It was evaluated the castability of four copper-aluminium alloy according the melting casting method used. The specimens were made using polyester mesh screen, with 11 x 11 filaments of 0.26 mm thick, fixed along of two adjacent edges in wax bar, with the sprue attached at their junction. The alloys were in an electrical casting machine and a centrifugal casting machine with an air/gas torch. The castability values were obtained by the percentage of completed segments of the resulting cast alloy screen. It was verified that the use of the electrical casting machine produced higher castability values to the copper-aluminium alloys than those produced by a centrifugal casting machine with an air/gas torch.
Resumo:
It was evaluated the Vickers hardness of five high-copper casting alloys, in their original package form and after casting, according to the casting method used. That way, ten ingots, supplied by the manufacturers of each alloy, were included in self-curing acrylic resin, polished, numerated and submitted to Vickers hardness test at load of 200 g during 30 seconds. Afterwards the numerated ingots were removed from the acrylic resin and five of those were cast in an electrical casting machine and the other five in a centrifugal casting machine with an air/gas torch. The specimens obtained were included in self-curing acrylic resin, polished and submitted to Vickers hardness test. As a result it was verified that there is a variation of hardness among the alloys tested, and the use of the electrical casting machine produced lower hardness values than those produced when used the centrifugal casting machine with an air/gas torch. Also, there is a decrease of hardness of the cast alloys when they are tested in their original form and after casting.
Resumo:
The authors analysed the simultaneous effects of the dimensional and weight alteration of resins utilized for esthetic facets submitted to warehousing conditions and periods of time. The resins showed different behaviour and a neat correlation between dimensional alteration and weight. The condition of immersion promoted dimensional alteration 50% lower and an alteration of weight three times higher.
Resumo:
The purpose of this study was to compare the enamel/resin/metal bond tensile strength by using human canines, in which castings were bonded. These castings were obtained by Co-Cr or Ni-Cr alloys and showed four types of mechanisms of retention: 50 micrograms aluminum oxide abrasive, electrochemical etch, acrylic beads metal mesh. The castings were bonded utilizing Comspan Opaque and Panavia Ex. The specimens were subjected to tensile forces after 24 hours in an Instron machine. The castings subjected to 50 micrograms aluminum oxide abrasive and bonded utilizing Panavia EX showed the biggest bond tensile strength.
Resumo:
The authors looked for the verification of the fatigue of retentive clasps utilized on the removable partial denture. According to this, it was idealized and built on assay machine, that through movements, simulate the insertion and removal of the clasp for a pattern tooth, manufactured on cobalt-chromium which has all the preparation normally utilized to the correct confection of this type of prosthesis. It was utilized three different commercial alloys based on cobalt-chromium: L1-Biosil; L2-Steldent; L3-Duracron. It was utilized the T clasp of Roach, with was tested upon three different proportions among width and thickness: E1-1.7;E2-2.0 and E3-2.3 and was casted through two casting techniques: F1-oxygen-gas and F2-oxygen-acetylene. The clasps were tested on the machine, which allowed the reading of the number of insertion and removal cycles made until fatigue appeared. The obtained results were submitted to the statistic analysis and the authors concluded that: a) L3 (Duracrom) obtained the best results followed by L1 (Biosil) and finally L3 (Steldent); b) among the analyzed thickness, the best results were obtained by E3, followed by E2 and after this E1; c) form the casting techniques, F2 gave us the best results.
