Resumo:

LiNbO3 thin films were grown on (0001) sapphire substrates by a chemical route, using the polymeric precursor method. The overall process consists of preparing a coating solution from the Pechini process, based on metallic citrate polymerization, the precursor films, deposited by dip coating, are then heat treated to eliminate the organic material and to synthesize the phase. In this work, we studied the influence of the heat treatment on the structural and optical properties of single-layered films. Two routes were also investigated to increase the film thickness: increasing the viscosity of the coating solution and/or increasing the number of successively deposited layers. The x-ray diffraction theta -2 theta scans revealed the c-axis orientation of the single- and multilayered films and showed that efficient crystallization can be obtained at temperatures as low as 400 degreesC, the phi-scan diffraction evidenced the epitaxial growth with two in-plane variants, A microstructural study revealed that the films were crack free, homogeneous, and relatively dense. Finally, the investigation of the optical properties (optical transmittance and refractive index) confirmed the good quality of the films. These results indicate that the polymeric precursor method is a promising process to develop lithium niobate waveguides.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The electrical properties of the grain boundary region of electroceramic sensor temperature based on inverse spinel Zn7Sb2O12 were investigated at high temperature. The zinc antimoniate was synthesized by a chemical route based on the modified Pechini method. The electric properties of Zn7Sb2O12 were investigated by impedance spectroscopy in the frequency range from 5 Hz to 13 MHz and from 250 up to 600 degreesC. The grain boundary conductivity follows the Arrhenius law, with two linear branches of different slopes. These branches exhibit activation energies with very similar values; the low-temperature (less than or equal to350 degreesC) and high-temperature (greater than or equal to400 degreesC) regions are equal to 1.15 and 1.16 eV, respectively. Dissimilar behavior is observed on the relaxation time (tau) curve as a function of temperature, where a single slope is identified. The negative temperature coefficient parameters and nature of the polarization phenomenon of the grain boundary are discussed. (C) 2003 American Institute of Physics.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The present work presents results on natural sintering of tin dioxide ceramics, prepared by a chemical route or by conventional mixing and containing manganese (X-Mn = Mn/(Mn + Sn)(atomic) with 0 less than or equal to X(Mn)less than or equal to 0.15). This cation, which is practically insoluble in SnO2 network, stays at the grain surface. During thermal treatment (500 degrees C less than or equal to T-s less than or equal to 1400 degrees C), as long as the manganese surface concentration is lower than a critical value, equal to 5.10(-6) mol m(-2), no densification takes place. As soon as this value is reached, densification and grain growth occur simultaneously. The shrinkage kinetics is fast and high rho/rho(t) values can be obtained (for example. rho/rho(t)=0.95 for T-s=1300 degrees C and X-Mn=0.004). The dependence between manganese content, manganese distribution, grain size and sintering behaviour is also discussed. (C) 1998 Published by Elsevier B.V. Limited.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Zinc oxide (ZnO) is an electroluminescent (EL) material that can emit light in different regions of electromagnetic spectrum when electrically excited. Since ZnO is chemically stable, inexpensive and environmentally friendly material, its EL property can be useful to construct solid-state lamps for illumination or as UV emitter. We present here two wet chemical methods to prepare ZnO thin-films: the Pechini method and the sol-gel method, with both methods resulting in crystalline and transparent films with transmittance > 85% at 550 nm. These films were used to make thin-film electroluminescent devices (TFELD) using two different insulator layers: lithium fluoride (LiF) or silica (SiO2). All the devices exhibit at least two wide emission bands in the visible range centered at 420 nm and at 380 nm attributed to the electronic defects in the ZnO optical band gap. Besides these two bands, the device using SiO2 and ZnO film obtained via sol-gel exhibits an additional band in the UV range centered at 350 nm which can be attributed to excitonic emission. These emission bands of ZnO can transfer their energy when a proper dopant is present. For the devices produced the voltage-current characteristics were measured in a specific range of applied voltage. