Introduction: Photodynamic antimicrobial chemotherapy studies regarding dental caries have been present more frequently in the literature. However, photodynamic antimicrobial chemotherapy depends on the adjustment of variables such as the type of light source and, photosensitisers target microorganism; this makes it difficult to draw meaningful comparisons. The purpose of this paper was to provide a critical review related to this coadjuvant approach in the prevention and treatment of dental caries. Materials and Methods: A database search was made via Medline/PubMed (keywords: photodynamic therapy and dental caries) and 33 articles were found. Results: Twelve articles were included after using the filter tool, being excluded reviews and manuscripts reporting works not related to the studied area. Conclusion: The manuscripts showed that photodynamic therapy presents optimal results against dental caries, even though better understanding of photodynamic antimicrobial chemotherapy and its components are necessary before the clinical application of this alternative modality in the dental practice.
Resumo:
To evaluate the short-term response of human pulps to ethanol-wet bonding technique. Methods Deep class V cavities were prepared on 17 sound premolars and divided into three groups. After acid-etching, the cavities from groups 1 (G1) and 2 (G2) were filled with 100% ethanol or distilled water, respectively, for 60 s before the application of Single Bond 2. In group 3 (G3, control), the cavity floor was lined with calcium hydroxide before etching and bonding. All cavities were restored with resin composite. Two teeth were used as intact control. The teeth were extracted 48 h after the clinical procedures. From each tooth serial sections were obtained and stained with haematoxylin and eosin (H/E) and Masson's trichrome. Bacteria microleakage was assessed using Brown & Brenn. All sections were blindly evaluated for five histological features. Results Mean remaining dentine thickness was 463 ± 65 μm (G1); 425 ± 184 μm (G2); and 348 ± 194 μm (G3). Similar pulp reactions followed ethanol- or water-wet bonding techniques. Slight inflammatory responses and disruption of the odontoblast layer related to the cavity floor were seen in all groups. Stained bacteria were not detected in any cavities. Normal pulp tissue was observed in G3 except for one case. Conclusions After 48 h, ethanol-wet bonding does not increase pulpal damage compared to water-wet bonding technique. Clinical significance Ethanol-wet bonding may increase resin-dentine bond durability. This study reported the in vivo response of human pulp tissue when 100% ethanol was applied previously to an etch-and-rinse simplified adhesive system.
Resumo:
This study evaluated in vitro the shear bond strength of brackets bonded with xenon plasma arc light, light-emitting diode (LED) and conventional halogen light using different curing times. Brackets were bonded to the buccal surface of 60 human maxillary premolars allocated to five groups. In groups 1 and 2, the resin was cured with the plasma arc for three and six seconds (s), respectively; in groups 3 and 4, the LED was used for five and ten s, respectively; and in group 5, the halogen light was used for 40 s. The specimens were stored in water for 24 hours and subjected to a shear force until bracket failure. The debonding pattern was classified according to the adhesive remnant index (ARI). The results were assessed by Anova and the SNK post-hoc test. No differences were detected among groups 2, 4 and 5, which showed higher averages than groups 1 and 3, which were not different between themselves. The ARI scores showed no differences among the three types of light sources in all times tested. Plasma arc and LED lights can be used with shorter curing times, within certain limits, than conventional halogen light for bonding orthodontic brackets, without decreasing bond strength.
Resumo:
The aim of this study was to evaluate and compare the roughness and superficial morphology of enamel and a composite restorative resin after different bleaching techniques application. Material and Methods: Bovine incisors were selected and standardized cavities were prepared on the buccal surface, which were restored with composite resin. The teeth were distributed according to the following treatments: G1- bleaching with 10% carbamide peroxide (CP); G2 - bleaching with 38% hydrogen peroxide (HP); and G3 - bleaching with 38% of HP associated to light irradiation. For G1, the bleaching gel was applied for 8 hours daily during 21 days. For G2 and G3, 3 sessions were performed, consisting of 3 applications of 15 minutes each, with 7 days of intervals between the sessions. For G3, the LED (470nm) light was used to activate the bleaching agent for 6 minutes. The surface of enamel and composite resin were evaluated before and after the bleaching procedures using a roughness tester and an atomic force microscope. Results: The results showed significant differences in surface roughness of enamel after bleaching only for G1 (Wilcoxon, p<0.05). For composite resin, neither group showed a statistical difference compared to control (Mann-Whitney, p>0.05). Conclusion: It was concluded that the increase in the roughness of enamel occurred only after bleaching therapy using a gel with 10% of CP. The bleaching procedures evaluated in this investigation did not increase the roughness or cause changes in the superficial morphology of the composite resin.
