456 resultados para dental ceramics


Relevância:

60.00% 60.00%

Publicador:

Resumo:

Objectives: Based on a maxillary premolar restored with laminate veneer and using the 3-D finite element analysis (FEA) and mCT data, the aim of this study was to evaluate the influence of different types of buccal cusp reduction on the stress distribution in the porcelain laminate veneer and in the resin luting cement layer. Methods: Two 3-D FEA models (M) of a maxillary premolar were built from mCT data. The buccal cusp reduction followed two configurations: Mt-buccal cusp completely covered by porcelain laminate veneer; and Mp-buccal cusp partially covered by porcelain laminate veneer. The loading (150 N in 458) was performed on the top of the buccal cusp. The finite element software (Ansys Workbench 10.0) was used to obtain the maximum shear stress (σmax) and maximum principal stress (σmax). Results: The Mp showed reduced the stress (σmax) in porcelain laminate veneer (from-2.3 to 24.5 MPa) in comparison with Mt (from-5.3 to 27.4 MPa). The difference between the peak and lower stress values of σmax in Mp (-6.8 to 26.7 MPa) and Mt (-5.3 to 27.4 MPa) was similar for the resin luting cement layer. The structures not exceeded the ultimate tensile strength or the shear bond strength. Conclusions: Cusp reduction did not affect significant increase in σmax and τmax. The Mt showed better stress distribution (τmax) than Mp. © 2011 Published by Elsevier Ireland on behalf of Japan Prosthodontic Society.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

It is known that several factors can affect the clinical success and durability of fixed partial dentures. Therefore, the aim of the present study was to present a literature review about the longevity, clinical success, and quality, as well as, patients' and dental surgeons' satisfaction of ceramic fixed dentures. High rate of patients' satisfaction has been observed in relation to the esthetic of ceramic crowns. In addition, the literature has shown that dental ceramics can be used in several clinical situations with high success rate and longevity. Despite of failures and complications of ceramic restorations, nowadays, with the improvement of mechanical properties of such materials, ceramic crowns present a favorable prognosis and can be used in several clinical situations with high success rate, clinical quality, and great patients' satisfaction. © 2013 The American Ceramic Society.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This study evaluated the effect of different air-particle abrasion protocols on the biaxial flexural strength and structural stability of zirconia ceramics. Zirconia ceramic specimens (ISO 6872) (Lava, 3M ESPE) were obtained (N=336). The specimens (N=118, n=20 per group) were randomly assigned to one of the air-abrasion protocols: Gr1: Control (as-sintered); Gr2: 50 μm Al2O3 (2.5 bar); Gr3: 50 μm Al2O3 (3.5 bar); Gr4: 110 μm Al2O3(2.5 bar); Gr5: 110 μm Al2O3 (3.5 bar); Gr6: 30 μm SiO2 (2.5 bar) (CoJet); Gr7: 30 μm SiO2(3.5 bar); Gr8: 110 μm SiO2 (2.5 bar) (Rocatec Plus); and Gr9: 110 μm SiO2 (3.5 bar) (duration: 20 s, distance: 10 mm). While half of the specimens were tested immediately, the other half was subjected to cyclic loading in water (100,000 cycles; 50 N, 4 Hz, 37 °°C) prior to biaxial flexural strength test (ISO 6872). Phase transformation (t→m), relative amount of transformed monoclinic zirconia (FM), transformed zone depth (TZD) and surface roughness were measured. Particle type (p=0.2746), pressure (p=0.5084) and cyclic loading (p=0.1610) did not influence the flexural strength. Except for the air-abraded group with 110 μm Al2O3 at 3.5 bar, all air-abrasion protocols increased the biaxial flexural strength (MPa) (Controlnon-aged: 1030±153, Controlaged: 1138±138; Experimentalnon-aged: 1307±184-1554±124; Experimentalaged: 1308±118-1451±135) in both non-aged and aged conditions, respectively. Surface roughness (Ra) was the highest with 110 μm Al2O3(0.84 μm. FM values ranged from 0% to 27.21%, higher value for the Rocatec Plus (110 μm SiO2) and 110 μm Al2O3 groups at 3.5 bar pressure. TZD ranged between 0 and 1.43 μm, with the highest values for Rocatec Plus and 110 μm Al2O3 groups at 3.5 bar pressure. © 2013 Elsevier Ltd.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pós-graduação em Odontologia Restauradora - ICT

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pós-graduação em Odontologia Restauradora - ICT

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pós-graduação em Odontologia Restauradora - ICT

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The continuing advances in technology, dental materials and equipment have contributed significantly to improve the level of esthetic dentistry today. Among these innovations, development of pure ceramic restorations has evolved to give different alternatives. Dental ceramics have presented a rapidly technological changing to improve mechanical and optical properties. Currently there are several systems of metal free ceramics with excellent mechanical and optical properties, for making crowns and plurals. These modern systems are presented with various compositions and different preparation techniques, making these more versatile. Within this perspective, the dental market offers a huge range of new indirect and metal-free materials for prostheses, providing new options, plus also new questions to decide among the available alternatives. The aim of this review is take a view of the different ceramic systems in terms of its composition and different techniques of production.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Society's change of parameters for health and aesthetics has resulted in an increased demand for dental treatments. Nowadays, ceramics systems have shown a substantial development, becoming more reliable and predictable. Dental ceramics, besides being chemically stable, present excellent optical properties when compared to dental structures, thus assuring a special position in the list of aesthetic restorative materials. OBJECTIVE, CASE REPORT AND CONCLUSION: This article describes a successful clinical procedure involving the anterior teeth aesthetics, which were restored with all-ceramic crowns (IPS e.max® Ivoclar Vivadent).