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The electric and dielectric properties of the grain boundary of Na0.85Li0.15NbO3 lead-free ferroelectric-semiconductor perovskite were investigated. The impedance spectroscopy was carried out as a function of a thermal cycle. The sodium lithium niobate was synthesized by a chemical route based on the evaporation method. Dense ceramic, relative density of 97%, was prepared at 1423 K for 2 h in air atmosphere. ac measurements were carried out in the frequency range of 5 Hz-13 MHz and from 673 to 1023 K. Theoretical adjust of the impedance data was performed to deriving the electric parameters of the grain boundary. The electric conductivity follows the Arrhenius law, with activation energy values equal to 1.55 and 1.54 eV for heating and cooling cycle, respectively. The nonferroelectric state of the grain boundary and its correlation with symmetry are discussed in the temperature domain. (C) 2003 American Institute of Physics.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Antimony doped tin oxide thin films were deposited on glass by a chemical route derived from Pechini method. Particular emphasis was given to the microstructure of crystallized films. Crystalline phase formation was studied by grazing incident X-ray diffraction and by thermal analyses. Scanning electron microscopy was carried out for microstructure characterization, surface roughness was observed using scanning tunneling microscope and the optical transmittance measurements were performed in the wavelength range of 200-800 nm. (C) 2002 Kluwer Academic Publishers.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Polycrystalline Co7Sb2O12 compounds have been synthesized by a chemical route, which is based on a modified polymeric precursor method. In order to study the physical properties of the samples, X-ray diffraction (XRD), thermal analyses (TG and DSC), infrared spectroscopy (IR), specific surface area (BET), and magnetization measurements were performed on these materials. Characterization through XRD revealed that the samples are single-phase after a heat-treatment at 1100degreesC for 2h, while the X-ray patterns of the samples heat-treated at lower temperatures revealed the presence of additional Bragg reflections belonging to the Co6Sb2O6 phase. These data were analyzed by means of Rietveld refinement and further analyze showed that Co7Sb2O12 displays an inverse spinel crystalline structure. In this structure, the Co2+ ions occupy the eight tetrahedral positions, and the sixteen octahedral positions are randomly occupied by the Sb5+ and Co2+ ions. IR studies disclosed two strong absorption bands, v(1) and v(2), in the expected spectral range for a spinel-type binary oxide with space group Fd3m. Exploratory studies concerning the magnetic properties indicated that this sample presents a spin-glass transition at T-f similar to 64 K. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Glass ionomer cements (GICs) are largely employed in Dentistry for several applications, such as luting cements for the attachment of crowns, bridges, and orthodontic brackets as well as restorative materials. The development of new glass systems is very important in Dentistry to improve of the mechanical properties and chemical stability. The aim of this study is the preparation of two glass systems containing niobium in their compositions for use as GICs. Glass systems based on the composition SiO2,Al2O3-Nb2O5-CaO were prepared by chemical route at 700degreesC. The XRD and DTA results confirmed that the prepared materials are glasses. The structures of the obtained glasses were compared to commercial material using FTIR, Al-27 and Si-29 MAS-NMR. The analysis of FTIR and MAS-NMR spectra indicated that the systems developed and commercial material are formed by SiO4 and AlO4 linked tetrahedra. These structures are essential to get the set time control and to have cements. These results encourage further applications of the experimental glasses in the formation of GICs. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The crystal structure of the Aurivillius compound Bi2BaTa2O9 prepared via the chemical route was determined by direct methods using EXPO97, and refined using the Rietveld method with conventional X-ray diffraction data. The structure was found to be tetragonal (space group I4/mmm, number 139) and Z = 2, isomorphic of the Bi2BaNb2O9 reported by Blake and co-workers in the literature (1997). Two refinements were performed using the two asymmetry functions of DBWS-9807 (release 20/May/99). The unit cell for each case are: a = 3.932 22(6) Å, c = 25.5053(6) Å (RA) and a = 3.93250(7) Å, c = 25.5069(6) Å (RCF). The differences for atom positions, interatomic distances and angles are in the range of one standard deviation. Final agreements factors are: Rwp = 7.97%, S = 1.84, RBragg = 4.28%(RA), Rwp = 7.98%, S = 1.84, RBragg = 4.30% (RCF). The occupancies of Ba and Bi in site 2b were refined but constrained to have their summation equal to 1.00. The same constraints were applied to the Ba and Bi of the 4e site. The results show that on site 2b there are 70% of Ba and 30% of Bi and on the site 4e there are 82% of Bi and 18% of Ba. The charge equilibrium is maintained for one standard deviation of the site occupancies. © 2000 International Centre for Diffraction Data.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pós-graduação em Ciências Farmacêuticas - FCFAR

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)