Resumo:
The authors tested the T clasp of Roach in three differents proportions among width and thickness: E1-1.7; E2-2.0 and E3-2.3, with a constant length of 15 mm. These clasps were casted with three cobalt-chromium alloys (L1-Biosil; L2-Steldent and L3-Duracrom), through two casting techniques (F1-oxygen-gas and F2-oxygen-acetylene). The fatigue of the clasps were verified by using and assay machine, that through movements, simulate the insertion and removal of the clasps for a pattern which were obtained from a premolar, prepared in a surveyor. This machine detect the fatigue of the clasps and count the number of cycles of insertion and removal realized. The obtained results of the interaction between the analysed factors, were submitted to the statistic analysis and the authors concluded that: a) the interaction of factors, Alloy x Thickness, Alloy x Casting Technique and Thickness x Casting Technique did not change the order of effects that the factors showed separately but gave rise to effects of different magnitude for any observed sense; b) the simultaneous interaction of the factors Alloy x Thickness x Casting Technique confirmed the superiority of the L3 alloy, the thickness E3 and the F2 casting technique.
Resumo:
The authors studied 201 school children form both sexes, aging 12 to 14 years, in order to identify anodontia, including in third molars. The results indicated a congenital absence of teeth in 24.37% of the examined children, distributed into 10.44% of boys and 13.93% of girls. Anodontia was observed concerning third molar teeth and other teeth, and the correlation was calculated by the total, sex, and hemiarch. The data were presented and discussed, and the results included several conclusions.
Resumo:
In a sample of Brazilian white young adults between 18-23 years old, the A.A. studied the third molar roots, in anatomical aspects, using the orthopantomographic radiographic method. They concluded that the superior third molar shows a biggest number of fusionated roots (19.50% in the right side and 19.66% in the left side) and the inferior third molar shows a biggest number of separated roots (21.48% in the right side and 19.66% in the left side).
Resumo:
This paper reports the composition change of the dmf-teeth index, outcome from dental health program for the 3 to 6 year old pre-school children population, enrolled in kindergartens in Araraquara-SP, in 1988. The program performance promotes a major contribution of the f component to the dmf-teeth index.
Resumo:
The effects of ultrasound on the wound healing process after teeth extractions were studied histologically. The right upper incisor was extracted in 56 rats. They were divided into 2 groups, one control (I) and one experimental (II). Group II received ultrasound stimulation that was applied with the frequency of repetition of 1,000 Hz and pulse length of 2,000 us continuously, during five minutes daily since the extraction day until 24 hours before the death. The rats were sacrificed at 3, 6, 9, 12, 15, 18, and 21 postoperative days. The results showed a precocious granulation tissue formation, faster remodeling of osseous ridges, and consequently acceleration of the alveolar wound healing process.
Resumo:
We made some measurements from the region of the symphysis menti in 308 dried mandibles; 247 belong to the collection of the cranial museum of the discipline of Anatomy of the UNIFESP- Escola Paulista de Medicina- EPM and 61 belong to the didactic laboratory of the discipline of Anatomy from the Faculdade de Odontologia de Araraquara- UNESP, Brasil. On the dentate mandibles, the highest value founded was of 43,46 mm and the lowest of 22,67 mm. On the edentate mandibles, the highest value founded was of 37,24 mm and the lowest of 6,22mm. We hope that with the following discoveries we could contribute to a better knowledge of the symphysis menti region, not only to the professionals in Surgery and Implantology areas, but the industrials of related areas, to the confection of instruments used in these practices. © 2007 Sociedad Chilena de Anatom•br>.
Resumo:
Alginate or irreversible hydrocolloid is one the most accepted and frequently employed impression materials in dental practice. Substances like zinc, cadmium, lead silicate and fluorides, which are included in several alginate brands with the aim of improving their physical, chemical and mechanical properties, are a source of serious concern as regards their toxicity. Some brands of alginate have been reported to contain potentially toxic fluorides and metals such as cadmium, lead and zinc silicates, either singly or combined. Consequently, special care should be taken while preparing of these materials. It is necessary to monitor potentially toxic chemicals and metals in the alginates continually to avoid contamination of dental professionals and patients. In this review, alginates used in dentistry are analyzed for potential toxicity.
