477 resultados para decomposition of polymeric precursor method (DPP)
Resumo:
Intense and broad visible photoluminescent (PL) band in structurally disordered SrWO4 compounds was observed at room temperature. The polycrystalline scheelite strontium tungstate (SrWO4) samples prepared by the polymeric precursor method at different temperatures of annealing were structurally characterized by x-ray diffraction and Fourier transform Raman spectroscopy measurements. Quantum-mechanical calculations showed that the local disorder in the cluster of the network modifiers Sr has a very important role in the charge transfer. The experimental and theoretical results are in good agreement, indicating that the generation of the intense visible PL band can be related to short-range order-disorder degree in the scheelite structure. (c) 2006 American Institute of Physics.
Resumo:
Solid compounds of general formula ML(2) . nH(2)O [where M is Mg, Ca, Sr or Ba; L=4 methoxybenzylidenepyruvate (4-MeO-BP); n = 4, 1 or 0] have been synthetized. Thermogravimetry (TG), derivative thermogravimetry (DTG), differential scanning calorimetry (DSC), x-ray diffraction powder patterns and elemental analysis have been used to characterize the compounds. The thermal stability of these compounds as well as that of the decomposition products were studied using Pt or Al2O3 crucibles in an air or a CO2 atmosphere.
Resumo:
The dielectric properties and loss of Bi1.5ZnSb1.5O7 a poor-semiconducting ceramic were investigated by impedance spectroscopy, in the frequency range from 5 Hz to 13 MHz. Electric measurements were performed from 100 to 700 degreesC. Pyrochlore type phase was synthesized by the polymeric precursor method. Dense ceramic with 97% of the theoretical density was prepared by sintering via constant heating rate. The dielectric permittivity dependence as a function of frequency and temperature showed a strong dispersion at frequency lower than 10 kHz. The losses (tan delta) exhibit slight dependence with the frequency at low temperatures presenting a strong increase at temperatures higher than 400 degreesC. A decrease of the loss magnitude occurs with increasing frequency. Relaxation times were extracted using the dielectric functions Z(omega) and M(omega). The plots of the relaxation times tau(Z'), and tau(M) as a function of temperature follow the Arrhenius law, where a single slope is observed with activation energy values equal to 1.38 and 1.37 eV, respectively. (C) 2003 Elsevier Ltd. All rights reserved.
SrBi2Ta2O9 ferroelectric thick films prepared by electrophoretic deposition using aqueous suspension
Resumo:
SrBi2Ta2O9 ferroelectric thick films were prepared by electrophoretic deposition (EPD). For that, ceramic powders were prepared by chemical method in order to obtain compounds with chemical homogeneity. The polymeric precursor method was used for the synthesis of the SrBi2Ta2O9 powder. The crystallographic structure of the powder was examined by X-ray diffraction, and the surface area was determined by single point BET adsorption. The 0.03 vol.% suspension was formed by dispersing the powder in water using two different polymers as dispersants: an ester polyphosphate (C213) and an ammonium polyacrilate (Darvan 821-A). It was investigated the influence of the different dispersants in the surface properties of the powder by zeta potential measurements. The films were deposited on platinum-coated alumina and Pt/Ti/SiO2/Si substrates by a 4 mA constant current, for 10 min, using two parallel electrodes placed at a separation distance of 3 min in the suspension. Several cycles of deposition-drying of the deposit were carried out until reaching the desired thickness. After thermal treatment at temperatures ranging from 700 to 1000 degreesC, the films were characterized by X-ray diffraction and scanning electron microscopy for the microstructure observation. (C) 2003 Elsevier Ltd. All rights reserved.
High Curie point CaBi2Nb2O9 thin films: A potential candidate for lead-free thin-film piezoelectrics
Resumo:
CaBi2Nb2O9 (CBNO) thin films deposited on platinum coated silicon substrates by the polymeric precursor method exhibited good structural, dielectric, and piezoelectric characteristics. Capacitance-voltage measurements indicated good ferroelectric polarization switching characteristics. Remanent polarization and drive voltage values were 4.2 mu C/cm(2) and 1.7 V for a maximum applied voltage of 10 V. The film has a piezoelectric coefficient d(33) equal to 60 pm/V, current density of 0.7 mu A/cm(2), and Curie temperature of 940 degrees C. The polar-axis-oriented CBNO is a promising candidate for use in lead-free high Curie point in ferroelectric and piezoelectric devices. (c) 2006 American Institute of Physics.
