in the 5-year postoperative follow-up period. Conclusions: The combination of biopsy and periodontal plastic surgery in a one-step procedure seems to be suitable to remove gingival overgrowths in most areas of the mouth, regardless of esthetic significance. Such procedures seem to restore gingival health, encourage healing, and create both esthetics and function in the excised area.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this study was to evaluate the effects of dentin surface treatments on the tensile bond strength (TBS) of the self-etching primer Clearfil SE Bond (CSE) and the one-step self-etching One-Up Bond F (OUB). The exposed flat dentin surfaces of twenty-four sound third molars were prepared with diamond bur at high-speed, carbide bur at low-speed or wet ground with #600 grit SiC paper. The adhesive systems were applied to the dentin surfaces and light-cured according to the manufacturers' instructions. A 6-mm high composite crown was incrementally built-up and each increment was light-cured for 40 seconds. After being stored in water (37°C/24 h), the samples were serially sectioned parallel to the long axis, forming beams (n = 20) with a cross-sectional area of approximately 0.8 mm 2. The specimens were tested in a Universal Testing Machine at 0.5 mm/min. The cross-sectional area was measured and the results (MPa) were analyzed by two-way ANOVA and Tukey Test (p < 0.05). Overall, the groups treated with CSE exhibited the highest TBS for all surface treatments. Dentin surfaces prepared with carbide bur at low speed reduced TBS in the CSE group; however, OUB was not affected by surface treatments. The effect of surface abrasive methods on TBS was material-dependent.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Pulp capping is a procedure that comprises adequate protection of the pulp tissue exposed to the oral environment, aiming at the preservation of its vitality and functions. This study evaluated the response of the dental pulps of dog teeth to capping with mineral trioxide aggregate (MTA) or calcium hydroxide P.A. For that purpose, 37 teeth were divided into two groups, according to the capping material employed. Two dogs were anesthetized and, after placement of a rubber dam, their pulps were exposed in a standardized manner and protected with the experimental capping materials. The cavities were then sealed with resin-modified glass ionomer cement and restored with composite resin. After sixty days, the animals were killed and the specimens were processed in order to be analyzed with optic microscopy. It was observed that MTA presented a higher success rate compared to calcium hydroxide, presenting a lower occurrence of infection and pulp necrosis.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The radiopacity of esthetic restorative materials has been established as an important requirement, improving the radiographic diagnosis. The aim of this study was to evaluate the radiopacity of six restorative materials using a direct digital image system, comparing them to the dental tissues (enamel-dentin), expressed as equivalent thickness of aluminum (millimeters of aluminum). Five specimens of each material were made. Three 2-mm thick longitudinal sections were cut from an intact extracted permanent molar tooth (including enamel and dentin). An aluminum step wedge with 9 steps was used. The samples of different materials were placed on a phosphor plate together with a tooth section, aluminum step wedge and metal code letter, and were exposed using a dental x-ray unit. Five measurements of radiographic density were obtained from each image of each item assessed (restorative material, enamel, dentin, each step of the aluminum step wedge) and the mean of these values was calculated. Radiopacity values were subsequently calculated as equivalents of aluminum thickness. Analysis of variance (ANOVA) indicated significant differences in radiopacity values among the materials (P<0.0001). The radiopacity values of the restorative materials evaluated were, in decreasing order: TPH, F2000, Synergy, Prisma Flow, Degufill, Luxat. Only Luxat had significantly lower radiopacity values than dentin. One material (Degufill) had similar radiopacity values to enamel and four (TPH, F2000, Synergy and Prisma Flow) had significantly higher radiopacity values than enamel. In conclusion, to assess the adequacy of posterior composite restorations it is important that the restorative material to be used has enough radiopacity, in order to be easily distinguished from the tooth structure in the radiographic image. Knowledge on the radiopacity of different materials helps professionals to select the most suitable material, along with other properties such as biocompatibility, adhesion and esthetic.