Resumo:
This study assessed the surface microhardness of compound resins cured by different light sources. Methods Three micro hybrid (Vit-l-escence, Amelogen Plus, Opallis) and one nanoparticle (Filtek Z350, 3M ESPETM Dental Products, St. Paul, USA) compound resins were selected. The resins were polymerized by a halogen light unit (Ultralux, Dabi Atlante, Ribeirão Preto, Brasil) with two tips, one semi-guided made of glass and another of painted acrylic and a LED-based source (UltraLume 2, Ultradent®, South Jordan, USA). Specimens constructed from a circular aluminum matrix were photopolymerized for 40 second after they received the compound resin and stored dry for 24 hours. After this period, a Vickers surface microhardness assay was performed, measuring the top (hardness 1) and base (hardness 2) surfaces four times each. Variance analyses were complemented by Newman-Keuls method, with significance set at 5%. Results The Opallis (FGM, Santa Catarina, Brasil) resin subjected to UltraLume 2 (Ultradent®, South Jordan, USA) obtained the lowest mean hardness values for the top surface. The Vit-l-escence (Ultradent®, South Jordan, USA) compound cured by Led UltraLume 2 (Ultradent®, South Jordan, USA) and by Ultralux PCP (Dabi Atlante, Ribeirão Preto, Brasil) halogen light obtained the highest mean hardness, followed by the Filtek Z350 (3M ESPETM Dental Products, St. Paul, USA) resin subjected to UltraLume 2 (Ultradent® South Jordan, USA). The Opallis (FGM, Santa Catarina, Brasil) resin cured by LED UltraLume 2 (Ultradent®, South Jordan, USA) also obtained the lowest mean hardness for the base surface and the Vit-L-Escence (Ultradent®, South Jordan, USA) resin obtained the highest value, followed by Amelogen Plus, when cured by Ultralux (Dabi Atlante, Ribeirão Preto, Brasil) using the semi-guided tip. Conclusion The polymerization and, consequently, the microhardness achieved by the LED unit was equivalent to those achieved by conventional halogen units for three of the four composites tested.
Resumo:
The purpose of this study was to use a fluorescent dye and CLSM microscope to observe the effect of different light intensities on dentin tensile bond strength. Flat dentin surfaces were created on 16 intact human third molars and divided in 4 groups: Group G1 - halogen - KM -200R®; Group G2 - LED - Ultraled®; Group G3 - LED - UltraLume LED5® and Group G4 - LED - Biolux Single V®. For all the groups, the restoration procedure used Single Bond® adhesive, mixed with rodamin B and InTen-S® composite resin. Then, they were cut on serial sections to obtain 1 mm2 area and submitted to micro tensile test and after words, the fractures were analyzed with a digital microscope and CLSM. The statistical analysis showed that all in all groups, except Group G2, which had a significant smaller tensile bond strength ratio. The fracture mode analysis showed that there were significant differences when comparing groups G1 / G2, and G2 / G4. There is no evidence of relevant differences among the other groups. With these results, we conclude that the use of fluorescent dye and CLSM demonstrated to be a simple and nondestructive technique, and that there are evidences that light intensities influenced the dentine tensile.
Resumo:
Ideally projected to be applied on soft tissues, infrared lasers were improved by restorative dentistry to be used in hard dental tissues cavity preparations-namely enamel and dentin. This paper evidentiates the relevant aspects of infrared Erbium laser's action mechanism and its effects, and characterizes the different effects deriving from the laser's beams emission. The criteria for use and selection of optimal parameters for the correct application of laser systems and infuence of supporting factors on the process, such as water amount and its presence in the ablation process, protection exerted by the plasma shielding and structural factors, which are indispensable in dental tissues cavity preparation related to restorative technique, are subordinated to optical modifcations caused by the interaction of the energy dissipated by these laser light emission systems in the targeted tissue substrate. Clinical relevance: Differences in the action of infrared Erbium laser system in regard to the nature of the ablation process and variations on the morphological aspects observed in the super-fcial structure of the target tissue irradiated, may be correlated to the structural optical modifcations of the substrate produced by an interaction of the energy propagated by laser systems.
Resumo:
This study sought to assess the use of chlorhexidine with several excipients as a dentin surface treatment and its effect on marginal adaptation of class V restorations with current-generation dentin bonding agents. A total of 120 human third molars were selected and allocated into 12 groups, with standardized buccal class V restorations randomly divided into preconditioned dentin rinsed with: water; water + chlorhexidine; ethanol; or ethanol + chlorhexidine. After rinsing of dentin (previously conditioned with 35% phosphoric acid) with the test solutions, the Adper single bond 2, prime and bond 2.1, and Excite bonding systems were applied randomly. Restorations were performed with FiltekTM Z350 XT composite resin. The resulting specimens were subjected to thermal and mechanical load cycling. Quantitative analysis of marginal adaptation was performed on epoxy replicas by means of scanning electron microscopy. Results were assessed by means of the Kruskal-Wallis test (percentages of continuous margins) and Wilcoxon test (differences between percentages of continuous margins before and after thermal cycling and mechanical loading), at a significance level of p < 0.05. Outcomes in the chlorhexidine-treated groups were not superior to those obtained with other treatments.