Resumo:
Pure and W-doped PZT ceramics (PZT and PZTW) were prepared by a hybrid process consisting in the association of polymeric precursor and partial oxalate methods. The phase formation was investigated by simultaneous thermal analysis (TG/DSC) and X-ray diffraction (XRD). The effect of W doping PZT and their electrical properties was evaluated. Substitution of W by Ti leads to an increase of Curie temperature and broadening of dielectric constant. A typical hysteresis loop was observed at room temperature and the remnant polarization was increased with the content of W. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
The gap between the bulk materials and thin films can be filled with thick films suitably designed and appropriate processed. Thick films of complex system like lead-lanthanum-zirconium titanate (PLZT) is difficult to produce by simple solid-state reaction keeping compositional homogeneity and optimal grain size distribution. In the present work, PLZT thick films were fabricated by screen-printing technique from nanosized powders obtained through soft chemistry by polymeric precursor method. Thick film paste was obtained by mixing PLZT fine powders and organic vehicle. The upper and bottom electrodes based on Ag-Pd and functional component based on PLZT were screen-printed on alumina substrate and after that annealed in air atmosphere. The powder morphology, microstructure, dielectric and ferroelectric properties of 9.5/65/35 PLZT thick films were analysed. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Ca0.95Sm0.05TiO3 (CT:Sm) powder was prepared by the polymeric precursor method (PPM). Order-disorder at short and long range has been investigated by means of Raman spectroscopy, X-ray diffraction (XRD), and photoluminescence emission (PL) experimental techniques. The broad PL band and the Sm emission spectrum measured at room temperature indicate the increase of structural order with annealing temperature. The measured PL emission reveals that the PL intensity changes with the degree of disorder in the CT: Sm. The electronic structures were performed by the ab initio periodic method in the DFT level with the hybrid nonlocal B3LYP approximation. Theoretical results are analyzed in terms of DOS, charge densities, and Mulliken charges. Localized levels into the band gap of the CT: Sm material favor the creation of the electron-hole pair, supporting the observed room-temperature PL phenomenon.
Resumo:
Bi1.5ZnSb1.5O7 dielectric ceramic with pyrochlore structure was investigated by impedance spectroscopy from 400 to 750 degreesC. Pyrochlore was synthesized by the polymeric precursor method, a chemical synthesis route derived from Pechini's method. The grain or bulk resistance exhibits a sensor temperature characteristic, being a thermistor with a negative temperature coefficient (NTC). Only a single region was identified on the resistance curve investigated. The NTC thermistor characteristic parameter (beta) is equal to 7140 degreesC, in the temperature range investigated. The temperature coefficient of the resistance (alpha) was derived, being equal to -4.46x10(-2) degreesC(-1) at 400 degreesC. The conduction mechanism and relaxation are discussed. (C) 2003 American Institute of Physics.
Resumo:
We have studied the phase transition behavior of Pb0.76Ca0.24TiO3 thin films using Raman scattering and dielectric measurement techniques. We also have studied the leakage current conduction mechanism as a function of temperature for these thin films on platinized silicon substrates. A Pb0.76Ca0.24TiO3 thin film was prepared using a soft chemical process, called the polymeric precursor method. The results showed that the dependence of the dielectric constant upon the frequency does not reveal any relaxor behavior. However, a diffuse character-type phase transition was observed upon transformation from a cubic paraelectric phase to a tetragonal ferroelectric phase. The temperature dependency of Raman scattering spectra was investigated through the ferroelectric phase transition. The soft mode showed a marked dependence on temperature and its disappearance at about 598 K. on the other hand, Raman modes persist above the tetragonal to cubic phase transition temperature, although all optical modes should be Raman inactive above the phase transition temperature. The origin of these modes must be interpreted in terms of a local breakdown of cubic symmetry by some kind of disorder. The lack of a well-defined transition temperature suggested a diffuse-type phase transition. This result corroborate the dielectric constant versus temperature data, which showed a broad ferroelectric phase transition in the thin film. The leakage current density of the PCT24 thin film was studied at elevated temperatures, and the data were well fitted by the Schottky emission model. The Schottky barrier height of the PCT24 thin film was estimated to be 1.49 eV. (C) 2003 American Institute of Physics.
Resumo:
Photoluminescence (PL) at room temperature has been achieved in amorphous thin films and powders of the TiO2-PbO system. They were prepared by the polymeric precursor method with [PbO]/[TiO2] molar ratios ranging from 0.0 to 1.0. The energy position of maximum PL emission and the PL intensity showed dependence on Pb concentration. The Pb addition suggests an increase in the number of nonbridging oxygens (NBO) in the amorphous TiO2 network. These results support the relationship between photoluminescence and structure in TiO2-based amorphous materials.