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Objective: The aim of this in vitro study was to evaluate the cytotoxicity of resin-modified glass-ionomer lining cements submitted to different curing regimes and applied to an immortalized odontoblast-cell line (MDPC-23). Methods: Forty round-shaped specimens of each experimental material (Fuji Lining LC and Vitrebond) were prepared. They were light-cured for the manufacturers' recommended time (MRT = 30 s), under-cured (0.5 MRT = 15 s), over-cured (1.5 MRT = 45 s) or allowed to dark cure (0 MRT). Sterilized filter papers soaked with either 5 μL of PBS or HEMA were used as negative and positive control, respectively. After placing the specimens individually in wells of 24-well dishes, odontoblast-like cells MDPC-23 (30,000 cells/cm2) were plated in each well and incubated for 72 h in a humidified incubator at 37 °C with 5% CO2 and 95% air. The cytotoxicity was evaluated by the cell metabolism (MTT assay) and cell morphology (SEM). Results: Fuji Lining LC was less cytotoxic than Vitrebond (p < 0.05) in all the experimental conditions. However, the cytotoxicity of Fuji Lining LC was noticeably increased in the absence of light-curing while the same was not observed for Vitrebond. The length of light-curing (15, 30 or 45 s) did not influence the toxicity of both lining materials when they were applied on the odontoblast-cell line MDPC-23. Significance: The light-activation plays an important role in reducing the cytotoxicity of Fuji Lining LC. Following the manufacturer' recommendation regarding the light-curing regime may prevent toxic effect to the pulp cells. © 2005 Academy of Dental Materials.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Several pathologies have been diagnosed in children of hypertensive mothers; however, some studies that evaluated the alterations in their oral health are not conclusive. This study analyzed the salivary gland activity and dental mineralization of offsprings of spontaneously hypertensive rats (SHR). Thirty-day-old SHR males and Wistar rats were studied. The salivary flow was evaluated by injection of pilocarpine, the protein concentration and salivary amylase activity, by the Lowry method and kinetic method at 405 nm, respectively. Enamel and dentin mineralization of the mandibular incisors was quantified with aid of the microhardness meter. The results were analyzed by the ANOVA or Student's t test (p<0.05). It was noticed that the salivary flow rate (0.026 mL/min/100 g±0.002) and salivary protein concentration (2.26mg/mL±0.14) of SHR offspring were reduced compared to Wistar normotensive offspring (0.036 mL/min/100 g±0.003 and 2.91 mg/mL±0.27, respectively), yet there was no alteration in amylase activity (SHR: 242.4 U/mL±36.9; Wistar: 163.8 U/mL±14.1). Microhardness was lower both in enamel (255.8 KHN±2.6) and dentin (59.9 KHN±0.8) for the SHR teeth compared to the Wistar teeth (enamel: 328.7 KHN±3.3 and dentin: 67.1 KHN±1.0). These results suggest that the SHR offspring are more susceptible to development of pathologies impairing oral health, once they presented lesser flow and salivary protein concentration and lower dental mineralization.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this study was to examine the endothelial surface and to perform a morphometric analysis of the corneal endothelial cells in normal eyes of dogs using specular microscopy. Morphometric analysis with regard mean cell area and cell density was performed. Both eyes of ten mixed-breed, males and females, with 6 years of age, weighing about 15 kg euthanatized for reasons unrelated to this study were evaluated. Eyes were examined to determine that they did not have visible ocular disease and transported to the laboratory in moist chamber. Using a contact specular microscope the corneal endothelium was examined. Three images of the central corneal endothelium of each eye were obtained. The mean cell area and the cell density of the corneal endothelial cells were obtained using software for corneal endothelium analysis and density measurement. The mean cell area was 395 ± 36 μm 2 and the endothelial cell density was 2555 ± 240 cells/mm2. The present work demonstrates that the normal corneal endothelium of dog is similar to those described in human.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The purpose of this study was to evaluate in vitro three adhesive systems: a total etching single-component system (G1 Prime & Bond 2.1), a self-etching primer (G2 Clearfil SE Bond), and a self-etching adhesive (G3 One Up Bond F), through shear bond strength to enamel of human teeth, evaluating the type of fracture through stereomicroscopy, following the ISO guidance on adhesive testing. Thirty sound premolars were bisected mesiodistally and the buccal and lingual surfaces were embedded in acrylic resin, polished up to 600-grit sandpapers, and randomly assigned to three experimental groups (n = 20). Composite resin cylinders were added to the tested surfaces. The specimens were kept in distilled water (37°C/24 h), thermocycled for 500 cycles (5°C-55°C) and submitted to shear testing at a crosshead speed of 0.5 mm/min. The type of fracture was analyzed under stereomicroscopy and the data were submitted to Anova, Tukey and Chi-squared (5%) statistical analyses. The mean adhesive strengths were G1: 18.13 ± 6.49 MPa, (55% of resin cohesive fractures); G2: 17.12 ± 5.80 MPa (90% of adhesive fractures); and G3: 10.47 ± 3.14 MPa (85% of adhesive fractures). In terms of bond strength, there were no significant differences between G1 and G2, and G3 was significantly different from the other groups. G1 presented a different type of fracture from that of G2 and G3. In conclusion, although the total etching and self-etching systems presented similar shear bond strength values, the types of fracture presented by them were different, which can have clinical implications.