Resumo:
Objective: To assess the effect of bleaching agents on the microhardness of nanoparticle resin composite. Methods: Twenty-eight cylindrical test specimens (8× 1mm) of Filtek™ Supreme XT resin (3M/ESPE) were prepared and divided into 5 groups. The initial Vickers microhardness was measured (load of 50 grams force for 30 seconds) on the top surface of the test specimens. The groups were treated and divided as follows: G1 - artificial saliva (21 days - control); G2 - 7% hydrogen peroxide gel applied for 4h/day, for 14 days; G3 - 10% carbamide peroxide for 4h/day, for 14 days: G4 - 35% hydrogen peroxide gel applied in three sessions of 30 minutes each, with an interval of one week (21 days) between the sessions; G5 - 35% carbamide peroxide, three sessions of 30 minutes each, with an interval of one week (21 days) between the sessions. The top surfaces of the test specimens received treatment and were submitted to the Vickers microhardness test. Results: The results obtained were submitted to the Analysis of Variance at a fixed criterion, at a level of significance of p=0.05. No significant differences were observed among the treatments tested (p=0.42) when compared with G1. Significant differences (Tukey test) were found when the initial microhardness values were compared with the values after experimental treatments (p<0.01). Conclusion: The application of bleaching agents did not alter the microhardness of resin composites. Therefore, there is no need to change restorations after bleaching.
Resumo:
Objective: The aim of this study was to assess the bond strength of adhesive systems to dentin contaminated by temporary cements with or without eugenol. Method: Flat dentin surfaces were obtained from twenty-four human third molars. With exception of the control group (n=8), the surfaces were covered with Interim Restorative Material (Caulk Dentsplay, Milford, DE, USA) or Cavit (3M ESPE, St. Paul, MN, USA) and kept in an oven at 37°C for seven days. After removing the cements, the adhesive systems Adper Single Bond (3M ESPE, St. Paul, MN, USA) or Clearfil SE Bond (Kuraray Co. Ltd., Osaka, Japan) were applied in accordance with the manufacturers' recommendations, and then the crowns were constructed in of resin composite. The teeth were sectioned into specimens with a cross-sectional bond area of 0.81mm2, which were submitted to microtensile testing in a mechanical test machine at an actuator speed of 0.5mm/min. The data were analyzed by t- and ANOVA tests, complemented by Tukey tests (α=0.05). Results: For Adper Single Bond (3M ESPE, St. Paul, MN, USA), bond strength did not differ statistically (p>0.05) for all the experimental conditions. For Clearfil SE Bond (Kuraray Co. Ltd., Osaka, Japan), only the Interim Restorative Material (Caulk Dentsplay, Milford, DE, USA) Group showed significantly lower bond strength (30.1 ± 13.8 MPa) in comparison with the other groups; control (38.9 ± 13.5 MPa) and Cavit (3M ESPE, St. Paul, MN, USA) (42.1 ± 11.0 MPa), which showed no significant difference between them. Conclusion: It was concluded that the previous covering of dentin with temporary cement containing eugenol had a deleterious effect on the adhesive performance of the self-etching system only.
Resumo:
Objective: Understand the effect of chronic alcohol on the progression of periodontitis induced in Fischer-344 rats. Methods: For the study, 22 Fischer-344 rats, two months old were used, divided into groups: alcohol (n=8), ligature (n=7) and control (n=7). On the first day, the animals in the alcohol group were exposed to ingestion of a water solution containing 20% alcohol (size/size), up to day 90. After thirty days from the beginning of the experiment, the animals in the alcohol group and the ligature group were submitted to the placement of a silk thread around the right maxillary second molar. Nothing was performed on the left side, serving as control. All the groups were submitted to euthanasia 60 days after ligature placement. To assess the destruction of periodontitis, a radiographic exam was used to measure the destruction of bone height. Results: The results of the study showed that on the side in which periodontitis was induced, the group that ingested alcohol suffered an increase in destruction, with statistical differences when compared with the ligature and control groups and increased bone destruction in the ligature group when compared to control. Conclusion: Within the limitations of the study, it was concluded that chronic alcohol consumption by Fischer-344 rats led to greater progression of induced periodontitis.