Resumo:
The study evaluated the influence of light curing units and immersion media on superficial roughness and microhardness of the nanofilled composite resin Supreme XT (3M/ESPE). Light curing units used were: XL 3000 (3M/ESPE), Jet Lite 4000 Plus (JMorita) and Ultralume Led 5 (Ultradent) and immersion media were artificial saliva, Coke®, tea and coffee, totaling 12 experimental groups. Specimens (10mm x 2mm) were immersed in each respective solution for 5 seconds, three times a day, during 60 days and so, were submitted to measure of superficial roughness (Ra) and Vickers hardness. Data were subjected to two-way ANOVA test (p<0.05). Results showed that only the light source factor showed statistically difference for hardness. It was observed that the hardness of the composite resin Filtek Supreme XT (3M/ESPE) was influenced by the light source (p<0.01) independently of the immersion media (p= 0.35) and the Jet Lite 4000 Plus (JMorita) was the light curing unit that presented lower values. In relation to surface roughness, it was noted no-significant statistical difference for light source (p=0.84), when specimens were immersed in different beverages (p=0.35).
Resumo:
Composite resin is a dental material susceptible to color change over time which limits the longevity of restorations made with this material. The influence of light curing units and different fluoride mouthrinses on superficial morphology and color stability of a nanofilled composite resin was evaluated. Specimens (N = 150) were prepared and polished. The experimental groups were divided according to the type of light source (halogen and LED) and immersion media (artificial saliva, 0.05% sodium fluoride solution-manipulated, Fluordent Reach, Oral B, Fluorgard). Specimens remained in artificial saliva for 24-h baseline. For 60 days, they were immersed in solutions for 1 min. Color readout was taken at baseline and after 60 days of immersion. Surface morphology was analyzed by Scanning Electron Microscopy (SEM) after 60 days of immersion. Color change data were submitted to two-way Analysis of Variance and Tukey tests (α = 0.05). Surface morphology was qualitatively analyzed. The factor light source presented no significant variability (P = 0.281), the immersion media, significant variability (P < 0.001) and interaction between factors, no significant variability (P = 0.050). According to SEM observations, no difference was noted in the surface of the specimens polymerized by different light sources, irrespective of the immersion medium. It was concluded that the light source did not influence the color stability of composite, irrespective of the immersion media, and among the fluoride solutions analyzed, Fluorgard was the one that promoted the greatest color change, however, this was not clinically perceptible. The immersion media did not influence the morphology of the studied resin. Microsc. Res. Tech. 77:941–946, 2014. © 2014 Wiley Periodicals, Inc.
Resumo:
The aim of the present paper was to determine the effect of different types of ionizing radiation on the bond strength of three different dentin adhesive systems. Materials and Methods: One hundred twenty specimens of 60 human teeth (protocol number: 032/2007) sectioned mesiodistally were divided into 3 groups according to the adhesives systems used: SB (Adper Single Bond Plus), CB (Clearfil SE Bond) and AP (Adper Prompt Self-Etch). The adhesives were applied on dentin and photo-activated using LED (Lec 1000, MMoptics, 1000 mW/cm2). Customized elastomer molds (0.5 mm thickness) with three orifices of 1.2 mm diameter were placed onto the bonding areas and filled with composite resin (Filtek Z-250), which was photoactivated for 20 s. Each group was subdivided into 4 subgroups for application of the different types of ionizing radiation: ultraviolet radiation (UV), diagnostic x-ray radiation (DX), therapeutic x-ray radiation (TX) and without irradiation (control group, CG). Microshear tests were carried out (Instron, model 4411), and afterwards the modes of failure were evaluated by optical and scanning electron microscope and classified using 5 scores: adhesive failure, mixed failures with 3 significance levels, and cohesive failure. The results of the shear bond strength test were submitted to ANOVA with Tukey's test and Dunnett's test, and the data from the failure pattern evaluation were analyzed with the Mann Whitney test (p = 0.05). Results: No change in bond strength of CB and AP was observed after application of the different radiation types, only SB showed increase in bond strength after UV (p = 0.0267) irradiation. The UV also changed the failure patterns of SB (p = 0.0001). Conclusion: The radio-induced changes did not cause degradation of the restorations, which means that they can be exposed to these types of ionizing radiation without weakening the bond strength.