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The use of acid etchants to produce surface demineralization and collagen network exposure, allowing adhesive monomers interdiffusion and consequently the formation of a hybrid layer, has been considered the most efficient mechanism of dentin bonding. The aim of this study was to compare the tensile bond strength to dentin of three adhesive systems, two self-etching ones (Clearfil SE Bond - CSEB and One Up Bond F - OUBF) and one total-etching one (Single Bond - SB), under three dentinal substrate conditions (wet, dry and re-wet). Ninety human, freshly extracted third molars were sectioned at the occlusal surface to remove enamel and to form a flat dentin wall. The specimens were restored with composite resin (Filtek Z250) and submitted to tensile bond strength testing (TBS) in an MTS 810. The data were submitted to two-way ANOVA and Tukey's test (p = 0.05). Wet dentin presented the highest TBS values for SB and CSEB. Dry dentin and re-wet produced significantly lower TBS values when using SB. OUBF was not affected by the different conditions of the dentin substrate, producing similar TBS values regardless of the surface pretreatments.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Background: Since only a few data have been published concerning the effects of resinous dental materials on the pulp-dentin complex, the aim of this study was to evaluate the biocompatibility of resin-based materials applied as liners in deep cavities prepared in duman teeth. Methods: After preparing class V cavities, the following dental materials were applied on the axial walls: group 1, Vitrebond™ (VIT; 3M ESPE); group 2, Ultra-Blend® Plus™ (UBP; Untradent); and group 3, Clearfil™ SE Bond (CSEB; Kuraray). In group 4 (control), the hard-setting calcium hydroxide cement Dycal (CH; Caulk/Dentsply) was used. The teeth extracted at 7 days or between 30 and 85 days after the clinical procedures were processed for histological evaluation. Results: For all the experimental and control groups, most of specimens exhibited no pulpal response or slight inflammatory reaction associated with slight tissue disorganization at 7-day period. Moderate inflammatory pulpal response occurred only in one tooth (RDT = 262 μm) of group 3 in which transdentinal diffusion of resin components was observed. Conclusion: The resin-based dental cements VIT and UBP as well as the bonding agent CSEB presented acceptable biocompatibility when applied in deep cavities prepared in sound human teeth. © 2006 Wiley Periodicals, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Host-derived proteases have been reported to degrade the collagen matrix of incompletely-resin-infiltrated dentin. This study tested the hypothesis that interfacial degradation of resin-dentin bonds may be prevented or delayed by the application of chlorhexidine (CHX), a matrix metalloproteinase inhibitor, to dentin after phosphoric acid-etching. Contralateral pairs of resin-bonded Class I restorations in non-carious third molars were kept under intra-oral function for 14 months. Preservation of resin-dentin bonds was assessed by microtensile bond strength tests and TEM examination. In vivo bond strength remained stable in the CHX-treated specimens, while bond strength decreased significantly in control teeth. Resin-infiltrated dentin in CHX-treated specimens exhibited normal structural integrity of the collagen network. Conversely, progressive disintegration of the fibrillar network was identified in control specimens. Auto-degradation of collagen matrices can occur in resin-infiltrated dentin, but may be prevented by the application of a synthetic protease inhibitor, such as chlorhexidine.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We describe and begin to evaluate a parameterization to include the vertical transport of hot gases and particles emitted from biomass burning in low resolution atmospheric-chemistry transport models. This sub-grid transport mechanism is simulated by embedding a 1-D cloud-resolving model with appropriate lower boundary conditions in each column of the 3-D host model. Through assimilation of remote sensing fire products, we recognize which columns have fires. Using a land use dataset appropriate fire properties are selected. The host model provides the environmental conditions, allowing the plume rise to be simulated explicitly. The derived height of the plume is then used in the source emission field of the host model to determine the effective injection height, releasing the material emitted during the flaming phase at this height. Model results are compared with CO aircraft profiles from an Amazon basin field campaign and with satellite data, showing the huge impact that this mechanism has on model performance. We also show the relative role of each main vertical transport mechanisms, shallow and deep moist convection and the pyro-convection (dry or moist) induced by vegetation fires, on the distribution of biomass burning CO emissions in the troposphere.